| HS Code | 961545 |
| Resintype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene |
| Density | 0.920 g/cm³ |
| Meltindex | 0.75 g/10 min |
| Meltingpoint | 124 °C |
| Vicatsofteningpoint | 100 °C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 33.1 MPa |
| Elongationatbreak | 800 % |
| Tensilemodulus | 0.200 GPa |
| Dartimpact | 190 g |
| Elmendorftearmd | 300 g |
| Elmendorfteartd | 500 g |
| Haze | 11 % |
| Gloss | 65 % |
| Coefficientoffriction | 0.2 |
As an accredited NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin is supplied in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL: 18 pallets, 990 x 25 kg bags, 24.75 MT net NOVA Chemicals Sclair® 12J1 octene LLDPE film resin. |
| Shipping | NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin is not regulated for transport. It ships as non-hazardous solid pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Store in a cool, dry, clean area; protect from moisture, heat, and contamination. Use standard industrial handling; keep palletized loads stretch-wrapped. |
| Storage | Store Sclair® 12J1 Octene LLDPE Film Resin in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original bags or containers closed, clean, and on pallets to prevent moisture, dust, and contamination. Avoid strong oxidizing agents and physical damage. Use first-in, first-out inventory, good housekeeping, and ambient conditions. Ensure labels remain legible. |
| Shelf Life | Typically 24 months from date of manufacture when stored unopened in original packaging under dry, ambient conditions, away from direct sunlight. |
In monolayer and three-layer blown film structures for frozen-food packaging, Sclair® 12J1 is used as the sealant or core polymer where hexyl branches from the octene comonomer reduce secondary crystallization that causes brittle failure at freezer holding temperatures. The resin is characterized by a nominal density of 0.912 g/cm³ under ASTM D1505 and a nominal melt index of 1.0 dg/min under ASTM D1238 at 190 °C/2.16 kg. In a three-layer blown-film line equipped with a 55 mm grooved-feed extruder and a 250 mm spiral mandrel die with a die gap between 1.8 mm and 2.3 mm, the polymer is processed at melt temperatures from 205 °C to 230 °C with a blow-up ratio of 2.2:1 to 2.8:1. Internal bubble cooling is required above 150 kg/h throughput to hold frost line height within 450 mm–750 mm and prevent bubble instability during high cooling gradients. The formulation for freezer laminates commonly includes 10–20 wt% high-pressure LDPE to raise elongational viscosity, 0.5–1.0 wt% of a synthetic silica antiblock masterbatch, and an active erucamide slip concentration held below 450 ppm to avoid slip migration into the sealant interface after eight weeks of ambient warehousing at 23 °C. Heat-seal strength is measured according to ASTM F88/F88M-21 after sealing at 115 °C–125 °C with 0.5 s dwell. The peak force at 25 µm gauge must exceed 6 N/15 mm for vertical form-fill-seal operations. Food-contact conformance rests on FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm² by EN 1186-1. Terminal film is converted into frozen vegetable pouches, IQF poultry bags, and seafood barrier laminations where the sealant web is stored at -25 °C and then subjected to drop impacts. The operational boundary is that the resin should not be held at melt temperatures above 260 °C for more than 15 min during line stoppages because surface gel formation increases and the seal initiation temperature shifts upward by 2–4 °C.
