Nova Chemicals Sclair 11p2 Butene Lldpe Film Resin

NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 331717
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Density 0.920 g/cm³
    Melt Flow Ratio I21 I2 30
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Tensile Strength At Break Md 30.0 MPa
    Tensile Strength At Break Td 25.0 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Dart Drop Impact 120 g
    Haze 12%
    Gloss 45 60%
    Coefficient Of Friction 0.2
    Blocking 25 g
    Film Thickness 1.0 mil
    Blow Up Ratio 2.5:1

    As an accredited NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin is supplied in 25 kg polyethylene bags, palletized, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL: approximately 18 metric tons net of NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin, in 25 kg bags.
    Shipping NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin ships as non-hazardous pellets in 25 kg polyethylene-lined bags, 500–1000 kg bulk bags, or bulk hopper trucks/railcars. Keep dry, cool, and away from ignition sources; avoid UV exposure and excessive dust inhalation. Bagged loads are palletized and stretch-wrapped.
    Storage Store Sclair 11P2 Butene LLDPE Film Resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Stack securely, avoid punctures, rotate stock first-in, first-out, and maintain clean, dry conditions with good housekeeping. Protect from prolonged UV exposure and physical damage.
    Shelf Life Shelf life is typically 12 months from manufacture when stored in original unopened packaging, cool, dry, and away from direct sunlight.
    Application of NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin

    In direct food-contact monolayer blown-film production, Sclair® 11P2 butene LLDPE is processed at melt temperatures of 190–205 °C on single-screw extruders having barrier screws with an L/D of 30:1–33:1 and a spiral mandrel die with a die gap of 1.8–2.2 mm. The nominal density of 0.918 g/cm³ (ASTM D1505) and melt index of 1.0 g/10 min at 190 °C/2.16 kg (ASTM D1238) establish a process window in which bubble stability remains adequate up to a blow-up ratio of approximately 2.8:1 without incurring excessive MD tensile loss. Compliance references for direct food contact include 21 CFR 177.1520(c) and EU Regulation (EC) No 10/2011, Annex I and Annex III; converters are responsible for verifying overall migration below 10 mg/dm² under the intended food type and time–temperature conditions. The formulation addition ratio is 80–100 wt% 11P2, 0–20 wt% LDPE homopolymer, and 0–2 wt% slip/antiblock masterbatch; LDPE additions above 20 wt% reduce dart impact (ASTM D1709) but improve bubble stability. Downstream processing on a 250 mm spiral mandrel die runs a blow-up ratio of 2.0:1–2.8:1, frost-line height of 6–10 die diameters, web thickness of 25–75 µm, and dual-lip air-ring cooling with exhaust temperatures below 40 °C. Terminal finished products are frozen vegetable pouches, cereal liner films, bakery overwrap, and barrier lamination base webs where the LLDPE sealant function is separated from the barrier layer. Pre-drying is not required when the resin remains sealed; if silo or hopper storage exceeds 60% RH, surface moisture can produce bubble defects and a vented hopper dry at 60–70 °C for 2–4 h is recommended.

    What Changes When 11P2 Is Blended with Post-Industrial Reclaim in Heavy-Duty Industrial Liners?

    The primary process conflict in heavy-duty liner extrusion occurs when post-industrial reclaim and carbon black masterbatch are introduced into a film grade whose butene branch distribution produces a lower shear sensitivity than hexene LLDPE. On grooved-feed extruders with L/D ratios of 25:1–30:1 and screen packs of 80/120/80 mesh, head pressure typically increases by 15–30% when reclaim content exceeds 20 wt%; this requires lowering melt temperature to 180–195 °C and reducing screw speed to avoid gel oxidation and bubble-hole formation. Compliance references include ASTM D4976 for polyethylene film-grade classification, ASTM D1709 dart drop impact, and ASTM D1922 Elmendorf tear. Where UN-certified dangerous goods liners are produced, packaging performance testing follows UN Model Regulations Part 6 and applicable national 49 CFR provisions. The formulation addition ratio is 55–75 wt% 11P2, 10–20 wt% LDPE homopolymer, 10–25 wt% clean post-industrial reclaim, and 1–3 wt% carbon black masterbatch. Downstream processing on a spiral mandrel die with a die gap of 2.0–2.5 mm and blow-up ratio of 2.2:1–3.0:1 includes tandem air-ring cooling, gusseting boards, and web thickness of 100–250 µm. Melt filtration through the 80/120/80 mesh screen pack is retained as a critical control because reclaim-derived gel particles above 250 µm create die-lip streaks and localized gauge variation. Dart impact retention in such blends is tested under ASTM D1709 Method A at 23 °C; converter experience indicates that reclaim loadings above 25 wt% can reduce dart drop values by more than 15% relative to virgin film. Terminal products are heavy-duty sacks, FIBC liners, construction-grade temporary containment film, and industrial bin liners. Published data for 11P2-specific blends above 25 wt% reclaim is limited; converter trials are required to validate dart impact and tear retention because reclaim source variability can shift additive distribution and gel content.

