| HS Code | 701756 |
| Productname | NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene-1 |
| Form | Pellets |
| Density | 0.918 g/cm³ |
| Meltindex | 0.75 g/10 min |
| Meltflowratio | 30 |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 24.1 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 221 MPa |
| Vicatsofteningpoint | 100 °C |
| Brittlenesstemperature | < -70 °C |
| Escr | >1000 h |
| Dartdropimpact | 200 g |
| Elmendorftearstrengthmd | 300 g |
| Elmendorftearstrengthtd | 400 g |
| Haze | 12% |
| Gloss | 60% |
As an accredited NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin is supplied in 25 kg polyethylene bags, palletized for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading: 25 kg bags of NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin, palletized and secured. |
| Shipping | NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin is a non-hazardous thermoplastic pellet. It typically ships in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars, palletized and stretch-wrapped. Store dry, away from heat, moisture, and contaminants. No special DOT/IMDG/IATA hazard classification is usually required. |
| Storage | Store NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture and contamination. Avoid strong oxidizing agents. Maintain clean handling areas, use first-in, first-out rotation, and follow local regulations and SDS recommendations. |
| Shelf Life | Stable under normal storage conditions; shelf life is indefinite when kept dry, cool, and away from heat and ignition sources. |
Sclair® 61C is processed as the core-layer resin in machine-gauge cast stretch film because the octene short-chain branching architecture raises the machine-direction tensile modulus at 300% elongation without proportionally reducing Elmendorf tear propagation resistance. The nominal melt index of 1.0 g/10 min under ASTM D1238 at 190°C and 2.16 kg and the nominal density of 0.919 g/cm³ under ASTM D1505 allow a die temperature window of 240–270°C on cast-film extrusion lines. In a three-layer A/B/A structure, the core layer is fed with 70–80 wt% neat Sclair® 61C, while the skin layers carry 0.5–2.0 wt% cling additive masterbatch and 0.3–1.0 wt% antiblock masterbatch. A production-scale cast line using a 90 mm core extruder and 65 mm skin extruders typically operates with a coat-hanger die gap of 0.8–1.0 mm, die width of 2,500–3,000 mm, and chill roll temperature of 15–25°C. Chill roll temperatures above 25°C slow the quench rate and permit post-crystallization that reduces ultimate stretch and increases stress-whitening. Final machine rolls are targeted at 20–35 µm gauge. Edge trim reintroduction above 15 wt% raises gel count and reduces puncture resistance measured by ASTM D5748. For food-contact applications, the finished film is subject to FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation 10/2011 with an overall migration limit of 10 mg/dm²; the resin itself must be formulated only with approved antioxidants and neutralizers. High ambient humidity above 70% RH can introduce surface moisture on pellets and cause splay at the die exit, so hopper temperature and feed-throat cooling must be controlled to prevent condensation.
On a 75 mm grooved-feed single-screw extruder with L/D 30:1 and a barrier screw, running 100% Sclair® 61C at a melt temperature of 210–230°C generates a screen-changer melt pressure of 380–420 bar at 180 kg/h. The low nominal melt index of 1.0 g/10 min increases shear heating in the metering zone, and lot-to-lot melt index variation of ±0.1 g/10 min shifts motor load by 4–6% on this screw geometry. To keep bubble stability within a 2.5:1–3.5:1 blow-up ratio, converters let down the resin with 10–20 wt% LDPE or MDPE having a melt index of 0.3–0.7 g/10 min; this is not a filler addition but a rheological modifier that reduces melt pressure at the die lip. The blown-film die uses a die gap of 1.6–2.0 mm, and frost line height is maintained at 8–12 times the die diameter to balance quench and bubble stability. Barrel temperatures are profiled from 170°C at the feed zone to 210°C at the metering zone, with adapter and die zones at 220–230°C. Final heavy-duty shipping sacks are extruded at 75–140 µm gauge and are tested by ASTM D1709 dart impact and ASTM D1922 Elmendorf tear. No food-contact claim applies to most heavy-duty industrial sacks; compliance instead follows REACH Article 33 communication obligations for candidate list substances above 0.1 wt%. The resin must not be processed above 260°C melt temperature in this application, because oxidative degradation of octene short-chain branches increases gel count and reduces dart impact by more than 10% in converter trials.
