Overview Of Materials For Linear Low Density Polyethylene Lldpe Film Grade

Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade

    • Product Name: Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 199653
    Density 0.910 - 0.940 g/cm3
    Melt Flow Rate 0.50 - 3.5 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 8.00 - 16.0 MPa
    Tensile Strength At Break 20.0 - 40.0 MPa
    Elongation At Break 300 - 800%
    Flexural Modulus 0.200 - 0.500 GPa
    Dart Drop Impact 80.0 - 300 g
    Elmendorf Tear Strength Md 100 - 400 g
    Elmendorf Tear Strength Td 200 - 600 g
    Haze 5.00 - 20.0%
    Gloss 45 50.0 - 90.0
    Melting Point 120 - 130°C
    Vicat Softening Point 90.0 - 110°C
    Coefficient Of Friction 0.100 - 0.300
    Water Vapor Transmission Rate 10.0 - 30.0 g/m2/day
    Oxygen Transmission Rate 1500 - 4000 cm3/m2/day

    As an accredited Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LLDPE film-grade material supplied in 25 kg sealed polyethylene-lined bags, stacked on pallets, labeled for industrial use.
    Container Loading (20′ FCL) 20′ FCL loading: LLDPE film-grade resin in 25 kg bags, palletized, stretch-wrapped; approx. 18–20 metric tons per container.
    Shipping Linear low density polyethylene (LLDPE), film grade, is typically shipped as non-hazardous resin pellets in 25 kg sacks, jumbo bags, or bulk trucks/railcars. Keep packages dry, clean, and away from excessive heat, sunlight, and moisture. Follow local transport regulations, maintain proper labeling/documentation, and avoid contamination during handling or damage.
    Storage Store LLDPE Film Grade in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep material in original sealed bags or containers on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and stacking that may damage packaging. Follow manufacturer’s SDS and local regulations. Maintain good housekeeping to prevent slipping on spilled pellets.
    Shelf Life LLDPE film grade has no fixed shelf life when stored cool, dry, and protected from UV light in original packaging.
    Application of Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade

    Cast pallet-wrapping lines configured with 3,000–5,000 mm slot dies and chilled rolls at 18–25°C typically run film-grade LLDPE with density 0.917–0.919 g/cm³ (ASTM D1505) and melt index 2.0–3.5 g/10 min at 190°C/2.16 kg (ASTM D1238). Pre-stretch sections set at 250–300% require low gel counts and monotonic stress–strain response. Cast film producers meter 2–5 wt% LDPE of melt index 1.8–2.5 g/10 min into the extruder to stabilise the web and reduce edge neck-in. Polyisobutylene cling agent at 0.5–1.2 wt% is added to the core or skin layer; addition above 1.5 wt% increases unwind force and produces telescoping rolls at winding tension 15–25 N/m. Machine-direction tensile stress at break under ASTM D882 for 20 µm film is typically 25–40 MPa, with elongation at break 350–500% in the machine direction and 500–700% in the transverse direction. Puncture resistance measured under ASTM D5748 is used to reject film with inconsistent gauge bands; field data from automatic wrappers show that coefficient of friction below 0.15 (ASTM D1894) leads to roll telescoping, while values above 0.45 cause film tears at pre-stretch rollers. Blown stretch film lines running the same resin at blow-up ratio 3.0:1–3.5:1 and die gap 1.8–2.4 mm produce higher dart impact but lower machine-direction elongation; gauges below 12 µm are generally shifted to metallocene-catalysed LLDPE to survive pre-stretch above 250% without burst-through. Terminal products include machine pallet wrap, hand stretch film, and pre-stretched ancillary wrap. Edge trim is recycled at 10–20 wt%; higher regrind levels create gels and reduce puncture retention by more than 10%.

    How Does UV Stabilizer Dose and BUR Control Season-Long Silage Film Integrity?

