    Specifications
    HS Code 608030
    Productname NOVA Chemicals Sclair 2316 LLDPE Injection Molding Resin
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.923 g/cm³
    Meltindex 20 g/10 min (190°C/2.16 kg)
    Tensileyieldstrength 10.3 MPa
    Tensilebreakstrength 12.1 MPa
    Elongationatbreak 800%
    Flexuralmodulus 210 MPa
    Vicatsofteningpoint 90 °C
    Heatdeflectiontemperature 50 °C at 0.45 MPa
    Notchedizodimpact 80 J/m
    Shoredhardness 50
    Moldshrinkage 1.5-2.0%
    Meltingtemperature 120 °C
    Crystallizationtemperature 100 °C

    As an accredited NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg polyethylene bags on wooden pallets, 55 bags per pallet (1,375 kg net), stretch-wrapped for transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin, palletized and shrink-wrapped.
    Shipping NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin is shipped as a non-hazardous thermoplastic in moisture-proof 25 kg bags on stretch-wrapped pallets, or in bulk trucks/railcars. Store in a dry, cool, ventilated area away from direct sunlight, heat, and ignition sources. Handle according to the SDS.
    Storage Store NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin in a cool, dry, well-ventilated warehouse at ambient temperature and low humidity. Keep original bags closed, palletized, and off the floor. Protect from direct sunlight, moisture, excessive heat, flames, sparks, and oxidizing agents. Follow first-in, first-out stock rotation. Avoid crushing, contamination, or damaged packaging.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original, unopened packaging in a cool, dry area.
    Application of NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin

    At the thin-wall end of food-service packaging, a melt flow rate of 55 g/10 min at 190 °C/2.16 kg under ASTM D1238 and ISO 1133-1:2022 permits NOVA Chemicals Sclair® 2316 to fill 0.5–1.0 mm nominal wall sections at lower injection pressures than fractional-melt injection grades. On stacked tooling with valve-gated hot runners and chilled water held at 8–12 °C, accumulator-assisted injection speeds in the 150–250 mm/s range are required to prevent premature freeze-off in cavity-to-gate flow-length ratios above 150:1. The critical processing conflict is that excessive screw speed and back pressure can raise melt temperature above 230 °C, where oxidative degradation reduces ring-stiffness retention and creates an off-taste risk in dairy packaging; conversely, insufficient melt homogeneity produces visible flow lines at the stacking shoulder. Regulatory compliance for direct food contact rests on FDA 21 CFR 177.1520(c) for olefin polymers and on Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm² for the finished article. In monolayer structures, Sclair 2316 is used at 96–100 wt%, with a white TiO₂ concentrate added at 2–4 wt% where opacity is required; reprocessed sprues and edge trim from the same conversion line may be reintroduced up to 20–30 wt% only if the resulting melt flow rate remains within the processor's validated control window. Downstream molding uses closed-loop cavity pressure transducers and two-stage injection units to decouple plastication from injection; the resulting parts—deli cups, condiment cups, dairy single-serve cups, and snap-on lids in 0.5–1.0 mm wall stock—are inspected for sealing-rim flatness and drop impact after chilled storage. The table below consolidates the compliance test framework for monolayer LLDPE food-contact lids and cups.

    Monolayer LLDPE food-contact compliance and resin fluidity test framework
    Control areaStandard or regulationTest condition or limit
    Melt flow rateASTM D1238, ISO 1133-1:2022190 °C/2.16 kg; typical value 55 g/10 min
    Solid-phase densityASTM D792, ISO 1183-1:20190.924 g/cm³
    U.S. food contactFDA 21 CFR 177.1520(c)Olefin polymer; conditions of use A–H; extractives limits apply
    EU food contactRegulation (EU) No 10/2011Overall migration limit 10 mg/dm²; Annex II specific migration limits

    What Gate Geometry and Cooling Configuration Reduce Ovality in High-Flow LLDPE Lids?

