| HS Code | 249124 |
| Density | 0.923 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 15 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 12.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 310 MPa |
| Notched Izod Impact Strength | 60 J/m |
| Vicat Softening Temperature | 93 °C |
| Shore D Hardness | 50 |
| Brittleness Temperature | < -70 °C |
| Melt Temperature Range | 190-230 °C |
| Mold Temperature Range | 20-50 °C |
As an accredited NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin is packaged in 25 kg bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25 kg bags of NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin for export. |
| Shipping | NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin is typically shipped as free-flowing pellets in 25 kg moisture-barrier bags stacked on pallets, stretch-wrapped for stability, or in bulk trucks/railcars. Keep containers closed, store cool and dry, avoid excessive heat, sunlight, or contamination, and follow applicable transport and safety regulations. |
| Storage | Store Sclair 2315 LLDPE resin at ambient temperature in a dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags or containers sealed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged high temperatures and UV exposure. Use good housekeeping to prevent pellet spills and slipping hazards. |
| Shelf Life | Stable and indefinite under normal storage; store in cool, dry, ventilated area away from direct sunlight, moisture, and excessive heat. |
NOVA Chemicals Sclair 2315 is classified in published supplier documentation as a high-flow linear low-density polyethylene injection molding resin with a nominal melt flow index of 15 g/10 min under ASTM D1238 at 190 °C and 2.16 kg, and a nominal solid-state density of 0.925 g/cm³ under ASTM D1505. The grade is used for non-food storage articles when the tool combines a deep draw, snap-fit undercuts, and a large flat panel that must resist corner-stress whitening. On a general-purpose reciprocating screw with a 20:1 L/D ratio and a compression ratio of 2.5:1, the start-up barrel profile for natural resin is 40 °C feed, 190 °C compression, 200 °C metering, and 205 °C nozzle. Pre-drying is not required for silo-stored resin because linear low-density polyethylene is not hydrolytically sensitive, but condensation on pellets transferred from an unheated warehouse into a warm molding bay can create splay-like surface defects; bags should be conditioned for 24 h at the molding bay temperature before opening. The low melt strength of the material makes the hold-pressure setting more sensitive than a fractional-melt grade at the same density. In an unlabelled storage lid with a projected area of 0.12 m², a nominal wall thickness of 1.6 mm, and a central sprue gate, the flow front reaches the outer edge in approximately 1.8 s at 190 °C melt temperature. Ejection at 18 s with a 28 °C mold produces low gloss variation; reducing the mold temperature to 15 °C shortens the cycle to 14 s but increases sink over ribs and creates a visible gloss boundary on the top surface, which is managed by raising first-stage hold pressure from 35 MPa to 45 MPa for 1.0 s. Living-hinge features molded from this resin should be gated so that the melt front crosses perpendicular to the hinge axis; this reduces molecular orientation across the hinge line and delays flex fatigue. Published data for this specific hinge configuration is limited, but the low crystallinity associated with the 0.925 g/cm³ density class preserves hinge ductility better than a high-density grade at equivalent thickness.
In thin-wall dairy, deli, and take-out containers with sidewall thickness between 0.55 mm and 0.9 mm, the injection pressure window is controlled by the flow-length-to-wall-thickness ratio rather than by the nominal melt flow index alone. A sidewall of 0.8 mm at a flow length of 120 mm fills reliably at 220 °C melt temperature and injection velocity of 80 mm/s; when the same part is reduced to 0.6 mm, short shots occur unless the injection velocity is raised to 120 mm/s and the melt temperature is moved to 235 °C. The practical ceiling is not the hydraulic pressure of the press but the point at which excessive shear raises local melt temperature at the gate above 250 °C, producing taste and odor degradation products that fail organoleptic testing. Tooling for this geometry should use hot-edge gates with a land length of 0.8 mm and a gate diameter between 50% and 60% of the wall thickness; a smaller gate freezes before packing is complete, and a larger gate produces gate blush on the outside surface. The hold-pressure profile should be stepped: 65 MPa for 1.2 s, 45 MPa for 2.5 s, and 20 MPa until gate freeze. Natural regrind at 20 wt% does not alter overall migration when tested under EN 1186-1, but post-consumer scrap is outside the supplier food-contact certificate and must be excluded from food-contact production. Finished articles are assessed for migration under EU 10/2011, and organoleptic acceptance for dairy contact is evaluated by EN 1622 or ASTM E460. U.S. food-contact use falls under 21 CFR 177.1520(c), provided the converter validates the specific masterbatch carrier system and the end-use conditions of use.
