Petroquimica Triunfo Trilene Ts 8056 Lldpe C8 And Ldpe Blend

Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend

    • Product Name: Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 738193
    Polymer Type LLDPE-C8 and LDPE blend
    Comonomer Octene (C8)
    Density 0.921 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 0.80 g/10 min
    Melt Flow Ratio I21 I2 28
    Melting Point 124 °C
    Vicat Softening Point 102 °C
    Tensile Strength At Yield Md 11 MPa
    Tensile Strength At Break Md 30 MPa
    Elongation At Break Md 700 %
    1 Secant Modulus Md 220 MPa
    Dart Drop Impact 250 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 12 %
    Gloss 45 60
    Coefficient Of Friction 0.20

    As an accredited Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Petroquimica Triunfo Trilene® TS 8056 supplied in 25 kg polyethylene bags, 40 bags per stretch-wrapped pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL container: Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8/LDPE Blend in 25 kg bags, palletized, shrink-wrapped, securely stowed.
    Shipping Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend is a non-hazardous polyethylene resin supplied as solid pellets. It ships in 25 kg bags, palletized and shrink-wrapped, or in bulk bags/containers. Not regulated for transport. Keep dry, clean, and away from heat, moisture, and UV during truck or container shipping.
    Storage Store Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend indoors in a cool, dry, well-ventilated area, away from sunlight, heat, sparks, and flames. Keep original packaging closed, elevated on pallets, and protected from moisture, dust, and contamination. Avoid strong oxidizers. Maintain clean, static-controlled conditions; do not store near food, feed, or incompatible materials. Follow SDS and local regulations.
    Shelf Life Typically 12 months in original packaging, stored cool, dry, away from direct sunlight; may remain stable longer under ideal conditions.
    Application of Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend

    In blown-film lines producing silage wrap and greenhouse covers, the blend is commonly measured at 0.55 g/10 min per ISO 1133-1:2022 and 0.921 g/cm³ per ASTM D1505-18. When Trilene TS 8056 is used at 75–85 wt% with 15–25 wt% LDPE-rich reclaim, bubble symmetry is maintained on 55 mm grooved-feed extruders with L/D 30:1 only if the die gap is held at 2.0–2.4 mm, the melt temperature remains in the 190–205°C band, and the frost-line height is kept between 7 and 9 die diameters. Process deviations recorded on 3-layer agricultural film lines show that raising the TS 8056 addition above 85 wt% reduces dart impact resistance per ASTM D1709-16a from 600–700 g to 450–520 g at 120 µm, a cliff-edge that defines the upper formulation boundary for silage wrap. The production equipment comprises 45/55/45 mm coextrusion screws, a 300 mm spiral mandrel die, internal bubble cooling at 18°C, and a blow-up ratio of 2.5:1 with output in the 120–150 kg/h range. Compliance is assessed under EN 13206:2017 for agricultural films, ISO 527-3:2018 for tensile properties, ASTM D882-18 for thin-film tensile, and ASTM D3985-17 for oxygen transmission where silage barrier is required. Terminal product types include 25 µm silage stretch wrap, 50 µm mulch film, 150 µm greenhouse cover, and 200 µm pit silage cover.

    Blown-film property gradient at 120 µm as function of Trilene TS 8056 addition
    TS 8056 addition wt%Dart impact ASTM D1709-16a Method BMD tear ASTM D1922-15Observed processing condition
    70580–640 g135–160 N/mmStable bubble at 2.5:1 blow-up ratio
    80540–600 g125–145 N/mmAcceptable at frost-line 8 die diameters
    85450–520 g115–130 N/mmBubble flutter at 2.7:1; reduce internal cooling
    90380–440 g100–120 N/mmEdge instability; not recommended for silage wrap

    Why Does Cast Stretch Film Retain 85% Pre-Stretch at 23°C When the LLDPE-C8 Fraction Exceeds 80 wt%?