    Agricultural silage cover lines using 11P2 differ from food-film lines principally in that UV stabilization, long outdoor exposure, and high puncture resistance dominate formulation choices rather than organoleptic neutrality. Compliance under EN 13206:2017 for thermoplastic silage covering films is evaluated by resistance to tear, puncture, and thickness retention after field exposure; REACH (EC) No 1907/2006 applies to the polymer and any added UV stabilizer substances, though the polymer itself is exempt from registration. The formulation addition ratio is 70–90 wt% 11P2, 10–20 wt% LDPE homopolymer, and 1–5 wt% UV/HALS masterbatch; higher HALS loadings above 5 wt% may create surface bloom and reduce film-to-film friction needed for bale wrap retention. Downstream processing on a three-layer coextrusion line with a 250 mm die, die gap 2.0–2.5 mm, blow-up ratio 2.3:1–2.8:1, and film thickness 100–200 µm produces a core-rich structure in which 11P2 is used in the skin or core for tear propagation resistance. Terminal finished products are silage bunker covers, round bale wrap film, and temporary greenhouse end-wall covering. Published data for 11P2 under EN 13206:2017 field-aging protocols is limited; converter weathering trials should validate UV masterbatch concentration against the intended exposure duration.

    Blown Stretch Film Cling-Layer Design with Butene LLDPE

    Cling-layer formulation on a three-layer blown stretch line requires control of migration of cling additives into the backing layer over a rolled-storage period of up to 90 days. The formulation addition ratio is 75–85 wt% 11P2, 10–20 wt% LDPE homopolymer, and 2–5 wt% cling masterbatch; cling additive migration is assessed by peel cling test ASTM D5458 and blocking force under ASTM D3354. Compliance references include ASTM D5458 for stretch wrap cling, ASTM D4649 for stretch film selection, and REACH (EC) No 1907/2006 for the additive package. Downstream processing on a three-layer coex blown line with melt temperatures of 190–210 °C, die gap 1.5–2.0 mm, BUR 2.0:1–2.5:1, and frost-line height 4–7 die diameters maintains a low level of MD orientation and preserves load retention. Terminal products are hand pallet wrap, machine pallet wrap, and stretch hood film. Blocking can occur if wound rolls are stored above 30 °C or if cling additive concentration exceeds 5 wt%; published data for additive migration rates in 11P2 is limited, so converter trials are required for specific roll diameters and storage intervals.

    Laminators converting PET-BOPP-foil structures select a blown LLDPE sealant web at 40–70 µm thickness when low seal initiation and puncture resistance are required for stand-up pouches. Compliance references for food contact laminates are 21 CFR 177.1520(c) and EU Regulation (EC) No 10/2011, Annex I and Annex III; the converter must verify the finished laminate migration under the intended surface-to-volume ratio. The formulation addition ratio is 70–90 wt% 11P2, 10–30 wt% LDPE homopolymer, and 0–2 wt% antiblock masterbatch; LDPE above 30 wt% increases seal initiation temperature and lowers hot-tack strength under ASTM F1921. Downstream processing uses a blown-film line with a die gap of 1.8–2.2 mm, BUR 2.0:1–2.5:1, frost-line height 5–8 die diameters, followed by corona treatment to 40–42 mN/m (ASTM D2578) and solventless adhesive lamination at line speeds of 150–250 m/min. Terminal finished products are stand-up pouches, lidding films, dry food bags, and bakery rollstock. Seal initiation for butene LLDPE is generally reported at 90–100 °C in converter specifications; published hot-tack data for 11P2 under ASTM F1921 is limited and must be generated per lamination structure.

