Overview Of Materials For Linear Low Density Polyethylene Lldpe Butene Film

Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film

    • Product Name: Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 131276
    Material Type Linear Low Density Polyethylene (LLDPE)/Butene, Film
    Density 0.920 - 0.935 g/cm³
    Melt Flow Rate 0.5 - 3.0 g/10 min
    Melting Point 120 - 130 °C
    Vicat Softening Point 90 - 110 °C
    Tensile Strength At Yield 8 - 15 MPa
    Tensile Strength At Break 20 - 40 MPa
    Elongation At Break 500 - 800 %
    Tensile Modulus 0.200 - 0.500 GPa
    Flexural Modulus 0.200 - 0.500 GPa
    Tear Strength 200 - 500 g/mil
    Dart Drop Impact 100 - 300 g
    Haze 5 - 15 %
    Gloss 50 - 90 %
    Coefficient Of Friction 0.20 - 0.50
    Water Absorption < 0.010 %
    Dielectric Constant 2.3
    Volume Resistivity > 1e15 ohm-cm

    As an accredited Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Linear Low Density Polyethylene (LLDPE)/Butene Film supplied in 25 kg sealed bags, palletized and stretch-wrapped for secure industrial transport.
    Container Loading (20′ FCL) Maximum load for a 20-foot full container load: approximately 18–20 metric tons of LLDPE/Butene film, based on packaging and volume.
    Shipping Linear low density polyethylene (LLDPE)/butene film is shipped as a non-hazardous solid, typically in rolls, pallets, or bags. Store and transport in dry, clean, covered containers away from heat, sunlight, sharp objects, and incompatible chemicals. No special hazard classification is required; handle carefully to prevent tears and contamination.
    Storage Store LLDPE/Butene film in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep in original, sealed packaging on pallets to prevent moisture, dust, and physical damage. Avoid prolonged UV exposure and extreme temperatures. Maintain clear aisles; stack safely to prevent crushing or deformation. No special ventilation is normally required.
    Shelf Life LLDPE/butene film has no defined shelf life when stored cool, dry, and out of direct sunlight; properties remain stable for years.
    Application of Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film

    In cast pallet-wrapping lines operating at 300–600 m/min, butene-copolymer LLDPE with a density of 0.918–0.922 g/cm³ and a melt index of 0.8–2.0 g/10 min under ASTM D1238 at 190°C/2.16 kg is extruded through a slot die onto a chill roll held between 18°C and 30°C. On cast film lines equipped with screw diameters of 75–150 mm, 30:1–36:1 L/D barrier screws, and die gaps of 0.5–0.8 mm, the butene comonomer provides sufficient molecular weight distribution breadth for acceptable draw-down but less strain hardening than octene-copolymer LLDPE. Pallet stretch film is produced at 10–20 µm thickness with additive packages that include polyisobutylene or ultra-low-density ethylene copolymer cling concentrate at 0.5–2.0 wt%, erucamide slip at 500–1500 ppm, and synthetic silica antiblock at 1000–3000 ppm. Tensile properties measured under ASTM D882 typically show elongation at break of 300–500% in the machine direction. Dart impact for 20 µm monolayer cast film generally falls between 150 g and 300 g under ASTM D1709 Method A. Coefficient of friction values after additive bloom stabilize between 0.20 and 0.50 under ASTM D1894, while cling force is measured on pre-stretched film under ASTM D5458. Pre-stretch capability on powered wrapper carriages is typically limited to 150–250%; above 300% ultimate stretch, butene LLDPE grades often fail through local puncture propagation or edge tear because their short-chain branching does not generate the same network strain hardening as higher alpha-olefin copolymers. No pre-drying is required under normal indoor storage, but pellet surface moisture above 0.05 wt% can produce splay defects at melt temperatures above 250°C. The operational boundary for downgauging below 12 µm is controlled by cling uniformity and cast edge stability rather than tensile strength alone.

    What Limits Hot Tack Strength in Butene LLDPE Sealant Webs When HFFS Equipment Exceeds 40 Cycles per Minute?

