Nova Chemicals Sclair 11p3 Butene Lldpe Film Resin

NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 955502
    Productname NOVA Chemicals Sclair 11P3 Butene LLDPE Film Resin
    Manufacturer NOVA Chemicals
    Brand Sclair
    Grade 11P3
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Application Film Resin

    As an accredited NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin supplied in 25 kg polyethylene-lined bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin, palletized, shrink-wrapped, and secured.
    Shipping NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin is shipped as non-hazardous, solid polyethylene pellets. Standard packaging includes 25 kg bags on stretch-wrapped pallets or bulk trucks/railcars. Transport under cool, dry conditions; avoid moisture, heat, direct sunlight, and packaging damage. Not classified as dangerous goods for transport.
    Storage Store Sclair® 11P3 LLDPE resin in a cool, dry, well-ventilated area in sealed original containers. Keep away from heat, sparks, open flames, direct sunlight, moisture, and strong oxidizers. Protect from contamination and use first-in, first-out stock rotation. Avoid dust accumulation, as pellets may create slipping hazards. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original unopened packaging in a dry, well-ventilated area.
    Application of NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin

    On blown-film lines converting frozen vegetable packaging, Sclair 11P3 is run as the sealant layer because the butene-branch crystallisation behaviour produces a broader heat-seal initiation envelope than a high-crystallinity HDPE layer. The grade has a published melt index of 1.0 g/10 min under ASTM D1238-20 at 190 °C/2.16 kg and a published density of 0.920 g/cm³ under ASTM D792-20. The food-contact position is governed by FDA 21 CFR 177.1520(c)(2.1) and (3.1) for olefin polymers, with a maximum overall migration limit of 10 mg/dm² under EU Regulation (EU) No 10/2011, Annex I. A standard formulation uses 85 wt% Sclair 11P3 and 15 wt% LDPE with a melt index of 0.25 g/10 min; the addition ratio of a 5% active silica antiblock masterbatch is 1.0–1.5 wt%, and erucamide slip is compounded to 500–800 ppm active. The conversion line is a single-screw blown-film extruder with a 30:1 L/D barrier screw, 100 mm annular die, and 1.8–2.0 mm die gap. The melt is extruded at 196–210 °C and expanded at a blow-up ratio of 2.0:1–2.5:1; the frost line is held at 2.0–2.5 die diameters. Terminal items are 25–50 μm IQF vegetable pillow bags, bread bags, produce bags, and ice cube bags. The film is tested for dart impact under ASTM D1709-16a with a converter target of 90–130 g at 25 μm, for Elmendorf tear under ASTM D1922-15, and for haze under ASTM D1003-13. An operational boundary exists at blow-up ratios above 2.5:1, where melt strength is insufficient to maintain gauge stability below ±15% on conventional single-lip air rings.

    When 4 m Construction Vapour Barriers Must Survive Wind Load Without Post-Extrusion Orientation

    The gauge uniformity of a 4 m construction vapour barrier exposed to wind load becomes a more stringent acceptance criterion than surface gloss once the film is used as a concrete curing membrane. The applicable compliance references are ASTM C171-20 for sheet materials for curing concrete and ASTM E1745-17 for plastic water vapour retarders used in contact with soil or granular fill. The blending ratio for wind-exposed vapour barriers is 70–80 wt% Sclair 11P3, 20–30 wt% LDPE with a melt index of 0.2–0.4 g/10 min, and 2–3 wt% of a 40% carbon black masterbatch for ultraviolet screening. Production on an accumulator-equipped blown-film tower uses an annular die of 300–450 mm, internal bubble cooling, and a die gap of 2.2–2.6 mm. The melt temperature is 210–220 °C, the blow-up ratio is 1.8:1–2.2:1, and take-off speed for 100 μm film is limited to approximately 55 m/min because bubble flutter becomes the main gauge-control constraint. Converter output is wound into 4 m × 50 m vapour retarder rolls, concrete curing blankets, temporary weather enclosures, industrial drum liners, and heavy-duty refuse sacks. The limitation is equally specific: this butene LLDPE formulation is not a primary geomembrane; its permeation resistance is lower than HDPE and it should not replace a 1.0 mm HDPE geomembrane in landfill or pond-liner service.