    In closure overcaps and snap-fit lids, radial flow from a center gate freezes orientation stresses that later relax as ovality; the problem intensifies when a single hot tip feeds multiple cavities through unbalanced runners. The accepted corrective approach is to move gating to a diaphragm gate or a three-plate pin gate that distributes flow circumferentially, while mold cooling at 10–16 °C with beryllium copper core inserts extracts heat from the thick hinge and rim regions at rates sufficient to prevent post-ejection distortion. Compliance for these articles follows FDA 21 CFR 177.1520(c) for food-contact lids and REACH 1907/2006 for the EU market; if colored masterbatches are used, pigment selection must respect REACH Annex XVII restrictions for cadmium, lead, and hexavalent chromium. The formulation addition ratio for lids that must denest on high-speed filling lines is 97–100 wt% Sclair 2316, with erucamide slip at 500–1,000 mg/kg and silica antiblock at 1,000–2,000 mg/kg where warm warehouse blocking is observed; the additive letdown is made as a split masterbatch to avoid screw slippage in single-stage reciprocating screws. Slip additive migration kinetics is time- and temperature-dependent, and lids stored above 35 °C may show denesting changes within 14 days if the erucamide dosage is too high. Downstream processing uses high-speed injection units with 20–40 mm screw diameters and clamp forces sized to maintain cavity pressure below 70–80 MPa across the projected area; holding pressure is maintained until gate freeze, then terminated to avoid overpacking the rim. Finished terminal products include coffee can overcaps, aerosol dust covers, thin-wall container snap lids, and cosmetic jar overcaps.

    Unlike thin-wall food-service parts, rigid houseware and storage articles produced from Sclair 2316 are typically filled at wall sections of 1.5–3.0 mm, where the processing risk shifts from flash and freeze-off to sink marks, warp after unmolding, and rib-base cracking under stacking loads. Compliance for this segment is dominated by REACH 1907/2006 Annex XVII and, where articles may store dry food, FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; articles marketed as toy boxes may additionally require mechanical testing under ASTM F963 or EN 71-1. The formulation addition ratio for storage totes and crates is 94–100 wt% Sclair 2316, with a UV stabilizer masterbatch at 1–3 wt% for garage or outdoor use and a color concentrate at 2–5 wt%; post-industrial regrind is used at 20–40 wt% only after notched Izod impact retention is verified under ASTM D256 across five heat histories. Downstream production uses cold-runner direct sprue gating into multi-cavity tools with polished ejection surfaces; packing pressure is held at 60–80% of the injection peak, and cooling time is controlled by the thickest rib intersection rather than the nominal wall. Terminal part types include under-bed storage bins, stackable distribution crates, drawer organizers, and lidded garage totes. The operational boundary for unpigmented LLDPE in this segment is continuous service above 60 °C, where load-induced deformation becomes significant relative to stacking loads.

    Living-Hinge and Snap-Fit Fatigue Boundaries in Toy Components

    Toy and recreational component molding with Sclair 2316 uses the material's low-temperature impact to satisfy drop-test requirements, but regrind-induced viscosity loss narrows the processing window and can produce brittle failure at knit lines in multi-cavity tools. Under ASTM F963 and EN 71-1, finished toys must pass small-object and use-and-abuse mechanical tests; material compliance under EN 71-3 restricts migration of elements, and REACH Annex XVII restricts phthalates and certain heavy metals in the plasticized compound. Formulation addition ratio for toy components is 95–100 wt% Sclair 2316, with a non-phthalate color masterbatch at 1–4 wt%; regrind is capped at 25 wt% unless drop-weight impact and notched Izod values under ASTM D256 and ASTM D1822 tension-impact testing are confirmed for the specific cavity layout. Downstream processing employs low-compression screws with reverse-taper nozzles to prevent drool at melt temperatures of 190–230 °C, and cavity pressure monitoring prevents overpack in thin hinge regions. Terminal finished product types include flexible toy vehicle wheels, doll furniture components, construction set connectors, and snap-fit recreational parts.

    When Post-Industrial Regrind Is Restricted in Pharmaceutical Dosing-Aid Molding

    For pharmaceutical packaging and dosing aids, validation requirements tighten because melt-flow drift affects the dimensional stability of graduation markings and interference fit. Materials are assessed under USP <661.1> and USP <661.2> for plastic packaging systems, while direct and indirect food-contact applications require FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; good manufacturing practice does not permit rework from non-controlled sources. The formulation addition ratio is 95–100 wt% Sclair 2316, with an antistatic and slip masterbatch at 0.5–1.5 wt% where automatic dosing equipment requires consistent surface resistivity and denesting. Downstream processing occurs in cleanroom injection molding with positive-pressure HEPA filtration, and pre-drying is not required below 60% relative humidity because LLDPE does not hydrolyze, though surface moisture at higher RH is removed by hopper drying at 60–70 °C for 1–2 h. Cavity pressure curves are validated across multiple production lots to maintain the fill length of dosing graduations. Terminal product types include oral dosing cups, measuring spoons, bottle adapters, and desiccant cartridge housings.

