| HS Code | 614510 |
| Density | 0.920 g/cm³ |
| Meltindex | 0.75 g/10 min |
| Meltingpoint | 124 °C |
| Vicatsofteningpoint | 100 °C |
| Tensilestrengthatyield | 10 MPa |
| Tensilestrengthatbreak | 27 MPa |
| Elongationatbreak | 800 % |
| Flexuralmodulus | 250 MPa |
| Filmhaze | 12 % |
| Filmgloss | 60 % |
| Dartimpact | 120 g |
| Elmendorftearmd | 300 g |
| Elmendorfteartd | 400 g |
As an accredited NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin is packaged in 25 kg multiwall bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL loaded with 25 kg bags of NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin, approximately 20 metric tons total. |
| Shipping | NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin is typically shipped in 25 kg polyethylene bags on stretch-wrapped pallets, or in bulk trucks and railcars. It should be kept dry, away from heat, direct sunlight, and contamination. The resin is non-hazardous under normal transport conditions; follow supplier guidance. |
| Storage | Store NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin in a cool, dry, well-ventilated area away from heat, sparks, flames, and oxidizing agents. Keep containers sealed and protect from moisture, sunlight, and contamination. Use original packaging, handle with clean equipment, and avoid prolonged direct UV exposure. Maintain good housekeeping to prevent slipping from spills. |
| Shelf Life | No specific shelf life; stable under recommended storage conditions. Store cool, dry, ventilated, away from direct sunlight and ignition sources. |
In blown film lines producing 100–250 µm heavy-duty industrial liners, Sclair® 31E is processed through a grooved-feed single-screw extruder with a barrel length-to-diameter ratio of 24:1 to 30:1 and a barrier screw fitted with a Maddock mixing section. The resin is a butene linear low density polyethylene with nominal density 0.920 g/cm³ by ASTM D792 and melt index 1.0 g/10 min by ASTM D1238 at 190 °C/2.16 kg. Extrusion temperature profiling places feed-zone temperatures at 160–180 °C, barrel zones at 190–210 °C, adapter at 205–215 °C, and die zones at 215–225 °C. Melt temperature at the die exit is maintained between 205 °C and 220 °C to balance melt strength and screw motor load. Die gap is set at 1.8–2.5 mm for this gauge range; gaps below 1.8 mm elevate die pressure and can initiate sharkskin surface roughness, while gaps above 2.5 mm reduce gauge uniformity unless dual-lip air-ring cooling is increased accordingly.
Gauge uniformity in this application is governed more by bubble cooling symmetry than by screw design. For 100 µm liner film, die gap is fixed between 2.0 mm and 2.5 mm, blow-up ratio is held between 2.5:1 and 3.2:1, and frost-line height is positioned 500–700 mm above a 250 mm die. Dual-lip air rings with internal bubble cooling reduce gauge coefficient of variation to 4–6%; without IBC, gauge scatter commonly increases to 8–12%. Lower frost-line positions improve transverse direction tear and dart impact, while higher positions increase machine direction orientation and reduce drop impact. Terminal liners produced under these conditions are tested against ASTM D5748 puncture resistance, ASTM D1709 dart drop impact, and ASTM D882 tensile properties. Food-contact status is evaluated under 21 CFR 177.1520(c) and EU Regulation 10/2011 as amended, with migration testing conducted according to the food simulant and time-temperature condition specified in the end-use requirement. The butene branch architecture yields lower dart impact and tear strength than comparable hexene LLDPE at equivalent density; converters commonly compensate by increasing gauge by 10–15% or blending with 20–30 wt% hexene LLDPE. Storage above 50 °C or unprotected outdoor exposure should be avoided because the base resin is not UV-stabilized beyond the standard processing package.
