| HS Code | 749606 |
| Density | 0.915 - 0.941 g/cm³ |
| Melt Flow Rate | 0.5 - 5 g/10 min |
| Melting Point | 120 - 130 °C |
| Crystallinity | 35 - 55 % |
| Tensile Strength At Yield | 8 - 20 MPa |
| Tensile Strength At Break | 15 - 35 MPa |
| Elongation At Break | 300 - 900 % |
| Flexural Modulus | 200 - 800 MPa |
| Notched Izod Impact Strength | 50 - 500 J/m |
| Vicat Softening Point | 90 - 110 °C |
| Linear Thermal Expansion Coefficient | 1.5 - 2.5 ×10^-4 /°C |
| Specific Heat Capacity | 1.9 - 2.3 J/g·°C |
| Thermal Conductivity | 0.3 - 0.5 W/m·K |
| Water Absorption 24 Hr | < 0.01 % |
| Dielectric Constant At 1 Mhz | 2.2 - 2.4 |
| Volume Resistivity | > 10^15 ohm·cm |
As an accredited Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Linear Low Density Polyethylene (LLDPE) Extrusion Grade is supplied in 25 kg polyethylene bags and 1,000 kg bulk bags, palletized. |
| Container Loading (20′ FCL) | 20′ FCL loading for Linear Low Density Polyethylene (LLDPE), Extrusion Grade: typically 25-kg bags, palletized or floor-loaded, around 20–25 tonnes. |
| Shipping | LLDPE extrusion grade ships as non-hazardous solid resin pellets. Standard packaging includes 25 kg bags, bulk bags, octabins, bulk trucks, or railcars. Keep containers clean, dry, and closed, away from heat, moisture, and direct sunlight. No special ventilation or hazardous-materials placards are typically required; follow local transport regulations. |
| Storage | Store LLDPE extrusion grade in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizing agents. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Keep away from food, drink, and animal feed. Ensure proper grounding during conveying to prevent static buildup. Follow manufacturer instructions. |
| Shelf Life | LLDPE extrusion grade has indefinite shelf life when stored cool, dry, well-ventilated, away from direct sunlight, heat, moisture, and contaminants. |
Monoextrusion of an 0.920 g/cm³ octene-based LLDPE with an MFI of 0.8–1.0 g/10 min at 190 °C/2.16 kg has displaced part of the LDPE fraction on heavy-duty sack and agricultural film lines because of improved Elmendorf tear and dart impact at comparable gauge. The blend is dry-blended rather than compounded: 20–40 wt% LLDPE is combined with 60–80 wt% LDPE on a single-screw extruder having an L/D of 24:1–30:1 and a barrier feed section. The annular die gap is held at 1.8–2.5 mm, blow-up ratio is set between 2.0:1 and 2.8:1, and frost line position is maintained 5–8 die diameters above the air ring. Melt temperature is kept within 185–215 °C because LLDPE generates higher head pressure than autoclave LDPE and can produce sharkskin melt fracture at the die lip; a fluoropolymer processing aid at 300–800 ppm is therefore dry-dosed to reduce surface drag. The formed film is tested under ASTM D1709-22 for dart impact, ASTM D1922-15 for Elmendorf tear, and ASTM D882-18 for tensile at break. Food-contact batches reference FDA 21 CFR 177.1520 and EU 10/2011.
At addition levels above 40 wt%, bubble stability deteriorates on conventional low-stalk lines unless air ring and internal bubble cooling are adjusted. In high-stalk film operations, LLDPE fractions above 30 wt% can destabilise the neck because melt strength is lower than in autoclave LDPE; the preferred modification is to use 10–20 wt% of a hexene-based LLDPE rather than a butene grade when tear propagation resistance is critical. The operational boundary is a frost line position within ±1 die diameter of the validated setting. Larger deviations produce gauge bands and machine-direction tear sensitivity. Silage and mulch film variants typically contain carbon black masterbatch at 2.0–2.5 wt% for UV resistance, but the same loading raises melt viscosity and narrows the bubble window at high output.
Cast stretch film formulations use a 0.912–0.918 g/cm³ hexene-based LLDPE with an MFI of 2.5–5.0 g/10 min as the major resin, and a metallocene LLDPE or plastomer at 10–25 wt% for puncture and cling. The melt is pumped through a 30:1 L/D barrier screw to a slot die with a lip gap of 0.9–1.5 mm, an air gap of 20–40 mm, and a chill roll held at 15–25 °C. Line speed is not limited by extruder output alone; it is constrained by melt resonance and die-lip buildup when MFI falls below 3.0 g/10 min or when melt temperature exceeds 260–280 °C and generates volatile degradation products. A fluoropolymer processing aid at 200–600 ppm reduces die-lip accumulation, but the die must still be cleaned on the cycle established for plate-out. Final 23 µm film is tested for puncture propagation under ASTM D5748-19 and tensile at break under ASTM D882-18.