Because the octene branch distribution lowers seal initiation temperature relative to butene LLDPE of equivalent density, flexible packaging lamination webs use Sclair® 61C as the sealant layer in coextruded structures. In a tandem extrusion lamination line, the resin is processed at 260–300°C through a T-slot die with a nominal die gap of 0.5–0.8 mm and drawn down to 15–25 µm onto corona-treated BOPP or metallized BOPP. The blend is 95–98 wt% Sclair® 61C, 1–3 wt% maleic anhydride grafted polyethylene tie resin, and 0.2–0.5 wt% processing aid masterbatch as permitted by the finished article specification. Substrate pre-treatment is maintained at 42–46 dyn/cm wetting tension before the melt curtain contacts the substrate, and the air gap is controlled between 80 mm and 120 mm to balance adhesion and neck-in. For food-contact laminates, the finished structure is evaluated under EU Regulation 10/2011 Annex I, and the olefin polymer layer is assessed under FDA 21 CFR 177.1520(c) with conditions of use. Lap seal strength measured by ASTM F88/F88M after 24 h at 23°C and 50% RH is used as the release criterion. Melt temperature above 300°C is an operational boundary because oxidation increases carbonyl index and lowers seal strength; published data for this specific configuration is limited.
In high pre-stretch manual pallet wrap, the cast-film line is operated with a vacuum box between the die and chill roll, and the resin is drawn to a 250–350% pre-stretch ratio. At draw ratios above 250%, stress-whitening appears if the core layer contains more than 10 wt% reprocessed edge trim; the whitening threshold is also shifted by chill roll temperature above 20°C. The resin is fed neat at 85–90 wt% in the core, with the skin layers carrying 1.5–3.0 wt% cling additive masterbatch and 0.2–0.5 wt% antiblock. Vacuum box pressure is controlled between –0.5 kPa and –1.0 kPa to stabilize the web before it reaches the chill roll. Web tension oscillations above ±5% at 350% draw ratio are a known failure mode that triggers transverse tear propagation at the winder; load-cell calibration and differential shaft speed control are required to maintain tension. Film thickness is targeted at 12–20 µm. The application is non-food industrial, so compliance is limited to REACH and occupational exposure obligations rather than FDA 21 CFR. The resin should not be processed above 270°C in this configuration because gel formation at the die lip increases and the cling force measured by ASTM D5458 declines after 72 h film aging. Published data for this draw ratio on Sclair® 61C is limited, so converter trials are required to fix the exact edge-trim ceiling.
A three-layer blown-film line running a high-stalk bubble geometry extrudes Sclair® 61C at 80–90 wt% with 10–20 wt% metallocene LLDPE for puncture resistance and dart impact. The die gap is 1.8–2.4 mm, blow-up ratio is 3.5:1–4:1, and melt temperature is held at 180–210°C to minimize thermal degradation and to preserve self-adhesion without butyl acrylate tackifiers. Final silage wrap is produced at 25 µm thickness and is tested for dart impact by ASTM D1709 and puncture propagation by ASTM D5748. Agricultural silage wrap is not a food-contact article, so compliance is limited to REACH and national agricultural film regulations; no FDA 21 CFR claim applies. The resin is not inherently UV-stabilized, and outdoor storage beyond 12 months requires 0.5–1.5 wt% HALS masterbatch plus 0.2–0.5 wt% carbon black or titanium dioxide masterbatch. The processing boundary is the high-stalk bubble, which becomes unstable when the extruder output fluctuates by more than ±3%; a gravimetric feeder and melt pump are required on the core extruder. Output per die diameter is typically held at 0.8–1.1 kg/h/mm, and the film roll is converted at 750 mm × 1,500 m dimensions for round-bale wrapping equipment.
Industrial can liners and form-fill-seal packaging use Sclair® 61C as a direct replacement for butene LLDPE in cast-film lines at a layer distribution of 70–80 wt% core and 20–30 wt% combined skin grade. The resin is processed on a 65 mm single-screw extruder with L/D 28:1, die temperature 230–260°C, and chill roll temperature 18–22°C. Film gauge is held at 25–50 µm depending on end use. The finished liners are evaluated by ASTM D1709 dart impact and ASTM D1922 Elmendorf tear, but no food-contact standard is invoked for non-food industrial liners. Reprocessed trim is limited to 20 wt% because higher levels reduce dart impact and create visible gels in thin-gauge sections. The main process incompatibility is the use of high levels of acid-containing additives, which can deactivate some processing aid systems and cause die-lip buildup; additive selection must be confirmed by pilot extrusion before production.
