| HS Code | 528508 |
| Density | 0.918 - 0.926 g/cm3 |
| Melt Index | 0.8 - 2.0 g/10 min |
| Tensile Strength At Yield | 8 - 12 MPa |
| Tensile Strength At Break | 20 - 40 MPa |
| Elongation At Break | 500 - 800 % |
| Tear Strength | 80 - 300 g |
| Dart Drop Impact | 100 - 500 g |
| Haze | 5 - 15 % |
| Gloss At 45 Degrees | 50 - 90 % |
| Melting Point | 120 - 130 C |
| Vicat Softening Point | 90 - 110 C |
| Coefficient Of Friction | 0.1 - 0.3 |
| Water Absorption | < 0.01 % |
| Flexural Modulus | 200 - 500 MPa |
| Hardness Shore D | 50 - 60 |
As an accredited Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied as 25 kg polyethylene-lined bags of LLDPE/hexene film-grade pellets; also available in 500 kg and 1,000 kg bulk sacks. |
| Container Loading (20′ FCL) | 20′ FCL typically loads about 20 metric tons of LLDPE/hexene film-grade resin in 25 kg bags, subject to weight and palletization limits. |
| Shipping | LLDPE/hexene film-grade resin is typically shipped as dry, free-flowing pellets in 25-kg bags, lined boxes, or bulk octabins. Store in a cool, dry, ventilated area away from direct sunlight and ignition sources. It is not classified as dangerous goods for transport under normal conditions. |
| Storage | Store LLDPE/hexene film-grade resin in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers or bags closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and static buildup. Use clean handling equipment and follow first-in, first-out stock rotation. Consult the SDS for specific temperature, ventilation, and local regulatory requirements. |
| Shelf Life | No shelf life limit; store cool, dry, sealed, away from direct sunlight, moisture, and contaminants to preserve LLDPE/Hexene film-grade properties. |
In cast stretch film production, LLDPE/hexene film-grade resins with density 0.917–0.920 g/cm³ and melt flow index 2.0–3.5 g/10 min according to ISO 1183-1:2022 and ISO 1133-1:2022 are extruded through a slot die at melt temperature 245–280°C and pinned to a chill roll stack held at 15–35°C. The hexene comonomer produces longer short-chain branches than butene, raising tie-molecule concentration during film stretching; this is observed at the winder as a puncture break force of 20–40 N at 20 µm under ASTM D5748 after 200% pre-stretch. Formulation boundaries for monolayer and multi-layer machine film include 100 parts hexene LLDPE, 0–30 parts LDPE for neck-in reduction, and 0.5–2.5 phr polyisobutylene-based cling concentrate in the cling layer, while the release layer carries 1000–3000 mg/kg silica antiblock. On a cast line with die gap 0.5–0.8 mm, line speed 300–800 m/min, and vacuum-box edge pinning, excessive draw above 600 m/min increases neck-in beyond 15% unless the edge bead is kept below 5 cm width; draw resonance is typically suppressed by keeping melt temperature above 240°C. Packaging compliance normally references EU 94/62/EC heavy metal concentration limit 100 ppm, REACH SVHC reporting at 0.1 wt%, and ASTM D5458 for cling force; food-contact secondary packaging must meet FDA 21 CFR 177.1520(c)3.2a. Finished goods are machine stretch film 12–35 µm, pre-stretched rolls 8–15 µm, and hand-wrap rolls 15–25 µm. Published data for PIB migration kinetics at line speeds above 700 m/min is limited; end-use trials are required to avoid cling-force drift in warm warehouses.
Blown film food-contact sealant web production blends LLDPE/hexene film grade with slip erucamide masterbatch at 500–1200 mg/kg active and silica-based antiblock at 2000–5000 mg/kg total formulation weight; fluoropolymer processing aid is added at 300–800 mg/kg only when melt fracture is observed on grooved-feed single-screw extruders with L/D 30:1. The resin is processed on spiral mandrel dies with die gap 1.5–2.5 mm, blow-up ratio 2.0–3.5, frost line height 3–6 die diameters, and melt temperature 190–230°C. Field data from high-stalk bubble lines show that lowering frost line height below 4 die diameters improves ASTM D1922 MD tear but increases blocking tendency if the film enters the nip above 45°C. Compliance is anchored to FDA 21 CFR 177.1520(c)3.2a and EU 10/2011 with an overall migration limit of 10 mg/dm²; erucamide migration requires verification under EU 10/2011 specific migration rules after 10 days at 40°C if used above 1000 mg/kg. Downstream conversion includes corona treatment to 38–42 mN/m, extrusion lamination or adhesive lamination to BOPP and PET, and sealant-web gauge reduction to 15–40 µm. End products are bakery bags, dry snack pouches, and laminate sealant layers for frozen and ambient foods. Published data for mineral hydrocarbon migration from recycled-content sealant webs is limited; converters using post-industrial regrind above 20 wt% must run sensory and migration validation on the finished laminate.