    Silage bale wrap and greenhouse covering are produced on three-layer blown film lines from LLDPE with density 0.918–0.921 g/cm³ (ISO 1183) and melt index 0.5–1.0 g/10 min (ISO 1133-1). Outer layers receive hindered amine light stabiliser at 0.20–0.45 wt% and benzotriazole or triazine UV absorber at 0.10–0.25 wt%. Black silage covers use carbon black at 2.0–3.5 wt%; white greenhouse films use titanium dioxide at 4.0–8.0 wt% to retain reflectance and reduce infra-red load. Blow-up ratio is held at 2.5:1–3.5:1 with frost line height 600–900 mm above the die and die gap 1.8–2.4 mm. Raising blow-up ratio above 3.5:1 improves transverse tear resistance but introduces bubble instability and gauge variation up to ±12% on thin silage film. Oxygen transmission rate of 25 µm black film at 23°C and 0% RH under ISO 15105-2 is 2,500–4,000 cm³/(m²·day·bar); moisture vapour transmission rate under ISO 15106-2 at 38°C and 90% RH is 15–25 g/(m²·day). Weathering validation is conducted under ISO 4892-2 xenon-arc or ASTM G154 UVA 340; black formulations retaining more than 60% of original machine-direction elongation after 3,000 h exposure are often accepted for multi-season use. Low levels of liquid polybutene at 0.5–1.0 wt% provide bale-wrap self-adhesion; overdosing reduces oxygen barrier and can transfer tackifier to silage. Anti-block silica above 1,000 ppm destroys cling and is avoided in silage wrap. Terminal products include bale wrap, silage cover, greenhouse side sheet, and mulch film. In greenhouse service, the film must maintain tensile retention under ASTM D882 and tear resistance under ISO 6383-2 after 12–24 months of solar load.

    Heavy-Duty Shipping Sacks and Form-Fill-Seal Resin Blends

    In heavy-duty shipping sacks, film-grade LLDPE copolymers with hexene or octene comonomer are specified at melt index 0.4–1.0 g/10 min and density 0.920–0.924 g/cm³ (ASTM D1505). Three-layer coextrusion structures typically use HDPE-rich skins and an LLDPE-rich core; a skin ratio of 20/60/20 across the layers is common. Internal bubble cooling and die gaps of 1.8–2.4 mm are used with blow-up ratio 2.0:1–3.0:1. Open-mouth bags are converted at 80–180 µm; form-fill-seal film is supplied at 60–150 µm. Dart drop impact under ASTM D1709 for 100 µm FFS film on a 38 mm diameter dart is commonly specified at not less than 300 g for butene-based LLDPE and not less than 500 g for hexene or octene types. Tensile break stress in the machine direction under ASTM D882 is 25–35 MPa; secant modulus at 1% strain is 180–250 MPa. Seal strength under ASTM F88 at 140–160°C, 1.5 N/mm² seal pressure, and 0.5 s dwell is 10–20 N/15 mm. Seal initiation for hexene LLDPE begins at 105–115°C, which permits high line speeds on FFS spouts. Creep is evaluated under ASTM D2990 at 23°C and 20% of yield stress; published data for stacked-sack creep in tropical warehouses is limited, but field audits indicate that storage above 40°C can produce visible deformation when LLDPE content falls below 50 wt% of the total structure. Terminal products include open-mouth sacks, valve sacks, and FFS gusseted bags for resins, fertilisers, and construction chemicals.

    When a Three-Layer Coextrusion Line Produces Collation Shrink at Line Speeds Above 120 m/min

    Three-layer collation shrink film processed at line speeds above 120 m/min requires melt temperature 195–215°C and die pressure below 350 bar to avoid shark-skin texture. Skin layers contain 20–40 wt% hexene LLDPE with density 0.917–0.920 g/cm³ and melt index 0.9–1.2 g/10 min; the core uses LDPE with melt index 0.3–0.5 g/10 min. The line uses die gap 1.8–2.2 mm, blow-up ratio 3.0:1–3.5:1, and frost line height 700–1,000 mm. Output per 1,200 mm die is typically 120–180 kg/h. Film thickness is 25–35 µm for bottle and can multipacks. Free shrink under ASTM D2732 at 120°C is 50–70% in machine direction and 0–10% in transverse direction; shrink force under ASTM D2838 is 0.15–0.35 MPa. Slip and anti-block masterbatch in the skin layers at 2–4 wt% maintains coefficient of friction at 0.20–0.35; values above 0.45 cause misaligned bands on collation drums. When line speed exceeds 120 m/min, polymer processing aid below 300 ppm results in melt fracture, while addition above 800 ppm can plate out on the die lip. Seal initiation temperature for the structure is 105–115°C at 1.5 N/mm² and 0.5 s dwell under ASTM F88. Seal strength is 8–14 N/15 mm. Terminal products include shrink wrap for canned food, water bottle multipacks, and promotional packs. A blown film line with L/D 30:1 and a barrier screw is used; feed zone temperatures are kept below 120°C to avoid pellet bridging from premature melting.

