Nova Chemicals Sclair 11p4 Butene Lldpe Film Resin

NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 324712
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Density 0.918 g/cm³
    Melting Point 122 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1400 psi
    Tensile Strength At Break Md 4000 psi
    Tensile Strength At Break Td 3500 psi
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 12%
    Gloss 45 60

    As an accredited NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg), palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin; cargo secured.
    Shipping NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin is a non-hazardous, non-DOT-regulated plastic resin. It is typically shipped in 25-kg bags, bulk bags, or bulk trucks/railcars. Keep packages dry, clean, and away from excessive heat; avoid contamination. Store indoors, protected from moisture, UV, and odor contamination.
    Storage Store Sclair® 11P4 Butene LLDPE Film Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep bags or containers tightly closed and palletized to prevent moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Maintain stable ambient temperatures, practice first-in, first-out stock rotation, and follow the supplier’s SDS.
    Shelf Life NOVA Sclair 11P4: recommended shelf life 24 months from manufacture when stored unopened, clean, dry, protected from direct sunlight.
    Application of NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin

    NOVA Chemicals Sclair® 11P4 is a butene linear-low-density polyethylene film resin with nominal density 0.918 g/cm³ per ASTM D1505 and nominal melt index 1.0 g/10 min per ASTM D1238 at 190 °C/2.16 kg. On blown-film lines dedicated to bale wrap, the resin is dry-blended at 70–80 wt% with 15–25 wt% high-pressure LDPE and 5–8 wt% UV-stabilized white masterbatch; the LDPE fraction stabilizes the bubble and the white masterbatch reduces infrared transmission across 25–35 µm film. Downstream processing is carried out on grooved-feed single-screw extruders with barrier screws of 30:1 L/D and annular dies of 250–350 mm diameter, using a die gap of 1.6–2.4 mm, blow-up ratio between 2.2:1 and 3.0:1, and melt discharge temperatures of 200–230 °C; internal bubble cooling is required to prevent flutter when output exceeds 300 kg/h. Screen packs of 40/60/80 mesh with breaker-plate pressure transducers are used to detect gel accumulation, and a pressure rise exceeding 15% across an 8 h run triggers screen replacement. Industry compliance is governed by EN 13207:2018 and EN 14932 for silage and bale-wrap films, with puncture resistance, tear propagation, and UV aging verified under the methods referenced in EN 13207:2018. Terminal product types include 750 mm × 1500 m bale wrap rolls, 25–35 µm silage sheets, and pre-perforated cover films. The butene comonomer distribution narrows the low-temperature dart impact window, so values should be verified per ASTM D1709-16a Method A before downgauging below 25 µm.

    Can a Butene LLDPE Film Resin Replace LDPE in 25 kg Export Sack Structures Without Trade-Offs in Dart Impact?

    Formulation trials on coextruded heavy-duty sack film use Sclair 11P4 at 85–100 wt% in the core and skin layers, with 0–15 wt% high-pressure LDPE to reduce melt fracture when die gaps fall below 2.0 mm, plus 1–3 wt% processing-aid/antiblock masterbatch. The downstream process is three-layer coextrusion blown film with a feedblock or spiral mandrel die, layer distribution 20/60/20, die diameter 350–450 mm, die gap 1.8–2.4 mm, blow-up ratio 2.0:1–2.8:1, and melt temperatures of 195–225 °C. Dart impact is measured on film conditioned at 23 °C and 50% relative humidity per ASTM D618; pre-drying is not required under normal indoor conditions, but condensation on pellets at ambient humidity above 80% RH can reduce feed stability and should be controlled with hopper blankets. Compliance for export sacks references ASTM D1709-16a Method A for dart impact, ASTM D882-18 for tensile properties, ISO 527-3:2018 for film tensile, and ASTM D1922-15 for Elmendorf tear; end-user specifications typically require minimum dart impact and tear values that must be obtained through the converter’s statistical process control, not extrapolated from resin data sheets. Terminal product types include 25 kg chemical export sacks, FIBC inner liners, asphalt and carbon black packaging, and drum liners in 50–125 µm thicknesses. The resin’s butene linear backbone gives lower melt strength than LDPE, so bubble stability must be maintained with internal bubble cooling and a frost-line height not exceeding 8 die diameters; published data for this specific configuration in FIBC liner formats is limited, and line qualification should be conducted on the target extrusion line.