    Silage covers and round bale stretch film made from butene LLDPE are specified by the creep resistance of the folded edge under UV exposure, not by melt strength alone, because a torn folded edge exposes silage to oxygen ingress. Compliance is defined by EN 13206:2017 for thermoplastic covering films used in agriculture and by REACH Regulation (EC) No 1907/2006 for UV stabilizer registration. The resin proportion in silage cover formulations is 80 wt% Sclair 11P3, 15 wt% LDPE or hexene LLDPE, and 5 wt% of a 40% carbon black masterbatch; for round bale wrap, a polyisobutylene tackifier is added at 1.5 wt% of a 20% active concentrate. Silage covers are converted on a rotating haul-off blown-film line with a 1400 mm die, 2.0 mm die gap, 2.5:1 blow-up ratio, and melt temperature of 200–215 °C; output is 200–250 kg/h, and an edge-folding station is placed before the winder. Finished goods are silage pit covers, bunker silo covers, agricultural mulch film, and round bale wrap. The operational boundary is exposure time: for greenhouse cladding beyond 18 months requiring high-molecular-weight HALS packages, a hexene or octene metallocene PE grade is specified instead, because the butene short-chain branch distribution cannot maintain the same tensile elongation retention under ISO 527-3:2018 after 18 months of UV exposure.

    Can a 1.0 g/10 min Butene LLDPE Withstand the Draw Ratios of a 15 μm Cast Stretch Line Without Melt Resonance?

    Cast-film trials with this butene LLDPE run at lower draw ratios than octene metallocene grades because the melt extensibility reaches its limit when the film enters the air-knife thinning zone at line speeds above 250 m/min. The applicable stretch-film references are ASTM D4649-20 for selection and use of stretch wrap films, ASTM D5458-95 for peel cling of stretch wrap film, EN 14477:2004 for puncture resistance, and ISTA 3E for unitized load simulation. The cast-web formulation sets the resin fraction at 80–90 wt% Sclair 11P3, 10–20 wt% ultralow-density polyethylene with a density of 0.905 g/cm³, and 1.0–2.0 wt% of a 30% active polyisobutylene cling concentrate; no slip additive is added. The production process is cast-film extrusion through a 120 mm single-screw extruder with 30:1 L/D, a 1800 mm slot die with air-knife, and a chill-roll temperature of 18–22 °C. Line speed is 180–260 m/min, film thickness is 15–23 μm, and output is approximately 450 kg/h. End-product formats are hand stretch wrap rolls, machine pre-stretch cast film, and bundling film. The operational boundary is prestretch ratio: above 200% prestretch on high-speed wrappers, butene LLDPE shows chain stretch break more frequently than hexene/octene grades, and it should not replace those resins in lines designed for 300% prestretch.

    Adhesive-backed surface protection films require the base film to delaminate at a controlled peel force between 0.2 N/25 mm and 1.5 N/25 mm without transferring residue to a powder-coated coil after three months of direct UV exposure. The compliance layer is defined by REACH Regulation (EC) No 1907/2006 SVHC screening and RoHS Directive 2011/65/EU Annex II substance restrictions, while peel adhesion is measured under ASTM D3330/D3330M-04(2018). The base-layer formulation uses 65–75 wt% Sclair 11P3, 15–25 wt% LDPE with a melt index of 2.0 g/10 min, and 5–10 wt% EVA containing 18% vinyl acetate; a polyisobutylene tackifier is loaded at 1.0–2.5 wt% of a 20% active concentrate, and the exposed film surface is corona-treated to 38–42 mN/m. The downstream process is a three-layer blown-film coextrusion with a 200 mm die, 1.8 mm die gap, 2.0:1 blow-up ratio, and layer distribution of 15/70/15. In-line corona treatment and slitting at 150 m/min produce the final roll widths. Terminal roll stock is slit into coil-coating mask, pre-painted metal protection, and decorative laminate protection films. Published peel-force data for Sclair 11P3 in this specific configuration is limited; converter validation under ASTM D3330/D3330M-04(2018) at 23 °C and 50% relative humidity is required before specifying the grade for post-formed automotive exterior parts.

    Heat-Seal Integrity Through Powder Contamination on Horizontal Form-Fill-Seal Lines

    Dusty, granulated products create a sealing interface with powdered fines trapped in the heat-seal zone; butene LLDPE with a broader seal window reduces leakers by allowing higher sealing temperatures before the film scorches. Food-contact sachet compliance is set by FDA 21 CFR 177.1520(c)(2.1)/(3.1) and EU Regulation (EU) No 10/2011 with overall migration not exceeding 10 mg/dm², while seal strength is tested under ASTM F88/F88M-21. For industrial chemical powders, the inner liner is validated against the packaging requirements of ADR/RID 6.1.5 when used within a UN fibreboard outer. The formulation for powdered-food sachets is run at 90–100 wt% Sclair 11P3, with 0.5–1.0 wt% of a 5% active silica antiblock masterbatch and slip controlled below 200 ppm; for vertical FFS units, 5–10 wt% LDPE is added to reduce seal misalignment. The packaging line is a horizontal form-fill-seal machine with seal bar dwell of 0.2–0.4 s, seal pressure of 0.4–0.7 N/mm², and seal temperature in the range of 115–135 °C. Film thickness is 35–60 μm, and final item forms are bag-in-box liners, pillow packs for dry powders, granulated fertilizer pouches, and buffered salt sachets. Above 60% relative humidity, pre-drying of recycled content is required if post-industrial reclaim is included; virgin Sclair 11P3 is not hygroscopic and requires no drying under normal ambient storage.