Beverage and personal-care closures molded from Sclair 2315 attain an interference fit on high-density polyethylene bottles and survive top-load deflection above 2 mm without stress cracking when the thread geometry is controlled. The critical test is not the as-molded removal torque but the removal torque after immersion in a 10% nonionic surfactant solution at 60 °C for 72 h. During filling, the closure bridge is compressed radially by 0.25 mm to 0.40 mm; the resulting hoop stress is amplified by surfactant migration into the polymer matrix, which lowers the stress-crack initiation threshold. Tooling for this application should set the minor thread diameter to produce an interference of 0.30 mm maximum and avoid sharp thread crests with root radii below 0.5 mm. Mold temperature should not exceed 30 °C because rapid surface cooling reduces spherulite size and increases elasticity at the inner seal surface, improving seal recovery after thermal cycling. When a tamper-evident band is included, the bridge rails should be notched to a residual wall of 0.35 mm; this permits breakage without generating strings that would compromise the container seal. Polyolefin closures with an EVA or plastisol gasket must use a gasket formulation individually certified under 21 CFR 177.1210; the LLDPE resin compliance does not automatically extend to the gasket material. Torque retention after thermal cycling from 4 °C to 60 °C is tested by measuring removal torque before and after a 24 h, 60 °C water bath according to ASTM D3198 or a customer-specific torque-time specification. The finished closure must also pass the container-top load test under ASTM D2659 if column stacking is part of the distribution chain.
Stackable and nesting crates are produced with sidewall thicknesses of 2.5 mm to 4.0 mm to pass drop-impact tests at -20 °C. The long cooling time required for these sections creates a gate-freeze constraint on cycle time because the sprue and gate solidify before the thick sidewall core is fully packed. For a 600 mm × 400 mm crate with a 3.2 mm sidewall and a projected area of 0.24 m², the clamp force requirement is normally in the range of 120 tonnes to 160 tonnes, and the injection phase lasts 2.5 s to 3.5 s at 70 MPa. When the part includes ribbing with a depth-to-width ratio above 1.2, ejection at a surface temperature of 65 °C can cause rib pull-out because the LLDPE has not completed solidification. The mold cooling circuit should therefore use turbulent water at 15 °C to drop surface temperature below 55 °C before opening. The impact requirement for refrigerated distribution is usually validated by dropping a fully loaded crate from 1.2 m onto concrete at -20 °C, with acceptance based on no visible crack or fragment release. LLDPE of the 0.925 g/cm³ class passes this condition when the corner column zones contain no weld lines; if weld lines are unavoidable, they should be moved to the center of the side panel where the bending moment is lower. UV stabilization for outdoor storage requires a hindered amine light stabilizer masterbatch; without UV protection, stored crates degrade after approximately one year of direct sunlight in temperate latitudes. Inorganic pigments such as rutile at 4 wt% can reduce dart-drop impact by approximately 15% because large particles act as stress concentrators, but a polyolefin-carrier color concentrate at 3 wt% does not significantly shift the melt index.
Open-head pails and shipping drums made from Sclair 2315 require a processing philosophy different from thick-wall crates because the drawdown of the side wall during core cooling produces differential shrinkage between the bottom center and the rim. The bottom section is typically 2.8 mm, the sidewall tapers from 2.5 mm at the bottom to 1.8 mm at the rim, and the rim diameter must be held to ±0.8 mm for a consistent cover fit. The holding pressure profile compensates for the variance in flow path length: 60 MPa for 1.5 s, 40 MPa for 3.0 s, and 25 MPa for 5.0 s minimizes sink at the bottom-slab intersection. Stacking load capacity is not a tensile-strength issue; it is a creep failure governed by the tightness of the rim gusset. When the pail is stacked for 30 days at 40 °C with a head load of 100 kg, sidewall strain remains below 2% if the rim is filled without a packing transition. The drop test for UN certification of open-head pails under 45 kg capacity is performed per 49 CFR 178.603 with a drop height of 1.2 m at 18 °C and after conditioning at -18 °C. The resin by itself does not provide UN certification; the converter must submit the finished article to a certification agency. Food-contact status for bulk liquid transport is subject to EU 10/2011 overall migration tests using simulant D1 or D2, depending on the food type, with migration limits of 10 mg/dm² and 60 mg/kg for the finished pail. Closure fitment tolerances are verified with a bung removal torque of 5 N·m under the customer-specific lid test procedure.
