| HS Code | 295636 |
| Melt Flow Rate 190 C 2 16 Kg | 0.9 g/10 min |
| Density | 0.922 g/cm³ |
| Melting Point | 121 °C |
| Vicat Softening Point | 96 °C |
| Tensile Strength At Break Md Td | 28/24 MPa |
| Elongation At Break Md Td | 700/800 % |
| Elmendorf Tear Strength Md Td | 80/200 g |
| Dart Drop Impact | 120 g |
| Haze | 14 % |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.15 |
| Blocking | 50 g |
As an accredited Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE blend is packaged in 25 kg polyethylene-lined bags, palletized, stretch-wrapped, 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend, securely stowed for ocean export. |
| Shipping | Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4/LDPE Blend is generally shipped as a non-hazardous polymer resin and not regulated as dangerous goods. Standard packaging: 25 kg bags, palletized and shrink-wrapped. Store dry, away from heat, sunlight, and ignition sources; follow SDS and local transport rules. Use standard PPE and avoid dust generation. |
| Storage | Store Trilene® TS 5009 in its original, sealed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, flames, and ignition sources. Keep away from oxidizers and incompatible materials. Maintain clean, dust-free conditions; avoid bag damage and contamination. Store pallets stably off the floor. Use FIFO rotation. Consult the SDS for specific storage temperature and handling guidance. |
| Shelf Life | Shelf life: typically 12 months from production, stored unopened in original packaging, dry, ventilated, below 50°C, away from sunlight. |
In pallet-load stabilisation lines producing 23 µm machine film on three-layer cast coextrusion equipment with 90 mm barrier screws and 30:1 L/D, Trilene® TS 5009 LLDPE-C4/LDPE Blend is introduced at 70–80 wt% of the core layer, with C6-mLLDPE at 20–30 wt%. The skin layers contain 0–10 wt% TS 5009, 87–95 wt% C6-mLLDPE, and 3–8 wt% PIB-based cling masterbatch. This distribution preserves tack and reduces neck-in at the slot die while the C4-LLDPE component contributes machine-direction stretch force and puncture resistance. Film for indirect food contact must satisfy FDA 21 CFR 177.1520 olefin polymer requirements and EU Regulation No 10/2011 overall migration limits of 10 mg/dm²; mechanical acceptance typically uses ASTM D5748-95(2012) for puncture propagation and ASTM D5459-96(2012) for machine-direction elastic recovery. On a 1200 mm slot die with a 32°C chill roll, the air gap is maintained between 80 mm and 150 mm, and line speed is 400–600 m/min. Melt temperature is held at 240–260°C; excursions above 270°C produce gel formation at the die lip. At warehouse relative humidity above 60%, PIB cling masterbatch is pre-dried at 70°C for 2 h to prevent surface streaking. Terminal products are 10–30 µm automatic machine stretch film and 12–15 µm hand-grade stretch film on 38 mm or 50 mm paper cores.
| Layer | TS 5009 (wt%) | C6-mLLDPE (wt%) | PIB cling masterbatch (wt%) |
|---|---|---|---|
| Core | 70–80 | 20–30 | 0 |
| Skin A | 0–10 | 87–95 | 3–8 |
| Skin B | 0–10 | 87–95 | 3–8 |
Where UV-stabilised silage covers and greenhouse claddings require a balance between dart-impact retention after multi-season solar exposure and flex-crack resistance at fold lines, TS 5009 is processed in the core layer at 75–90 wt%, with a UV/HALS masterbatch at 3–6 wt% in the exterior skin and an anti-fog or IR-additive masterbatch at 2–4 wt% in the interior skin. Compliance for silage bale wrap is assessed under EN 13206:2017, and tensile elongation after weathering is measured according to ISO 527-3:2018; REACH documentation follows EC 1907/2006. Three-layer blown-film lines with 65 mm, 90 mm, and 65 mm grooved-feed extruders, a 300 mm die, and a die gap of 2.2 mm run at BUR 2.5:1–3.0:1. The frost line is held at 8 die diameters to stabilise bubble turbulence; output on the 90 mm core extruder is typically limited to 280 kg/h before melt-pressure variability exceeds ±6%. Films above 150 µm are extruded as three-layer structures rather than monolayer to avoid UV masterbatch agglomeration at high thickness. Terminal products are 25 µm silage bale wrap, 150–200 µm greenhouse cover film, and 50–80 µm low-tunnel film.