    When Collation Shrink Film Requires Balanced MD/TD Shrinkage

    If the bubble is run above a 2.6:1 blow-up ratio without sufficient frost-line height, 11P2-based collation shrink blends can develop uneven MD/TD orientation and insufficient shrink tension around can or bottle multipacks. The formulation addition ratio is 80–90 wt% 11P2 and 10–20 wt% LDPE homopolymer; adding LDPE above 20 wt% raises TD shrinkage and improves optics but may lower puncture resistance under ASTM D5748. Compliance references include ASTM D2732 for unrestrained linear thermal shrinkage and ISO 14616 for shrinkage tension and contraction stress. Downstream processing on a double-bubble or high-stalk blown line uses die gap 1.8–2.2 mm, melt temperature 195–215 °C, first-bubble BUR 2.0:1–2.5:1, and second-bubble temperature 110–130 °C to fix orientation without producing curved bags. Frost-line height must be maintained at 8–12 die diameters when first-bubble BUR exceeds 2.4:1; insufficient cooling produces a broad crystalline size distribution that can reduce shrink tension under ISO 14616. Terminal finished products are collation shrink bundles for bottled water, canned goods, and industrial multi-pack overwrap. Published data for this specific configuration is limited; shrink tension targets are converter-specific and should be measured on production film because bubble cooling rate affects final shrinkage anisotropy.

    Free Quote

    Competitive NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Sclair® 11P2 is a butene linear low density polyethylene film resin supplied in pellet form for cast film conversion and selected blown film processes where a nominal density of 0.918 g/cm³ (ASTM D792 / ISO 1183-1) and a melt index of 1.0 g/10 min (ASTM D1238 / ISO 1133-1, 190°C/2.16 kg) are specified. The butene comonomer introduces short-chain branches that reduce crystalline density and produce a semicrystalline morphology with a peak melting point near 122°C under ASTM D3418 / ISO 11357-3 differential scanning calorimetry. The resin is typically processed without predrying; LLDPE has a water absorption below 0.01% at 23°C and 50% relative humidity, and surface condensation on cold pellets transferred from outdoor silos remains the primary source of moisture in the hopper. Lot-specific certificates of analysis should be used to confirm slip, antiblock, and processing stabilizer concentrations because those additive levels vary with production campaign and are not included in an abbreviated technical data sheet. In cast film applications, the resin is used for thin-gauge stretch wrap, industrial liners, and lamination films where a balance of drawdown, toughness, and optical quality is required. The grade is not intended for high-melt-strength processes such as large-part blow molding or deep-draw thermoforming unless blend trials establish adequate sag resistance.

    Quality control laboratories verify melt index by ASTM D1238 and density by ASTM D792 on each lot. Additional tests such as gel count on a 25 µm cast film sample are used to monitor melt homogeneity; gel counts above 10 per m² at a size threshold above 600 µm generally indicate oxidative degradation or unmelted resin. Brabender torque rheometry at 190°C and 50 rpm can compare lot-to-lot viscosity stability, and a torque variation greater than 5% may indicate molecular weight drift. The melt flow ratio obtained by dividing ASTM D1238 high-load melt index at 21.6 kg by the standard 2.16 kg melt index is a practical indicator of molecular weight distribution. For Ziegler-Natta butene LLDPE of this grade, melt flow ratio values typically fall between 22 and 28, indicating a moderately broad distribution suitable for cast film. Capillary rheometry under ASTM D3835 at 190°C and 100 s⁻¹ typically shows apparent viscosity in the 800–1200 Pa·s range, but the exact value depends on molecular weight distribution and comonomer incorporation.

    How Does 11P2 Differ From Hexene, Octene, and Metallocene LLDPE Resins of Similar Melt Index?