    Pallet Unitization Film on High-Speed Cast Lines and the Butene Melt-Fracture Boundary

    On high-speed cast film lines, Sclair 11P4 is blended at 60–80 wt% with 20–40 wt% metallocene-catalyzed octene LLDPE or plastomer for machine-grade pallet wrap because the butene comonomer alone does not provide sufficient puncture resistance below 15 µm. Downstream processing uses cast film lines with 100–150 mm extruders, 30:1 L/D barrier screws, 1.8–3.0 m slot dies, 0.5–0.7 mm die lip gaps, chill roll temperatures of 15–25 °C, air knife and vacuum box edge pinning, and line speeds of 300–700 m/min; edge trim is reintroduced at 5–15 wt% after grind and blend. Compliance testing includes ASTM D5458-18 for peel cling, ASTM D5459-18 for machine-direction elastic recovery, ASTM D882-18 for tensile strength, and ASTM D5748-19 for puncture resistance; full pallet load retention is evaluated under EUMOS 40509 where applicable. Terminal product types include 12–23 µm machine film, 15–20 µm hand stretch film, and pre-stretched rolls. A processing boundary occurs at the melt fracture onset: with Sclair 11P4, increasing line speed above 450 m/min without processing aid commonly produces visible sharkskin, so fluoropolymer processing aid masterbatch at 200–800 ppm active content is added and die lip temperatures are maintained 5–10 °C above melt temperature. Published data for this specific configuration is limited; line qualification must verify cling and puncture before conversion.

    In three-layer coextruded sealant webs for frozen food form-fill-seal, Sclair 11P4 is added at 20–35 wt% of the total structure as the heat-seal skin, while the barrier core comprises EVOH at 5–10 wt% and tie layers at 5–10 wt%; the remainder is an outer LDPE/LLDPE blend. Processing is conducted on coextruded blown-film lines with die diameters 250–400 mm, die gaps 1.8–2.2 mm, blow-up ratios 2.0:1–2.6:1, and melt temperatures limited to 195–215 °C to prevent EVOH degradation; barrier layer residence time is controlled below 10 minutes. Food-contact compliance is based on FDA 21 CFR 177.1520(c) for olefin polymers under conditions of use B through H, and Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² in food simulants assigned to frozen storage; organoleptic testing is performed according to DIN 10955 for high-fat frozen products. Terminal product types include frozen vegetable pouches, ice cream packaging, seafood vacuum bags, and frozen bakery carton liners in 40–80 µm thicknesses. The lower density and butene comonomer of Sclair 11P4 improve low-temperature seal initiation relative to LDPE, but cold-seal strength should be verified per ASTM F88/F88M-21 after sealing at 115–135 °C jaw temperatures.

    Application compliance matrix
    Application contextStandard or test methodProperty verified
    Silage bale wrapEN 13207:2018; EN 14932; ASTM D1709-16a Method APuncture, tear propagation, UV aging, low-temperature dart impact
    Heavy-duty export sacksASTM D1709-16a Method A; ASTM D882-18; ISO 527-3:2018; ASTM D1922-15Dart impact, tensile, tear
    Pallet stretch wrapASTM D5458-18; ASTM D5459-18; ASTM D882-18; ASTM D5748-19; EUMOS 40509Cling, elastic recovery, tensile, puncture, load stability
    Frozen food sealant webFDA 21 CFR 177.1520(c); EU 10/2011; DIN 10955; ASTM F88/F88M-21Migration, organoleptics, seal strength
    Construction vapor barrierASTM D4397-16; ASTM E96/E96M-22; ASTM D1709-16a Method A; ASTM D882-18Permeance, dart impact, tensile
    Refuse sack and can linerEN 13592:2017; ASTM D1709-16a Method A; ASTM D1922-15; ASTM D882-18Dart impact, tear, tensile

    When Under-Slab Vapor Retarders Require Both Low Permeance and Jobsite Puncture Resistance