Cast stretch cling film in the 12–20 µm gauge range is produced on single-screw cast lines with barrel diameters from 75 mm to 150 mm, screw L/D from 30:1 to 36:1, and die gaps between 0.5 mm and 0.9 mm. The melt temperature at the die lip is kept between 235 °C and 250 °C. Above 255 °C, thermo-oxidative scission of the octene copolymer lowers elongational viscosity and triggers draw resonance above 250 m/min. Chill roll temperature is held at 18–24 °C. The air gap is fixed between 10 mm and 15 mm to stabilize neck-in below 8% of die width. The formulation for cling performance normally includes 2.5–5.0 wt% of a polyisobutylene or low-density metallocene polyolefin tackifier masterbatch. The tackifier level is reduced by 0.5 wt% for each 5% increase in machine-direction pre-stretch above 200%. Edge curl is controlled by maintaining the difference between core and edge melt temperatures below 3 °C and by adjusting edge thickness by 0.5–1.0 µm relative to the sheet centre. Web tension on the primary unwind is limited to 10 N/cm at 12 µm gauge to prevent core collapse and blocking on the finished roll. Cling and puncture resistance are evaluated under ASTM D5458 and ASTM D5748. The internal release limit for puncture peak force at 17 µm is 12 N. Published data for this specific Sclair® grade in a 400% pre-stretch cast cling configuration is limited. Qualification on a single-ply lab coater with a 200 mm slot die is required before scale-up. The terminal film is used for A- and B-grade pallet wrapping of corrugated shippers, beverage trays, and white-goods containers at turntable speeds up to 35 rpm. The operational boundary is that the cast film line must be shut down for drying if raw resin moisture content exceeds 350 ppm by ISO 15512 because microscopic steam pockets at 250 °C melt temperature generate optical haze and pinhole defects.
Because the nominal melt index is 1.0 dg/min, the resin generates higher screw torque than 2.0–2.5 dg/min hexene LLDPE grades typically run on the same cast line. At screw speeds above 110 min⁻¹ on a 90 mm shallow-taper screw, barrel pressure rises above 320 bar and the melt temperature can exceed 250 °C. The extruder drive load is therefore limited to 75% of nameplate in continuous operation. This torque limit is the binding constraint for converters running 10 µm film at line speeds above 220 m/min. Converters blend 30–50 wt% of a 2.3 dg/min butene or hexene LLDPE to reduce pressure drop through the screen changer. The addition of a low-viscosity LLDPE, however, reduces dart impact under ASTM D1709-22 from the high-value range near 300 g at 25 µm to approximately 180–220 g. The blend ratio must be fixed by lot-to-lot film property testing rather than by pressure alone.
When spiral mandrel blown-film lines are configured for heavy-duty shipping sacks with finished aseptic liners, 12J1 is compounded in the core layer at 70–85 wt% with 15–30 wt% of a 0.3 dg/min high-pressure LDPE and 1.5–2.0 wt% of a carbon black or TiO2 masterbatch. The wide die gap of 2.0–2.8 mm is maintained with a blow-up ratio from 2.5:1 to 3.0:1 and a neck height of 600–900 mm to distribute melt stress and avoid shark-skin melt fracture beyond 320 s⁻¹ wall shear rate. Melt temperature at the die exit is set between 210 °C and 235 °C. The upper limit is constrained by the oxidation induction time of the polyethylene compounds, measured by ISO 11357-6 at 200 °C, which must remain above 20 min. For sacks intended for polymer granule export, the film is validated for dart impact according to ASTM D1709-22 Method A, Elmendorf tear according to ASTM D1922, and stress crack resistance according to ASTM D1693-15 Condition B in 10% Igepal CO-630. The terminal sack is also tested for drop failure after filling 25 kg of low-bulk-density flake at -10 °C. The accepted failure rate across three production campaigns is below 2% from a 1.2 m drop height. On a 65 mm grooved-feed extruder with barrel profile 180/200/215/220/225 °C and screw speed 90 min⁻¹, throughput is limited to 160 kg/h because higher screw speeds raise melt temperature above 235 °C and cause back pressure instability at the screen pack. The boundary condition for converters is that no more than 20 wt% recycled post-industrial edge trim should be introduced into the core layer without increasing antioxidant level by 0.05 wt%. Otherwise microgel content above 0.2% of web area reduces weld line integrity on the bottom gusset.