| Processing Variable | Setpoint Range | Observed Effect | Reference Method |
|---|---|---|---|
| Barrel Zone 1 | 160–180 °C | Feed stability, melting onset | ASTM D1238 |
| Barrel Zone 2–4 | 190–210 °C | Homogeneous melt | ASTM D1238 |
| Adapter | 205–215 °C | Melt temperature control | Plant thermocouple |
| Die Zones | 215–225 °C | Gauge uniformity, surface finish | ASTM D1238 |
| Die Gap | 1.8–2.5 mm | Melt fracture threshold, gauge spread | Die lip measurement |
| Blow-Up Ratio | 2.5:1–3.2:1 | TD tensile, impact balance | Bubble geometry |
| Frost-Line Height | 500–700 mm | MD/TD property shift | Line observation |
Down-gauging Sclair® 31E in silage overwrap shifts the limiting constraint from extruder throughput to bubble stability and transverse direction tear retention. At 25 µm, film is processed with a die gap of 1.8 mm and blow-up ratio between 2.0:1 and 2.5:1. Higher blow-up ratio raises transverse direction tear strength but reduces machine direction drawdown capacity. Melt temperature is held at 195–210 °C, lower than heavy-gauge liner settings, to raise melt strength and reduce bubble oscillation. Frost-line height is adjusted to 400–600 mm; increasing frost-line height beyond 700 mm produces excessive machine direction orientation and a measurable loss of puncture resistance. Output rates on a 250 mm die commonly flatten below 120 kg/h because the thin bubble becomes sensitive to ambient air fluctuations; side shields or enclosed towers are required to maintain stable gauge.
The agricultural overwrap compound is dry-blended with a UV stabilizer masterbatch at 6–8 wt%, typically containing hindered amine light stabilizers and carbon black with 40–60 nm primary particle size. Carbon black loading is selected to achieve UV transmission below 1% across the 290–400 nm range; incomplete dispersion increases pinhole formation measured by ASTM D5151 water bath testing. Silage overwrap requires high puncture and snag resistance during corn stalk wrapping; film is tested by ASTM D5748 and ASTM D4833. Published data for this specific configuration is limited, but comparable butene LLDPE films show a 20–30% loss of tear resistance when machine direction orientation is increased through nip roll overspeed beyond 5%. The terminal wrapped bale relies on cling and tension retention; Sclair® 31E without tackifier delivers limited cling, so the overwrap design typically uses a coextruded tackified surface layer or mechanical film interlocking rather than relying on the base resin. Compliance for non-food agricultural film is not governed by 21 CFR 177.1520 in most jurisdictions, but REACH and RoHS recast 2011/65/EU restrictions on heavy metals apply to the UV masterbatch and black concentrate.
In cast film lines producing protective masking and surface-protection film, Sclair® 31E is processed at melt temperatures between 230 °C and 250 °C through a flat die with lip gap 0.6–0.9 mm. The melt curtain is pinned to a chrome-plated chill roll held at 15–25 °C; air gap is set at 60–120 mm. Higher melt temperatures reduce melt viscosity and permit faster line speed but increase surface oxidation and haze development. A dual-chamber air knife and vacuum box combination is standard; without pinning, edge neck-in and draw resonance at line speeds above 150 m/min generate gauge bands measurable by ASTM D6988. Chill roll diameter and water flow are balanced to achieve a roll surface temperature differential below ±2 °C across the web width.
Film haze and clarity are controlled by chill roll polishing, melt curtain temperature uniformity, and cooling roll fouling. Compared with C6 or C8 LLDPE grades, the butene comonomer in Sclair® 31E produces lower extractables, but roll fouling still accumulates when chill roll temperature is maintained below 10 °C or when melt temperature exceeds 260 °C. Haze targets for cast protective masking are often below 5% by ASTM D1003; achieving this requires 60/80/100 mesh melt filter packs and chill roll release agents that do not transfer to the film surface. Terminal cast film is tested for tensile elongation at break, Elmendorf tear per ASTM D1922, and coefficient of friction per ASTM D1894. Addition of slip masterbatch above 1.5 wt% reduces blocking but raises haze by 1–2 percentage points. The product format is a non-cling protective layer; cling additives are absent unless coextruded as a separate skin layer, which is the preferred structure because molecular diffusion of low-molecular-weight cling agents into the Sclair® 31E core would alter its static coefficient of friction over time.