    On horizontal form-fill-seal lines running more than 40 cycles/min, heat seal dwell declines below 0.3 s, making hot tack the controlling variable for package integrity. A blown butene LLDPE sealant layer of 15–35 µm exhibits seal initiation between 95°C and 110°C and peak hot tack between 120°C and 140°C, measured under ASTM F1921 and ASTM F88. Seal strength at 130°C, 0.5 s dwell, and 0.4 N/mm² jaw pressure commonly ranges from 3.0 N/15 mm to 6.0 N/15 mm, depending on web thickness and seal bar geometry. The process conflict is that higher seal-bar temperatures increase seal strength but can induce film puckering if the web lacks dimensional stability; lower seal initiation requires density reduction or coextrusion with ethylene-vinyl acetate containing 6–12% vinyl acetate or a plastomer. Three-layer and five-layer lines can place the butene LLDPE in the sealant skin while retaining stiffness in the core. Food-contact use requires compliance with FDA 21 CFR 177.1520(c) under Conditions of Use A through H and with EU 10/2011 overall migration below 10 mg/dm². The lower elongation at break and tear resistance of butene LLDPE relative to octene LLDPE are generally acceptable in HFFS snack and dry-food packages, but high-speed vertical form-fill-seal applications with heavy fill weights above 500 g may require a minor plastomer addition to maintain seal-through-contamination performance. Seal bar pressure must be maintained within 0.3–0.7 N/mm² because excessive pressure thins the molten sealant and reduces local seal thickness, producing channel leakers at side gussets.

    Food-contact compliance matrix for butene LLDPE sealant webs
    RegulationScopeTest or clauseLimit
    FDA 21 CFR 177.1520(c)Olefin polymers in contact with foodDensity, melt index, and extraction specificationsConditions of Use A through H
    EU 10/2011Plastic materials and articles intended for food contactOverall migration and specific migration10 mg/dm² or 60 mg/kg
    REACHSVHC screening and Annex XVII restrictionsArticle 33 communicationSVHC above 0.1 wt% triggers declaration

    Tubular agricultural film lines running butene LLDPE at blow-up ratios of 2.0:1–3.0:1 are used for silage wrap, greenhouse covers, and black mulch. In silage wrap, a three-layer structure with 60–80 wt% butene LLDPE and an EVA or metallocene skin at 25–45 µm total thickness provides puncture resistance during baling and sufficient oxygen barrier for short-season ensiling. Oxygen transmission for 25 µm monolayer butene LLDPE under ASTM D3985 at 23°C and 0% RH is generally 1800–3500 cm³/(m²·day·atm), depending on crystallinity and additive loading; for extended storage beyond 12 months, a barrier coextrusion is required. Greenhouse films at 100–200 µm use a hindered amine light stabilizer package of 0.2–0.6 wt% plus a UV absorber at 0.1–0.3 wt%, and light transmission measured under ASTM D1003 remains above 85% with haze below 20% when a clean antiblock package is used. Black mulch film at 15–30 µm with carbon black masterbatch at 2–4 wt% must retain tensile strength above 20 MPa under ASTM D882 after installation. On the production line, die gap is set at 1.5–2.5 mm, melt temperature is limited to 185–210°C, and the frost line is held at approximately 6–10 times the die diameter to reduce MD/TD orientation imbalance. The operational boundary is clear: monolayer butene LLDPE greenhouse film without sufficient HALS will embrittle before 2 years in south-facing installations; published long-term UV data for butene-copolymer film exposed under ISO 4892-2 cycles is limited, so outdoor validation remains required for specific geographic sites.

    Heavy-duty sack film line configurations with internal bubble cooling bypass the melt strength ceiling of butene comonomer.