    Material handling trays and dunnage platforms molded from Sclair 2316 are a lower-complexity segment in which cost is driven by cycle time and regrind tolerance rather than appearance. Compliance is usually limited to REACH 1907/2006 and RoHS Directive 2011/65/EU; if reusable food logistics containers are produced, EC 1935/2004 and EU 10/2011 apply as framework support. The typical formulation addition ratio is 90–100 wt% Sclair 2316, with 0–10 wt% compatible polyolefin regrind and a UV stabilizer masterbatch at 2–4 wt% for outdoor yard exposure. Processing uses low-cost open-runner tools with wall thicknesses of 2.5–4.0 mm, direct sprue gating, and flat-plate ejection. Terminal product types include stackable order-picking trays, interlayer dunnage sheets, and distribution-center tote inserts.

    Free Quote

    Competitive NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin is a high-flow linear low-density polyethylene formulated for thin-wall injection molding, closures, overcaps, and disposable packaging applications. The nominal density is 0.924 g/cm³ when tested under ASTM D792, and the nominal melt index is 50 g/10 min at 190 °C/2.16 kg under ASTM D1238. These values place the grade in the LLDPE density range but at a melt-flow range substantially higher than conventional blow-molding, cast-film, or general-purpose LLDPE grades. The resin is supplied in pellet form with a stabilization package intended for injection molding thermal history. Lot-specific release data should be obtained from the manufacturer certificate of analysis for mold-filling simulation and clamp-force calculation.

    Typical mechanical values reported for injection-molded specimens include tensile yield strength of approximately 11 MPa under ASTM D638, tensile elongation at break above 500 %, secant flexural modulus at 1 % strain of approximately 260 MPa under ASTM D790, Shore D hardness of 51 under ASTM D2240, and Vicat softening temperature near 86 °C under ASTM D1525. These values are typical laboratory results and do not constitute release specifications. Changes in gate geometry, cooling rate, regrind content, and pigment loading can shift the final part properties.

    Rheological Signature and High-Shear Processing Boundaries

    Under capillary flow at apparent shear rates from 10 s−1 to 1000 s−1, the high melt index of Sclair® 2316 suppresses melt pressure accumulation in thin-wall fills. The grade exhibits shear-thinning behavior, but the lower elastic memory associated with its molecular architecture reduces die swell at the nozzle and flash at the sprue gate. Reciprocating-screw injection machines with L/D ratios of 20:1 to 24:1 and compression ratios of 2.5:1 to 3.5:1 are suitable. Barrel temperature profiles from feed zone to nozzle typically range from 160 °C to 220 °C. A flat or slightly rising profile is acceptable; the nozzle should not exceed 230 °C unless cycle-time constraints require a short deviation.

    Injection pressure depends on flow length, wall section, and gate type. For thin-wall closures with nominal wall thickness of 0.5 mm to 1.0 mm, injection pressure commonly remains below 80 MPa. Mold temperature should be maintained between 10 °C and 40 °C to promote fast solidification and economical cycle times. Projected-area clamp force calculations of 3 kN/cm² to 5 kN/cm² reduce the risk of flash in multi-cavity tools. Back pressure should be limited to 0.5 MPa to 1.0 MPa to avoid excessive shear work. Screw speed is typically set between 80 r/min and 150 r/min, although the screw diameter and shot size must govern the final recovery rate.

    What Distinguishes a Narrow Molecular Weight Distribution in Injection Molding?

    Molecular weight distribution affects melt elasticity, frozen-in orientation, die swell, and dimensional repeatability. A narrow-distribution grade such as Sclair® 2316 reduces the high-molecular-weight tail responsible for pronounced die swell and shear-induced melt fracture. This architecture produces lower orientation-driven shrinkage differentials along flow and transverse axes and improves dimensional control in flat lids and continuous-thickness packaging. The trade-off is lower melt tension, which makes the resin unsuitable for blown-film bubble stability, extrusion coating, blow molding, or profile extrusion operations requiring high melt strength.

    Compared with a fractional-melt LDPE injection grade of density 0.920 g/cm³ and melt index 2 g/10 min, Sclair® 2316 fills thin sections at lower injection pressure and permits shorter gate-freeze time, but may exhibit lower environmental stress crack resistance and reduced sub-ambient impact strength. The product is positioned for injection molding only and should not be substituted into rotational molding, pipe, film, or sheet processes without process-specific validation.

