Nova Chemicals Sclair 11l4b Octene Lldpe Film Resin

NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin

    • Product Name: NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 988220
    Meltindex 0.8 g/10 min (190°C/2.16 kg)
    Density 0.920 g/cm3
    Comonomer Octene
    Tensilestrengthatyieldmd 10 MPa
    Tensilestrengthatyieldtd 10 MPa
    Tensilestrengthatbreakmd 31 MPa
    Tensilestrengthatbreaktd 28 MPa
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Dartdropimpact 250 g
    Elmendorftearmd 250 g
    Elmendorfteartd 400 g
    1 Secantmodulusmd 170 MPa
    1 Secantmodulustd 190 MPa
    Haze 12%
    Gloss 60%
    Meltingpoint 122°C
    Vicatsofteningpoint 100°C
    Brittlenesstemperature -70°C

    As an accredited NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin is packaged in 25 kg polyethylene bags, palletized for bulk shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin, securely stowed for ocean shipment.
    Shipping NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin is typically shipped as non-hazardous polyethylene pellets in 25 kg bags, bulk bags, or bulk trucks/railcars, usually palletized and stretch-wrapped. Keep containers closed, dry, and away from heat, sunlight, and ignition sources. Follow standard handling and local transport regulations.
    Storage Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure, excessive stacking, and storage near strong oxidizers. Maintain moderate temperatures, practice first-in/first-out rotation, and consult the SDS for complete handling and storage requirements.
    Shelf Life Two years from date of manufacture when stored in original unopened packaging below 50°C, away from direct sunlight.
    Application of NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin

    Why Does Thin-Gauge Cast Pallet Film Lose Puncture Resistance at High Draw Ratios?

    Cast pallet wrap built around Sclair 11L4B is run at melt temperatures between 245 °C and 275 °C; the octene branch distribution provides lower melt-viscosity retention than a butene copolymer at equivalent 0.919 g/cm³ density, allowing extrudate to be drawn down to 12–23 µm without excessive neck-in. The resin is supplied with a melt index of 1.0 g/10 min under ISO 1133-1:2022, and density is controlled under ISO 1183-1:2019. On high-speed cast lines the loss of puncture resistance is not caused by resin degradation but by unbalanced machine-direction orientation at draw ratios above 30:1; the film develops a fibrous machine-direction internal structure that reduces dart impact energy absorption.

    The applicable industrial benchmark is ASTM D4649-20, which sets out load retention and stretch wrap evaluation procedures for pallet unitization. Cling properties are tested in accordance with ASTM D5458-19, and film tear resistance is ranked under ASTM D1922. For shipment within the European Union, the grade is covered by REACH 1907/2006 declaration and contains no SVHC above 0.1 wt%.

    In monolayer cast film, the grade is used at 100 wt%. In two-layer and three-layer structures, the main layer contains 90–98 wt% Sclair 11L4B, while the cling layer carries 2–8 wt% polyisobutylene or EVA tackifier in a carrier matrix. Addition of LDPE above 15 wt% is avoided because it increases melt tension and widens the molecular weight distribution, reducing draw stability at line speeds above 450 m/min.

    Production-scale cast lines use 90–120 mm single-screw extruders with 30:1 L/D barrier compression screws, flat dies with 0.8–1.2 mm die gap, and chill roll temperatures of 15–25 °C. Line speed ranges from 300 m/min to 700 m/min. Edge pinning by vacuum box retains neck-in at 5–8%; without edge encapsulation, neck-in rises to 14–18% at 550 m/min. This edge instability is the primary process boundary for thin-gauge cast grades.

    Terminal film types include machine pallet wrap at 12–23 µm, hand pallet wrap at 20–30 µm, and pre-stretched cast films wound after 180–250% pre-stretch. The same formulations are converted into light bundling films and industrial overwrap where high retained load force is required.

    Blown-film conversion of Sclair 11L4B for frozen food packaging places the frost line higher in the bubble than a butene LLDPE of equal density because the octene side-chain distribution delays strain-hardening during bubble expansion. Melt temperature is controlled at 210–240 °C, and die exit pressure is maintained below the point where melt fracture initiates at the outer lip. The resulting film retains dart impact strength at freezer temperatures; compliance testing for dart impact follows ASTM D1709-15a, and tear resistance follows ASTM D1922.

    Standard/RegulationDesignationControl Point
    U.S. food contact21 CFR 177.1520(c)Olefin polymers in contact with food
    EU food contactEU 10/2011 Annex IOverall migration limit 10 mg/dm²
    Melt flow rateISO 1133-1:2022190 °C, 2.16 kg
    Dart impactASTM D1709-15aLow-temperature impact classification
    Tear resistanceASTM D1922Elmendorf tear

    In three-layer coextruded structures, the core layer contains 60–85 wt% Sclair 11L4B, while the outer skins contain 15–40 wt% LDPE to maintain bubble stability. Slip and antiblock masterbatch is added at 0.5–2.0 wt% depending on film gauge and converting speed. A monolayer film at 100 wt% 11L4B is limited to gauge ≤60 µm because bubble oscillation becomes difficult to correct above that thickness on monolayer towers without internal bubble cooling.