At 23 µm machine film, pre-stretch above 200–300% on high-speed wrappers shifts failure from puncture to transverse-direction tear. The limiting factor is frequently the comonomer type rather than film gauge. Production records show that changing from a butene-based grade to a hexene-based grade alters the on-machine stretch and tear balance, but no single published conversion factor applies across all film lines because chill roll temperature, core speed, and prestretch roller geometry interact. The chill roll process window is ±5 °C; below 10 °C condensation can form and create surface defects, while above 30 °C film blocking reduces roll unwind and increases dart impact variability. Published data for this specific configuration is limited without a defined line audit.
On a tandem extrusion coating and lamination line, an 0.918–0.920 g/cm³ octene-based LLDPE with an MFI of 7.0–10.0 g/10 min at 190 °C/2.16 kg is used as the sealant web on paperboard, aluminium foil, and oriented polyester. The resin is processed at 280–310 °C melt temperature through a slot die with a 0.8–1.2 mm lip gap and coated at 18–25 g/m² onto a corona-treated substrate. The principal defect is neck-in; at line speeds above 150–300 m/min, the melt curtain narrows at the die ends and produces heavy edges. Converters therefore blend 20–40 wt% LDPE into the LLDPE sealant layer or use internally cooled edge decks to hold neck-in within 50 mm per side. Adhesion to aluminium foil is checked by peel strength under ASTM D1876-15, and seal initiation is checked by hot-tack testing under ASTM F1921-18.
Because the sealant layer is direct food-contact in liquid packaging, the grade must comply with FDA 21 CFR 177.1520 and EU 10/2011, including overall migration limits of 10 mg/dm² for food-contact conditions. The same line may produce a 15–25 µm sealant on retort and hot-fill structures; here the LLDPE layer is often blended with 10–15 wt% polybutene-1 or a plastomer to improve seal-through-contamination performance. Wet feedstock is a process hazard: pre-drying is not normally required below 60% relative humidity, but surface moisture above 0.05 wt% from outdoor silo storage produces splay in the curtain and adhesion loss on foil.
A 0.8–3.0 mm thermoformable sheet containing 20–40 wt% post-consumer LDPE/LLDPE reclaim is extruded on a 30:1–36:1 L/D single-screw line with a two-stage vented screw. The flat die is set at 1.0–1.5 mm for the target sheet gauge, and the three-roll stack is maintained at 75–95 °C to control sheet flatness. Melt temperature is held between 210–240 °C; exceeding 250 °C increases odour and gels from the reclaim fraction and narrows the thermoforming window. Thermoforming is run at a sheet surface temperature of 140–160 °C with plug-assist ratios between 1.5:1 and 3.0:1. The formed parts are typically industrial dunnage trays, collapsible containers, and automotive trunk liners. Tensile properties are measured under ISO 527-3:2018, and density under ISO 1183-1:2019.
The limitation of LLDPE-rich sheet is lower flexural modulus than a comparable HDPE sheet. At a density of 0.935 g/cm³, the secant modulus remains below that of a 0.950 g/cm³ HDPE grade; designers compensate by increasing sheet thickness 10–20% instead of changing resin, but this increases cycle time. The vacuum forming line runs at lower clamp tonnage than HDPE, and heating banks are set to a delta of ±10 °C across the sheet to avoid sagging. If regrind content exceeds 40 wt%, sheet surface typically shows pinholes and black specks that violate accepted quality limits for food-contact dunnage under FDA 21 CFR 177.1520.