    Monolayer and three-layer heavy-duty sack films at 75–200 µm are extruded on grooved-feed blown film lines with screw diameters from 45 mm to 75 mm, L/D ratios of 25:1–30:1, and internal bubble cooling. Butene LLDPE provides high dart impact and tear resistance, but lower melt strength than high-pressure LDPE; therefore, 10–30 wt% LDPE is commonly added to stabilize the bubble at blow-up ratios of 1.8:1–2.5:1. Melt temperatures are held at 185–215°C, die gaps range from 1.6 mm to 2.4 mm, and output on a three-layer line can reach 150–300 kg/h depending on screw cooling capacity. Dart impact values for 100 µm monolayer butene LLDPE blown film typically range from 500 g to 900 g under ASTM D1709 Method B. Elmendorf tear under ASTM D1922 typically shows MD values of 120–300 g and TD values of 300–600 g, reflecting transverse orientation. For filled sacks of 10–50 kg, drop pack integrity is validated under ASTM D5276 or equivalent ISTA procedures. Impulse sealing uses seal bar temperatures of 150–180°C, dwell times of 0.5–1.5 s, and pressure of 0.5–1.0 N/mm². The main process conflict is additive loading: reprocessed in-plant trim at 10–25 wt% can be reintroduced, but above 30 wt% gels and dart impact variability increase; lower MI grades of 0.5–0.8 g/10 min improve toughness but raise extruder motor load and reduce throughput. Butene LLDPE sacks are not suitable for long-term outdoor exposure without a UV-stabilized outer layer because tear retention after solar exposure is lower than stabilized octene LLDPE in the same thickness.

    Representative mechanical property ranges by downstream application
    SegmentThicknessKey propertyTest methodTypical range
    Cast stretch film10–20 µmDart impactASTM D1709 Method A150–300 g
    Heavy-duty sack75–200 µmDart impact at 100 µmASTM D1709 Method B500–900 g
    Agricultural silage25–45 µmOxygen transmissionASTM D39851800–3500 cm³/(m²·day·atm)
    Breathable backsheet25–60 µmWater vapour transmissionASTM E96/E96M1000–5000 g/m²/day
    Collation shrink45–100 µmMD free shrinkISO 1461650–70%

    When Calcium Carbonate-Filled Butene LLDPE Is Stretched into Microporous Hygiene Backsheets

    Breathable hygiene backsheet production starts with cast film at 25–60 µm thickness from butene LLDPE containing 45–60 wt% stearate-coated calcium carbonate with a median particle size of 1.0–2.0 µm. The base resin uses an MI of 2.0–5.0 g/10 min to accept filler without excessive torque. The cast web is fed through a machine direction orientation unit with preheat roll temperatures between 50°C and 80°C, stretching roll temperatures between 70°C and 95°C, and annealing roll temperatures between 80°C and 100°C; the draw ratio is set from 2.0:1 to 4.0:1. Microvoid formation around the calcium carbonate particles produces a water vapour transmission rate under ASTM E96/E96M of 1000–5000 g/m²/day, with the upper range corresponding to lower basis weight and higher draw ratio. Opacity is raised with rutile TiO₂ at 1–3 wt%, and fluoropolymer processing aid at 0.05–0.2 wt% prevents melt fracture at high filler loadings. Tensile properties after orientation show MD break strength of 8–20 MPa and MD elongation of 50–150% under ASTM D882. The operational limit is web instability: if stretching temperature is below 60°C or calcium carbonate dispersion is poor, pinhole density increases and WVTR uniformity degrades across the web. Published pore size distribution data for butene-copolymer breathable films is limited, so process validation on specific MDO equipment is required. Precompounding of the calcium carbonate masterbatch on a twin-screw extruder with 30:1 L/D or longer is preferred to prevent agglomerates larger than 5 µm, which produce visible pinholes and lower hydrostatic head.

    For lamination sealant webs in snack-barrier structures and aseptic pouches, a butene LLDPE blown film of 20–50 µm is used as the innermost heat-seal layer. The material is selected because it offers higher seal strength and puncture resistance than LDPE at similar thickness, with seal initiation between 90°C and 110°C and plateau seal strength of 3.0–6.0 N/15 mm at 130°C, 0.5 s dwell, and 0.4 N/mm² pressure, measured under ASTM F88. Food-contact use requires compliance with FDA 21 CFR 177.1520(c) under Conditions of Use A through H and with EU 10/2011 overall migration below 10 mg/dm². The film surface is corona-treated to a wetting tension above 38 mN/m prior to solventless or solvent-based lamination; stored reels must be protected from high humidity because surface additives can migrate and reduce adhesion. Solventless adhesive systems with isocyanate and polyol chemistries are common, but the sealant web must be free of slip-additive bloom before lamination. A limitation is that butene LLDPE sealant layers can exhibit seal contamination sensitivity when packaging dusty powders; seal bar cleanliness and hot bar pressure must be monitored to prevent channel leakers. In retort or hot-fill structures, a higher temperature-resistant layer must carry mechanical load because butene LLDPE softens and loses seal creep resistance above 110°C.

