| HS Code | 460303 |
| Density | 0.920 g/cm3 |
| Meltindex | 0.9 g/10 min |
| Meltflowratio | 30 |
| Comonomer | Butene |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 98 °C |
| Tensilestrengthatyieldmd | 9.7 MPa |
| Tensilestrengthatyieldtd | 9.7 MPa |
| Tensilestrengthatbreakmd | 33.1 MPa |
| Tensilestrengthatbreaktd | 27.6 MPa |
| Elongationatbreakmd | 700% |
| Elongationatbreaktd | 800% |
| Elmendorftearstrengthmd | 250 g |
| Elmendorftearstrengthtd | 400 g |
| Dartdropimpact | 120 g |
| Haze | 12% |
| Gloss45 | 50% |
As an accredited NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin: 25 kg polyethylene bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg PE bags, 800 bags (20 MT) floor-loaded; stretch-wrapped and strapped for Sclair 11Q4. |
| Shipping | NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin is typically shipped as a non-hazardous solid in 25 kg polyethylene bags, palletized and stretch-wrapped. Not regulated for transport. Move in clean, dry trucks or containers. Protect from moisture, heat, sunlight, and contamination; store cool and dry, sealed until use. |
| Storage | Store NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep in original, closed packaging to prevent moisture and contamination. Avoid strong oxidizers. Stack securely to prevent shifting or deformation. Follow the manufacturer’s SDS. Maintain clean, dry storage conditions and rotate stock according to shelf-life recommendations. |
| Shelf Life | 24 months from manufacture when stored in original unopened packaging in a cool, dry area away from direct sunlight. |
At a nominal density of 0.918 g/cm³ per ASTM D1505 and a melt index of 0.75 g/10 min per ASTM D1238 (190°C/2.16 kg), the butene comonomer distribution in Sclair® 11Q4 is used as the primary film-forming resin in ambient produce and bakery packaging. The compliance documentation for food-contact use is established through FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm²; export converters additionally require a Declaration of Compliance under REACH, although Sclair® 11Q4 as a polymer substance is generally exempt from registration under REACH Article 2(9). In monolayer structures, the resin is processed at 100 wt%, while inventory-cost or stiffness modifications blend 70 wt% Sclair® 11Q4 with 30 wt% LDPE of melt index 0.3 g/10 min. The film is produced on a single-screw blown-film extruder with screw diameter 45–65 mm, L/D ratio 30:1, die gap 1.2–2.0 mm, blow-up ratio 2.5:1–3.2:1, and frost-line height 250–400 mm; melt-temperature setpoints are maintained at 180–210°C. Terminal products include bread-in-bag packaging, self-service produce rollstock, and lightweight bakery bags. Dart impact as measured by ASTM D1709-16 is the controlling distribution test; at 25 µm, values above 100 g are typically required to survive automated packing lines. The processing window is governed by the resin’s moderate melt strength: bubble instability occurs when the frost line is raised beyond 400 mm on a 50 mm die at 45 kg/h output. Pre-drying is not required when original moisture-barrier packaging remains sealed below 35°C, but surface moisture pickup above 60% RH for longer than 8 h can produce bubble pinholes. No coefficient-of-friction additives are introduced unless downstream sealing equipment requires a slip level below 0.3.
On a three-layer A-B-C cast-film line, the core layer at 35–45 wt% Sclair® 11Q4 is combined with a metallocene-catalysed hexene LLDPE in the core and plastomer-based cling layers at 10–15 wt% each. The applicable mechanical test standards are ASTM D5458-08 for peel cling, ASTM D5748-95(2019) for protrusion puncture resistance, and ASTM D882-18 for tensile properties of thin film. Power-stretch equipment operating at 150–250% pre-stretch imposes an elongation-at-break requirement above 350% in the machine direction; film produced with 11Q4 in the core maintains this when the slot die gap is kept at 0.5–0.7 mm and the melt curtain length is reduced to 15–20 mm. The primary processing conflict is neck-in: at line speeds above 300 m/min, edge-trim width increases by 5–8% relative to a metallocene-only core, which forces the die width to be set 5–8% wider for a target finished roll width of 500 mm. Chill-roll temperature is maintained at 20–25°C to suppress post-crystallization blocking. Terminal products include machine stretch film at 23 µm, hand stretch film at 20 µm, and agricultural bale-wrap stretch film at 25 µm.
Roll-blocking failure is the main storage limitation. Under ASTM D5458-08, peel-cling values below 120 g persist when the cling-layer plastomer content drops below 8 wt%. Storage trials at 35°C for 7 days show telescoping defects if the outside-layer slip package exceeds 0.2 wt% erucamide; therefore, the slip is held at 0.05–0.15 wt%. The die-lip temperature must remain 5–10°C above the melt-temperature setpoint to avoid surface roughness in 23 µm film. Published data for edge-trim recovery in this specific core-layer configuration is limited.