Extrusion coating of kraft paperboard for moisture barrier laminates places Sclair® 31E under high-temperature, short-residence conditions that differ from blown and cast film processing. The resin is melted in a single-screw extruder with a 30:1 L/D barrier screw, filtered through 40/80/40 mesh screen packs, and delivered to a slot die set at 280–315 °C. The elevated melt temperature is required to promote adhesion to the paperboard through polar oxidation at the melt-substrate interface; air gap is typically 150–250 mm. Under these conditions the butene LLDPE exhibits higher neck-in than LDPE coating grades, and line trials show edge bead formation unless die width is adjusted by 5–8% at each edge. Drawdown ratios above 40:1 are possible only when the die lip is clean and the melt curtain is protected from ambient air movement.
Adhesion to kraft paperboard is measured by peel strength per TAPPI T 540 or ASTM F88. Untreated paperboard usually gives peel values below 0.5 N/15 mm; corona treatment of the board at 2.0–3.0 kW/m² and internal ozone treatment of the melt curtain raise peel strength to 1.5–3.0 N/15 mm. Barrier properties are tested by water vapor transmission rate per ASTM F1249 at 38 °C and 90% RH; a 20 µm coating layer reduces WVTR to 20–30 g/m²/day depending on paperboard porosity and coating uniformity. The terminal laminate is used for dry food, cement, and chemical powder sacks where moisture protection and dust containment are required. Food-contact status is evaluated under 21 CFR 177.1520(c) for the polyolefin coating layer; the paperboard substrate is separately regulated under 21 CFR 176.170. Process limitations include rapid edge cooling at the die ends, which locally raises viscosity and produces edge tear during trimming; deckle rod adjustments must maintain a uniform melt bank at the nip.
| Compliance Requirement | Standard Designation | Condition or Scope |
|---|---|---|
| Olefin polymer food contact | 21 CFR 177.1520(c) | Polyolefin coating layer |
| Paperboard food contact | 21 CFR 176.170 | Paper component |
| EU food contact | EU Regulation 10/2011 as amended | Plastic layer migration |
| Water vapor transmission | ASTM F1249 | 38 °C, 90% RH |
| Peel adhesion | ASTM F88 or TAPPI T 540 | Coating-to-board bond |
| Heavy metals | RoHS Recast 2011/65/EU | Applicable to electrical/electronic packaging |
When Sclair® 31E is used as a heat-seal layer in coextruded lidstock laminates, the critical variables are seal initiation temperature, hot tack strength, and seal bar pressure. The resin is coextruded at 220–240 °C as a 20–30 µm sealant layer over a tie layer and barrier layer. Seal initiation is measured by ASTM F2029; typical seal initiation for a 0.920 g/cm³ butene LLDPE falls between 85 °C and 105 °C on a flat jaw sealer at 275 kPa seal pressure and 0.5 s dwell. Hot tack strength measured by ASTM F1921 at 110–130 °C must exceed 1.0 N/15 mm to prevent seal creep on high-speed packaging lines; below that level, film retraction behind the jaw produces channel leaks and field-failure returns.
The butene comonomer in Sclair® 31E lowers seal initiation compared with ethylene homopolymers and produces a wider seal plateau than high-density grades. However, sealing against rigid polypropylene exposes the lidstock sealant to asymmetric heat transfer through the rigid flange; seal bar temperature must be raised by 10–15 °C to compensate for heat loss into the flange. Seal strength after 24 h ageing is measured by ASTM F88 and typically remains above 1.5 N/15 mm for a 25 µm sealant layer. The lidstock is tested for seal integrity by vacuum decay per ASTM F2338 and for migration compliance under 21 CFR 177.1520(c) and EU Regulation 10/2011. If the package is retorted, Sclair® 31E is not suitable above 121 °C sustained thermal load because seal geometry deforms and creep reduces residual seal force. The terminal product format is a peelable or medium-tight lidding film for dairy, fresh produce, or dry food tubs; peelability is adjusted with a blended polypropylene or polybutene modifier rather than by altering Sclair® 31E alone, which otherwise produces a hard lock-up seal above 130 °C.