    Tube Film Collation Shrink and Protective Packaging Orientation Balance

    Collation shrink bundling of bottled water and cans uses tube film at 45–100 µm thickness in which butene LLDPE is blended with high-pressure LDPE at 20–40 wt% to balance shrink force and dart impact. The film is produced on blown film towers with a blow-up ratio of 2.5:1–4.0:1 and a low frost line to generate high transverse orientation while retaining MD shrink. Shrink measurements under ISO 14616 or ASTM D2732 typically show TD free shrink of 10–20% and MD free shrink of 50–70% at 120–140°C. Butene LLDPE lowers shrink tension relative to LDPE but substantially improves Elmendorf tear and puncture resistance, which reduces corner failure during tunnel shrinking. Melt temperature is limited to 190–220°C, and an oscillating haul-off distributes gauge variation. The main operational risk is MD splitting when the frost line is set too low; the orientation balance must be verified by measuring shrink properties at multiple points across the web. Butene LLDPE is also limited in high-shrink force applications where tight bundling is required on low-speed tunnels, because its lower crystallinity and short-chain branching generate lower recovery force than LDPE at the same thickness. In such cases, the LDPE fraction is raised to 60–80 wt% and the butene LLDPE portion is retained primarily for dart impact improvement.

    Free Quote

    Competitive Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Film-grade linear low density polyethylene (LLDPE)/butene resins are ethylene/1-butene copolymers in which the short-chain branching comonomer is intentionally introduced during polymerisation to disrupt crystallinity and lower density. Commercial model designations typically encode density and melt index; for example, a grade labelled 0.918/1.0 denotes a nominal density of 0.918 g/cm³ and a melt mass-flow rate of 1.0 g/10 min. Blown-film grades are usually specified with a density of 0.918–0.922 g/cm³ according to ASTM D1505 or ISO 1183-1:2019 and a melt mass-flow rate of 0.8–1.2 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. The butene comonomer inserts ethyl branches along the polyethylene backbone; these branches are shorter than the butyl branches generated by 1-hexene and the hexyl branches generated by 1-octene. The resulting crystalline network contains fewer stress-transmitting tie chains and exhibits lower solid-state toughness than hexene- or octene-modified LLDPE of equivalent density and melt index. Conversely, the butene grades often retain broader processing latitude on standard blown film lines and are widely used in applications where gauge reduction below 20 µm is not the governing specification. Both Ziegler-Natta and metallocene-catalysed LLDPE/butene grades are commercially available; the metallocene versions show narrower molecular weight distribution, lower extractables, and improved puncture resistance at the same density.

    Table 1 lists representative physical property ranges for a general-purpose blown-film LLDPE/butene resin with density 0.918 g/cm³ and melt index 1.0 g/10 min, based on published datasheets and laboratory reports. Values are not a single product specification.

    PropertyTest methodTypical range
    DensityASTM D15050.917–0.920 g/cm³
    Melt indexISO 1133-1:20220.9–1.1 g/10 min
    Dart impact, 25 µm filmASTM D1709A80–130 g
    Elmendorf tear, MD, 25 µm filmASTM D1922350–550 g
    Elmendorf tear, TD, 25 µm filmASTM D1922250–400 g
    Tensile stress at break, MDASTM D88235–45 MPa
    Tensile stress at break, TDASTM D88228–38 MPa
    Elongation at break, MDASTM D882500–700%
    Elongation at break, TDASTM D882600–800%
    Haze, 25 µm filmASTM D10038–12%
    Gloss, 60°ASTM D245760–75 units
    Water vapour transmission rate, 25 µm at 38 °C/90% RHASTM F124918–22 g/m²·day
    Oxygen transmission rate, 25 µm at 23 °C/0% RHASTM D39853,000–4,500 cm³/m²·day

    Does Butene Short-Chain Branching Limit Film Toughness at High Line Speeds?

