| HS Code | 145395 |
| Melt Index 190 C 2 16 Kg | 20 g/10 min |
| Density | 0.924 g/cm³ |
| Tensile Strength At Yield | 9.7 MPa |
| Tensile Strength At Break | 12.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 241 MPa |
| Vicat Softening Point | 94°C |
| Brittleness Temperature | < -70°C |
| Hardness Shore D | 50 |
| Environmental Stress Crack Resistance | >1000 h |
| Mold Shrinkage | 0.015-0.020 cm/cm |
| Coefficient Of Thermal Expansion | 1.7E-4 cm/cm/°C |
As an accredited NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaging: 25 kg polyethylene bags, palletized and shrink-wrapped, for NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags, 55 bags per pallet, 10 pallets per container, totaling 13.75 MT of Sclair® 8111 LLDPE resin. |
| Shipping | NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin is typically shipped as a non-hazardous solid in 25-kg polyethylene bags, palletized, stretch-wrapped, and labeled. Transport in clean, dry trucks or containers. Keep away from moisture, heat, direct sunlight, and sharp objects; follow applicable local and international regulations. |
| Storage | Store NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers. Use grounding/bonding where required to control static, and maintain good housekeeping to prevent pellet accumulation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Recommended shelf life is 24 months from manufacture when stored in original packaging under cool, dry conditions away from sunlight. |
High-flow linear low density polyethylene with a nominal melt flow index of 50 g/10 min at 190 °C and 2.16 kg load under ASTM D1238-23 and a nominal density of 0.924 g/cm³ under ASTM D792-20 is specified in refrigerated dairy cups, portion-control containers and hingeless snap-over lids where wall sections fall between 0.45 mm and 0.80 mm. On accumulator-assisted hydraulic injection molding machines of 120 t to 250 t clamp force fitted with a 20:1 L/D general-purpose polyolefin screw and a check-ring non-return valve, the resin is processed at barrel temperatures from 180 °C to 220 °C and mold temperatures from 10 °C to 25 °C. The injection phase is completed in less than 0.5 s for thin lids with flow lengths below 120 mm, after which hold pressure is applied at 50% to 65% of peak hydraulic pressure for 0.5 s to 1.5 s to gate-seal the part before ejector actuation. Food-contact compliance is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers and under EU Regulation (EU) No 10/2011 when overall migration is tested to a limit of 10 mg/dm² according to the EN 1186 series. Dairy-contact parts are screened for environmental stress crack resistance using ASTM D1693-21 condition A with 10% Igepal CO-630 at 50 °C; LLDPE in this density class typically exceeds 500 h without failure, but lot-specific confirmation for Sclair® 8111 is required because NOVA Chemicals’ published datasheet does not list ESCR for every batch configuration. Finished articles include hingeless snap-over lids with positive detent rings, tamper-evident tear strips and square dairy cups with stack ledges.
Replacement of HDPE with Sclair® 8111 in industrial pails, utility totes and reusable crates shifts the design basis from high flexural modulus toward higher environmental stress crack resistance and low-temperature impact. A 0.924 g/cm³ density LLDPE has a lower secant flexural modulus than conventional blast-molding or injection HDPE; sidewall deflections under stacking load are therefore managed by increasing vertical ribs, thickening corner columns or widening the top rim rather than relying on material stiffness alone. On medium-tonnage hydraulic machines of 250 t to 500 t clamp force with screw diameters between 60 mm and 80 mm and a 22:1 L/D barrier screw, the melt temperature is controlled at 200 °C to 230 °C and the mold at 15 °C to 35 °C. For pail wall sections of 2.0 mm to 3.5 mm, hold pressure is set from 40 MPa to 60 MPa, and cooling time is dominated by the square of wall thickness; a 3.0 mm wall may require 8 s to 12 s of post-fill cooling before ejection. Where greater top-load rigidity is required, Sclair® 8111 is dry blended with fractional-melt HDPE at 10% to 30% by weight, but this blend raises injection pressure and reduces the benefit of the high melt index. Outdoor crates and fish boxes require a hindered amine light stabilizer package at 0.20% to 0.40% by weight and a phenolic antioxidant at 0.05% to 0.10% by weight to withstand UV exposure and freezer handling; low-temperature brittleness is screened by ASTM D746-20, where LLDPE of this density class typically reports values below -70 °C. For food-ingredient pails, the same olefin polymer clearance under FDA 21 CFR 177.1520(c) applies; for dangerous goods pails, the molded article must pass the UN Model Regulations drop test from 1.2 m for packing group II and a stacking load of 1.2 times rated mass for 24 h at 40 °C. Finished products include reusable crates, fish handling boxes, utility totes and light industrial pails.