    Under-slab vapor retarder webs are produced from Sclair 11P4 at 98–100 wt% with 2–4 wt% carbon black or UV-stabilizer masterbatch and 1–2 wt% antiblock to produce construction-grade polyethylene sheeting. The downstream process is monolayer or two-layer blown-film extrusion on wide-die lines with die diameters up to 600 mm, die gaps 1.8–2.5 mm, blow-up ratios 1.8:1–2.4:1, and melt temperatures of 195–230 °C; because thickness ranges from 150 µm to 250 µm, output is constrained by bubble cooling capacity rather than screw recovery. Compliance is specified under ASTM D4397-16 for polyethylene sheeting for construction, ASTM E96/E96M-22 desiccant method for water vapor permeance, and ASTM D882-18 for tensile and elongation; project documents commonly require water vapor permeance below 0.01 U.S. perms and puncture resistance per ASTM D1709-16a Method A. Terminal product types include 6 mil under-slab vapor barriers, crawl space liners, and temporary weather protection for steel framing. The butene copolymer’s lower melt viscosity supports higher throughput at equivalent head pressure, but pinhole formation is controlled by 40/60/80 mesh screen packs and bubble stability; field seams must use polyethylene-compatible tape or adhesive per manufacturer’s installation guidelines, and the resin itself is not ignition-resistant and is not a substitute for a flame-retardant membrane.

    Carbon Black Masterbatch Loading Shifts Elmendorf Tear Retention in Butene LLDPE Refuse Sacks

    Monolayer refuse sack extrusion with Sclair 11P4 begins with 100 wt% resin and separate additions of 2–4 wt% carbon black masterbatch and 0.5–1.5 wt% processing aid/antiblock; some converters add 10–20 wt% clean post-industrial recycled LLDPE from edge trim and start-up scrap, but tear retention must be verified because recycled content narrows the Elmendorf tear distribution. The downstream process uses monolayer blown film with grooved-feed extruders of 25:1–30:1 L/D, die diameters 150–350 mm, die gaps 1.5–2.0 mm, blow-up ratio 2.2:1–2.8:1, and melt temperatures 190–220 °C; frost line height is kept within 5–8 die diameters to maintain gauge uniformity in 25–80 µm film. Compliance for waste sacks references EN 13592:2017 for household refuse sacks, ASTM D1709-16a Method A for dart impact, ASTM D1922-15 for Elmendorf tear, and ASTM D882-18 for tensile elongation. Terminal product types include institutional can liners, heavy-duty refuse sacks from 40 L to 240 L, hospital waste bags, and industrial cleanup bags. The butene linear-low density backbone provides higher puncture resistance than LDPE at equivalent gauge as measured by ASTM D1709-16a, but tear propagation is sensitive to carbon black dispersion; a 40/60/80 mesh screen pack and carbon black masterbatch at 40–50 wt% carbon black concentration are typical.

    Free Quote

    Competitive NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Sclair® 11P4 is a butene-copolymer linear low-density polyethylene film resin classified under polyethylene CAS 9002-88-4. The manufacturer specifies a nominal melt flow rate of 1.0 g/10 min when measured at 190 °C under a 2.16 kg load according to ASTM D1238 and ISO 1133-1:2022, and a nominal density of 0.918 g/cm³ according to ASTM D792 and ISO 1183-1:2019. These values define a film-grade LLDPE intended for cast and thin-gauge blown-film extrusion. The use of 1-butene as the short-chain branching comonomer differentiates the product from hexene- and octene-based LLDPE grades; it yields a measurable reduction in crystalline density relative to HDPE homopolymer while retaining easier extrusion than narrow-molecular-weight metallocene grades at equivalent melt index.

    How Does Butene Short-Chain Branching Govern Film Mechanical Response?

    Short-chain branching in Sclair® 11P4 arises from insertion of 1-butene during polymerisation. Because butene introduces ethyl branches along the polymer backbone, the intermolecular chain packing is interrupted. The crystalline lamellae are thinner than in an unbranched high-density polyethylene of equivalent melt index; this is reflected in the suppressed density of 0.918 g/cm³ and in a broader melting endotherm. Under ASTM D3418 differential scanning calorimetry at a standard scan rate of 10 °C/min, the main melting endotherm for this class of butene LLDPE typically peaks near 122 °C. The lower crystalline fraction increases molecular mobility in the amorphous phase, which contributes to ductility and impact toughness, but reduces tensile modulus compared with a film-grade HDPE of the same melt index.