    The effect of butene on film toughness is measurable in high-speed packaging operations. For a 25 µm monolayer film, dart impact values under ASTM D1709A typically fall between 80 g and 130 g; equivalent-density LLDPE/octene films commonly exceed 150 g. On vertical form-fill-seal lines running above 120 packages/min, pinhole failures caused by abrasive contact with former shoulders and fill-tube surfaces are reported more frequently with butene-based films than with octene-based films of equal thickness. The shorter ethyl branch reduces tie-chain connectivity, which lowers the energy required for fibril rupture during rapid deformation. Down-gauging below 12 µm in printed overwrap applications is therefore possible only when the butene resin is blended with a tougher LLDPE/octene fraction or coextruded with high-strength skins. The property cliff-edge is particularly evident in machine-direction orientation at draw ratios above 5:1; draw resonance and transverse gauge variation increase when butene-rich formulations are processed on cast film lines equipped with 300 mm slot dies and 20–25 °C chill rolls.

    Seal initiation temperature for a 30 µm monolayer LLDPE/butene film is typically 95–105 °C when measured at 0.5 s dwell time and 0.275 MPa sealing pressure under ASTM F2029. Heat seal strength at 130 °C under ASTM F88 typically reaches 6–9 N/15 mm for the same thickness. Hot tack strength at 110 °C remains below that of an octene-based LLDPE of equivalent density because the butene comonomer forms fewer interlamellar entanglements in the melt-sealed region. Converters using vertical form-fill-seal machines with cycle times shorter than 90 packages/min should verify hot tack on the production unit; published data for this specific configuration is limited. Addition of LDPE at 20–30 wt% lowers seal initiation temperature by 3–5 °C, but narrows the hot tack plateau and reduces the maximum operating speed of the sealing jaw.

    Blown Film Processing Windows and Screw Design Requirements

    LLDPE/butene is typically processed on grooved-feed or smooth-bore blown film extruders with screw L/D ratios of 24:1 to 30:1. Barrier screws with dispersive mixing sections are preferred because the high-molecular-weight fraction can form micro-gels at melt temperatures above 230 °C. Die gaps of 1.2–2.0 mm support stable bubble formation at blow-up ratios of 2.0:1 to 3.0:1; gaps below 1.0 mm raise extrusion backpressure and promote melt-temperature excursions. Typical melt temperatures are 190–210 °C, with die temperatures maintained 5–10 °C above melt temperature to reduce surface roughness. Bubble stability at low gauge is lower than that of LDPE, so a blend with 10–20 wt% LDPE is common on lines producing film below 20 µm. For a 50 µm film produced at 100 kg/h on a 250 mm die, the frost line height is typically 250–350 mm; a frost line shorter than 200 mm increases haze and reduces machine-direction tear strength because of faster crystallisation and lower orientation relaxation.

    Water vapour transmission rate for a 25 µm monolayer LLDPE/butene film at 38 °C and 90% RH is generally 18–22 g/m²·day by ASTM F1249. Oxygen transmission rate at 23 °C and 0% RH is 3,000–4,500 cm³/m²·day by ASTM D3985. These values exclude the material from barrier-resin classification; coextrusion with EVOH or polyamide is required when oxygen transmission below 100 cm³/m²·day is specified. Optical behaviour under ASTM D1003 shows haze of 8–12% and 60° gloss of 60–75 units for 25 µm film. The ethyl branch has less influence on surface crystallisation than longer branches, so gloss retention is comparable to hexene-based LLDPE but below metallocene-catalysed hexene grades with narrower composition distribution.

    What Controls Tear Anisotropy in Blown LLDPE/Butene Film?

    The mechanical response of LLDPE/butene film is anisotropic because of the preferential orientation of lamellar crystals along the machine direction. At a blow-up ratio of 2.5:1, ASTM D1922 Elmendorf tear values for 25 µm film are commonly 350–550 g in MD and 250–400 g in TD. Tensile stress at break under ASTM D882 is typically 35–45 MPa in MD and 28–38 MPa in TD. Elongation at break is higher in TD, often 600–800%, compared with 500–700% in MD. Puncture resistance measured by ASTM D5748 on 25 µm film is typically 40–60 N/mm, depending on comonomer distribution and catalyst type. At −20 °C, dart impact retention is lower than that of LLDPE/octene by roughly 15–25 percentage points when both materials are compared at the same density and melt index; published data for this specific configuration is limited to laboratory-cast films and may not represent full-scale blown film output.