Solventless lamination structures using 12J1 as the sealant web in three-layer coextruded blown film are produced at 25–40 µm gauge. The core layer consists of 85–100 wt% 12J1 and the skins are made from an EVA or high-MFI LDPE sealing blend. The blown film tower is operated with a 1.8–2.2 mm die gap, 2.2:1–2.6:1 blow-up ratio, and melt temperatures from 205 °C to 225 °C. The lower melt temperature is used when solventless lamination bond strength must remain above 2.5 N/15 mm after seven days of cure at 35 °C. Corona treatment is applied inline to raise surface wetting tension to 38–42 mN/m measured by ASTM D2578. The treated surface is then laminated to PET or OPP within 12 h because corona decay on the ethylene-octene surface proceeds at approximately 2 mN/m per day under 50% RH. The adhesive coating weight of the solventless polyurethane system is kept between 1.2 g/m² and 1.8 g/m². Above 2.0 g/m², free isocyanate migration can interact with erucamide slip and reduce heat-seal strength at the finished pouch. For this reason the active erucamide content is limited to 350 ppm and the slip masterbatch is added only to the sealant skin, not to the lamination surface. The finished film is converted into stand-up pouches for dry powders, frozen custard inclusions, and pillow packs for grated cheese. Seal integrity is checked on a 10 kg dead-weight leak tester after 30 s at 650 mbar. The key incompatibility is that amine-based antifog concentrates should not be compounded into the same skin as the sealing layer because amine migration can shift the heat-seal initiation temperature upward by 5 °C. Acid-neutralized EVA skins are used where antifog performance is required.
| Regulatory scope | Test method or statute | Boundary condition for 12J1 packaging grade |
|---|---|---|
| United States food contact | FDA 21 CFR 177.1520(c) | Olefin polymer recognized for food contact; finished film must comply with extractable fraction limits in the regulation for frozen-food use condition G. |
| European Union food contact | Regulation (EU) No 10/2011 | Overall migration below 10 mg/dm² under EN 1186-1; specific migration of heavy metals per Annex II. |
| REACH SVHC | Regulation (EC) No 1907/2006 | Candidate list substances each below 0.1 wt% in the finished article. |
| RoHS recast | Directive 2011/65/EU | Lead, mercury and hexavalent chromium each below 0.1 wt%; cadmium below 0.01 wt%. |
Agricultural silage wrap in the 25–30 µm gauge range is produced on blown-film lines with a 2.0–2.5 mm die gap and a blow-up ratio of 2.3:1–2.8:1. The melt temperature is restricted to 205–225 °C to minimize degradation of the hindered amine light stabilizer package. The formulation comprises 100 parts by weight 12J1, 2.5 wt% of a 40% carbon black masterbatch for UV screening, 0.3 wt% of a HALS masterbatch, and 0.2 wt% of a benzophenone UV absorber. Film is tested for puncture peak force according to ASTM D5748. The acceptance threshold at 25 µm is 55 N when tested at 23 °C. The same film must retain at least 70% of that peak force after 500 h of accelerated weathering under ASTM G154-16 Cycle 1. Elmendorf tear in the machine direction is measured by ASTM D1922. The minimum value for a 25 µm film is 45 g at -10 °C after conditioning for 24 h. Terminal film is used to wrap round bales of grass silage with 8–10 layers on a bale wrapper operating at 24–28 rpm. The operational boundary is that films exposed to UV for more than 18 months in areas above 40° latitude are not suitable for reuse as top covers because transverse tear resistance falls below the safe handling limit. Field inspection for edge cracking is required every 6 months.
Thin-gauge bakery overwrap and paper-towel bundling films, where 12J1 is blended with 10–20 wt% high-pressure LDPE for stiffness, require only melt flow rate conformance to ASTM D1238 and seal initiation measurement per ASTM F88/F88M-21; no additional formulation auxiliaries are mandated beyond standard processing antioxidant, and the blown-film line is configured with a 1.0–1.2 mm die gap.