| Application | Formulation boundary | Critical processing threshold | Primary compliance / test anchor |
|---|---|---|---|
| Cast stretch film | 100 parts hexene LLDPE, 0–30 parts LDPE, 0.5–2.5 phr cling concentrate | Melt temperature 245–280°C, line speed 300–800 m/min | EU 94/62/EC; ASTM D5748 |
| Food-contact sealant web | 500–1200 mg/kg erucamide, 2000–5000 mg/kg silica | Frost line height 3–6 die diameters, nip temperature < 45°C | FDA 21 CFR 177.1520(c)3.2a; EU 10/2011 OML 10 mg/dm² |
| Heavy-duty sacks | 60–100 wt% hexene LLDPE, 0–40 wt% LDPE, 3–8 wt% white masterbatch | Melt temperature 200–240°C, die gap 1.8–2.4 mm | UN 13H4 under ADR 6.5.2 for hazardous fills; EU 94/62/EC |
| Agricultural silage wrap | 100 wt% hexene LLDPE; HALS 2000–6000 mg/kg, UVA 1000–3000 mg/kg | Blow-up ratio 2.5–3.5, die gap 1.5–2.0 mm | EN 13206:2017; ISO 4892-2 |
| Frozen food packaging | 70–100 wt% hexene LLDPE, 0–30 wt% mLLDPE; slip 500–1000 mg/kg | Melt temperature 190–220°C, corona 38–42 mN/m | FDA 21 CFR 177.1520(c)3.2a/3.2b; EU 10/2011 |
| Industrial stretch hood | 70–100 wt% hexene LLDPE, 10–40 wt% mLLDPE, 5–20 wt% LDPE | Die gap 0.6–0.8 mm, melt temperature 250–280°C | EU 94/62/EC; ASTM D5748 |
Because thick-gauge heavy-duty sack film is extruded on high-output blown film towers with die head sizes from 250–600 mm, LLDPE/hexene film-grade resin with density 0.918–0.922 g/cm³ and melt flow index 0.7–1.5 g/10 min is selected for its retention of tear resistance after gusset creasing. The formulation boundary includes 60–100 wt% hexene LLDPE, 0–40 wt% LDPE to stabilize bubble geometry, 3–8 wt% white masterbatch for opacity and UV screening, and 0.5–1.5 wt% slip/antiblock concentrate. On monolayer and 3-layer lines running sheet thickness 80–150 µm, die gap is held at 1.8–2.4 mm and melt temperature at 200–240°C; blow-up ratio is limited to 2.0–2.8 because higher BUR creates MD–TD imbalance in gusseted sections. The critical processing defect appears during gusset creasing: if frost line height exceeds 6 die diameters, the crease orientation aligns with low tear resistance and ASTM D1922 tear drops below 200 g at 100 µm, whereas a lower frost line retains transverse tear above 350 g. ASTM D1709 Method B dart impact on finished sacks is typically 700–1200 g for 100 µm monolayer film when the bubble is stabilized with internal bubble cooling. Compliance for non-hazardous sacks falls under EU 94/62/EC heavy metal limits of 100 ppm; sacks intended for dangerous goods are certified as UN 13H4 design type under ADR 6.5.2, requiring drop and stacking tests. Downstream conversion includes flexographic printing, bag making by heat sealing or sewing, and optional woven bag lamination. End products are PE shipping sacks for resin pellets, fertilizers, construction chemicals, and agricultural produce. Condensation on pellets stored at relative humidity above 60% in unheated silos causes metering instability and melt pressure fluctuations on grooved-feed extruders; pre-drying is recommended at 60–70°C for 2–4 h when visible surface moisture is present.