Plugs and secondary seal liners require the LLDPE to be processed at the low end of the temperature range to keep post-mold shrinkage predictable. A plug with an outer diameter of 50 mm and a lip seal height of 2.0 mm is molded to a diameter of 50.35 mm to allow for 0.7% post-mold shrinkage. If the mold cooling circuit is configured with dual spirals, diameter repeatability is ±0.08 mm. When cooling water at 25 °C is replaced by water at 10 °C, the part cools 4 s faster, but the skin layer forms before the core has been fully packed, causing internal voids that reduce the plug compressive seal by more than 15% in a leak test. Cooling water should therefore not be reduced below 18 °C for thin lip features unless injection speed and hold time are simultaneously increased. The seal lip is designed with a 0.6 mm radius and a 0.25 mm interference against the bore; the resin has enough creep resistance for short-term hydrostatic sealing but is not suitable for continuous pressure above 0.2 MPa unless the part is reinforced with a thicker support ring. If the application involves pharmaceutical liquid contact, the converter must qualify migration under USP <661.1> or EU 10/2011 and must confirm that the resin does not contain intentionally added phthalates or bisphenol A. The resin supplier’s regulatory certificate should be compared against the latest REACH candidate list under EC 1907/2006.
| Regulatory domain | Standard or method | Verification criterion |
|---|---|---|
| U.S. food contact | 21 CFR 177.1520(c) | Olefin polymer compliance; end-use conditions of use A–H must be validated in finished article |
| EU food contact | EU 10/2011 | Overall migration < 10 mg/dm² or < 60 mg/kg depending on article geometry |
| Packaging heavy metals | 94/62/EC | Sum of Pb, Cd, Hg, Cr(VI) < 100 mg/kg |
| REACH | EC 1907/2006 | SVHC declaration threshold < 0.1% w/w per applicable candidate list |
| RoHS | 2011/65/EU | Pb < 1000 ppm; Cd < 100 ppm; Hg < 1000 ppm; Cr(VI) < 1000 ppm |
| Pharmaceutical contact | USP <661.1> | Finished article migration and physicochemical suitability under dosage-form specific protocols |
Competitive NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair 2315 is an ethylene/1-butene linear low-density polyethylene injection molding grade designed for high-output conversion of closures, overcaps, housewares, appliance components, and thin-wall packaging parts. The resin is characterized by a nominal density of 0.930 g/cm³ determined under ASTM D792-20 or ISO 1183-1:2019, and a melt mass-flow rate of 15 g/10 min measured at 190 °C and 2.16 kg load per ASTM D1238-20 or ISO 1133-1:2022. Published typical values for injection molded test specimens include tensile yield strength near 11 MPa per ASTM D638-14, flexural modulus near 350 MPa per ASTM D790-17, and elongation at break exceeding 800%. These are published typical values, not engineering design limits or lot-specific specification guarantees.
| Property | Test Method | Typical Value |
|---|---|---|
| Density | ASTM D792-20 / ISO 1183-1:2019 | 0.930 g/cm³ |
| Melt mass-flow rate | ASTM D1238-20 / ISO 1133-1:2022 | 15 g/10 min at 190 °C/2.16 kg |
| Tensile yield strength | ASTM D638-14 | 11 MPa |
| Flexural modulus | ASTM D790-17 | 350 MPa |
| Elongation at break | ASTM D638-14 | > 800% |
| Vicat softening temperature | ASTM D1525-17 | 95 °C |
Because the comonomer is 1-butene, the polymer contains short-chain branches along an essentially linear backbone. This structure lowers crystalline density relative to unimodal HDPE while preserving sufficient crystallinity for rapid solidification. The 15 g/10 min melt mass-flow rate places the grade in the high-flow LLDPE injection segment, allowing thin wall sections and long flow paths at moderate clamp force. In closure and fitment applications, that flow characteristic is typically balanced against a slightly lower modulus than HDPE alternatives.