Competitive NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 12J1 is an ethylene–1-octene copolymer supplied as a linear low-density polyethylene film resin for blown film extrusion. The nominal density is 0.912 g/cm³ and the nominal melt index is 1.0 g/10 min when measured at 190 °C under a 2.16 kg load in accordance with ASTM D1238. The density–melt index pairing places the material in a high-toughness, downgauging-oriented segment of the LLDPE film market, but the octene comonomer is the defining structural variable. Unlike butene-based resins of equivalent density, 1-octene incorporation introduces hexyl short-chain branches, which alter the distribution of intercrystalline tie chains and shift the balance between stiffness, impact, tear, and low-temperature ductility.
Typical converting routes include monolayer and coextruded blown film for heavy-duty sacks, industrial liners, frozen food packaging, produce bags, and clear overwrap where puncture resistance and cold-room integrity are required. The grade may be used as a surface layer over HDPE or MDPE cores to obtain a structure with higher flexural stiffness while retaining the impact contribution from the octene-rich skin. Because film properties respond strongly to die geometry, quench rate, stalk height, and additive package, the values presented in this document are representative starting points and are not specification limits. The current certificate of analysis and the supplier’s technical data sheet remain the authoritative sources for lot-specific compliance.
At equivalent density and melt index, the length of the short-chain branch directly influences the probability of forming load-bearing tie molecules between lamellae. 1-Butene contributes ethyl branches with two carbon atoms, 1-hexene contributes butyl branches with four carbon atoms, and 1-octene contributes hexyl branches with six carbon atoms. The longer hexyl branch is excluded more efficiently from the orthorhombic polyethylene crystal lattice, leaving a greater portion of the chain in the amorphous phase where it can participate in interlamellar tie-chain formation. This structural difference is observed empirically as higher dart drop impact by ASTM D1709 and higher Elmendorf tear by ASTM D1922 when compared with butene-based LLDPE of the same nominal density and melt index.
The performance differential cannot be read reliably from melt index and density alone. Quench rate, frost line height, die gap, and film orientation all influence tie-chain concentration, and therefore a direct side-by-side evaluation on the target blown-film line is required before downgauging. Published side-by-side data for Sclair 12J1 and specific butene or hexene grades is limited; processors should generate comparative values using identical die, output, and blow-up ratio. Environmental stress-cracking resistance, commonly assessed by ASTM D1693, is also generally higher for octene-based LLDPE than for butene-based LLDPE, but the improvement should be quantified for the specific film structure and chemical exposure.
Sclair 12J1 is processed on single-screw extruders with L/D 24–30 and barrier screws designed for LLDPE. General-purpose polyolefin screws should be evaluated for melt-temperature uniformity and pressure stability before production runs. Starting conditions on conventional blown-film lines typically include a melt temperature of 210–230 °C at the die, a die gap of 1.0–2.0 mm, and a blow-up ratio of 2.0–3.0:1. The low melt index of 1.0 g/10 min will produce higher melt pressure and motor load than a 2.0 g/10 min resin of equivalent density, but the higher viscosity may improve bubble stability on high-stalk lines. Feed-throat water temperature is commonly maintained at 40–50 °C on grooved-feed extruders to avoid premature pellet fusion. Die temperatures above 250 °C increase the risk of additive degradation, gel formation, and odour; residence time in the die and adapter should therefore be limited.