Heavy-gauge collation shrink converted by double-bubble orientation places a specific requirement on the C4-butene branch content of the LLDPE phase because short-chain branching controls crystallisation kinetics and final shrink force. TS 5009 is incorporated at 70–85 wt% with 10–20 wt% high-pressure LDPE to increase transverse-direction shrink and 3–5 wt% fluoropolymer processing aid to suppress melt fracture at the annular die. The relevant test methods are ASTM D2732-14 for free shrink and ISO 14616 for shrink stress; when the film is used for food-contact bundling, EU Regulation No 10/2011 and FDA 21 CFR 177.1520 migration limits apply. Production equipment consists of a heavy-gauge blown-film line with a 90 mm single-screw extruder, 30:1 L/D, die gap 2.8–3.2 mm, and BUR 3.0:1; post-orientation, the tube is slit and passed through a 170–190°C hot-air tunnel for 45–60 s. Terminal products are heavy-gauge pallet shrink covers and collation bundles for glass, metal, and paperboard containers. Published shrink-force data for this specific LLDPE-C4/LDPE configuration is limited; converter line trials with a shrink-tunnel thermocouple map are required to establish final MD/TD shrink ratios.
At 250 kg/h output on 150–250 µm heavy-duty sack film lines, the blend is exposed to high melt pressure and requires a die gap of 2.5–3.5 mm to avoid melt fracture. TS 5009 is introduced at 80–95 wt% with 1–2 wt% fluoroelastomer processing aid and 0.5–1.5 wt% slip/antiblock masterbatch. Mechanical specifications are tested using ASTM D1709-15a for dart impact and ISO 527-3:2018 for tensile properties; food-contact liners must comply with FDA 21 CFR 177.1520 and EU Regulation No 10/2011. The line uses a 90 mm extruder with 30:1 L/D, a BUR of 2.2:1–3.5:1, and melt temperature 195–215°C. Terminal products include FIBC liners, gusseted heavy-duty shipping sacks, and construction film. Batch-to-batch dart impact variance increases when recycled trim exceeds 15 wt% or when the die gap is reduced below 2.2 mm, because the C4-LLDPE component undergoes molecular orientation at the die lip.
Sealant webs coextruded or tandem-laminated with TS 5009 require a surface energy of 38–42 mN/m for adhesion to aluminium foil, PET, or BOPP in dry-food laminations. The blend is used at 85–100 wt% in the sealant layer, with 2–5 wt% antiblock masterbatch and 0.5–1.0 wt% slip additive. Food-contact compliance is anchored to FDA 21 CFR 177.1520 and EU Regulation No 10/2011, with overall migration limited to 10 mg/dm². Process conditions include tandem extrusion lamination at 260–320°C, a 15–25 g/m² coating weight, and an air-cooled corona treater with watt density below 1.2 W/m²/min. Seal initiation temperature rises by 3–5°C when corona output exceeds 46 mN/m, which reduces high-speed sealing latitude. Terminal products are dry-food stand-up pouches, bag-in-box liners, and sachet films.
When distribution temperatures fall below -18°C, frozen vegetable bags, ice cream liners, and cold-chain mailers are blown from a compound containing 85–95 wt% TS 5009 with 2–4 wt% high-slip masterbatch and 3–6 wt% white masterbatch for 40–70 µm film. Testing uses ASTM D1709-15a for dart impact at -18°C and ISO 527-3:2018 for tensile properties; direct food contact requires FDA 21 CFR 177.1520 and EU Regulation No 10/2011. The blown-film line is configured with a 2.0–2.4 mm die gap, BUR 2.5:1, and melt temperature 190–210°C. The practical lower operating limit is -25°C; below this temperature, blends containing more than 10 wt% HDPE recycled content show reduced dart impact, and converter validation by frozen-drop testing is required.
Competitive Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Petroquimica Triunfo Trilene® TS 5009 is a blown-film polyethylene blend composed of a linear low-density ethylene-1-butene copolymer fraction and a high-pressure low-density polyethylene fraction. The product is specified for general-purpose flexible packaging, refuse sacks, construction and agricultural liners, carrier film, and secondary overwrap. Manufacturer-published nominal values place the melt flow rate at 0.9 g/10 min when measured according to ASTM D1238 at 190 °C/2.16 kg, and the density at 0.920 g/cm³ when measured according to ASTM D792. The C4-based LLDPE fraction contributes short-chain branching, while the LDPE fraction contributes long-chain branching. This combination produces a melt with higher apparent extensional strain hardening than a neat butene LLDPE, while retaining a broader processing window than many high-pressure LDPE grades at equivalent melt index.