Closure applications use the 50 g/10 min melt index of Sclair® 8111 to fill long-flow, multi-cavity tools where seal beads and snap detents require complete replication. Multi-cavity food lids for wipe tubs, snap-on hoods for dry powder cans and overcaps for trigger sprayers are molded in cold-runner or hot-runner tools of 32 to 64 cavities; valve-gate hot runners prevent stringing and improve gate quality at high filling speeds. The melt is held at 195 °C to 225 °C and the mold at 10 °C to 30 °C; fill time is normally below 0.35 s per cavity to maintain a stable flow front across the seal lip. Post-fill pressure is applied at 45 MPa to 65 MPa to pack the annulus of the plug seal against the core, and gate freeze is confirmed by screw-recovery-pressure transition. Dimensional control is affected by mold shrinkage measured according to ASTM D955-21 on 3.2 mm plaques; closures in this density range require compensation for anisotropic shrinkage that can produce ovality in thread or snap-bead diameters. Food-contact closures are evaluated under FDA 21 CFR 177.1520(c) for olefin polymers; for pharmaceutical dry dosage closures, USP <661.1> physicochemical testing may be requested, but Sclair® 8111 is not supplied with medical device certification unless explicitly confirmed by NOVA Chemicals for the specific lot and application. The resin is not suitable for carbonated beverage closures because low oxygen barrier and stress relaxation permit seal-lip creep and product loss. Finished products include flexible snap-on lids, overcap housings and dry-product dispensing hoods.
In storage totes and domestic housewares, the injection molder observes lower switch-over pressure and reduced splay when Sclair® 8111 is processed at a melt temperature between 195 °C and 220 °C and a mold temperature between 15 °C and 30 °C. Houseware articles with nominal wall thickness from 1.5 mm to 2.5 mm use rib-to-wall ratios not exceeding 0.5:1 to avoid sink marks and to reduce the cycle-time penalty from thick intersections. Stackable totes and drawer organizers are designed with rim reinforcements because the lower flexural modulus of a 0.924 g/cm³ LLDPE allows sidewall creep under sustained load at warehouse temperatures near 40 °C. ESCR testing for household cleaners and surfactants uses ASTM D1693-21 condition A in 10% Igepal CO-630 at 50 °C; the density class resists stress cracking better than HDPE, which reduces field failure in laundry rooms and kitchen environments. Pigment concentrates are added at 2% to 3% by weight; the carrier polymer should be an LDPE or LLDPE grade to maintain low-temperature impact and food-contact status where required under FDA 21 CFR 177.1520(c). Finished articles include stackable storage bins, drawer dividers and household utility totes.
| Wall thickness class | Melt temperature | Mold temperature | Injection fill time | Hold pressure | Clamp force estimation |
|---|---|---|---|---|---|
| Thin-wall ≤0.8 mm | 180–220 °C | 10–25 °C | <0.5 s | 50–70 MPa | 4–6 kN/cm² projected area |
| Intermediate 1.0–2.5 mm | 195–230 °C | 15–35 °C | 0.5–1.5 s | 40–60 MPa | 3–4 kN/cm² projected area |
| Thick >2.5 mm | 200–230 °C | 20–40 °C | 1.0–3.0 s | 30–50 MPa | 2–3 kN/cm² projected area |
When flexible packaging lines move toward mono-material polyethylene structures for recyclability, injection-molded fitments made from Sclair® 8111 replace PP spouts and allow the entire pouch body and spout to enter a single PE recycle stream. The high melt index fills thin annular sections around the spout bore; fitments with bore diameters from 8 mm to 20 mm and wall thickness as low as 0.8 mm are produced on 60 t to 120 t injection machines with melt temperatures of 185 °C to 210 °C and mold temperatures of 10 °C to 25 °C. Heat sealing of the fitment to blown PE film is performed at bar temperatures from 140 °C to 170 °C, dwell times from 0.8 s to 2.0 s and seal pressures from 0.2 MPa to 0.5 MPa. Seal strength is measured under ASTM F88/F88M-23; acceptable values depend on pouch volume and drop requirements, but published data for Sclair® 8111 in spout heat-seal bonds is limited, so line-specific seal curves must be developed. The resin alone is not a high-barrier structure and is unsuitable for oxygen-sensitive products unless combined with a coated PE film or an EVOH layer that remains protected under recycle regulations. Finished products include spouts for refill pouches, fitments for home care packages and dispensing nozzles for dry food pouches.