The following table lists representative physical property values for Sclair 12J1. Film values are for 25 µm monolayer blown film unless otherwise noted, and the table is not a specification. The current manufacturer’s technical data sheet must be consulted for acceptance criteria.
| Property | Test method | Representative value |
|---|---|---|
| Nominal density | ASTM D1505 | 0.912 g/cm³ |
| Melt index | ASTM D1238 at 190 °C/2.16 kg | 1.0 g/10 min |
| Melting temperature | ASTM D3418 | 121 °C |
| Vicat softening temperature | ASTM D1525 | 100 °C |
| Tensile strength at yield, MD/TD | ASTM D882 | 10 MPa/10 MPa |
| Tensile strength at break, MD/TD | ASTM D882 | 42 MPa/34 MPa |
| Elongation at break, MD/TD | ASTM D882 | 600%/750% |
| Elmendorf tear, MD/TD | ASTM D1922 | 250 g/450 g |
| Dart drop impact, F50 | ASTM D1709 Method A | 850 g |
| Haze | ASTM D1003 | 6% |
| Gloss at 45° | ASTM D2457 | 70 |
Optical properties are particularly sensitive to line configuration. An IBC-equipped line with a dual-lip air ring and controlled frost line typically produces lower haze than an un-cooled line with a poorly adjusted air ring. For any specification-critical application, the above values should be reproduced on the target extruder using the intended film gauge and additive package.
For coextruded structures containing Sclair 12J1 in the skin layer, the resin is often combined with HDPE or MDPE in the core to raise stiffness while retaining the impact contribution from the octene phase. Corona treatment is commonly required when the film is printed or laminated. Surface tension should be raised to at least 38 dyn/cm for water-based inks and to 40–42 dyn/cm for solventless lamination. Treatment decay on low-density LLDPE can reduce surface tension by 2–4 dyn/cm within 24 h; in-line treatment or immediate converting is therefore preferred. Moisture uptake of LLDPE is low, and predrying is not normally required for pellets stored in closed containers at RH < 60%. If condensation has occurred during cold-weather unloading, a desiccant hot-air hopper dryer set at 70–80 °C for 2 h removes surface moisture. Hopper temperature should not exceed 80 °C because pellet agglomeration in the feed throat may occur.
Seal initiation for Sclair 12J1 is typically in the range of 95–110 °C when measured on 50 µm blown film with a 0.5 s dwell and 0.3 MPa jaw pressure; actual values depend on seal geometry, film thickness, and heat-transfer conditions. Hot tack measurements under ASTM F1921 are appropriate for high-speed packaging lines. Blending with LDPE at 5–20 wt% improves bubble stability and shrink characteristics but reduces dart impact and increases haze. The exact blend ratio should be established by a designed experiment using the target film gauge, seal jaw profile, and converting speed.
Cold-room overwrap, frozen food packaging, and ice storage liners require films that remain ductile below -20 °C. The low density and hexyl-branch architecture of Sclair 12J1 make it a candidate for such applications, but suitability must be demonstrated on the finished film because coextrusion, orientation, regrind loading, and additive variation can shift the ductile-to-brittle transition by several degrees. Testing should include ASTM D1709 dart impact after conditioning at -30 °C for 24 h and ASTM D3420 puncture at the same temperature. European specifications may use ISO 7765-2 for dynamic puncture evaluation.
For high-clarity overwrap, haze below 10% is achievable on film lines with optimized frost line, air ring, and die temperature; however, clarity claims must be measured on the target line using ASTM D1003. The grade is not intended for hot-fill or retort applications above 100 °C because mechanical integrity decreases near the Vicat softening range. Food-contact status may be assessed under FDA 21 CFR 177.1520(c) for olefin polymers, provided the finished film meets extractive limitations and the resin is used in accordance with the supplier’s food-contact letter. For European Union applications, compliance with EU 10/2011 requires migration testing specific to the intended food simulant and contact time.
Within the NOVA Chemicals Sclair LLDPE portfolio, Sclair 12J1 occupies the low-density, high-toughness segment. It should be compared with lower-density grades when extreme softness or higher dart impact is required, and with higher-density grades where stiffness and moisture barrier dominate. Differences in additive package, particularly slip and antiblock loadings, can influence film handling and converting performance. The choice between Sclair 12J1 and a metallocene octene LLDPE will depend on the relative importance of bubble stability, clarity, extractables, and melt pressure on the available extrusion equipment.