On single-screw blown-film extrusion lines with grooved-feed sections and screw L/D ratios of 24:1 to 30:1, the resin can usually be processed without pre-drying when pellet moisture remains below 100 ppm. If storage relative humidity has exceeded 60%, surface moisture can create bubble chatter and pinhole-like defects; a common corrective step is drying in a desiccant hopper at 60 °C for 2 h. Barrel set temperatures from 170 °C to 210 °C and a melt temperature not exceeding 230 °C reduce the risk of oxidation gel formation. Starting die gaps of 1.2 mm to 2.0 mm and blow-up ratios from 2.2:1 to 3.0:1 are practical reference points, but the air-ring pattern, die diameter, frost-line position, and takeoff speed must be optimized on the specific line. The LDPE fraction improves bubble stability and reduces die-level neck-in; however, this benefit is lost if the frost line is raised beyond the cooling capacity of the air ring or if the bubble is exposed to uneven airflow.
Typical additive packages for film-grade polyolefins include antioxidants, slip agents, and antiblocking additives. The exact additive formulation of TS 5009 must be verified from the supplier’s technical data sheet and certificate of analysis. The resin is supplied in pellet form and is compatible with conventional polyethylene recycling streams when not contaminated with inks, adhesives, or incompatible polymers.
The following test methods are used for incoming lot qualification and film evaluation:
| Property | Standard method |
|---|---|
| Melt flow rate | ASTM D1238, ISO 1133-1:2022 |
| Density | ASTM D792, ISO 1183-1 |
| Tensile properties of film | ASTM D882, ISO 527-3 |
| Dart impact resistance | ASTM D1709, ISO 7765-1 |
| Elmendorf tear strength | ASTM D1922, ISO 6383-2 |
| Haze and luminous transmittance | ASTM D1003, ISO 14782 |
| Coefficient of friction | ASTM D1894, ISO 8295 |
Film specimens should be conditioned at 23 °C and 50% relative humidity for at least 40 h before mechanical testing under ASTM D882. Results obtained without conditioning or at different thicknesses are not directly comparable. In blown film, the tensile and tear balance is strongly influenced by blow-up ratio; higher blow-up ratios usually reduce machine-direction orientation and improve transverse-direction elongation, while lower blow-up ratios increase machine-direction stiffness. Dart impact testing by ASTM D1709 must state whether Method A or Method B is used, because the methods differ in dart geometry and drop energy range.
Compared with a high-pressure LDPE of the same density, Trilene® TS 5009 may require higher die pressure for the same output, but it usually provides higher tensile strength, better puncture resistance, and improved environmental stress-crack resistance. In applications where optical clarity is the main criterion, a homopolymer LDPE or a narrow-composition LLDPE may be preferred; the blend should not be selected solely on haze without comparing the target film thickness, blow-up ratio, and melt temperature.
The LLDPE fraction is copolymerized with 1-butene, producing ethyl branches along the polyethylene backbone. At the same density and melt index, a C4 LLDPE generally contains a lower concentration of stress-transmitting tie molecules than a C6 or C8 LLDPE, because the shorter branch length is less effective at creating intercrystalline connectivity. In solid-state film tests, this structural difference usually appears as lower dart impact and lower slow-puncture toughness relative to hexene- or octene-based LLDPE formulations. The LDPE fraction in TS 5009 reintroduces long-chain branching that improves extensional hardening in the melt and helps the bubble carry higher takeoff tension, but it does not erase the solid-state toughness difference created by the C4 branch length. At a product density of 0.920 g/cm³, the crystalline fraction is moderate, so tensile yield stress is lower than a high-density polyethylene, while elongation at break is high and tear propagation is more ductile than a corresponding HDPE film. The broad molecular weight distribution of the conventional Ziegler-Natta LLDPE fraction also produces a less uniform crystal thickness distribution than a single-site metallocene grade, which has implications for optical haze, gloss, and heat-seal plateau.
For general-purpose film, the lower comonomer length is often acceptable because the blend provides sufficient toughness at low thickness. However, sealing performance should be evaluated separately because the broad melting distribution governs hot-tack and seal-initiation temperature. Seal strength testing under ASTM F88 and hot-tack testing under ASTM F1921 should be conducted at the specific jaw pressure, dwell time, and film thickness used on the packaging line. The blend’s broad melting range can produce a seal plateau that begins at a lower temperature than a narrow-composition metallocene LLDPE, but the seal strength near the initiation temperature may be lower. Published data for this specific configuration is limited, so converter validation at the target line speed and seal-bar pressure is required.