| Application segment | Normative anchor | Test method / parameter | Typical process window |
|---|---|---|---|
| Blown film heavy-duty sack | FDA 21 CFR 177.1520; EU 10/2011 | ASTM D1709-22 dart impact; ASTM D1922-15 Elmendorf tear | 185–215 °C melt; 1.8–2.5 mm die gap |
| Cast stretch film | ASTM D5748-19; ASTM D882-18 | Puncture propagation; tensile at break | 20–40 mm air gap; 15–25 °C chill roll |
| Extrusion coating sealant web | FDA 21 CFR 177.1520; EU 10/2011 | ASTM F1921-18 hot tack; ASTM D1876-15 peel | 280–310 °C melt; 18–25 g/m² coat weight |
| Sheet / thermoforming | ISO 527-3:2018; ISO 1183-1:2019 | Tensile properties; density | 210–240 °C melt; 75–95 °C roll stack |
| LLDPE geomembrane | GRI-GM17 | ASTM D6693-16 tensile; ASTM D4833-07 puncture | 200–230 °C melt; 0.75–3.0 mm sheet |
For LLDPE geomembrane sheet produced on a flat die and three-roll stack, density is specified between 0.932 g/cm³ and 0.939 g/cm³ under ISO 1183-1:2019. The melt is extruded at 200–230 °C through a 1.5–2.5 mm die gap and calendered into a 0.75–3.0 mm sheet at widths up to 10.5 m. The lower density ceiling distinguishes LLDPE from HDPE geomembrane grades; crossing 0.940 g/cm³ changes flexural stiffness and can invalidate smooth-film bending assumptions under the same installation conditions. Production quality is controlled under GRI-GM17 for LLDPE geomembranes, with tensile properties measured by ASTM D6693-16, puncture by ASTM D4833-07, and thickness by ASTM D5199-12(2019).
Sheet flatness is managed by roll temperatures of 60–90 °C and an air gap of 10–30 mm; excessive roll speed differential creates transverse tensile stress and can preset wrinkles during field unrolling. The extrusion line uses automatic gauge control linked to an 8–10 point scanning frame, because a thickness deviation of ±10% exceeds allowable variation for seam strength. Welding and seam testing follow the fabricator’s project specification; no single ISO number applies to all seams. Low-temperature brittleness must be verified on the candidate sheet under ASTM D746-20 rather than assumed from density.
Grooved-feed single-screw lines process extrusion-grade LLDPE with a density of 0.918–0.930 g/cm³ and an MFI of 0.5–1.0 g/10 min at 190 °C/2.16 kg for low-pressure agricultural irrigation conduits. The die head is held at 190–210 °C and the melt is pulled through a vacuum calibration tank at −0.06 to −0.08 MPa with water temperature of 20–35 °C. The product is typically a 6–20 mm outside diameter lateral with a wall thickness of 0.5–1.0 mm, used for integral drip lines and micro-irrigation conduit. Carbon black masterbatch at 2.0–2.5 wt% provides UV stabilization, and the formulation requires a hindered phenol/phosphite antioxidant package at 500–1500 ppm to prevent oxidative degradation during extrusion.
The pipe is not specified for potable water pressure mains under ISO 4427; it is restricted to agricultural and low-pressure suction/drain duty. Product dimensions are checked against the manufacturer’s internal specification and, where applicable, emitter spacing and flow-rate uniformity under ISO 9261. A key processing limitation is melt strength: wall thickness below 0.5 mm can tear at the sizer entry unless line speed is reduced or melt temperature is lowered to 185 °C. Repeatability of outer diameter within ±0.15 mm is required for barbed fittings; batch-to-batch MFI variation of ±0.2 g/10 min changes head pressure and must be corrected by screw speed adjustment, not by raising barrel temperatures above 220 °C.
Competitive Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Linear low density polyethylene (LLDPE) designated as extrusion grade is a copolymer of ethylene with a C4–C8 α-olefin produced in low-pressure gas-phase, solution, or slurry processes. The product class is specified by a density band of 0.916–0.940 g/cm³ measured under ASTM D1505-18, a peak melting range of 118–126 °C by differential scanning calorimetry at 10 K/min under ISO 11357-3:2018, and a melt index range of 0.3–12 g/10 min at 190 °C and 2.16 kg according to ASTM D1238-20 or ISO 1133-1:2022. Blown film grades occupy the lower melt-index segment from 0.5 g/10 min to 2.0 g/10 min; cast stretch film grades from 2.0 g/10 min to 5.0 g/10 min; extrusion coating and thin-wall sheet grades may extend to 12 g/10 min. The resin identification code is 4 under ASTM D7611/D7611M-21. Unlike high-pressure low-density polyethylene, extrusion-grade LLDPE gains short-chain branches from comonomer insertion rather than from intramolecular chain transfer, producing a linear backbone with controlled branch length and placement. Extrusion-grade LLDPE therefore exhibits lower melt strength than an equivalent-melt-index LDPE but higher tensile strength under ASTM D882-18, puncture resistance under ASTM D5748-19, and downgaged seal strength under ASTM F88/F88M-15.