    Butene-based short-chain branching is less efficient than octene or hexene at generating tie chains between adjacent crystalline lamellae. As a result, the dart impact and Elmendorf tear strengths of Sclair® 11P4 are expected to be lower than those of an octene-copolymer LLDPE at equal density and melt index, especially at film thicknesses below 25 µm. The practical advantage is that butene comonomer reduces catalyst complexity and can yield lower gel-count film at equal barrel residence time, particularly on converters with limited purge capacity. This difference is not visible from melt flow rate alone; it becomes measurable in the film fracture mode, where octene grades tend to exhibit a higher fraction of ductile draw during dart drop testing under ASTM D1709 Method A.

    The following representative values are compiled from current manufacturer technical literature for 25 µm cast film produced on a single-screw extruder fitted with a declining-pressure barrier screw and a coat-hanger slot die. They are typical values, not product specifications, and should be verified against the lot-specific certificate of analysis.

    PropertyTest methodNominal value
    Melt flow rateASTM D1238, 190 °C, 2.16 kg1.0 g/10 min
    DensityASTM D7920.918 g/cm³
    Main melting peakASTM D3418122 °C
    Vicat softening pointASTM D1525101 °C
    Film dart impact, F50ASTM D1709 Method A, 25 µm130 g
    Tensile strength at break, MD / TDASTM D88235 / 22 MPa
    Elongation at break, MD / TDASTM D882650 / 700 %
    Elmendorf tear, MD / TDASTM D1922120 / 310 g
    HazeASTM D10037.0 %
    Gloss at 60 °ASTM D245775

    For film property development, the nominal 25 µm cast-film values place Sclair® 11P4 in the moderate-toughness segment of LLDPE film resins. The tensile elongation at break in the transverse direction typically exceeds the machine-direction value because cast-film orientation is unbalanced; the film is drawn primarily in the machine direction before contact with a chill roll held at 15–25 °C, while transverse shrinkage is partially restrained by web edges. Haze and gloss values are sensitive to die lip cleanliness and cooling-water quality; an unclean die can raise haze above 10 % even when the resin is within specification.

    Cast-Film Line Parameters for Sclair® 11P4

    This grade is processed on single-screw extruders with grooved feed sections and L/D ratios in the range of 27:1 to 33:1. A barrier flight section followed by a pinned or spiral-baffle mixing element is preferred; the barrel profile should progress from a feed zone at 170–185 °C to a metering zone at 210–230 °C, with the adapter and die body held at 230–250 °C. Melt temperature at the die exit should not exceed 260 °C for routine operation. At melt temperatures above 260 °C, the residence-time-dependent formation of oxidized gels becomes a process risk; on a line with an active screen changer, pressure-drop monitoring at the breaker plate provides an early indication of gel accumulation. The die gap is normally set between 0.5 and 0.8 mm for cast film; thinner die gaps reduce machine-direction draw residence and generally improve transverse gauge uniformity, but they raise die pressure and the risk of melt fracture at a given output rate.

    Chill roll temperature is a first-order variable for optical and thermal shrinkage behavior. A roll surface temperature of 15–25 °C is typical for quench-rate optimization; lower temperatures increase film flatness and reduce blocking tendency, while higher temperatures reduce curl but may lower gloss and increase haze due to slower crystallization. Air-knife pressure and position should be set to keep the web uniformly pinned to the chill roll within the first 1–2 cm of contact. In blown-film trials, a die gap of 1.0–2.0 mm with a blow-up ratio of 2.0:1 to 2.5:1 has been used; frost line height should be held below 4–6 die diameters to maintain bubble stability. The resin’s 1.0 g/10 min melt flow rate gives moderate extruder back pressure; field reports on a 75 mm grooved-feed single-screw line at 30:1 L/D indicate head pressure in the range of 200–300 bar depending on screw wear and melt filtration configuration. Published data for this specific equipment configuration is limited, so the pressure range is indicative rather than a specification.

    In machine-direction oriented cast stretch film, Sclair® 11P4 is used as a core or skin layer in coextruded structures where the cling layer is composed of an ultra-low-density ethylene copolymer and the opposite skin uses a higher-density slip-containing LLDPE. The butene base resin provides seal and puncture contributions at low gauge; on a high-speed MDO line operating at draw ratios of 2.0:1 to 3.5:1, unwinding and stretching are influenced by the resin’s yield stress and strain-hardening behavior. Because butene LLDPE has a lower strain-hardening modulus than octene LLDPE of comparable density, the power draw on the stretch section may be slightly lower, but ultimate stretch performance at very high draw ratios may be reduced. Converters running 12–15 µm films often calibrate pre-stretch to 200–250 % rather than 300–350 % to avoid localized necking when this butene grade is used as the primary structural layer.