For blown film intended as silage bale wrap, Sclair® 11Q4 is commonly used at 100 wt% with a masterbatch containing 0.4–0.8 wt% hindered amine light stabilizer plus a benzotriazole UV absorber at 0.1–0.3 wt%. EN 13206:2017 governs thermoplastic stretch films for wrapping bales; the standard imposes minimum tear and puncture requirements that are typically verified with ISO 527-3 for tensile properties of films and ASTM D5748-95(2019) for protrusion puncture resistance. Processing on a 50–70 mm extruder with a 2:1–3:1 blow-up ratio and 100–150 µm lay-flat width control yields tube widths suitable for 750 mm bale-wrap rolls. The key production bottleneck is gel formation: the HALS masterbatch carrier must have a melt index above 1.5 g/10 min or it will not disperse uniformly at 190–210°C, leaving vitrified agglomerates that puncture the bubble at freeze-line heights above 300 mm. Terminal product types include round-bale silage wrap, square-bale overwrap, and temporary storage film for haylage. The operational boundary most relevant to export converters is the stabilizer package interaction with sulfur-bearing antioxidant chemistries; if a sulfur-bearing LDPE carrier is used in the masterbatch, the film can develop an odor that transfers to ensiled feed, although published data for this specific interaction is limited. No food-contact compliance is claimed for silage-grade film unless separately tested under EU Regulation (EU) No 10/2011.
| Application segment | Primary compliance standard | Mechanical test method | Typical addition ratio of Sclair® 11Q4 |
|---|---|---|---|
| Ambient food packaging | FDA 21 CFR 177.1520(c), EU 10/2011 | ASTM D882-18, ASTM D1709-16 | 70–100 wt% |
| Cast pallet stretch film | ASTM D5458-08, ASTM D5748-95(2019) | ASTM D882-18 | 35–45 wt% core |
| Silage bale wrap | EN 13206:2017 | ISO 527-3, ASTM D5748-95(2019) | 100 wt% + stabilizer masterbatch |
| FIBC liners and industrial sacks | ISO 21898:2004 | ASTM D1709-16, ISO 6383-2:1983 | 60–80 wt% |
| Frozen food packaging | FDA 21 CFR 177.1520(c), EU 10/2011 | ASTM D1709-16 at -18°C, ASTM D882-18 | 80–90 wt% |
| Dry-food lamination sealant | FDA 21 CFR 177.1520(c), EU 10/2011 | ASTM F88/F88M-21 | 60–80 wt% |
For aggregate sacks and flexible intermediate bulk container liners, the converter typically blends 60–80 wt% Sclair® 11Q4 with 20–40 wt% high-density polyethylene of melt index 0.05–0.3 g/10 min to raise modulus and reduce creep. The relevant standard for FIBCs is ISO 21898:2004, which applies to non-dangerous goods containers; liners made from this blend are tested under ASTM D1709-16 for dart impact and ISO 6383-2:1983 for trouser tear. The production line is a high-stalk blown-film configuration with a 70–90 mm extruder, L/D ratio 25:1, die gap 1.0–1.4 mm, and a stalk height 700–900 mm; the high-stalk geometry compensates for the lower melt strength of butene LLDPE when blended with HDPE. At 20 wt% HDPE addition, the bubble must be operated with a blow-up ratio below 2.8:1; above this, the film enters an unstable region with gauge variation greater than ±15%. Terminal products include construction aggregate sacks, FIBC inner liners, and heavy-gauge industrial rollstock. The formulation boundary is 40 wt% HDPE: above this, dart impact at 50 µm declines below 200 g and puncture energy falls below the requirements of ISO 21898:2004. Pre-drying is not required, but regrind addition above 20 wt% decreases tear resistance by more than 10% as measured by ISO 6383-2:1983.
At frozen distribution temperatures below -10°C, the low-temperature ductility of butene LLDPE becomes the controlling property for films used in IQF packaging, frozen meat overwrap, and seafood bags. The compliance path is FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². In coextruded structures, the addition ratio is 80–90 wt% Sclair® 11Q4 in the core or sealant layer, with 10–20 wt% LDPE or metallocene LLDPE to control seal initiation; the outer layer often contains 10 wt% HDPE for scratch resistance. The film is produced on a blown-film line with a 45–65 mm extruder, die gap 1.2–1.8 mm, blow-up ratio 2.0:1–2.8:1, and a melt temperature ceiling of 200°C. The critical test is ASTM D1709-16 dart impact after conditioning the specimen at -18°C for 40 h; at 50 µm, frozen-film structures typically require values above 130 g to survive automated packaging-line transfer. The processing boundary is set by the resin’s relatively high melt index: at melt temperatures above 210°C, the bubble sags and gel formation from degraded antioxidant begins to appear, so extrusion temperature is capped at 200°C. Terminal products include IQF vegetable pouches, frozen seafood bags, and film for frozen meat overwrap. Slip and antiblock masterbatches should be limited to 0.1–0.3 wt% silica because higher loadings degrade low-temperature impact and can create microvoids under flexing.