High-drawdown film structures for frozen food packaging expose Sclair® 31E to shear rates that approach the onset of sharkskin melt fracture. The resin is processed through a spiral mandrel die with die gap 2.0 mm; shear rate at the die land is estimated from apparent melt viscosity and die pressure. For this grade, sharkskin is generally absent below 300 s⁻¹ but may appear above 500 s⁻¹ if melt temperature is below 195 °C. Raising melt temperature to 215–225 °C or increasing die gap to 2.5 mm suppresses surface roughness without changing the resin. Fluoropolymer processing aids are added at 200–500 ppm when high output is required; above 500 ppm, surface haze increases and print adhesion can decrease unless corona treatment is adjusted.
Frozen food films require low-temperature impact resistance; the butene LLDPE backbone provides ductility below -30 °C as measured by ASTM D746 brittleness temperature. Processing at drawdown ratios above 30:1 uses a high-stalk bubble configuration in which the bubble is allowed to rise 8–12 die diameters before expansion. Machine direction tear properties fall as drawdown increases, while dart drop impact and transverse direction tear increase when blow-up ratio is maintained above 2.5:1. The terminal film is evaluated by ASTM D1709 for impact, ASTM D1922 for tear, and ASTM D882 for tensile modulus. Compliance for frozen food packaging falls under 21 CFR 177.1520(c) for the olefin polymer; low-temperature performance is specified at -20 °C storage conditions. The resin should not be combined with amine-based additives or high-pH fillers because these species can accelerate thermo-oxidative degradation in the high-shear melt zone and produce gel particles downstream.
Competitive NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 31E is a butene linear low-density polyethylene extrusion resin supplied in pellet form for blown film and cast film conversion. The grade is defined at release by two primary specifications: nominal melt index of 1.0 g/10 min when measured at 190 °C with a 2.16 kg load in accordance with ASTM D1238, and nominal density of 0.920 g/cm³ in accordance with ASTM D1505. These values place the product in the heavy-duty film LLDPE segment, where converters evaluate gauge reduction, dart impact, Elmendorf tear, and seal strength against high-pressure LDPE and higher-α-olefin LLDPE alternatives. The comonomer is butene; the short-chain branch length is therefore C4, which has direct consequences for the tie-molecule population and the low-temperature impact response of the finished film. The product is stabilized for normal thermoplastic processing, but the exact antioxidant and additive package is a producer-specific formulation and should be confirmed with the supplier for each commercial lot.
Commercial designation 31E identifies a butene LLDPE extrusion resin within the Sclair portfolio. The two primary release properties are melt index and density, but a single-point melt index does not define the full molecular weight distribution. For die design and pressure-drop modeling, a capillary rheometer sweep between 100 s⁻¹ and 1000 s⁻¹ at 190 °C is recommended; the data should include entrance-pressure correction if orifice dies are used. The density of 0.920 g/cm³ corresponds to a moderate crystalline fraction and differentiates the grade from lower-density film grades in the 0.918 g/cm³ class and from higher-density extrusion grades above 0.925 g/cm³.
| Parameter | Nominal value | Reference method |
|---|---|---|
| Melt index | 1.0 g/10 min | ASTM D1238 |
| Density | 0.920 g/cm³ | ASTM D1505 |
| Comonomer type | butene | producer disclosure |
| Physical form | pellet | producer disclosure |
The melt index of 1.0 g/10 min indicates an intermediate flow behavior: it is lower than that of many cast film and extrusion lamination resins, but higher than fractional-melt blown film grades. The consequence on a production line is moderate back pressure, controllable bubble stability, and the ability to run at acceptable melt temperatures without excessive motor load. Molecular weight distribution and long-chain branching are not specified by the standard certificate of analysis; if a converter needs polydispersity or melt flow ratio data, the supplier should be requested to provide the analytical method and lot-specific result. Because density is measured after annealing and conditioning, film density in the final product may differ slightly due to orientation and cooling rate. A blown film line with a fast quench produces smaller spherulites and lower haze, but may also reduce the effective crystallinity measured on the film sample. For the purpose of comparing grades, density should be measured on compression-molded plaques rather than on film; film density is not a valid material specification. The melting temperature of LLDPE of this density class is commonly in the range of 120 °C to 125 °C by differential scanning calorimetry, but the exact peak and crystallinity distribution should be determined by ASTM D3418 for the lot. The Vicat softening temperature is not the primary grade-selection parameter for film applications; if required, it can be measured by ASTM D1525.