    Frozen food lamination films require seal initiation temperatures below 100°C to protect low-melting tie layers and prevent scorch. A cast coextruded sealant web based on hexene LLDPE with density 0.916–0.920 g/cm³ and melt index 1.0–2.0 g/10 min is blended with 10–20 wt% LDPE of melt index 2.0 g/10 min. The food-contact layer is controlled under FDA 21 CFR 177.1520 and EU 10/2011. Overall migration remains below 10 mg/dm² under EU 10/2011 test conditions. Seal strength is measured by ASTM F88 at 115–125°C seal bar temperature, 1.5–2.5 N/mm² pressure, and 0.5–1.0 s dwell; values are 8–14 N/15 mm. Water vapour transmission rate for 25 µm film under ASTM F1249 at 38°C and 90% RH is 15–25 g/(m²·day). The film is produced on cast lines at 180–300 m/min with die gap 0.8–1.2 mm, chill roll temperature 18–22°C, and winding tension 8–15 N/m. Gauge variation is held within ±4% to avoid seal bar gaps. Erucamide slip additive is dosed at 500–1,000 ppm and silica anti-block at 1,000–2,500 ppm; coefficient of friction above 0.35 causes misfeed in vertical form-fill-seal equipment, while below 0.10 creates rewind drift. The LLDPE sealant web is laminated to oriented polyester or biaxially oriented polypropylene; laminating bond strength after cure is 1.0–3.0 N/15 mm under ASTM F904. Terminal products include frozen vegetable pouches, ice cream wrap, cheese packaging, and liquid pouch film. Moisture barrier of LLDPE is insufficient for oxygen-sensitive products; EVOH or metallised films are used for extended shelf life. Regulatory compliance and barrier targets are summarised below.

    Table 1: Food-contact compliance and barrier test matrix for LLDPE sealant webs
    Requirement / propertyStandard or regulationTypical industrial target
    US food-contact complianceFDA 21 CFR 177.1520Compliant for food types and conditions of use
    EU plastics food-contact complianceEU 10/2011Overall migration < 10 mg/dm²
    Seal strengthASTM F888–14 N/15 mm
    Water vapour transmissionASTM F124915–25 g/(m²·day)
    Film tensileASTM D882MD break stress 25–40 MPa
    Coefficient of frictionASTM D18940.10–0.35

    Geomembrane Service Life Is Governed by Stress-Crack Resistance in Direct Leachate Contact

    In secondary containment liners, film-grade LLDPE with density 0.932–0.940 g/cm³ and melt index 0.5–1.0 g/10 min is used for sheet thicknesses of 0.5–2.5 mm. The resin is processed on single-screw extruders with L/D 30:1 and barrier screws at melt temperature 190–210°C. Stress-crack resistance under ASTM D5397 or ISO 6252 is measured in a 10% Igepal CO-630 solution at 50°C; failure times above 400 hours are commonly required for liner-grade LLDPE, but comonomer type, density, and cooling rate create wide variance. Tensile break stress under ISO 527-3 is typically 25–40 MPa; elongation at break is 600–800%. Hot wedge welding is performed at 280–350°C with seam peel strength under ASTM D6392 above 80% of parent sheet yield strength. Chemical resistance is evaluated with site-specific leachate because municipal waste leachate composition varies; the material is not recommended for continuous contact with aromatic solvents above 5% by volume or with strong oxidising acids. Field deployment on subgrade with moisture content above 10% creates wrinkles and prevents intimate contact with compacted soil. Welding below 5°C lowers peel strength and increases seam failure risk. Terminal products include lagoon liners, floating covers, secondary containment basins, and methane barrier membranes.