    Free Quote

    Competitive NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sclair® 11P3 is an ethylene-1-butene linear low-density polyethylene film resin produced by NOVA Chemicals. The resin is manufactured using conventional Ziegler-Natta catalysis, which yields a broader molecular weight distribution than the narrow distribution characteristic of metallocene-catalyzed LLDPE grades. Nominal melt index is 1.0 g/10 min at 190 °C under a 2.16 kg load per ASTM D1238, and nominal density is 0.918 g/cm³ per ASTM D792. The peak melting point determined by differential scanning calorimetry is approximately 122 °C per ASTM D3418. The resin is intended for heavy-duty sacks, industrial liners, agricultural film, and general-purpose blown-film structures in which tensile strength, elongation, and tear resistance are primary design criteria. It is not formulated as a high-clarity packaging resin, and its base additive package does not include slip or antiblock.

    Nominal resin property data for Sclair® 11P3
    PropertyNominal valueTest method
    Density0.918 g/cm³ASTM D792
    Melt index1.0 g/10 minASTM D1238
    Peak melting point122 °CASTM D3418

    On conventional blown-film lines, processing conditions for Sclair® 11P3 are bounded by melt temperature and die geometry. A typical barrel profile begins near 165 °C in the feed section and rises to 205–215 °C at the die adapter. Melt temperature at the die inlet should be maintained between 190 °C and 230 °C. Sustained operation above 240 °C accelerates consumption of the hindered phenolic stabilizer and can generate gel particles; operation below 180 °C may leave unmelted resin domains and raise screw motor load beyond the drive rating on 45–75 mm grooved-feed extruders. Die gaps from 1.2 mm to 2.3 mm are commonly used, with blow-up ratios of 2.0:1 to 3.0:1. Higher blow-up ratios increase transverse-direction orientation and reduce machine-direction tear resistance; lower blow-up ratios raise machine-direction orientation and can make the bubble more sensitive to frost-line disturbance.

    The resin does not require routine drying unless condensation occurs during outdoor silo storage. If relative humidity exceeds 60 % or cold resin is conveyed into a warm plant, surface moisture can introduce steam splay in the film and pressure fluctuation at the die. In such cases, low-dew-point purge air at the hopper and a feed-throat temperature above 40 °C are used. Screen pack configuration on many lines follows a 20/40/60 mesh stack to provide back pressure; omission of a breaker plate can increase melt-temperature variation across the die. Spiral mandrel dies with land length ratios of 10:1 to 15:1 reduce flow marks at higher shear rates. On a 65 mm extruder with a 1.6 mm die gap and 3:1 blow-up ratio, die head pressure generally remains between 20 MPa and 30 MPa; sustained pressure above 35 MPa may indicate an undersized die gap or insufficient melt temperature.

    What separates a butene-copolymer LLDPE from a hexene or octene grade under identical blown-film conditions?

    The short-chain branch type introduced by 1-butene differs from that introduced by 1-hexene or 1-octene. Butene insertion produces ethyl branches, whereas hexene and octene introduce butyl and hexyl branches. Under equivalent density and melt index, the longer branches in hexene and octene copolymers increase the probability of tie-molecule formation between crystallites. This raises dart drop impact per ASTM D1709, Elmendorf tear strength per ASTM D1922, and slow puncture propagation resistance per ASTM D5748 relative to butene-copolymer LLDPE. The effect is most pronounced in films below 50 µm and in low-deformation-rate abuse events. This structure-property relationship places butene-copolymer LLDPE at the lower end of the toughness envelope among ethylene-α-olefin copolymers, but it also simplifies processing on older lines with limited cooling capacity. The following table provides a qualitative ranking for materials of equivalent density and melt index.

    Comparative toughness ranking at equivalent density and melt index
    Performance propertyTest methodButene LLDPEHexene LLDPEOctene LLDPE
    Dart drop impactASTM D1709LowestIntermediateHighest
    Machine-direction Elmendorf tearASTM D1922LowestIntermediateHighest
    Slow puncture propagationASTM D5748LowerHigherHigher

    Published data for Sclair® 11P3 in direct side-by-side film evaluations against hexene and octene LLDPE is limited; the rankings should be treated as a validation framework rather than a fixed specification. Converter-specific results depend on die gap, blow-up ratio, frost-line height, film thickness, and output rate. In heavy-duty sacks produced at 75–150 µm, the lower dart impact of a butene-copolymer LLDPE can be offset by the sack design, but the end-use drop-test requirement should be verified on the converted film.