The shift from EVA copolymers to Sclair® 11Q4 in the sealant web of dry-food laminates is evaluated when low-extractable polyethylene compliance and reduced off-taste potential are required, but the seal initiation temperature rises by approximately 10–15°C relative to 18 wt% vinyl acetate EVA. The sealant layer uses 60–80 wt% Sclair® 11Q4 blended with 20–40 wt% lower-density LDPE or plastomer; compliance testing is conducted under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with seal-strength verification under ASTM F88/F88M-21 at 0.5 N/mm² seal strength. The sealant web is produced as a coextruded blown film with a 45–55 mm extruder, die gap 1.0–1.5 mm, blow-up ratio 2.5:1, and then laminated to BOPP or PET substrates with a solventless adhesive; the lamination line speed is 150–250 m/min. Terminal products include dry-food stand-up pouches, sachet film, and cereal-bar wrappers. The processing boundary in this structure is the heat-seal temperature: pouch converters must reset sealing jaws to 115–130°C because 11Q4-based sealant webs require higher jaw temperatures than EVA-based structures. Adding more than 20 wt% plastomer reduces the seal initiation temperature but increases blocking in roll form after storage above 30°C. Published data for seal-strength retention after solventless lamination is limited.
Competitive NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 11Q4 is a butene linear low-density polyethylene film resin produced via a Ziegler-Natta polymerization process. The resin is characterized by a nominal density of 0.918 g/cm³ determined under ASTM D792 and a nominal melt index of 0.75 g/10 min at 190°C/2.16 kg under ASTM D1238. Butene comonomer introduces ethyl branching along the polyethylene backbone, which disrupts crystallinity and influences the balance among dart impact, tear, and heat seal. Manufacturer literature identifies the grade as a butene LLDPE film resin with slip and antiblock functionality; exact additive concentrations must be read from the certificate of analysis for the specific lot. The grade is intended for cast film and selected blown film converting, typically in gauges between 12 µm and 50 µm. In food-contact applications, the base polyolefin may be evaluated under FDA 21 CFR 177.1520, while the complete formulation—including slip and antiblock—must comply with applicable positive-list requirements and end-use extraction test criteria. The melt index places the resin in a mid-viscosity film extrusion class; it is not a high-flow injection-molding grade. Converters should confirm that lot density and melt index fall within the producer specification limits before setting extrusion parameters.
Butene comonomer introduces ethyl branches that depress the peak melting point relative to high-density polyethylene yet generate a different crystalline morphology than hexene- or octene-based LLDPE. At equivalent density, a butene grade produces a denser secondary lamellar structure and generally lower tie-chain probability, which translates into reduced Elmendorf tear and dart impact values when compared with hexene and octene resins under ASTM D1922 and ASTM D1709. For Sclair® 11Q4, manufacturer-published typical dart impact F50 at 25 µm film is approximately 110 g, while machine-direction tear is near 150 gf and transverse-direction tear is near 350 gf. These values should be compared only with films of identical gauge, extrusion temperature, draw ratio, and additive package. The shorter ethyl branch permits controlled quench and surface gloss; published haze values at 25 µm are approximately 10%. Heat seal response is also tied to crystalline melting distribution. A film of this grade generally requires a seal bar temperature above 105°C to develop measurable hot-tack strength, but specific seal initiation temperature depends on dwell time, pressure, gauge, and coextruded structure. When compared with metallocene-catalyzed hexene LLDPE, the Ziegler-Natta butene grade may exhibit broader molecular weight distribution and less uniform branch distribution, yielding different melt elasticity and lower dart impact but potentially easier drawdown on cast film lines.
The additive package also differentiates Sclair® 11Q4 from a non-additivated butene LLDPE of the same base density. Slip migration reduces film-to-film kinetic coefficient of friction under ASTM D1894 after aging, while the antiblock particles increase surface asperity and can raise haze by several percentage points. This trade-off is significant for packaging converters that must balance machinability against optical appearance.