Compounders use Sclair® 8111 as a carrier resin in colour and additive masterbatches where the target let-down ratio is 2% to 4% in injection molding and blow molding polyolefins. The carrier is fed through a co-rotating twin-screw extruder with a 40:1 L/D barrel and screw speeds from 800 rpm to 1,200 rpm; melt temperature is controlled at 180 °C to 210 °C to limit thermal degradation of azo colourants and hindered amine additives. A typical pigment black masterbatch uses 40% pigment loading, 30% carrier resin and 30% combined dispersants and processing aids; the 50 g/10 min melt index reduces melt pressure and increases wetting at high pigment concentration. Strand die pelletizing is maintained with strand temperatures below 220 °C and pellet lengths from 2.5 mm to 3.5 mm for consistent screw feeding. If the masterbatch is intended for food-contact packaging, the carrier must meet FDA 21 CFR 177.1520(c) and the pigments and additives must have their own food-contact authorizations under the relevant jurisdiction. Finished products include pelletized colour concentrates and additive masterbatches for polyolefin converters.
Competitive NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 8111 is a linear low-density polyethylene resin formulated for injection molding of thin-wall packaging, closures, overcaps, housewares, and general-purpose molded goods. The grade is supplied in pellet form and is characterized by a high melt flow rate that supports short filling times in multi-cavity tools and reduced injection pressure requirements. Under ASTM D1238, at 190°C with a 2.16 kg load, the typical melt flow rate is 20 g/10 min. Under ASTM D792, the typical density is approximately 0.924 g/cm³. These values identify the material as an injection-molding-specific LLDPE rather than a film or rotomolding grade, because the elevated melt flow rate is incompatible with stable film bubble formation but well suited to shear-thinning flow through gates and narrow wall sections.
Representative physical property values reported for this grade are listed below. They are not specification limits, and current manufacturer technical data should be consulted for lot-specific control ranges.
| Property | Test method | Typical value |
|---|---|---|
| Density | ASTM D792 | 0.924 g/cm³ |
| Melt flow rate | ASTM D1238, 190°C/2.16 kg | 20 g/10 min |
| Tensile strength at yield | ASTM D638 | 13 MPa |
| Tensile elongation at break | ASTM D638 | >800% |
| Flexural modulus, 1% secant | ASTM D790 | 220 MPa |
| Durometer hardness | ASTM D2240 | 52 Shore D |
| Vicat softening temperature | ASTM D1525 | 104°C |
These values should be interpreted as typical physical properties rather than design allowables. For load-bearing or safety-critical components, the converter should generate application-specific data at the intended service temperature, chemical environment, and weld-line location. The elongation value indicates a ductile failure mode under standard tensile conditions, but this behavior is rate-dependent and may be reduced by contamination, high regrind levels, sharp notch geometries, or exposure to oxidative environments.
The principal molecular distinction between Sclair® 8111 and lower-melt-index LLDPE grades is the deliberately elevated melt flow rate of 20 g/10 min. In a conventional butene LLDPE injection grade with a melt flow rate below 5 g/10 min, the higher viscosity produces greater frictional heating, higher injection pressure demand, and longer screw recovery time in a standard reciprocating screw. Sclair® 8111 shifts the processing envelope toward thin-wall filling and rapid cycling. The trade is that melt strength and some resistance to environmental stress cracking may be lower than a fractional-MI LLDPE of similar density. Published data for this specific configuration is limited, so comparative evaluations on the intended tool and part geometry are required before substitution.