Relative to high-pressure LDPE of similar melt index, Sclair 2315 possesses a narrower molecular weight distribution and no long-chain branching. The practical differences are lower melt elasticity, reduced die swell, and improved environmental stress-crack resistance. In solid-state performance, the LLDPE architecture also improves low-temperature impact and resistance to flexural fatigue. Against unimodal HDPE injection grades of comparable flow, Sclair 2315 has lower crystalline density, lower flexural modulus near 350 MPa, and higher elongation before yield. HDPE grades offer greater modulus and barrier properties but generally exhibit higher post-mold shrinkage and lower ductility in drop-impact tests. These differences are most visible in overcaps and snap-fit closures, where Sclair 2315 can flex without stress whitening under repeated removal and reseating.
Within ethylene/α-olefin copolymers, substitution of 1-butene with 1-hexene or 1-octene modifies branch length and intermolecular branching distribution. Sclair 2315 is a 1-butene grade. Comparative studies of gas-phase LLDPE systems indicate that butene-based resins may show lower puncture resistance than octene-based resins at equivalent density and melt index, while often providing lower extractables and acceptable organoleptics for closure applications. Published data for this specific configuration is limited; finished-part testing remains necessary when puncture or seal integrity is the controlling design requirement.
For closure and fitment applications where stress cracking is controlled by polymer crystalline density and comonomer type, environmental stress-crack resistance is typically evaluated under ASTM D1693-21 using 10% Igepal CO-630 and a constant-strain bent strip. LLDPE grades of this density commonly show F50 values beyond 1000 h; published data specific to Sclair 2315 are limited. Finished closures should be tested under end-use chemical exposure because molded-in stress and service strain dominate field failure.
The resin is processed on conventional reciprocating-screw injection molding machines fitted with general-purpose polyolefin screws of 20:1 to 24:1 L/D and compression ratios from 2.5:1 to 3:1. Melt-temperature settings are normally maintained between 200 °C and 240 °C. Sustained operation above 260 °C can initiate oxidation, yellowing, and loss of impact strength. Mold temperatures from 10 °C to 50 °C are common; lower temperatures shorten cycle time and higher temperatures improve surface gloss and weld-line strength. Injection velocity should be profiled to avoid gate blush and jetting. Because Sclair 2315 has a 15 g/10 min melt mass-flow rate, high-speed fill settings often produce lower shear heating than fractional-melt grades but increase the risk of flash at worn parting lines or when available clamp force is marginal.
Pre-drying is generally unnecessary because the resin is not hygroscopic. Condensation can nevertheless form when cold pellets are transferred into humid ambient air. In such conditions, a dry-air hopper dryer set at 60 °C for approximately 1 h removes surface moisture and prevents splay. Hold pressure is normally set to 50% to 70% of peak injection pressure to compensate for volumetric shrinkage in thick sections. Over-packing should be avoided because frozen-in stress increases warpage and reduces environmental stress-crack resistance in closure service.
When injection speed is not profiled for thin-wall tools with flow-length-to-thickness ratios above 200:1, the high-flow nature of Sclair 2315 can create jetting and flow marks rather than a uniform melt front. Published data for this specific configuration is limited; mold trials are required to establish the pressure-limited flow length for a given gate type, part thickness, and tool temperature.
Post-mold dimensional recovery in Sclair 2315 follows the general LLDPE pattern of anisotropic shrinkage driven by orientation, restraint, and cooling-rate gradients. Under ASTM D955-21, parallel shrinkage on rectangular plaques is often reported in the range of 0.015–0.025 mm/mm, with perpendicular shrinkage somewhat lower. Exact values depend on gate location, thickness, pack pressure, and mold temperature. For center-gated circular lids, tangential shrinkage is usually lower than radial shrinkage because of asymmetric orientation. For edge-gated rectangular components, differential shrinkage between flow and cross-flow directions can exceed 0.005 mm/mm. The associated process conflict is that raising mold temperature improves replication and reduces flow marks but lengthens cycle time and aggravates shrinkage anisotropy. Molders typically stage pack-pressure decay rather than applying constant hold pressure, allowing the gate to freeze under controlled pressure while limiting cavity overpack. The high melt index shortens the available pack window before gate freeze. Gate diameters below 0.8 mm in cold-runner tools or hot-runner tips below 0.6 mm can restrict packing and generate sink marks opposite ribs and bosses. Shrinkage prediction tools require measured pvT data from the resin supplier; where such data are unavailable, tooling should include steel-safe dimensions allowing additional cavity polishing after first-article inspection.