    Cast stretch film converting data show a draw-resonance threshold at 850 m/min when the TS 8056 addition is pushed above 80 wt% in the core layer on a 100 mm barrier screw with L/D 32:1 and a 0.8 mm coat-hanger die. The octene-comonomer branches reduce machine-direction orientation, which lowers F10 protrusion puncture force per ASTM D5748-19 at 23°C from 34 N to 29 N when the core layer exceeds 80 wt% and the chill-roll temperature is below 18°C. Production-scale addition is therefore set at 70–80 wt% Trilene TS 8056, 10–20 wt% LDPE-rich reclaim, and 5–10 wt% polyisobutylene tackifier masterbatch; this composition maintains pre-stretch retention above 85% at 23°C when assessed under ASTM D4649-20. Extrusion conditions on high-speed cast lines use melt filtration through 40/80/40 mesh screens, die temperature 240–260°C, air gap 100–150 mm, chill roll 20–28°C, and winder tension below 18 N/m to prevent blocking. Compliance is evaluated under ASTM D5458-13 for peel cling, ASTM D5748-19 for puncture resistance, ASTM D882-18 for tensile elongation at break, and ISO 527-3:2018 for film tensile modulus. Terminal product types include 17 µm pre-stretched hand wrap, 23 µm machine film, and 30 µm agricultural bale wrap.

    Extrusion Coating of Liquid Packaging Board at 22 g/m²

    At coating weights from 18 g/m² to 25 g/m², 100 wt% Trilene TS 8056 is used where the line runs below 450 m/min; above that speed, 10–20 wt% high-pressure LDPE is added to control neck-in below 35 mm on a 2,400 mm slot die. The coating complex meets FDA 21 CFR 177.1520(c) 2.2 for polyolefin food-contact layers and EU 10/2011/EC overall migration below 10 mg/dm² under simulated dairy and aqueous food stimulants. The converting route uses a 90 mm single-screw extruder with L/D 30:1, melt temperature 310–320°C, 120 mm air gap, and a 18°C matte chill roll at 350–500 m/min. No pre-drying is required when the material is stored below 80% relative humidity; surface condensation from cold silo transfer causes melt fracture. Terminal product types include liquid milk carton board, juice gable-top carton stock, and poly-lined paper sachets.

    When Form-Fill-Seal Lines Run 120 Pouches/min at 150°C Jaw Temperature

    Heat-seal strength per ASTM F88/F88M-21 remains above 18 N/15 mm on vertical form-fill-seal equipment running 120 pouches/min at 150°C when the sealant layer contains 85–95 wt% Trilene TS 8056 and 5–15 wt% slip/antiblock masterbatch. Seal creep and film blocking appear when jaw temperature exceeds 160°C because the LDPE fraction lowers the peak melting point; this limitation demands closed-loop barrel cooling on 55/65/55 mm coextrusion blown-film dies with 1.8 mm die gap. Converting uses blow-up ratio 2.2:1, melt temperature 195–210°C, and corona treatment to 42–48 mN/m per ASTM D2578-23. Compliance is based on FDA 21 CFR 177.1520, EU 10/2011/EC, and REACH; seal integrity is validated under ISO 11607-2:2019 for packaging processes when aseptic barrier claims are made. Terminal products include 20 kg frozen vegetable pouches, 5 kg snack food bags, and 1 L liquid stand-up pouches.

    Thin-wall drip irrigation tape extrusion uses Trilene TS 8056 at 88–94 wt% with 6–12 wt% carbon black UV stabilizer masterbatch; the resulting compound is classified under ISO 4427-1:2019 MRS 8 material requirements and tested per ISO 8772:2006 for irrigation pipes. The tape is produced on 45 mm single-screw extruders with L/D 28:1, a 500 mm spiral mandrel die, melt temperature 180–195°C, and vacuum calibration at −25 kPa followed by in-line punching of labyrinth emitters at 0.20 m intervals. Hydrostatic burst strength at 20°C passes 150 kPa per ISO 1167-1:2006 only when MFR remains below 0.7 g/10 min; higher flow causes ovality after coiling and emitter weld-line cracks. Terminal products include 16 mm flat drip tape, 20 mm lateral piping, and 12 mm bubbler tape for row-crop irrigation.