On a conventional blown film line using a grooved-barrel single-screw extruder with L/D between 24:1 and 30:1, startup melt temperatures between 190 °C and 240 °C are appropriate. A barrier screw or a low-shear mixing section is preferred because it reduces the residence time distribution and lowers the risk of oxidation gels. Die gap is normally set between 1.5 mm and 2.5 mm; a gap below 1.0 mm may produce high head pressure and melt fracture, particularly when combined with high output and a short land length. A gap above 2.5 mm can increase melt residence time and degrade gauge uniformity because the film must be drawn from a thicker annulus. Blow-up ratios of 2.0:1 to 3.0:1 are typical. The 1.0 g/10 min melt index provides sufficient melt strength for bubble stability, but the frost line should be held within 1 to 3 die diameters from the air ring; a low-stalk or in-pocket bubble shape is generally more stable than a high-stalk configuration for this resin class. At melt temperatures above 250 °C, oxidation and gel formation become likely; the actual gel onset is a function of screw speed, residence time distribution, and the specific stabilization package. If the line is stopped for more than 15 min while the barrel remains above 240 °C, purging with a suitable LLDPE purge compound is required to remove thermally degraded resin.
Melt fracture on this grade appears as sharkskin or gross melt fracture depending on the die land surface, melt temperature, and shear rate. The critical shear stress for sharkskin in linear polyethylene is often in the range of 0.1 MPa to 0.3 MPa at the die lip, but die geometry and resin molecular weight distribution shift the threshold. Processors experiencing sharkskin can reduce output, raise melt temperature within the stable range, enlarge the die gap, or use a fluoropolymer processing aid. Die-lip deposit is influenced by low-molecular-weight waxes and crosslinked gel particles; periodic cleaning intervals should be established from production logs. Back pressure at a given output is lower for this grade than for a fractional-melt LLDPE, but higher than for a 2.0 g/10 min cast film grade. Cast film extrusion of Sclair 31E is feasible, but published data for this specific configuration is limited. Typical cast film conditions for LLDPE of this melt index include die temperatures from 210 °C to 260 °C, an air gap between 20 mm and 100 mm, and a chilled roll temperature between 15 °C and 30 °C. The quench rate and air gap determine film haze and tear balance; these settings must be optimized on the target line because the material’s response depends on the exact die design and haul-off speed.
At equivalent density and melt index, a 1-octene LLDPE typically produces higher dart impact and machine-direction Elmendorf tear than a butene LLDPE. The structural reason is that the longer C8 branch creates a more effective tie-molecule network between adjacent crystallites; the butene grade has a shorter C4 branch and therefore a different distribution of stress-transmitting chains. This difference is measurable by ASTM D1709 and ASTM D1922, but the magnitude is gauge-dependent and not fixed by the density specification alone. Seal performance also changes: butene LLDPE grades of this density class often show a lower heat-seal initiation temperature than LDPE, but the hot-tack plateau may be narrower than that of a comparable octene LLDPE at high line speeds.