Unlike high-pressure LDPE grades, which contain substantial long-chain branching, Sclair® 8111 possesses a predominantly linear backbone with short-chain branching. This structural difference alters shear-thinning response, extensional viscosity, and frozen-in molecular orientation. In practice, the linear architecture contributes to higher tensile yield strength and lower melt elasticity than a comparable high-pressure LDPE. That lower elasticity reduces die swell and can improve dimensional repeatability in injection molding, but it also reduces melt strength available for large unsupported flow fronts. The distinction becomes important when the same tool processes both LDPE and LLDPE: the LLDPE melt may fill at lower pressure but may also exhibit a different gate freeze-off time and a different post-mold shrinkage orientation.
Because the resin is supplied as a non-hygroscopic polyolefin, drying is not normally required before injection molding. However, if pellets are stored in conditions above 60% relative humidity or transferred from cold storage into a warm processing area, surface condensation may introduce moisture that appears as splay or surface silver streaks. In such cases, pre-drying at 70–80°C for 1–2 h in a desiccant dryer or circulated-air hopper dryer is sufficient to remove surface moisture. The resin should not be exposed to prolonged direct ultraviolet light during outdoor storage, because UV-induced chain scission can reduce molecular weight and shift melt flow rate.
In thin-wall closure production, the melt flow rate of 20 g/10 min becomes most relevant when wall thickness falls below 0.8 mm and flow length-to-wall-thickness ratios exceed 150:1. Under ASTM D1238 conditions, the high melt index is a single-point low-shear measurement; it does not fully describe injection-molding shear rates, which may reach 10,000 s⁻¹ or higher in narrow gates. Nevertheless, the value correlates with reduced filling pressure and faster cavity pressurization on equipment with sufficient injection velocity. Typical processing conditions for a 60 mm general-purpose reciprocating screw with a 20:1 L/D ratio and a compression ratio between 2.5:1 and 3.0:1 include barrel zone settings from approximately 160°C in the rear zone to 200–220°C at the nozzle. Mold temperatures of 10–40°C are common for LLDPE injection molding; lower mold temperatures reduce cycle time, while higher mold temperatures improve surface appearance and may reduce internal stress but extend cooling duration.
Back pressure should be kept low, typically 0.5–1.0 MPa, because the high melt-index material does not require aggressive shear mixing. High back pressure combined with fast screw speed can overheat the melt, produce localized oxidation at the screw tip, and cause yellowing or generation of acetic-acid-like odors. Screw speed for a 60 mm screw should generally be selected to maintain a stable melt cushion and complete screw recovery within the cooling phase. If screw recovery time is shorter than the cooling time, the screw tip may sit in hot melt for extended periods, increasing residence time and oxidation risk.
Clamp force requirements are not directly determined by melt flow rate; they depend on projected area and expected cavity pressure. In thin-wall closure tools, cavity pressures commonly range from 35–55 MPa depending on gate design, wall thickness, and packing intensity. A mold with a projected area of 0.1 m² and a cavity pressure of 40 MPa would require approximately 4,000 kN of clamp force, excluding safety margin. Sclair® 8111 may reduce the peak cavity pressure needed to fill the part compared with a lower-melt-index LLDPE, but the peak pressure remains highly dependent on injection speed and gate freeze-off. Therefore, changing from a fractional-MI LDPE to Sclair® 8111 on a live tool should be accompanied by a short-shot study and gate-seal study rather than an immediate reduction in clamp tonnage.
Regrind from sprues, runners, and rejected parts can be incorporated at typical levels of 20–30 wt% if the regrind is clean, dry, and generated from the same resin family. Higher regrind fractions can narrow the processing window, increase lot-to-lot flow variation, and reduce elongation at break. The use of mixed-color regrind, contamination with polypropylene overcaps, or repeated heat histories should be controlled because incompatible contamination can delaminate or create weld-line weakness. When measuring melt flow rate after regrind addition, the value may shift upward if chain scission has occurred or downward if crosslinking or high-viscosity contamination is present.
The substitution of Sclair® 8111 into a tool originally qualified with a 0.5–1.0 g/10 min LDPE requires attention to shot-size control and non-return valve leakage. Because the higher melt flow rate reduces melt viscosity, the screw tip non-return valve may allow greater backward flow during injection. A sliding-ring check valve with excessive clearance can produce shot-to-shot weight variation, especially at high injection speeds. Field observations on reciprocating-screw machines with 60–80 mm screw diameters indicate that non-return valve wear often appears as gradual cushion loss and part-weight drift rather than an immediate machine fault. On such tools, the cushion should be monitored continuously and the valve clearance inspected if weight dispersion exceeds ±0.5% of shot weight.