    For fertilizer and polymer pellet sack production, a 3-layer construction with 80–90 wt% Trilene TS 8056 and 10–20 wt% LDPE-rich reclaim is extruded on 65 mm grooved-feed extruders with L/D 30:1, 400 mm die, 2.2 mm die gap, blow-up ratio 2.0:1, and 200°C melt. Elmendorf tear strength per ASTM D1922-15 at 120 µm is 120–180 N/mm in the machine direction, and Method B dart impact per ASTM D1709-16a falls below 300 g when recycled LDPE exceeds 20 wt%, which limits reclaim addition. Compliance for non-dangerous goods packaging is assessed under ISO 21898:2004 for flexible intermediate bulk containers and UN 13M1 when the sack is certified for dangerous goods. The blown-film line uses a 1,000 mm collapsing frame with side gussets and inline corona at 42–48 mN/m per ASTM D2578-23. Terminal products include 25 kg flat-bottom fertilizer sacks, 50 kg gusseted polymer pellet bags, and 1,000 kg FIBC outer shell liners.

    Compliance checklist matrix for Trilene TS 8056 converted articles
    Application fieldMandatory standardCritical bound
    Agricultural filmEN 13206:2017Dart impact ≥450 g at 120 µm per ASTM D1709-16a
    Food-contact filmFDA 21 CFR 177.1520(c) 2.2Overall migration <10 mg/dm²
    Stretch filmASTM D5458-13Peel cling ≥120 g/cm at 23°C
    Drip irrigation tapeISO 8772:2006Burst ≥150 kPa at 20°C
    Dangerous goods sacksUN 13M1Drop test 2.5 m at −18°C if certified
    Medical device packagingISO 11607-1:2019Seal strength ≥18 N/15 mm per ASTM F88/F88M-21

    Sealant-Layer Performance of Medical Device Pouch Film After 25 kGy Electron-Beam Sterilization

    Pouches for terminally sterilized medical devices use a sealant layer containing 70–85 wt% Trilene TS 8056, 10–20 wt% LDPE-rich reclaim, and 5–10 wt% slip/antiblock masterbatch. After electron-beam sterilization at 25 kGy, seal strength per ASTM F88/F88M-21 typically declines by 10–15% if processing temperatures exceed 205°C; plant validation records show the drop is minimized when the film is extruded at 190–200°C and sealed at 135–150°C. The blown-film converting line uses 50/60/50 mm coextrusion screws, L/D 30:1, die gap 1.8 mm, blow-up ratio 2.0:1, and corona treatment at 44–48 mN/m per ASTM D2578-23. Compliance is governed by ISO 11607-1:2019 for packaging for terminally sterilized medical devices, ISO 10993-5:2009 for cytotoxicity, ISO 11137-1:2006 for radiation sterilization validation, and FDA 21 CFR 177.1520(c) 2.2 for the base polyolefin. Terminal products include catheter pouches, syringe blister lidding, and sterile drape overwrap.

    Free Quote

    Competitive Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend is supplied as a pelletized olefin copolymer blend in which the linear low-density polyethylene fraction is produced with 1-octene comonomer and is compounded with a low-density polyethylene fraction. The grade is specified for thin-gauge stretch film, industrial wrapping, pallet unitization, and food-contact overwrap structures where tear propagation resistance, dart impact strength, and extrusion bubble stability must be balanced against output rate. Melt flow rate is characterized under ASTM D1238 at 190 °C with 2.16 kg; typical producer literature places the value between 2.0 g/10 min and 2.5 g/10 min. Base density under ASTM D1505 typically lies between 0.918 g/cm³ and 0.921 g/cm³. The 1-octene branch distribution creates longer short-chain branches than butene or hexene LLDPE grades, increasing amorphous-phase tie chains and reducing the sharp yielding response observed at low temperature. The LDPE fraction contributes long-chain branching and broad molecular-weight distribution, which improves shear-thinning and bubble stability in blown-film extrusion. These characteristics differentiate the product from standard C4 or C6 LLDPE/LDPE blends, from pure LLDPE extrusion grades, and from metallocene narrow-molecular-weight resins.