    Relative to LDPE, LLDPE/butene provides higher tensile strength and elongation at break but lower melt strength and poorer bubble stability at low gauge. Relative to LLDPE/hexene, the butene variant has lower dart impact and tear strength at equivalent density and melt index; hexene grades are commonly selected for heavy-duty sacks and frozen food packaging where ASTM D1709A dart impact above 140 g is required. Relative to LLDPE/octene, the butene product shows lower puncture resistance and lower hot tack strength, but is preferred in thick-film and agricultural applications where the toughness differential is less decisive and resin cost per kilogram is a primary specification. Metallocene-catalysed LLDPE/butene exhibits narrower molecular weight distribution, lower extractables, and improved organoleptic properties relative to Ziegler-Natta grades, although it may require higher head pressure and more precise temperature control on single-screw extruders.

    Heavy-duty sack and liner applications use LLDPE/butene in thicknesses of 80–150 µm where dart impact requirements are moderate. Tear strength by ASTM D1922 in 100 µm film remains anisotropic, with MD values commonly 800–1,200 g and TD values 600–900 g; the thicker cross-section compensates for the lower intrinsic toughness of butene relative to hexene grades. Agricultural mulch films in the 25–50 µm range use butene-based LLDPE blends with LDPE to improve melt strength; tensile elongation under ISO 527-3:2018 typically exceeds 600% before weathering. After outdoor exposure, the film must be formulated with the appropriate hindered amine light stabiliser package to maintain the elongation retention required by the target service life; published data for specific formulations is limited.

    When Butene Comonomer Replaces Octene in Stretch Film Formulations

    Substitution of octene-based LLDPE with LLDPE/butene in cast stretch film generally reduces puncture resistance and on-pallet load retention. At a prestretch ratio of 250% on rollers running at 700 mm/s, the stretch-force retention after 24 h decreases measurably when the butene grade exceeds 50 wt% of the resin blend. Ultimate stretch before break is also lower: cast film lines with 40 mm single-screw extruders and 250 mm slot dies typically reach 300–350% prestretch with butene-rich blends, whereas octene-rich formulations may exceed 400% before film break. Butene-containing films remain suitable for hand-wrap and bundling applications where elongational integrity at moderate prestretch is acceptable. In these applications, the film is generally down-gauged only to 15 µm; attempts to reach 10 µm with butene-rich formulations increase the frequency of edge tear and core failure during winding.

    The food-contact status of LLDPE/butene film is determined by the base resin and the additive package. Table 2 summarises the regulatory instruments commonly cited for monolayer and coextruded film structures.

    Regulatory instrumentClause or test methodApplication boundary
    FDA 21 CFR 177.1520Olefin polymers, subpart BFood contact, subject to density and extraction limitations
    EU No 10/2011Annex I, Table 1Overall migration limit 10 mg/dm²; specific migration limits for additives
    REACH Regulation (EC) 1907/2006Annex XVIIMonomer and additive restrictions for EU market
    RoHS Directive 2011/65/EUAnnex IIHeavy metal restrictions in non-food electrical applications

    Coextruded Hygiene Film Structures Use Butene-Based LLDPE as a Core-Layer Modifier

    In coextruded hygiene backsheet and topsheet constructions, LLDPE/butene is often placed in the core layer at 20–40 wt% to reduce raw-material cost while metallocene LLDPE or impact-modified polypropylene forms the skin layers. The butene-rich core contributes limited melt strength to the coextruded bubble; therefore, the outer layers must stabilise the bubble at blow-up ratios below 2.5:1. Elastic recovery after extension is lower than that of octene-based LLDPE, which influences softness and drape of the final laminate. On cast film lines, the viscosity of the butene core is matched to metallocene skin resins at melt temperatures of 220–240 °C; mismatched viscosities above 50 Pa·s at 100 s-1 shear rate can cause layer thickness variation exceeding 5%. Published data for this specific configuration is limited.