    Comparative evaluations of butene, hexene, and octene LLDPE at equivalent density show that the choice of comonomer changes the tie-molecule population and the short-chain branching distribution. A Ziegler-Natta butene resin such as 11P2 typically exhibits lower dart impact under ASTM D1709 and lower Elmendorf tear under ASTM D1922 than a single-site hexene or octene LLDPE of the same melt index and density. The performance gap arises because butene-generated short-chain branches are shorter and less efficient at creating intercrystalline load-bearing tie chains than hexene or octene branches. In production-scale cast film trials, a converter may observe 20–40% lower dart impact at 20 µm gauge when replacing a hexene LLDPE with a butene LLDPE of equal melt index; published data for this specific configuration is limited and the actual difference depends on die gap, melt temperature, and quench rate. The same structural distribution that reduces toughness also reduces melt pressure and extruder amperage on smooth-bore cast film extruders. Compared with metallocene LLDPE, 11P2 provides a wider processing window and lower gel sensitivity but sacrifices ultimate haze, gloss, and puncture resistance. Metallocene resins require tighter melt temperature control and often produce higher backpressure; 11P2 tolerates a broader range of screw speeds without melt fracture. Compared with LDPE of similar density and melt index, 11P2 has higher tensile strength at break and greater dart impact because of the linear backbone and controlled short-chain branching. Compared with HDPE film resins, it has lower stiffness and lower temperature resistance; the Vicat softening point is near 103°C under ASTM D1525, whereas HDPE film grades often exceed 125°C. Compared with EVA and ULDPE, 11P2 provides lower cling and lower low-temperature seal initiation, but better thermal stability and lower extractables.

    On a 75 mm single-screw extruder with 30:1 L/D, a barrier screw, and a coat-hanger die, cast film processing of Sclair 11P2 typically uses barrel setpoints of 180°C in the feed zone, 220°C in the compression zone, 240°C in the metering zone, and 250–260°C at the die and adapter. Melt temperature measured at the adapter should not exceed 270°C; residence times above 5 min at melt temperatures above 260°C can produce oxidized gel specks and reduce film elongation at break under ASTM D882. A die gap of 0.5–0.8 mm and a chill roll temperature of 15–30°C are used to balance quench rate, web flatness, and optical quality. The 1.0 g/10 min melt index permits drawdown to gauges of 12–25 µm at line speeds of 150–300 m/min on chill-roll cast lines. Draw resonance may appear when draw ratio exceeds 20:1; the instability appears as periodic machine-direction thickness bands. Mitigation requires increasing die gap to 0.8 mm, reducing melt temperature by 5–10°C, or adjusting the air knife and electrostatic pinning to stabilize the melt web on the chill roll.

    A production-scale failure mode observed on chilled-roll cast film lines is edge instability caused by melt web neck-in. Neck-in increases with die-to-chill roll distance and low melt strength; at die-to-chill roll distances above 120 mm, neck-in can reduce usable web width by 10–15%. Edge pinning via electrostatic wire or air knife is therefore required at line speeds above 200 m/min. In multilayer coextrusion, 11P2 is placed in skin or subskin layers where its low gel count and drawdown reduce edge trim losses; the core layer may use lower-cost LLDPE or LDPE, provided interlayer viscosity ratio at the melt temperature remains within 0.7:1 to 1.3:1 to avoid interfacial instability. Thickness variation measured across the web on a 1.5 m wide cast line is typically maintained below ±3% using automatic die bolt control; excursions beyond ±5% correlate with draw resonance or die lip fouling. Melt filtration with a 80–120 mesh screen pack reduces gel particles but increases melt temperature by 2–5°C, and a head pressure above 35 MPa on a 75 mm extruder indicates excessive output or an undersized die gap.

    Cast Film Property Responses Require Gauge, Chill Roll Temperature, and Line Speed Measurement

    Film property data generated on a cast line with 25 µm gauge, 0.6 mm die gap, 20°C chill roll, and 200 m/min line speed typically fall within the envelope shown in Table 1. The values are not lot-specific guarantees; additive slip and antiblock levels influence coefficient of friction and haze.