Competitive NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 61C is an ethylene-1-octene linear low-density polyethylene extrusion resin. It is supplied without intentionally added slip or antiblock additives, and it is used primarily in cast film and coextruded packaging structures where converter-added masterbatch controls surface friction. The resin has a nominal density of 0.919 g/cm³ when measured under ASTM D792 and a melt index of 1.0 g/10 min when measured under ASTM D1238 at 190 °C with 2.16 kg load. The octene comonomer introduces short-chain branches containing 6 carbon atoms, while butene-based LLDPE introduces 2-carbon branches and hexene-based LLDPE introduces 4-carbon branches. In film conversion, Sclair 61C is specified for toughness, extensional flow stability, and seal integrity in monolayer and coextruded packaging films. The grade is not designed for injection molding, blow molding, or rotational molding; processing outside extrusion and compounding conditions is outside manufacturer-published guidance.
At equivalent density and melt index, an octene-based LLDPE typically exhibits higher dart impact strength, higher Elmendorf tear resistance in machine and transverse directions, and lower brittle fracture tendency at refrigerated temperatures than a butene-based LLDPE. The underlying structural difference is short-chain branch length. The 6-carbon octene short-chain branch is long enough to extend through the interlamellar amorphous layer and participate in tie-chain formation between adjacent crystalline lamellae, whereas the 2-carbon butene branch can be accommodated more readily at the crystal surface or within nearby amorphous regions. This structural distinction is not captured by melt index alone; it appears in film tests such as ASTM D1709 dart drop and ASTM D1922 Elmendorf tear. Hexene LLDPE occupies an intermediate position because its 4-carbon branch is longer than butene but shorter than octene. Metallocene octene grades may have more uniform comonomer distribution and lower seal initiation than Ziegler-Natta catalyzed grades, but can also exhibit a narrower molecular weight distribution and different shear thinning during extrusion. Sclair 61C is a Ziegler-Natta catalyzed octene LLDPE, according to manufacturer-published polymerization data. Comparative seal testing under ASTM F1921 and ASTM F88 is required to determine line-specific hot-tack and seal-strength differences when replacing another resin.
The following values are manufacturer-typical values, not release limits. A certificate of analysis should be reviewed for batch-specific melt index and density.
| Property | Typical value | Test method |
|---|---|---|
| Melt index | 1.0 g/10 min | ASTM D1238 / ISO 1133-1 (190 °C, 2.16 kg) |
| Density | 0.919 g/cm³ | ASTM D792 / ISO 1183-1 |
| DSC peak melting temperature | approximately 121 °C | ASTM D3418 |
| Vicat softening temperature | approximately 108 °C | ASTM D1525 |
| Additive package | no slip, no antiblock | manufacturer-published grade datasheet |
Because the grade is supplied without slip and antiblock, the coefficient of friction of converted film is set by downstream masterbatch addition. In coextruded structures, Sclair 61C is commonly placed in a core or sealant layer where surface friction is controlled by external skin layers. The absence of slip additives reduces the possibility of erucamide or oleamide migration into seal layers during film aging, which can raise seal initiation temperature if high additive loadings are used. Processors that require immediate machineability at the winding station typically add a slip/antiblock masterbatch at the throat or pre-compounded in a blend with the pellet stream.
On chill-roll cast film lines, Sclair 61C is processed through a single-screw extruder with barrier flight geometry and a die gap commonly between 0.5 mm and 1.0 mm. A typical starting barrel profile from feed throat to die is 180 °C, 210 °C, 230 °C, 240 °C, with adapter and die zones held at 240 °C to 250 °C. These temperatures are starting-point values, not universal setpoints; optimized profiles depend on line length, die width, and output. Melt temperatures above 260 °C are not recommended because the resin may undergo oxidative chain scission and crosslinking in the presence of oxygen or process residues, producing visible gels and reducing film appearance. Plant-scale observations on 30:1 L/D cast film extruders indicate stable operation when melt temperature remains below 250 °C and screw speed maintains a specific output range appropriate for the installed die width. The resin does not require drying at relative humidity below 60 %. If pellets are transferred from cold silos to warm extrusion plants without an adequate temperature equilibration period, surface condensation can occur. In such cases, pellets should be held in a hopper purged with ambient or dehumidified air until surface moisture is eliminated. Condensed moisture can cause bubble defects in extruded film and reduce adhesion to chill rolls.