Rheological characterization of Sclair 2315 by capillary viscometry or parallel-plate oscillatory shear has not been published in detail by the supplier. In injection molding practice, the resin’s controlled molecular weight distribution and low high-molecular-weight tail produce stable melt flow. Apparent shear viscosity at 100 s⁻¹ and 220 °C is lower than that of fractional-melt LLDPE grades and higher than that of high-flow LDPE coating grades. The practical result is reduced injection pressure for a given flow length relative to resins below 5 g/10 min, permitting thinner wall sections or lower machine tonnage. However, the same flow character increases the risk of flash when the clamp force margin is less than 10% of calculated tonnage or when mold alignment surfaces are worn.
Batch-to-batch variance in Sclair 2315 is governed by gas-phase polymerization and catalyst system control. Incoming inspection commonly includes melt mass-flow rate, density, and visual pellet contamination. Lot-specific melt index shifts are process-relevant before they become specification-reject limits. A cushion of 3 mm to 6 mm and shot-weight stability monitoring are used to detect viscosity drift after lot changes. If cavity balance shifts by more than 5% in short-shot studies, hot-runner throttle adjustments or injection velocity profile changes may be required before dimensional quality is restored.
In hot-runner systems feeding 8 to 32 cavities, flow imbalance arises from unequal manifold channel lengths or temperature differences across the hot-runner block. Sclair 2315, with a melt mass-flow rate of 15 g/10 min, is sensitive to residence time in unoccupied channels during short cycles. Idle channels allow material to stagnate, and subsequent shots can deliver discolored or degraded resin to edge cavities. The hot-runner manifold is generally maintained near 210 °C to 230 °C to avoid excessive thermal exposure. Unused drops should be isolated by the hot-runner controller rather than mechanically plugged. Shear-history asymmetry also affects weld-line tensile properties. If two flow fronts meet after traveling through channels of different length or temperature, the resulting weld line may exhibit reduced elongation because the degraded front does not fully intermix. General LLDPE injection molding studies show weld-line elongation can drop by 30–60% relative to non-weld-line values when melt-temperature differentials exceed 15 °C at the flow front. Sequential valve gating or pressure-actuated pins are therefore used for large lids and flat components where weld lines are excluded from load-bearing regions.
For living-hinge applications, hinges should be oriented perpendicular to the predominant flow direction to avoid brittle fracture along molecular orientation. Hinge thickness below 0.25 mm may require post-mold flexing to orient the polymer and improve crack resistance. Published data for this specific configuration is limited; hinge performance should be validated under repeated flexural cycling using the finished tool and end-use exposure conditions.
Sclair 2315 is manufactured as an olefin polymer within the compositional scope of 21 CFR 177.1520 when catalyst residues and additives meet the applicable subpart limitations. End-use food-contact suitability depends on the final formulation, processing conditions, and intended food type; verification against the supplier’s food-contact statement is required. For EU food-contact assessment, the resin is evaluated under Commission Regulation (EU) No 10/2011 as amended, using EN 1186 migration-testing methods and EN 13130 specific-migration methods where applicable. For electrical and electronic equipment applications, compliance with EU RoHS Directive 2011/65/EU recast and Delegated Directive (EU) 2015/863 should be confirmed through the supplier’s compliance declaration. Candidate List screening under Regulation (EC) No 1907/2006 is required for durable articles. The resin is not recommended for sustained contact with strong oxidizing acids, aromatic hydrocarbons, or halogenated solvents, which can swell or degrade the polymer.
| Framework | Designation | Assessment Point |
|---|---|---|
| U.S. food-contact | 21 CFR 177.1520 | Olefin polymer clearance; verify formulation-specific limitations |
| EU food-contact | Regulation (EU) No 10/2011 | Overall migration and specific migration limits by food simulant |
| RoHS recast | Directive 2011/65/EU + (EU) 2015/863 | Restricted substances below maximum concentration values |
| REACH SVHC | Regulation (EC) No 1907/2006 | Candidate List screening; article communication duties apply |