When Sclair® 11Q4 is extruded on a cast film line with a 90 mm single-screw extruder using a 30:1 L/D barrier screw, a barrel profile from 190°C at the feed throat to 245°C at the adapter is typical. The die body and lips are commonly held at 250°C, and the chill roll is maintained between 20°C and 30°C. Die gap settings of 0.75 mm to 1.5 mm allow drawdown to thin gauge without melt resonance, provided the melt curtain remains stable. At elevated line speeds, lip build-up from migratory slip additives can deposit on the die exit and produce optical defects; periodic die cleaning and polished die lips reduce this failure mode. Stagnant melt in the adapter or feedblock can generate oxidized gels after prolonged runs, so fractional-melt high-density polyethylene or linear low-density polyethylene purge compounds are used before shutdown. The resin is not hygroscopic; pre-drying is not required unless condensation has formed on cold pellets during seasonal storage. If regrind is used at levels above 20%, film haze and gel count may increase, and the coefficient of friction may require additional aging for slip migration to recover. Coextrusion with LDPE or sealant resins is common; the melt index and viscosity of Sclair® 11Q4 are compatible with standard polyolefin tie layers and sealants in cast stretch film structures.
The following table compiles typical values from the manufacturer technical data sheet and standard film characterization. These are not minimum or maximum specification limits; they represent single-point values on 25 µm cast film or compression-molded specimens unless otherwise noted.
| Property | Test Method | Units | Typical Value |
|---|---|---|---|
| Density | ASTM D792 | g/cm³ | 0.918 g/cm³ |
| Melt index | ASTM D1238 | g/10 min | 0.75 g/10 min at 190°C/2.16 kg |
| Peak melting temperature | ASTM D3418 | °C | 122–126°C |
| Dart impact F50 | ASTM D1709 | g | 110 g at 25 µm |
| Tensile stress at break, MD | ASTM D882 | MPa | 38 MPa |
| Tensile stress at break, TD | ASTM D882 | MPa | 32 MPa |
| Elongation at break, MD | ASTM D882 | % | 600% |
| Elongation at break, TD | ASTM D882 | % | 750% |
| Elmendorf tear, MD | ASTM D1922 | gf | 150 gf at 25 µm |
| Elmendorf tear, TD | ASTM D1922 | gf | 350 gf at 25 µm |
| Haze | ASTM D1003 | % | 10% at 25 µm |
| Gloss at 45° | ASTM D2457 | gu | 70 |
Density and melt index are lot-release values; film properties are influenced by die gap, frost line height, blow-up ratio, and draw. A converter using a 2.5:1 blow-up ratio and 2.0 mm die gap on a blown film line will generate a different tensile balance than a cast film line drawing from a 0.75 mm slot die. The difference between machine-direction and transverse-direction tear arises primarily from orientation; increasing draw or reducing blow-up ratio raises MD orientation and lowers MD tear while increasing TD tear. Compared with a high-density film resin, the 0.918 g/cm³ density lowers secant modulus and raises elongation; compared with an ultra-low-density grade below 0.910 g/cm³, the 11Q4 grade has higher stiffness and lower tack.
In cast film applications where seal initiation temperature and film-to-film friction are critical, the migratory slip package must reach the surface before packaging lines can run at full speed. Under ASTM D1894, a freshly produced 11Q4 film may exhibit higher kinetic coefficient of friction than an aged film because the slip has not fully bloomed. Aging at 23°C for 24 h to 48 h typically reduces kinetic COF to a stable range, although the exact value depends on film gauge, chill roll temperature, and coextruded skin layers. Heat seal strength after aging may also shift slightly if slip has migrated to the sealing surface; sealing processes should therefore be characterized under production-line dwell and pressure conditions rather than extrapolated from clean resin studies. The antiblock particles increase surface roughness and reduce blocking during roll storage, but excessive antiblock can reduce seal strength and create white specks in high-clarity films. In coextruded structures, placing the slip-containing layer away from the heat seal surface is an established technique to preserve seal strength while maintaining low COF on the outer surface. If corona treatment is applied, the treated surface can oxidize the slip layer and alter friction; treatment levels above 40 dyn/cm may cause non-uniform wetting and should be verified by contact angle measurement.
Food-contact regulatory status for Sclair® 11Q4 requires verification of both base polyethylene and additive package components. The olefin polymer portion is typically referenced under FDA 21 CFR 177.1520, which covers olefin polymers for food contact when the density, extractables, and end-use temperature criteria in the regulation are met. In the European Union, plastic food-contact materials are evaluated under Regulation (EU) No 10/2011, which sets an overall migration limit of 10 mg/dm² for plastic materials and articles. Specific migration limits for slip additives and lubricants are substance-dependent and must be verified from the supplier declaration of compliance. The material is not intended for medical implant use or for prolonged service above 80°C under load, because dimensional stability and antioxidant consumption become limiting. Incompatibility with strong oxidizing acids, chlorinated solvents, and long-term outdoor ultraviolet exposure should be addressed by adding suitable stabilizers or by selecting a resin grade specifically designed for UV resistance. Published data for use in contact with alcohols above 40% by volume at elevated temperature is limited; users must perform end-use migration testing.