For agricultural silage bale wrap, the film must sustain elongation at break above 400% after 12 months of field exposure, which eliminates high-density LLDPE grades and requires a stabilizer package that does not exude to the film surface. The typical formulation is 100 wt% LLDPE/hexene film grade with hindered amine light stabilizer at 2000–6000 mg/kg and ultraviolet absorber at 1000–3000 mg/kg; green or white color masterbatch is added at 2–5 wt%, and anti-static masterbatch at 0.1–0.3 wt% is optional for high-speed bale wrappers. Processing takes place on blown film equipment with die gap 1.5–2.0 mm, blow-up ratio 2.5–3.5, and melt temperature 190–220°C; bubble stability is maintained by using internal bubble cooling and a low frost line. Field failures on round bale wrappers generally occur when UV stabilizer dispersion is poor, leaving gel particles above 200 µm that tear during pre-stretch at 60–80% stretch ratio; extruder screen packs then require change every 2–4 h unless dispersive mixing elements are used. Compliance is evaluated against EN 13206:2017 for thermoplastic stretch films for wrapping bales, with weathering exposure conducted according to ISO 4892-2; finished films are specified at 20–50 µm thickness and roll lengths up to 1500 m. End products are round bale wrap, square bale wrap, and silage pit cover films. Stores above 30°C accelerate slip additive migration and reduce unwind tension; rolls should be stored away from direct sun and in widths not exceeding 750 mm for manual bale wrapping.
Low-temperature dart impact retention is evaluated by conditioning films at -20°C and testing under ASTM D1709 Method A after 24 h; hexene LLDPE film-grade resins with density 0.918–0.922 g/cm³ and melt flow index 0.8–1.2 g/10 min provide sufficient tie molecules to avoid brittle flex cracking at gauge 30–70 µm. The formulation boundary is 70–100 wt% hexene LLDPE and 0–30 wt% metallocene LLDPE; erucamide slip is added at 500–1000 mg/kg, silica antiblock at 2000–4000 mg/kg, and no wax-based slip is used because it can exude at freezer temperatures and reduce seal strength. Blown film lines operate with die gap 1.6–2.4 mm, high-stalk bubble geometry, blow-up ratio 2.0–3.0, melt temperature 190–220°C, and frost line height 5–8 die diameters; internal bubble cooling is required for frost line control on lines above 150 kg/h throughput. Seal initiation temperature for a 50 µm web is typically 95–110°C at dwell time 0.5 s and jaw pressure 2 bar, measured on hot-tack equipment; hot tack strength above 2.5 N/25 mm is critical for vertical form-fill-seal operations. Compliance anchors are FDA 21 CFR 177.1520(c)3.2a and 3.2b for olefin polymers, and EU 10/2011 with overall migration below 10 mg/dm²; specific migration of erucamide is verified when concentration exceeds 500 mg/kg. End products are IQF vegetable bags, seafood pouches, and frozen meat films. Published data for COF drift after six months of frozen storage under specific slip packages is limited; converters must run seal-strength and COF validation on finished pouches stored at -25°C before release.
In industrial stretch hood film production, LLDPE/hexene film grade is processed on cast coextrusion lines with final film width up to 2.4 m, using the hexene-based resin in the core and outer layers to resist corner puncture during pallet transit. The formulation is typically 70–100 wt% hexene LLDPE, 10–40 wt% metallocene LLDPE for toughness, and 5–20 wt% LDPE for neck-in control; no tackifier is used, and a release surface is created with silica antiblock at 1000–3000 mg/kg only in the slip layer. Cast lines run die gap 0.6–0.8 mm, melt temperature 250–280°C, and die width up to 2.6 m; edge trim is recycled into the core layer at 5–15 wt% regrind without loss of ASTM D5748 puncture resistance if regrind particle size remains below 8 mm. The primary failure mode on hooder machines is film collapse at the pre-stretch rollers when the film surface temperature exceeds 40°C; chill roll temperature is therefore held between 15–25°C. Compliance for the finished stretch hood film follows EU 94/62/EC heavy metal limit 100 ppm and REACH SVHC reporting at 0.1 wt%; performance qualification is done under ASTM D5748 puncture test and ASTM D5458 cling/shear. Finished goods are stretch hood films 50–120 µm thick for palletized construction materials, appliances, chemical drums, and beverage pallets. Published data for hood film performance above 120 µm on high-speed hooders is limited; field trials with specific machine pre-stretch ratios are required before commercial conversion.
Competitive Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Linear low density polyethylene copolymerized with 1-hexene is specified for blown film where the comonomer’s four-carbon butyl branch improves tie-molecule formation relative to shorter butene branches. Film-grade hexene LLDPE is commonly supplied in a density envelope of 0.916–0.920 g/cm³ and a melt index of 0.5–1.0 g/10 min measured by ASTM D1238 at 190°C/2.16 kg. The resin is pelletized with anti-block and slip additive packages and is used in heavy-duty sacks, stretch wrap, frozen-food film, agricultural silage film, and industrial liners. Model identification is supplier-specific but usually encodes density and melt index; specifying LLDPE/hexene, film grade, 0.918/1.0 selects the base resin architecture without selecting a particular additive package. Because the comonomer is 1-hexene rather than 1-butene, the resulting short-chain branches are butyl groups that introduce a measurable increase in dart impact and tear resistance at equivalent density and melt index.