Compared with high-pressure low-density polyethylene of the same nominal density, Sclair 31E has a linear backbone without the long-chain branching produced in autoclave or tubular LDPE reactors. The practical effect is lower melt strength and reduced shear thinning: LDPE is more shear-sensitive and displays higher melt tension, while the LLDPE can deliver more Newtonian flow and potentially lower extruder pressure at high shear rates. On existing LDPE film lines, conversion to 31E may require changes in die gap, air ring, or screw profile to maintain bubble stability. Within the Sclair butene LLDPE product family, the melt index of 1.0 g/10 min distinguishes the grade from higher-flow injection or cast film grades and from lower-flow heavy bubble grades. The density of 0.920 g/cm³ distinguishes it from lower-density film grades with higher impact and from higher-density extrusion grades with greater modulus.
Resin selection among butene, hexene, and octene LLDPE should be based on the specification of the finished article. In heavy-duty industrial bags where film thickness is above 100 µm, the toughness deficiency of a butene grade relative to an octene grade may be less significant because thick gauge carries the load; in thin gauge below 25 µm, the difference becomes more pronounced. LDPE may be blended with 31E to improve bubble stability and melt strength; the blend ratio must be optimized because density and melt index of the blend change linearly by weight fraction, but dart impact does not follow a simple rule of mixtures.
Film properties cannot be specified by the resin density and melt index alone; they are a function of gauge, blow-up ratio, frost line height, die design, and downstream treatment. Tensile properties are measured by ASTM D882 using machine-direction and transverse-direction specimens. Dart impact is measured by ASTM D1709 Method A or Method B; the two methods are not interchangeable because the dart geometry and drop height differ. Elmendorf tear is measured by ASTM D1922; the MD/TD ratio reflects molecular orientation and is often anisotropic in blown film. Haze is measured by ASTM D1003 and specular gloss at 45° by ASTM D2457. Seal strength is measured by ASTM F88 and hot-tack by ASTM F1921. Reported values without these standard designations and processing parameters are not suitable for specification purposes.
| Film property | Test method | Key variables affecting comparability |
|---|---|---|
| Dart impact | ASTM D1709 | Method A vs Method B, gauge |
| Elmendorf tear | ASTM D1922 | MD/TD, notch direction |
| Tensile properties | ASTM D882 | draw ratio, gauge profile |
| Seal strength | ASTM F88 | temperature, dwell, pressure |
| Haze | ASTM D1003 | film thickness, surface finish |
| Coefficient of friction | ASTM D1894 | slip/antiblock additive, corona |
Specimen conditioning is critical: ASTM D882 requires conditioning at 23 °C ± 2 °C and 50% ± 5% relative humidity, with thickness measured before testing. Thickness variation across the web can produce higher standard deviations in tensile and dart impact than resin lot variation. For valid comparison, samples should be collected after the line reaches steady state, not during startup or gauge adjustments. At a nominal gauge of 50 µm, blown film produced from butene LLDPE of 0.920 g/cm³ density and 1.0 g/10 min melt index may exhibit tensile and impact values within broad published ranges for this class; however, published data for this specific configuration is limited, and side-by-side trials on production equipment are required for reliable comparison. The coefficient of friction, if no slip or antiblock additive is present, is controlled by film surface oxidation, corona treatment, and roll tension rather than by resin melt properties alone. Outdoor film applications require UV stabilization; failure to add adequate hindered-amine light stabilizers can reduce elongation at break and impact after field exposure.
Regulatory assessments require the exact commercial formulation, because the base resin designation does not by itself clear a finished food-contact package. For U.S. food-contact applications, converters should verify that the specific grade meets FDA 21 CFR 177.1520(c) paragraphs 3.1a or 3.2a; the supplier’s food-contact letter should state the lot, additive package, and any conditions of use. For EU applications, compliance with EU 10/2011 and national migration limits must be assessed on the final film or article. The resin should not be processed in equipment contaminated with PVC or acetal; at LLDPE processing temperatures, such contamination can generate corrosive or odorous decomposition products. Storage in a dry warehouse at 40 °C or below, away from direct sunlight, maintains stabilization. Pre-drying is not required unless condensation is present; if surface moisture is observed, a hot-air dryer at 60 °C to 70 °C for 1 h is sufficient, but extended hot-air residence should be avoided to minimize fines generation.