    How Does an Octene-Comonomer Blend Change Tear and Dart Resistance Relative to C4 and C6 LLDPE?

    The comonomer type in the linear fraction controls the short-chain branch length and the probability that branch segments are excluded from the crystallite. Butene branches may be partially incorporated into the crystal lattice, which reduces their effectiveness as inter-lamellar spacers. Hexene branches are longer but less effective than octene at generating load-bearing tie-chain networks in the amorphous phase. At equivalent density and melt flow rate, a C8 LLDPE/LDPE blend therefore displays higher dart impact values under ASTM D1709, higher Elmendorf tear values under ASTM D1922, and generally higher slow puncture resistance than C4-containing sheet or film. This difference becomes operationally important when a converter down-gauges stretch film from 20 µm to 15 µm or when pallet corners create localized stress concentrations. The LDPE fraction further improves melt strength but may slightly reduce dart impact if the blend ratio is too high; therefore, the blend ratio is typically selected to maintain toughness while improving drawability. Published product-specific data for the exact blend ratio in TS 8056 should be confirmed against the current supplier certificate, because the exact balance of LDPE and C8 LLDPE is not always disclosed in summary literature.

    Class-representative film-property data for C8-LLDPE/LDPE blends at 23 µm and 25 µm nominal thickness are shown in Table 1. The ranges are drawn from publicly reported blown-film data for this product class, not from a certified grade-specific specification for TS 8056.

    PropertyTest methodTypical class range
    Melt flow rate, 190 °C/2.16 kgASTM D12382.0–2.5 g/10 min
    DensityASTM D15050.918–0.921 g/cm³
    Dart drop impact, 25 µm filmASTM D1709, Method A120–180 g
    Elmendorf tear, machine directionASTM D1922250–450 gf
    Elmendorf tear, transverse directionASTM D1922400–650 gf
    Tensile strength at break, machine directionASTM D88235–50 MPa
    Tensile elongation at break, machine directionASTM D882500–700 %

    Rheological Shear-Thinning and Extrusion Pressure Response

    The combined effect of the long-chain branched LDPE fraction and the C8 linear fraction is high shear-thinning across the die-lip shear-rate range. In extrusion, this translates into lower head pressure and lower screw torque than a pure C8 LLDPE of similar melt index. Typical blown-film starting conditions include barrel temperature zones from 180 °C to 225 °C, adapter and die temperature from 205 °C to 235 °C, die gap 1.8 mm to 2.5 mm, blow-up ratio 2.5:1 to 3.0:1, and frost-line height between 6 and 8 die diameters. On production-scale lines such as a 75 mm single-screw extruder with 30 L/D barrier screw and 250 mm annular die, the blend is generally less prone to bubble instability than a narrow-molecular-weight metallocene LLDPE. However, the exact pressure reduction and specific output depend on screw speed, temperature profile, and die-lip condition; published data for this specific configuration is limited.

    Purging with a low-melt-index polyethylene or commercial purge compound is required when transitioning from a polar resin such as EVA or from a high-pressure LDPE with a different antioxidant package. The C8 fraction is saturated and less vulnerable to moisture absorption than polyamide or polyester, but surface condensation on pellets stored in humid environments can create microbubbles in cast film. Drying at 60 °C for 2 h to 4 h is recommended for sacks that have been opened for more than 24 h or stored at relative humidity above 60 %. The material is typically supplied with an additive package that may include slip and antiblock agents; converters must not assume that the additive level is sufficient for all film-surface friction requirements.