Commercial model designation includes supplier-specific suffixes that encode comonomer type, density, and melt index. A resin identified as LLDPE/hexene 118N may denote a nominal density of 0.918 g/cm³ and a melt index of 1.0 g/10 min, but such nomenclature should be verified against the supplier’s product data sheet because there is no universal coding system. Purchase specifications should fix density, melt index, comonomer type, additive package, pellet color, and regulatory status. Film-grade hexene LLDPE is commonly supplied as cylindrical pellets with antiblock levels between 1000–3000 ppm and slip additive levels between 200–600 ppm, but the exact additive loading is application-specific.
Melt strength is the primary processing restriction. Hexene LLDPE has a linear chain structure with no intentional long-chain branching and a relatively narrow molecular weight distribution; as a result, the bubble exhibits less strain hardening than LDPE. On three-layer blown film dies, bubble stability commonly deteriorates when blow-up ratio exceeds 3.0–3.2 unless internal bubble cooling or a high-melt-strength blend is employed. A 60 mm barrier screw with 30:1 L/D, die gap 2.0 mm, and total output of 180 kg/h typically produces a melt pressure of 320–360 bar at the screen changer. Reducing the die gap to 1.2 mm at the same output causes sharkskin on 25 µm film and increases the onset of melt fracture; raising melt temperature above 230°C accelerates oxidative gel formation. Acceptable bubble stability is generally achieved with blow-up ratio 2.0–2.8, a dual-lip air ring, and screen packs of 40/60/100 mesh. In practice, processors adjust frost line height to 300–500 mm from the die face to balance MD/TD orientation and maintain stable freeze-line geometry.
Resin data sheets for film-grade hexene LLDPE report the following envelope when the material is converted on a 40 mm blown film line with 2.5:1 blow-up ratio, 25 µm gauge, and 2.0 mm die gap. The ranges are not single-point guarantees; orientation, frost line height, and line speed shift the balance between dart impact and tear properties.
| Property | Method | Typical range |
|---|---|---|
| Density | ASTM D1505 / ISO 1183 | 0.916–0.920 g/cm³ |
| Melt index | ASTM D1238 | 0.8–1.0 g/10 min at 190°C/2.16 kg |
| Melting peak | ASTM D3418 | 119–124°C |
| Dart impact | ASTM D1709A | 180–350 g on 25 µm film |
| Elmendorf tear MD | ASTM D1922 | 120–300 g |
| Elmendorf tear TD | ASTM D1922 | 400–650 g |
| Tensile strength at break MD | ASTM D882 | 35–50 MPa |
| Secant modulus 1% MD | ASTM D882 | 180–260 MPa |
| Haze | ASTM D1003 | 8–14% |
| Gloss 45° | ASTM D2457 | 45–60 |
The property envelope is relevant for heavy-duty sack and industrial liner specifications. Converters commonly require a minimum dart impact of 200 g per ASTM D1709A at 25 µm; hexene LLDPE typically clears this threshold in monolayer film, whereas butene LLDPE with equivalent density and melt index may require a gauge increase to meet the same value. For frozen-food packaging, the TD Elmendorf tear requirement below -20°C is frequently set at 400 g; film-grade hexene LLDPE is selected because the butyl branches maintain tear propagation resistance at low temperature.
Film-grade hexene LLDPE typically has a molecular weight distribution described by a polydispersity index of 3–5, but metallocene grades may be narrower. The comonomer distribution depends on the catalyst system; Ziegler-Natta grades place hexene preferentially in the lower-molecular-weight fraction, while metallocene grades produce more uniform comonomer placement. This difference affects film optics, seal initiation, and puncture resistance. A multimodal distribution can restore bubble stability while retaining dart impact. For precise comparisons, gel permeation chromatography and crystallization analysis fractionation should be requested from the resin supplier because standard density and melt index alone do not define comonomer distribution.
Substitution is not drop-in because the comonomer changes shear viscosity, melt tension, and film optics. At the same 0.918 g/cm³ density and 1.0 g/10 min melt index, hexene LLDPE has higher dart impact and puncture resistance than butene LLDPE but may show slightly higher haze. On a 25 µm monolayer film, representative evaluations report dart impact moving from 110–150 g for butene LLDPE to 170–250 g for hexene LLDPE under the same die and blow-up ratio. Elmendorf TD tear commonly increases by 30–60%, while MD tear may remain within the same range because orientation dominates. The replacement also lowers seal initiation temperature by 2–5°C in some supplier formulations, which is beneficial for form-fill-seal packaging. However, the effect is not universal; comonomer distribution, catalyst type, and additive package each shift the values. Processors must re-optimize blow-up ratio and frost line height because the hexene grade may exhibit less bubble stability at blow-up ratio above 3.0.