    Relative to high-pressure LDPE, Sclair® 11P3 has higher tensile stress at break and greater puncture tolerance at equivalent thickness, but lower melt elasticity. Lower melt elasticity makes the bubble more sensitive to air current fluctuations, particularly at high frost-line height. Dry blending with 10–30 wt% high-pressure LDPE increases bubble stability and improves tear propagation resistance in heavy-duty sacks. Blending with medium-density polyethylene increases modulus but reduces dart impact; if stiffness is required, a coextruded structure with a thin MDPE layer is usually preferable to a full-thickness dry blend.

    Molecular weight distribution also differentiates Sclair® 11P3 from metallocene-catalyzed butene resins. Conventional Ziegler-Natta resins have a broader molecular weight distribution, which increases melt strength and shear thinning. Metallocene butene LLDPE grades with similar density and melt index often provide lower extractables and better optical properties, but may have higher melt pressure and a narrower operating window on older extruders. The choice between a conventional butene resin and a metallocene resin is therefore not solely a toughness decision; it is also driven by extractable limits, haze specifications, and available extruder drive capacity.

    Heat-seal response, coefficient of friction, and additive package limitations

    Sclair® 11P3 is supplied with antioxidant stabilization and without intentionally added slip or antiblock. The absence of slip and antiblock means the coefficient of friction of the finished film is controlled by converter-added masterbatch. Automated form-fill-seal packaging lines requiring a coefficient of friction below 0.3 on metal surfaces per ASTM D1894 generally require a slip masterbatch. Erucamide slip agent migrates more slowly through LLDPE than through high-pressure LDPE; converters should allow 24–48 h of roll aging before testing coefficient of friction. Heat-seal initiation for LLDPE film of this density is generally near 110 °C, with full seal strength at 125–140 °C depending on dwell and pressure. Hot-tack force should be measured by ASTM F1921 if the resin replaces an LDPE seal layer in a forming-web or vertical form-fill-seal structure.

    Acid-modified ethylene copolymers and ionomer regrind can interact with the stabilizing package under high moisture conditions. Use of more than 5 wt% ionomer regrind without a vacuum vent may reduce oxidative induction time measured by ASTM D3895 and generate surface defects. The resin is compatible with conventional polyethylene color and UV masterbatches, provided the masterbatch supplier’s recommended let-down ratio is not exceeded. Excessive carrier resin can shift melt index and density of the final film. For outdoor agricultural film, a UV stabilizer masterbatch is required, and accelerated weathering should be validated by ASTM D4329 or ISO 4892-2 on the finished film.

    When the resin is run below 20 µm on high-speed converting lines

    Downgauging below 20 µm shifts the primary failure mode from tensile yield to defect-driven puncture and tear propagation. At this thickness, film dart impact becomes more dependent on die gap, blow-up ratio, and gauge uniformity than on melt index alone. A die gap of 1.2–1.6 mm is preferred to limit melt fracture and maintain thickness control. Frost-line height should be controlled within 1.5–2.5 times the die diameter, and the air ring should be set to avoid a concave bubble waist. In this regime, internal bubble cooling or a dual-lip air ring is often required to maintain symmetry at high haul-off speed. On a 50 mm die, stable operation has been observed at 5–7 kg/h per cm of die circumference; above that range, bubble diameter oscillation increases unless the frost line is lowered and the air ring is adjusted. These boundaries are equipment-specific and should not be used as a universal output limit. Melt temperature should be kept in the upper half of the recommended range to reduce melt viscosity at high shear, but below 240 °C to avoid gel formation.

    Regulatory clearances for food contact are limited to olefin polymer provisions

    In the United States, Sclair® 11P3 may be used in food-contact articles under 21 CFR 177.1520, provided the finished film meets extraction limitations and conditions of use specified in the regulation. The resin is not a medical-grade material, and no USP Class VI or ISO 10993 biocompatibility claim is supplied by the resin manufacturer. In the European Union, the finished film must comply with Commission Regulation (EU) No 10/2011 and its amendments; overall migration testing is conducted per EN 1186-1, and specific migration of 1-butene and any additives must be evaluated by the converter. For laminated structures, the presence of adhesives, inks, and other layers can raise overall migration; therefore, the converter must perform migration testing on the final article rather than relying on resin compliance alone. Under REACH, the polymer itself is exempt from registration, but monomer and additive obligations remain; the relevant tonnage band and use descriptors must be confirmed with the importer.