    Free Quote

    Competitive Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Film-grade linear low density polyethylene (LLDPE) comprises ethylene copolymers with 1-butene, 1-hexene, or 1-octene, polymerised in low-pressure gas-phase, solution, or slurry processes. The film-grade designation is normally defined by a melt mass-flow rate of 0.5 to 2.0 g/10 min at 190 °C and 2.16 kg load under ISO 1133-1:2022 or ASTM D1238-20 Procedure A, together with a density of 0.918 to 0.930 g/cm³ determined by ASTM D1505-18 or ISO 1183-1:2019. Cast film grades may extend to 4.0 g/10 min melt index. Commercial product datasheets identify the grade by comonomer type, nominal melt index, density, slip grade, antiblock loading, thermal stabiliser, and gel rating rather than by a single model. Film-grade LLDPE is used in blown and cast monofilm, stretch wrap, collation shrink film, heavy-duty sacks, liners, agricultural film, and sealant webs in multilayer packaging.

    Rheological Boundaries in Blown Film Extrusion of LLDPE

    Blown film extrusion of film-grade LLDPE is constrained by melt strength and shear-induced melt fracture in annular or spiral mandrel dies. A common production configuration uses a single-screw extruder with a 24:1 to 30:1 L/D barrier screw, an annular die gap of 1.5 to 2.5 mm, a blow-up ratio of 2.0:1 to 3.5:1, and a melt temperature of 195 to 230 °C. Because LLDPE lacks the long-chain branching of high-pressure LDPE, its extensional viscosity and melt tension are lower, making the bubble more sensitive to frost line height, air-ring velocity, and die-gap stress. Bubble breathing or oscillation can occur when the frost line height exceeds 4 to 8 die diameters under high cooling-air velocity. Melt index alone does not predict this behaviour; a capillary shear viscosity curve obtained under ISO 11443:2021 is normally required for die and screw design. On the same extruder, LLDPE of 0.9 g/10 min melt index may generate higher melt pressure and drive amperage than a low-density polyethylene of comparable melt index because of reduced shear thinning. Fluoropolymer processing aids at 200 to 800 mg/kg are used to lower die-lip shear stress and delay sharkskin. Where internal bubble cooling is fitted, production rates can increase by 15% to 30% over external cooling alone, but the control band narrows because the internal air pressure interacts with bubble geometry.

    Cast film lines process film-grade LLDPE through a flat die with a die gap of 0.4 to 0.8 mm, quenching the melt on a chill roll maintained at 20 to 35 °C and trimming the edge bead before winding. Grades with melt indices of 2.0 to 4.0 g/10 min are selected for cast stretch wrap to reduce motor load at high screw speeds. A vacuum box or air knife is used to pin the melt curtain to the chill roll; without it, neck-in and thickness variation increase. The die-to-roll air gap is commonly kept at 5 to 15 mm because a larger gap raises neck-in and allows draw resonance to develop. Edge encapsulation or coextrusion is sometimes used to control neck-in when a high-melt-index grade cannot meet the required toughness.

    What Separates Film-Grade LLDPE from High-Pressure LDPE in Down-Gauged Film?

    Film-grade LLDPE differs from high-pressure LDPE in molecular architecture, not merely in density. High-pressure LDPE contains long-chain branching, while LLDPE has a predominantly linear backbone with short-chain branches introduced by the comonomer. This difference reduces shear thinning in LLDPE, increases extensional stress at typical die shear rates, and contributes to higher film toughness at equal gauge. In a 25 µm monolayer blown film, dart impact resistance under ASTM D1709-22 Method A is commonly higher for film-grade LLDPE than for LDPE by 50% to 150%, although absolute values are grade-dependent and are typically reported from 80 to 300 g. Elmendorf tear performance measured by ASTM D1922-23 is also higher in LLDPE, but directional tear balance is influenced by blow-up ratio and frost line height. High-pressure LDPE retains an advantage in melt strength, bubble stability, and high-shear processing; LLDPE requires wider die gaps and more stable cooling to avoid melt fracture.