At high throughput, the controlling process limit is generally cooling capacity rather than extruder melting capacity. If the frost-line height exceeds approximately 3.0 times the die diameter on a single-lip air ring, the unsupported bubble length becomes sensitive to air turbulence and melt-temperature nonuniformity. Gauge bands can develop when the melt-temperature variation across the die circumference exceeds ±5 °C because local viscosity differences persist as local thickness differences after stretching. A rotating die or oscillating haul-off can distribute these bands but cannot correct the root cause if the die-lip temperature spread is too large. On production lines, bubble movement is often observed when the die pressure drop falls below 8 MPa because the resulting shear history is insufficient to homogenize the melt. A screen pack containing 80 mesh to 120 mesh filtration segments is commonly used to increase residence time and protect the die gap. If the ambient air temperature exceeds 30 °C or the relative humidity exceeds 60%, cooling capacity is reduced, and the bubble may become tacky before reaching the frost line. The melt temperature should not exceed 230 °C for extended periods; otherwise oxidative chain scission generates gel particles that are visible as hard agglomerates in the film and can accumulate behind the die lip.
Processors switching from a high-pressure LDPE to this blend should reduce the initial barrel temperature profile by 5 °C to 10 °C and watch for a rise in die pressure. The linear backbone of the LLDPE fraction increases melt viscosity at low shear rates relative to LDPE, so the same screw speed may increase motor load. If melt pressure exceeds the extruder or die limit, the feed-section temperature should be lowered only after confirming that the screw is not starved. If gel formation continues after temperature reduction, the screen pack should be inspected for channeling and the die lip for carbonized polymer deposits. Towers equipped with internal bubble cooling can extend the throughput before bubble instability occurs, but the exchange air must be filtered and dried, and the process air temperature and volume should follow the die manufacturer’s curves. For multilayer coextrusion, melt streams should be combined at the same temperature to avoid interfacial viscosity mismatch. Published data for TS 5009 in five-layer barrier structures is limited, so direct evaluation of interlayer peel and bubble stability on the target line is required.
In most film toughness tests, yes. A C4 LLDPE has shorter ethyl branches than a C6 or C8 LLDPE, and this reduces the number of long-chain tie molecules that can connect adjacent lamellae at equivalent density and comonomer incorporation. The result is lower dart impact, lower tearing resistance in the transverse direction, and lower slow-puncture toughness than a hexene- or octene-based LLDPE of the same melt index and film thickness. The LDPE fraction in TS 5009 provides processing advantages and can improve melt strength, but it does not align the solid-state impact resistance with that of a high-alpha-olefin LLDPE-rich product. A converter requiring high dart impact in thin-gauge food packaging, stretch film, or high-performance liners should consider a C6 or C8 LLDPE, a metallocene LLDPE, or a high-toughness blend. Conversely, when the application is a general-purpose sack or liner where loadings are moderate, the C4/LDPE blend may be preferred because it can be processed at lower melt temperature with acceptable film gauge control and because it often carries a lower cost per kilogram. Compared with a metallocene LLDPE, the broader molecular weight distribution of TS 5009 can reduce clarity and gloss, particularly below 25 µm thickness, an effect that is more pronounced if processing temperatures are low and quench rates are insufficient. In heat-seal operations, the broader melting distribution may require a wider seal-bar temperature profile to reach the same hot-tack strength as a metallocene grade.
Incoming lots should be verified for melt flow rate and density against the certificate of analysis. Storage should be in unopened containers, protected from direct sunlight and high-temperature environments above 40 °C. Prolonged UV exposure without carbon black or hindered amine light stabilizers causes chain scission, embrittlement, and loss of elongation at break. The product is not formulated for contact with strongly oxidizing acids, chlorinated solvents at elevated temperature, or high-pressure oxygen service. For food-contact packaging, the applicable regulatory status should be confirmed under 21 CFR 177.1520 and any relevant local legislation; specific end-use conditions, food types, and additive migration limits must be assessed from the supplier’s lot-specific documentation rather than generic olefin-polymer approvals. If pellet contamination or unusual odor is observed, the lot should be quarantined and sampled before extrusion. The blend should not be used in medical implant applications or in pressure piping where long-term hydrostatic strength is required without validated resin-specific performance data.