Screw design for extrusion-grade LLDPE typically specifies a 24:1 to 36:1 length/diameter ratio, with a barrier section and a Maddock or spiral mixer in the metering zone. Feed-section cooling is maintained at 60–90 °C to prevent premature melting and stagnation of hard pellets in the feed throat. Barrel temperature profiles are set in a rising sequence from 170 °C behind the feed zone to 210 °C at the adapter; the die temperature may be 210–230 °C for blown film and 260–290 °C for cast film. Because LLDPE has a narrower molecular weight distribution, its shear stress at the barrel wall remains higher than LDPE; motor load often becomes limiting before melt temperature exceeds 220 °C on a low-shear screw.
The first practical distinction is density: extrusion-grade LLDPE is specified between 0.916 g/cm³ and 0.940 g/cm³, while HDPE exceeds 0.940 g/cm³ and high-pressure LDPE often spans 0.912–0.930 g/cm³. The second distinction is branching architecture. LLDPE contains short-chain branches from 10 to 40 per 1000 backbone carbon atoms depending on comonomer content, whereas LDPE contains a broader distribution of short and long branches and HDPE carries minimal branches. Capillary rheometry under ASTM D3835-16 shows that LLDPE has lower shear-thinning sensitivity; pressures at high apparent shear rate remain closer to Newtonian than high-pressure LDPE. This means extrusion-grade LLDPE consumes more drive motor torque and generates higher head pressure at a given screw speed, but it gives better solid-state mechanical performance and heat-seal hot-tack at reduced thickness.
| Property | Test method | Extrusion-grade LLDPE | High-pressure LDPE | HDPE |
|---|---|---|---|---|
| Density | ASTM D1505-18 | 0.916–0.940 g/cm³ | 0.912–0.930 g/cm³ | 0.941–0.970 g/cm³ |
| Melt index | ASTM D1238-20 / ISO 1133-1:2022 | 0.3–12 g/10 min | 0.2–30 g/10 min | 0.05–50 g/10 min |
| Vicat softening temperature | ASTM D1525-17e1 | 85–100 °C | 80–95 °C | 120–130 °C |
| Heat seal initiation temperature | ASTM F88/F88M-15 | 95–110 °C | 105–120 °C | not heat sealable for flexible packaging |
| Short-chain branching | FTIR or 13C NMR | 10–40 per 1000 C | broad short/long distribution | <2 per 1000 C |
Fusion enthalpies for extrusion-grade LLDPE measured under ISO 11357-3:2018 typically range from 100 J/g to 140 J/g, lower than HDPE and consistent with a semicrystalline structure whose stiffness and toughness can be balanced by comonomer content. Extrusion-grade LLDPE is used as the sealant layer in three-layer and five-layer blown film dies, where it is paired with a high-pressure LDPE or HDPE structural layer. Seal initiation temperature is normally 95–110 °C; hot-tack strength remains above 4 N/25 mm over a sealing window of 20–40 °C when evaluated under ASTM F1921-12. This permits jaw speed increases of 20–30 cycles/min on vertical form-fill-seal machines compared with LDPE sealant webs, although the actual window is grade-specific and depends on slip and antiblock loading.
Grade nomenclature typically contains density and melt-index flags, such as LLDPE 1.0/0.918, where the first number is the nominal melt index in grams per 10 minutes and the second is the nominal density in grams per cubic centimetre. This convention permits downstream converters to compare grades from different manufacturers without brand-specific terminology.
The comonomer type determines the short-chain branch length: butene introduces ethyl branches, hexene introduces butyl branches, and octene introduces hexyl branches. These branch lengths alter the tie-chain concentration participating in load transfer across the crystalline lamellae. At a fixed density of 0.918 g/cm³ and melt index of 1.0 g/10 min, a switch from butene to hexene commonly raises dart drop impact strength by 20–35 % under ASTM D1709-16 and transverse-direction Elmendorf tear strength by 15–30 % under ASTM D1922-15; published data for this specific configuration is limited outside resin manufacturer datasheets. Octene-based grades are used when film elongation at break must exceed 500 % in both machine and transverse directions under ASTM D882-18, and when stretch film requires a lower density without sacrificing tensile strength. The processing window narrows with increasing comonomer length because melt elasticity declines; stable bubble operation on an octene blown film line may require a die gap of 2.0–2.5 mm, a blow-up ratio of 2.0:1 to 3.0:1, and a frost line height of 5–8 times the die diameter on a 30:1 barrier screw at melt temperature 190–210 °C. Butene grades tolerate lower frost line heights and slightly narrower die gaps with fewer bubble stability failures.