    Compared with high-density polyethylene film grades, which exhibit densities of 0.940 to 0.965 g/cm³, film-grade LLDPE has lower crystallinity, lower secant modulus, and higher puncture and tear resistance. HDPE is selected where stiffness, moisture-barrier contribution, and thermal resistance dominate; LLDPE is selected for stretch, puncture, and heat-seal performance. Metallocene-catalysed LLDPE is a distinct sub-class with a narrower short-chain branching distribution. At equivalent melt index and density, metallocene grades may show lower haze under ASTM D1003-21 and lower seal initiation temperature under ASTM F1921-12, but they may also raise extruder pressure and lower bubble stability on conventional blown film equipment.

    Parameter Test method Specification context for film-grade LLDPE
    Melt mass-flow rate ISO 1133-1:2022 / ASTM D1238-20 Blown film commonly 0.5–2.0 g/10 min; cast film commonly 2.0–4.0 g/10 min
    Density ISO 1183-1:2019 / ASTM D1505-18 0.918–0.930 g/cm³ for toughness-oriented film grades
    Dart impact resistance ASTM D1709-22 / ISO 7765-1:2004 Used for blown film quality control; values vary with gauge and comonomer type
    Elmendorf tear resistance ASTM D1922-23 / ISO 6383-2:1983 Measures directional tear propagation in machine and transverse directions
    Tensile properties ASTM D882-22 / ISO 527-3:2018 Secant modulus, yield stress, tensile strength, elongation at break
    Haze ASTM D1003-21 / ISO 14782:2021 Optical clarity control for packaging and agricultural film
    Gloss ASTM D2457-21 / ISO 2813:2014 Surface reflectance control for print-receptive webs
    Coefficient of friction ASTM D1894-14 / ISO 8295:1995 Controlled by slip and antiblock masterbatch in product formulation

    Hexene- and octene-based film-grade LLDPE resins are specified for sealant webs and high-toughness applications because longer comonomer branches increase tie-chain concentration in the amorphous phase. The sealant layer specification normally includes heat-seal strength, seal initiation temperature, hot-tack, and organoleptic performance. Food-contact status is established under FDA 21 CFR 177.1520(c) or the relevant positive list of EU Regulation No 10/2011. Organoleptic testing is required for high-temperature film extrusion or fatty food contact; residual hydrocarbon content and oxidation products are grade-sensitive. Published data for this specific configuration is limited unless a manufacturer datasheet is referenced, because seal initiation and hot-tack depend on film gauge, seal-jaw temperature, dwell time, and pressure.

    When Cast Film Neck-In and Draw Resonance Exceed Production Limits

    Cast film neck-in and draw resonance become process conflicts for film-grade LLDPE because the narrower molecular weight distribution and reduced shear thinning can generate high extensional forces across the die-to-chill-roll gap. Neck-in is measured as the percentage width reduction from die width to finished web width. For LLDPE cast film at an air gap of 5 to 15 mm, neck-in may be 15% to 30% depending on melt index, comonomer type, melt temperature, and vacuum-box contact. Draw resonance appears as periodic machine-direction thickness variation at high draw ratios and is influenced by chill roll temperature, air-knife position, and polymer relaxation time. Stable operation is typically restored by decreasing draw ratio, increasing melt temperature within 200 to 250 °C, or reducing die-lip shear stress with a fluoropolymer processing aid at 200 to 800 mg/kg. Edge trim and neck-in losses are recorded in production logs and compared with the material specification to distinguish polymer lot shifts from mechanical misalignment.

    Multilayer Coextrusion Die Systems and Layer-Ratio Limits

    Multilayer coextrusion combines film-grade LLDPE with ethylene-vinyl alcohol, polyamide, or tie resins to create barrier packaging structures. The LLDPE-rich skins provide sealability, toughness, and stretch; the core barrier layer is typically kept below 40% of total thickness to maintain bubble stability. On a three-layer blown film line with a 350 mm spiral mandrel die and 2.0 mm die gap, separate extruder temperature zones are required because LLDPE melt temperatures of 220 to 240 °C may exceed the processing window of the barrier resin. Interfacial instability is influenced by viscosity ratio, layer thickness, and die geometry; no single numerical limit applies across all die systems. When the viscosity mismatch is too high, gauge variation and interfacial waviness increase, and the edge-lamination quality of the finished web deteriorates. Coextrusion feedblock and spiral mandrel design are therefore specified alongside the polymer grades in the product qualification record.

    Top