Controlling neck-in and draw resonance in monolayer cast film requires balancing melt strength, melt temperature, and die-to-air-gap geometry. Sclair 61C contains octene branches but is still a linear polyethylene; its extensional viscosity and melt strength are lower than branched LDPE or certain high-pressure autoclave grades. Blending with LDPE at additions from 5 wt% to 20 wt% can reduce neck-in and stabilize draw resonance. Above 20 wt% LDPE, film dart impact and transverse tear may decline more rapidly because LDPE has lower strain at break and lower puncture resistance. For coextruded cast film, positioning Sclair 61C as a core layer preserves its toughness contribution while allowing HDPE, PP, or sealant ionomer skins to control surface properties. The die-to-chill-roll air gap should be kept as short as practical, typically 30 mm to 80 mm, to reduce neck-in and improve dimensional stability; exact settings depend on die width, polymer temperature, and chill-roll diameter.
Compared with high-pressure LDPE, Sclair 61C has lower melt strength and less shear thinning. On the same cast film line, this can require a shorter die-to-chill-roll air gap and faster chill-roll speed to maintain web stability. The resulting film has higher tensile elongation and superior puncture resistance but lower modulus and lower clarity in some gauge ranges. If evaluated on blown film lines, die gap, blow-up ratio, and frost line height must be reset for the lower melt strength and higher drawdown of Sclair 61C relative to LDPE.
If hopper storage encounters cyclic humidity above 60 % relative humidity, manual handling procedures should specify closed transfer lines and heated hoppers because polyethylene pellets can adsorb surface moisture even though bulk water absorption is negligible. High-humidity storage does not alter the thermal properties of Sclair 61C but can introduce surface defects during film conversion if condensation is carried into the feed throat. This operational boundary is not unique to Sclair 61C; it applies to general polyolefin extrusion resins. The resin should not be stored in direct sunlight for extended periods because UV exposure can form surface oxidation products that produce gel-like inclusions. Silo purging with dry air at 40 °C to 50 °C for 2 h to 4 h is used in some plants to equilibrate cold pellets before starting a high-output cast line, but published data for this specific configuration is limited.
When edge trim and regrind are introduced into the feed stream, the ratio of regrind to virgin pellets should be controlled gravimetrically. High regrind fractions increase thermal history and can raise gel formation risk if oxidized trim is present. If slip or antiblock masterbatch is added at the throat, the masterbatch carrier resin should be low-density and compatible with octene LLDPE; incompatible carriers can produce local viscosity variations that generate gauge bands in the cast film. For films that require immediate winding without blocking, a slip/antiblock masterbatch is typically added at 2 wt% to 5 wt%, but the exact loading depends on the masterbatch concentrate assay and the desired coefficient of friction. Published data for this specific configuration is limited.
Compliance with food-contact regulation begins with the base resin but is not automatically transferred to a multi-material laminate, coated structure, or printed film. Manufacturer-published product stewardship documentation references FDA 21 CFR 177.1520 paragraph (c)3.2a for olefin polymers and EU Regulation (EU) No 10/2011 for plastic materials intended to contact food. The final converter must assess overall migration under EN 1186 or applicable replacement standards and verify specific migration limits for additives and processing aids used in the final structure.
| Regulatory reference | Specific clause or test method | Applicability |
|---|---|---|
| FDA 21 CFR 177.1520 | (c)3.2a | olefin polymer base resin for food-contact applications |
| EU Regulation (EU) No 10/2011 | EN 1186 overall migration test series | plastic materials and articles intended for food contact |
| REACH Regulation (EC) No 1907/2006 | Article 33 communication requirements | no intentionally added SVHC above 0.1 wt% threshold |
| RoHS Directive 2011/65/EU | Annex II restricted substances | packaging films are typically outside scope unless incorporated into electrical or electronic equipment |
If the film is used in medical packaging or pharmaceutical pouches, converters must verify sterilization compatibility separately using the appropriate pharmacopoeia or ISO 11607 requirements. No claim is made for use in implantable devices or long-term critical medical applications.