Metallocene-catalyzed extrusion-grade LLDPE further narrows molecular weight distribution to a polydispersity index below 2.5, which improves optics and seal threshold but reduces extruder output because of higher viscosity at low shear. On a cast film line, the die pressure increase relative to Ziegler-Natta LLDPE may be 15–25 %, and a fluoropolymer processing aid is normally required at 400–800 ppm to suppress sharkskin. These narrow-distribution grades also exhibit a lower critical shear rate for melt fracture, so die lip shear must be managed more tightly than for conventional Ziegler-Natta LLDPE.
Where cast stretch film lines run above 150 m/min, the selected extrusion-grade LLDPE typically has a melt index of 2.5–4.0 g/10 min and a density of 0.917–0.920 g/cm³. The flat die gap is set at 0.3–0.6 mm, the chill roll is maintained at 20–35 °C, and an air-knife or vacuum box pins the melt curtain to prevent neck-in. Melt temperature should remain below 290 °C because oxidative degradation increases gel count and reduces optical clarity under ASTM D1003-13. High-speed cast lines generally use a barrier screw with a length/diameter ratio of 30:1 to 36:1 and a screen pack of 40/60/80 mesh to protect the die lip from aggregated additives and cross-linked gels.
For pipe, geomembrane, and cable jacket applications, extrusion-grade LLDPE is shifted to the upper end of the density range, from 0.930 g/cm³ to 0.940 g/cm³, and may be dry blended with a carbon black masterbatch at 2.0–2.5 wt% to meet the outdoor weathering classification requirements of ASTM D3350-21. In geomembrane sheet extrusion, the polishing stack and haul-off must compensate for lower sag resistance than HDPE; edge trim generated at the die can be higher because the narrower molecular weight distribution promotes neck-in before the first chill roll. Cable jacketing grades require oxidative induction time above 20 min at 200 °C under ISO 11357-6:2018 when measured on plaques with the production antioxidant package. In these applications, hopper-drying of regrind at 70–80 °C for 2–4 h is applied when ambient relative humidity exceeds 60%, because surface moisture on regrind and masterbatch can cause feed bridging and output variation.
| Compliance area | Standard or regulation | Extrusion-grade LLDPE condition |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520 | Olefin polymer; extraction limits per paragraph (c); density below 0.94 g/cm³ for relevant clearance categories |
| EU food contact overall migration | EU 10/2011 Annex V | 10 mg/dm² for film; 60 mg/kg for general food |
| REACH SVHC declaration | Regulation (EC) No 1907/2006 | SVHC content below 0.10 wt% in the finished article |
| RoHS restricted substances | Directive 2011/65/EU | Cd <100 ppm; Pb <1000 ppm; Hg <1000 ppm; Cr(VI) <1000 ppm |
Process conflicts in blown film often appear as helical instability at the frost line, not as melt fracture at the die lip. Because extrusion-grade LLDPE has a narrower molecular weight distribution and lower melt tension than LDPE, the upper stable output limit on a 65 mm grooved-barrel extruder may be reached at bubble deformation 5–8 times die diameter; above this, gauge variation can exceed ±8% on in-line film thickness profiling. Die lip shear rate should be kept below the critical shear rate for sharkskin, commonly between 400 s⁻¹ and 600 s⁻¹ for narrow-molecular-weight grades. When pressure differential across the screen pack exceeds 25 MPa, gel defects and melt-temperature nonuniformity increase; screen pack change is required. The use of internal bubble cooling can extend stable output by lowering bubble temperature, but the frost line height must then be actively controlled to avoid condensation on the inner bubble surface. Addition of recycled trim above 20 wt% can further reduce bubble stability because oxidized gel seeds and mixed melt fractions disturb the frost line; at high recycled content, screen pack differential pressure quickly becomes the controlling maintenance interval.
Because the extensional viscosities of extrusion-grade LLDPE do not show the strain-hardening plateau observed in high-pressure LDPE, additive selection is narrow. Fluoropolymer processing aids at 400–800 ppm suppress sharkskin but can reduce surface energy; corona treatment to 40–45 dyn/cm under ASTM D2578-17 is usually required before lamination or printing. Low-molecular-weight amine antistats above 0.10 wt% can bloom to the seal layer and reduce heat seal strength below 10 N/25 mm when tested under ASTM F88/F88M-15. These operational boundaries, rather than mechanical strength limits, frequently define the usable envelope for extrusion-grade LLDPE in high-speed packaging lines.