    Comparative molding trials for thin-walled closures demonstrate that a high-flow LLDPE of density 0.924 g/cm³ and melt index 50 g/10 min fills annular geometries at lower melt pressure than an LDPE injection grade with melt index 20 g/10 min. Against an HDPE injection grade of density 0.952 g/cm³, Sclair® 2316 shows lower flexural modulus and lower heat deflection temperature but higher elongation at break and improved conformity to dimensional variation in flexible closures. Against a clarified random copolymer polypropylene with melt flow rate 25 g/10 min at 230 °C/2.16 kg, the polypropylene produces higher stiffness and better living-hinge fatigue resistance, whereas the LLDPE provides greater low-temperature toughness. Published data for direct property comparisons under identical molding conditions is limited; converter trials on the intended mold remain the reference method for part-specific validation.

    When Process Temperatures Approach Thermal Oxidation Limits

    The high melt index of Sclair® 2316 permits fast injection at relatively low melt temperatures, so thermal stabilizer consumption is normally not the controlling variable in short-cycle work. However, prolonged residence time at melt temperatures above 240 °C can initiate oxidative chain scission and crosslinking, leading to gel defects, viscosity drift, and odor development. If hold-up time exceeds 5 min above 240 °C, purging with a low-melt-index polyolefin and reducing screw speed to limit shear heating are recommended. Vented barrels are unnecessary when moisture content is below 200 ppm. If storage relative humidity exceeds 60 %, pre-drying at 70 °C to 80 °C for 2 h is advisable. Purging with halogenated or acidic compounds should be avoided; polyolefin-grade purge materials are preferred.

    Interpreting Shrinkage Anisotropy in Polyolefin Molds

    Shrinkage measured after 24 h under ASTM D955 typically falls between 1.4 % and 2.2 %, with flow-direction shrinkage generally higher than transverse-direction shrinkage. The differential arises from chain orientation frozen into the part during filling and packing. Excessive pack pressure can increase flow-direction shrinkage, while insufficient pack time raises overall shrinkage and produces sink marks at rib intersections or boss locations. Maintaining core temperature 5 °C to 10 °C lower than cavity temperature biases crystallization toward the cavity surface and can reduce warpage in rectangular closures. Post-mold crystallization adds measurable incremental shrinkage during the first 24 h; dimensional inspection should therefore be delayed or normalized to ASTM D955 conditioning requirements.

    Gate geometry should provide a wide, short land to avoid excessive shear heating at thin wall sections. For parts under 0.6 mm wall thickness, hot-runner systems with valve gates and independent temperature control are preferred. Gate freeze-off time is shorter than that of lower-melt-index LLDPE because the high melt index accelerates solidification. Packing must therefore be completed before the gate freezes; otherwise sink marks develop on the opposite side of ribs and bosses. In multi-cavity tools, melt temperature variation greater than 5 °C across cavities can shift fill time and create dimensional outliers. Cold-runner sprue and runner scrap can be reground and reintroduced at 20 % to 30 % by weight where end-use conditions permit; higher regrind fractions may reduce impact strength and raise melt viscosity variation.

    Regulatory Conformance and Food-Contact Verification

    Food-contact suitability is typically assessed under FDA 21 CFR 177.1520(c) for olefin polymers and under EU Regulation (EU) No 10/2011. Under EU 10/2011, the overall migration limit is 10 mg/dm² of food-contact surface area. Specific migration of additives must be verified on the finished article by the converter because processing aids, colorants, and regrind incorporation can alter the migration profile. The resin is not a food additive and is not intended for medical implant, parenteral, or pharmaceutical primary packaging unless suitability is separately established under end-use requirements. REACH obligations under Regulation (EC) No 1907/2006 require article producers to confirm that no substance of very high concern exceeds 0.1 % w/w in the article. RoHS Directive 2011/65/EU restrictions for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE apply to electrical and electronic equipment applications only.

    Standard or Regulation Designation Applicability
    United States food contact FDA 21 CFR 177.1520(c) Olefin polymers; final article suitability subject to condition of use and additive compliance
    European food contact EU Regulation (EU) No 10/2011 Overall migration limit 10 mg/dm²; specific migration limits verified by converter
    REACH Regulation (EC) No 1907/2006 SVHC candidate list threshold 0.1 % w/w in the article
    RoHS Directive 2011/65/EU Pb, Hg, Cr(VI), PBB, PBDE at 0.1 % w/w; Cd at 0.01 % w/w in EEE applications

    Processors should confirm that the final molded article is evaluated against the applicable food-contact or safety standard under actual conversion conditions, because the migration behavior of a completed closure or lid may differ from that of the base resin pellet.