The lower melt elasticity of Sclair® 8111 can change gate-stringing or drool behavior in hot-runner systems. High-pressure LDPE with long-chain branching tends to exhibit more pronounced melt strength and can hold a gate seal more readily during decompression. Sclair® 8111 may require more aggressive screw decompression or melt decompression at the hot runner to prevent nozzle drool. The appropriate suck-back distance is tool-specific, but values between 2–5 mm on the injection screw are common starting points. Excessive decompression can introduce air into the melt stream, producing splay or unstable pressure in the next shot.
Melt temperature must be measured with a needle pyrometer rather than inferred only from barrel setpoints. For Sclair® 8111, a melt temperature of 190–230°C is typically sufficient. Temperatures above 250°C should be avoided because polyethylene degradation may begin to generate oxidized species, reduce molecular weight, and create surface defects. In hot-runner systems, long residence times at elevated temperatures can have the same effect even if barrel setpoints are within range. If a hot runner cannot provide uniform temperature control, published data for this specific configuration is limited, and a cold-runner tool may be preferable for color-sensitive applications.
The density of 0.924 g/cm³ places Sclair® 8111 in the medium-density region of the LLDPE family, which results in higher stiffness than low-density polyethylene grades with densities near 0.915–0.918 g/cm³. The flexural modulus of approximately 220 MPa under ASTM D790 is useful for closures and housewares that require some structural rigidity, but it is lower than that of polypropylene and high-density polyethylene. Consequently, when replacing a high-density polyethylene or polypropylene part with Sclair® 8111, the designer should evaluate the increased deflection under load and the potential need for rib or wall-thickness modification. Short-term tensile data under ASTM D638 do not substitute for creep or stress-relaxation testing if the component is continuously loaded or exposed to elevated temperature.
Shrinkage behavior also differs from high-pressure LDPE. LLDPE injection grades typically show higher and more anisotropic shrinkage than amorphous or low-crystallinity polymers. Sclair® 8111 is semicrystalline, and shrinkage after demolding depends on mold temperature, part thickness, gate location, and packing pressure. In a typical injection molding trial, a part thickness increase from 1 mm to 3 mm may increase cycle time and alter dimensional stability. Tooling should not be cut from a high-pressure LDPE shrinkage allowance unless the current mold has been tested with the intended LLDPE grade. Measurement of post-mold dimensions should follow a defined conditioning period, such as 24–48 h at 23°C, because polyethylene continues to shrink after ejection as crystallinity develops.
Food-contact suitability must be verified through the manufacturer’s current compliance documentation. Polyethylene resins are commonly evaluated against FDA 21 CFR 177.1520 for olefin polymers and European food-contact regulations such as Regulation (EU) No 10/2011. The converter bears responsibility for confirming the final article’s compliance under the intended food type, temperature, and contact duration. Sclair® 8111 is not a substitute for high-clarity polypropylene in applications requiring glass-like transparency, because the crystallinity of LLDPE produces a translucent to opaque appearance dependent on wall thickness and cooling rate. It is also not suitable for continuous exposure to strong oxidizing acids or for applications requiring high-temperature sterilization above the Vicat softening point.
When Sclair® 8111 is run in a mold with fine surface detail, higher mold temperature and adequate packing can improve replication, but the cycle must still allow gate seal before pressure can be reduced. A gate-seal study is required because premature transfer to holding pressure can create sink marks, while excessive hold time extends cycle without improving part properties. The processing window is therefore defined less by a single temperature setpoint and more by the interaction of injection velocity, gate freeze-off time, screw recovery capacity, and clamp force reserve. On manufacturing lines with limited clamp tonnage, the high melt flow rate of Sclair® 8111 may permit lower cavity pressure, but the clamp safety margin should be validated with a pressure transducer rather than inferred from an open nozzle.
The resin’s low water absorption and low-temperature toughness make it suitable for closure and houseware applications that experience occasional impact at refrigerator or freezer temperatures. However, low-temperature impact performance should be evaluated under ASTM D256 or ISO 179-1 on the actual part geometry, because weld lines, gate vestiges, and molded-in stress can reduce practical toughness relative to laboratory specimens. The absence of a standardized universal value for injection-molded parts means that published data for this specific configuration is limited, and application testing remains the only reliable basis for durability claims.