    For lamination film and general-purpose protective packaging, the resin provides a balance of tear and drop resistance that is sufficient for non-critical load cases. The absence of a specified slip or antiblock package in the base grade means surface coefficient of friction is controlled by converter-added masterbatch or by the opposing coextruded skin; bare-film-to-bare-film blocking may develop at storage temperatures above 35 °C or under high winding tension. In a coextruded structure, the use of an external skin with a slip package permits this butene core to supply puncture and seal performance without requiring reformulation of the base resin.

    When This Butene Resin Replaces LDPE or mLLDPE in Stretch and Lamination Structures

    Compared with a high-pressure LDPE of equal 0.918 g/cm³ density and 1.0 g/10 min melt flow rate, Sclair® 11P4 exhibits a more linear backbone architecture and fewer long-chain branches. The resulting shear viscosity is less shear-thinning, so the LLDPE grade generates higher die pressure at the same output rate on a fixed die gap. This characteristic must be accommodated by a wider die gap or a higher melt temperature; operators should not simply substitute the butene LLDPE into a screw designed for high-pressure LDPE without verifying motor amperage and melt-pressure limits. The LLDPE grade provides higher tensile elongation and improved puncture resistance at equivalent thickness, and it allows a measurable gauge reduction in some protective packaging structures when validated under ASTM D1709 dart impact and ASTM D5748 puncture testing.

    Compared with a metallocene-catalyzed LLDPE of equivalent density and melt index, Sclair® 11P4 has a broader molecular weight distribution and a more pronounced shear-thinning response at typical extrusion shear rates. This reduces melt entry-pressure fluctuations and improves bubble stability in blown film, but it also lowers dart impact and transverse-direction tear. At a 25 µm film thickness, an octene mLLDPE of equal density and melt index commonly shows a dart impact advantage exceeding 50 % over a butene LLDPE under ASTM D1709 Method A; the exact difference depends on catalyst type, molecular weight distribution, and film fabrication conditions. The butene grade is therefore selected when converter equipment is not configured for high-viscosity mLLDPE or when lot-to-lot gauge uniformity is more critical than ultimate impact.

    Heat sealing of Sclair® 11P4-containing films is generally performed at seal jaw temperatures of 110–140 °C at 0.5 s dwell and 1–2 bar pressure. The butene LLDPE has a lower melting point than HDPE and can provide a broader hot-tack window in coextruded sealant layers. Seal strength measured under ASTM F88 is strongly influenced by gauge and contamination from external slip additives; published data for Sclair® 11P4 under this specific test configuration is limited, so sealing conditions must be developed on-line.

    Food-contact compliance is governed by the converter’s finished-article assessment rather than the pellet alone. The resin grade is based on ethylene-1-butene copolymers that fall within the scope of 21 CFR 177.1520 for olefin polymers, provided the finished food-contact article meets the extractable and end-use temperature restrictions of that section. Good manufacturing practice requires verification that comonomer content and polymerization residues are below the levels specified in the same section. For European Union applications, compliance with Commission Regulation (EU) 10/2011 and its subsequent amendments, including the overall migration limit of 10 mg/dm², must be demonstrated on the final film, because the polymer’s additive package and processing history can affect migration. The resin is not classified as hazardous under current Globally Harmonized System criteria; the supplier safety data sheet should be consulted for handling, ventilation, and spill-control measures.

    Moisture sensitivity is not a critical drying requirement for this resin under normal pellet storage below 50 % relative humidity. However, condensation on cold pellet surfaces can introduce water into the feed throat and cause surface defects or reduced output; pellets stored in unheated silos during winter should be given sufficient hopper residence time to reach 20–25 °C before entering the extruder. The resin should not be blended with amine-based antifog or antistatic additives above the additive supplier’s recommended loading without thermal stability testing, because the interaction of such additives with oxidized film surfaces can alter seal initiation temperature. No drying is required under normal conditions; if pre-drying is used for regrind containing hygroscopic masterbatch, a desiccant dryer at 60 °C for 2–4 hours is sufficient.

    Top