    Typical cast film property envelope for Sclair 11P2 at 20–25 µm gauge
    PropertyTest methodTypical envelope
    Tensile strength at break, MDASTM D88235–45 MPa
    Tensile strength at break, TDASTM D88225–35 MPa
    Elongation at break, MDASTM D882500–650%
    Elongation at break, TDASTM D882650–800%
    Dart drop impactASTM D170980–120 g
    Elmendorf tear, MDASTM D192240–60 g
    Elmendorf tear, TDASTM D192260–100 g
    HazeASTM D10033–6%
    Gloss at 60°ASTM D245770–85
    Kinetic coefficient of frictionASTM D18940.10–0.30

    Optical and frictional properties are strongly influenced by the slip and antiblock additive package selected by the converter. A film without added slip may exhibit kinetic coefficient of friction above 0.50 under ASTM D1894, while a high-slip concentrate may lower film-to-film kinetic COF to 0.10–0.20. Because Sclair 11P2 is a butene LLDPE, haze values in cast film are typically higher than those of metallocene LLDPE of the same density and gauge, but lower than blown film made at the same gauge due to faster quench and reduced spherulite size. For stretch wrap evaluations, the converter should measure stretch force at 200% elongation, unwind force, and puncture resistance on a stretch film test stand; the exact stretch ceiling depends on film gauge and additive package. Tensile hysteresis measurements under ASTM D882 can be used to quantify load retention after stretching, but published data for this specific configuration is limited.

    Regulatory Compliance and Food-Contact Additive Boundaries

    Food contact applications require confirmation that the finished film meets the extraction limitations of FDA 21 CFR 177.1520(c) for olefin polymers. The supplier’s food-contact certificate should be obtained for each lot and must be matched to the intended Conditions of Use A through H. For European Union applications, EU Regulation No 10/2011 specifies an overall migration limit of 10 mg/dm² for plastic food-contact articles; specific migration limits for additives and monomers must be evaluated on the finished film, not on the resin pellet. The converter is responsible for ensuring that processing temperatures, trim recycle levels, and masterbatch additions do not create degradation products that exceed migration limits. Neat polyethylene does not normally contain RoHS-restricted heavy metals, but pigmented masterbatches may introduce lead or cadmium; the EU Packaging Directive 94/62/EC imposes a combined limit of 100 mg/kg for lead, cadmium, mercury, and hexavalent chromium in packaging materials. The resin should be referenced as registered under REACH where applicable; Safety Data Sheets and lot certificates provide SVHC declarations and additive identification.

    Regulatory verification matrix for film converters using Sclair 11P2
    RegulationScopeVerification measure
    FDA 21 CFR 177.1520(c)Olefin polymer food contactSupplier food-contact letter; end-use extraction testing
    EU Regulation No 10/2011Plastic food-contact materialsOverall migration 10 mg/dm²; specific migration limits
    REACH (EC) 1907/2006Registration and SVHCSDS and lot certificate
    EU Packaging Directive 94/62/ECPackaging heavy metalsCombined Pb, Cd, Hg, Cr VI 100 mg/kg

    When High-Toughness Film Specifications Require Gauge Compensation or Resin Blending

    Converters replacing a hexene LLDPE or metallocene LLDPE with Sclair 11P2 in stretch-wrap or heavy-duty sack applications should evaluate dart impact and puncture resistance at the same gauge. Where the target specification is a dart drop of 120 g under ASTM D1709 at 25 µm, a butene LLDPE may require a gauge increase of 10–20% or blending with hexene LLDPE or metallocene LLDPE to reach the same value; published data for this specific configuration is limited. The resin should not be processed at melt temperatures above 270°C or stored in direct sunlight for more than six months because UV exposure can initiate chain scission and reduce film tear performance. Predrying is not required, but cold pellet surface condensation at ambient relative humidity above 60% should be prevented by storing pellets in a closed silo or by heating the hopper to 40–50°C. Incompatibility with certain peroxide masterbatches can occur if the peroxide half-life temperature is below the extrusion melt temperature; uncontrolled free-radical reactions can produce crosslinked gels or alter the molecular weight distribution. Chemical blowing agent masterbatches intended for high-temperature processing should be evaluated before use because LLDPE film lines typically operate near 240–260°C.

    At ambient warehouse temperatures below 40°C, pellet flow in bulk handling systems remains stable, but high concentrations of fines generated from pneumatic conveying can accumulate at die lips and cause die lines. Conveying systems should use low-velocity dense phase or reduce elbow angles; fines are typically measured by sieve analysis under ASTM D1921 and should remain below 500 ppm before the extruder hopper.

    Top