    When Frost-Line Height Is Maintained Below Six Die Diameters in High-Draw Stretch Film

    When the frost-line height is held below six die diameters, the extrudate is quenched before substantial lamellar thickening can occur. This promotes smaller crystalline aggregates and improved optical clarity, but it also traps chain orientation and increases the residual stress in the machine direction. In stretch film, that orientation contributes to initial stretch force and load retention; however, edge nicks can propagate more readily if the oriented structure is not balanced by transverse relaxation. A higher frost line permits more melt relaxation and improves transverse toughness but can increase film haze and blocking tendency. The optimum frost-line position for TS 8056 is therefore set by the desired on-pallet retention force, film gauge, and chill-roll or bubble stability constraints rather than by a single universal value. Corona treatment levels, commonly expressed in dyn/cm measurements by ASTM D2578, are adjusted to the final surface tension required for printing or adhesion.

    Compliance under FDA 21 CFR 177.1520 for olefin polymers applies to the base resin when used in contact with food, but the final finished film must be tested under the conditions of use because the presence of surface modifiers, printing inks, or corona treatment may alter the regulatory status. EU food-contact evaluations fall under Regulation EU No 10/2011, with overall migration testing according to EN 1186 and specific migration according to the assigned food-simulant conditions. The product is expected to meet the substance restrictions in REACH 1907/2006/EC and the heavy-metal limits in RoHS 2011/65/EU, but users must verify the current supplier declaration for each lot.

    Gel Formation, Die-Lip Deposit, and Extrusion Boundary Conditions in the LDPE Fraction

    The LDPE fraction has unsaturated sites that can undergo thermo-oxidative crosslinking in the barrel, adapter, and die when melt temperature is sustained above 250 °C for 90 s or longer. Gel particles can then appear as optical defects in thin film and accumulate on the die lip. Processing should therefore avoid autothermal excursions caused by high screw speed and restrictive screen packs. Screens of 60 mesh to 80 mesh are adequate for general film use; finer filtration may raise melt temperature and increase shear work without removing all gels. Die-lip deposition is minimized by using a balanced die temperature profile, avoiding low-output idle periods, and purging with a suitable polyethylene purge compound when the line is stopped. The material is incompatible with excessive external lubricant concentrations that can lower film surface energy and interfere with corona treatment; amine-based antistatic additives may also contribute to color development under repeated extrusion. If the film is to be used in high-temperature wrapping near hot loads, the converter must validate that the additive package and the final film do not produce transferable substances beyond the applicable migration limit.

    Comparisons with metallocene C8 and C4/C6 blends are summarized in Table 2 for selection purposes when film gauge and stretch force requirements are being revised.

    Material systemBranch type and molecular-weight distributionProcessabilityToughness rankingPrincipal limitation
    Trilene TS 8056 C8 LLDPE/LDPEOctene linear branches plus LDPE long-chain branching; broadened distributionGood bubble stability; shear-thinning reduces head pressureHigh dart and tearGel potential if over-sheared above 250 °C
    C4 LLDPE/LDPEButene short branches; lower tie-chain densityGenerally easy to processLower dart and transverse tearReduced toughness at equal gauge
    C6 LLDPE/LDPEHexene intermediate branch lengthBalanced processing windowIntermediateLess shear-thinning than C8 blend
    mLLDPE C8Narrow molecular-weight distribution; uniform octene placementHigh head pressure; lower melt strengthHighest toughness and optical qualityRequires tighter bubble control and higher motor load

    In cast-film lines producing high-cling hand wrap, the C8 toughness of TS 8056 is used to survive localized thinning at pallet corners while the LDPE fraction maintains stable melt flow through the feedblock and die. The comparison with mLLDPE C8 becomes relevant when premium optical requirements or maximum puncture resistance are prioritized over extrusion pressure and bubble stability; in such cases, the broader molecular-weight distribution and LDPE long-chain branching of TS 8056 may present a lower-pressure processing alternative at the cost of slightly higher haze in critical optical applications. Operators should therefore establish the acceptable operating window on the specific line rather than transfer conditions from a C4 or mLLDPE grade.

    Top