When 1-octene is used instead of 1-hexene, the short-chain branch extends to a six-carbon hexyl group, further improving tie-molecule mobility. Film-grade octene LLDPE at equivalent density and melt index typically delivers greater dart impact, puncture resistance, and TD tear than hexene LLDPE, but at higher cost and with higher extrusion torque requirements in some lines. Hexene occupies the intermediate position between butene and octene; it is selected where toughness requirements exceed butene capability but octene economics are not justified. In multi-layer structures, hexene LLDPE is often placed in the core or outer layers to provide tear and abuse resistance, while LDPE is used in the seal or skin layer for melt strength and clarity.
Hexene LLDPE film grades show a shear-thinning profile typical of linear polyethylene, but the absence of long-chain branching results in higher screw torque than LDPE at the same output. On a 45 mm grooved-feed extruder with 28:1 L/D, a film-grade hexene LLDPE with melt index 1.0 g/10 min typically draws 70–80% of installed motor load at 150 kg/h, whereas an LDPE grade of similar melt index may draw 55–65%. Die melt pressure at 200°C is commonly 300–350 bar. Resin temperature should be held between 200°C and 230°C; at temperatures below 190°C, viscosity rises sharply and can overload the drive, whereas above 240°C thermal degradation accelerates. Film-grade hexene LLDPE is not hygroscopic; pre-drying is not normally required when stored below 60% relative humidity. If condensation is present after outdoor storage, dehumidified drying at 70–80°C for 2 h reduces surface moisture gels.
Under a constant die gap of 2.0 mm, increasing blow-up ratio from 2.0 to 3.0 typically increases TD tear by 20–40% while decreasing MD tear by 10–25% because transverse orientation is increased and machine-direction draw is reduced. Dart impact is usually maximized at intermediate blow-up ratio 2.2–2.8 where orientation is balanced. At blow-up ratio below 1.8, film gauge uniformity may degrade from die-lip build-up and non-uniform air flow. These effects are line-specific and must be confirmed by gauge profiling with a capacitive thickness scan across the bubble circumference.
The primary structural reason for specifying hexene LLDPE is tie-molecule concentration in the semi-crystalline network. The butyl branch from 1-hexene creates a longer short-chain branch than the ethyl branch from 1-butene, which reduces crystalline tightness and permits more tie chains to bridge adjacent lamellae. Under ASTM D1709A, this translates into higher dart impact at equivalent density. Under ASTM D1922, the effect is not symmetric: TD tear improves more than MD tear because blow-up ratio and draw orientation dominate MD properties. For a 25 µm film produced at blow-up ratio 2.5, typical dart impact values for hexene LLDPE are 180–350 g, while published data for butene LLDPE in the same gauge and density fall at 100–180 g. The same resin may show lower gloss and higher haze than butene equivalents, and the exact value depends on die gap, output, and frost line height. Processors that require both high toughness and clarity often run a coextruded structure with an LDPE skin over a hexene LLDPE core.
For food-contact film, the resin must be covered by the appropriate regulatory chapters or supplier-specific confirmation. Typical compliance checks include the following matrix.
| Standard or regulation | Applicability | Condition or method |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer food-contact use | Hexene comonomer in specified density; end-use migration evaluation per 21 CFR 177.1520(c)3.2 |
| EU No 10/2011 | Plastic food-contact materials | Overall migration 10 mg/dm²; simulant selection per Annex III |
| REACH 1907/2006 | EU registration and SVHC content | No SVHC above 0.1% w/w in supplied resin |
| RoHS 2011/65/EU | Electrical/electronic restricted substances | Pb, Hg, Cr VI, PBB, PBDE < 1000 mg/kg; Cd < 100 mg/kg |
| ISO 1133-1:2022 | Melt mass-flow rate | 190°C, 2.16 kg load |
The operational boundaries should be defined in the purchase specification. Film-grade hexene LLDPE is not recommended for continuous service above 70°C, for retort applications exceeding 121°C, or for direct contact with strong oxidizing acids, aromatic hydrocarbons, and chlorinated solvents, which reduce molecular weight or promote environmental stress cracking. In aggressive detergent packaging, environmental stress-crack resistance should be evaluated under full bottle or pouch conditions because standard film data do not predict stress-crack response. Published data for long-term field performance in specific packaging formats is limited; qualification trials on production-scale blown film lines are required.