    The standard blown-film process uses a 250 mm die, a die gap of 1.8–2.3 mm, and a blow-up ratio between 2.0 and 3.0. Internal bubble cooling is required for output rates above 180 kg/h. The film is corona-treated to 38–42 mN/m before slitting; treatment above 48 mN/m is not recommended because the seal initiation temperature shifts upward during subsequent pouch converting.

    Terminal formats include frozen vegetable and ready-meal pouches, ice cream lidding film, frozen seafood packaging, and box liners for quick-service restaurant supply chains. In each format, the film is sealed at 110–130 °C with dwell times from 0.3 s to 0.8 s on horizontal or vertical form-fill-seal equipment.

    Draw-Down Limits During Extrusion Coating onto Kraft Paperboard

    Extrusion coating of Sclair 11L4B onto kraft paperboard is performed at melt temperatures of 290–320 °C; at this range the resin forms a stable curtain without melt tearing at coat weights between 12 g/m² and 25 g/m². The octene comonomer reduces neck-in compared with similarly processed LDPE coatings, allowing narrower edge trim and less web waste. A 90 mm single-screw extruder with 28:1 L/D and a barrier screw is used, and the flat die gap is kept at 0.6–0.8 mm to maintain backpressure.

    Food-contact compliance for paperboard packages is governed by 21 CFR 176.170 for paper and paperboard components, together with EU 10/2011 Annex I for migration from the plastic layer. The grade is processed at 100 wt% in most extrusion-coating operations. Where adhesion to kraft board is marginal on a chilled matte roll, a blend of 10–30 wt% LDPE is introduced to increase oxidation sites at the melt curtain. Adhesion is established without a primer when ozone output is 0.8–1.2 kW and chill roll temperature is held at 5–12 °C.

    Line speed in production ranges from 150 m/min to 400 m/min. Above 400 m/min, edge tearing of the curtain occurs before draw-down failure; this is observed as microweb holes at the curtain edges and requires immediate edge trim adjustment. The air gap between die exit and nip is set at 150–250 mm to balance oxidation and neck-in.

    Terminal coated substrates include paperboard cups, folding carton stock, multi-wall paper sacks, and paper-based carrier materials for industrial goods. The coated layer also functions as a moisture barrier in dry food cartons and as a sealing surface on paperboard trays.

    In heavy-duty shipping sack production, the addition of Sclair 11L4B is governed by creep resistance at low temperature rather than by optical properties. On three-layer blown-film lines, the core layer contains 50–80 wt% of the octene LLDPE; the two surface layers contain 20–40 wt% blended with LDPE for surface smoothness and heat sealing. For a monolayer FIBC liner film, the resin is processed at 100 wt% at a gauge of 150–250 µm.

    Compliance for FIBC and liner constructions follows ISO 21898:2015, which specifies classification and test methods for flexible intermediate bulk containers. For sacks used in dangerous goods transport, the converter must additionally verify the construction against the applicable UN packaging certificate; the resin itself is supplied under REACH 1907/2006 with no SVHC above 0.1 wt%.

    The blown-film operation uses a die diameter of 250–300 mm, die gap 2.0–2.8 mm, and blow-up ratio 1.8–2.5. Internal bubble cooling is essential above 150 µm film thickness; at thicknesses above 180 µm, IBC air exchange must be raised to 80–120 m³/h per meter of die circumference. Collapsing frames with gussets maintain layflat width before winder tension is tapered from 30 N at core start to 10 N at finished roll diameter. Corona treatment is set at 40–44 mN/m for printing on the outer skin.

    Terminal products include fertilizer sacks, polymer granule bags, mineral and chemical shipping sacks, and vented FIBC liners. In these applications the film’s low-temperature puncture resistance is measured by ASTM D1709-15a and its tensile yield behavior by ISO 527-3:2018.

    When Bubble Stability Collapses Above 80 wt% in Agricultural Silage Film

    The upper addition limit of Sclair 11L4B in agricultural silage film is set by tear propagation under field tension rather than by extruder amperage. In a three-layer line, the core layer tolerates 70–80 wt% of the grade, with 10–20 wt% LDPE added to maintain melt strength and 5–10 wt% EVA to increase tack. The agricultural film converter typically adds a HALS UV stabilizer masterbatch at 2–6 wt% and, where black silage covers are required, carbon black at 0.5–2 wt%. Above 80 wt% 11L4B in the core, bubble teardrop instability appears during ambient-temperature startups because the low melt tension allows the bubble neck to elongate below the die face. Published converter data for this exact grade in silage-specific constructions is limited; the upper addition limit is inferred from parallel octene LLDPE grades on the same line.

    Compliance for non-food agricultural films falls under EN 13206:2018 for covering films, with durability tested by UV weathering methods defined in the standard. Where the film is exported into multiple jurisdictions, the converter verifies REACH 1907/2006 and local waste-incineration limits for metal-containing pigment masterbatches.

    Silage film is produced on monolayer or three-layer blown-film lines with a 300 mm die, die gap 2.0–2.5 mm, and blow-up ratio 2.2–3.0. Melt temperature is held at 190–220 °C to prevent degradation of the UV stabilizer package. Film thickness ranges from 100 µm to 200 µm. For silage bale wrap, an in-line pre-stretching unit is operated at 60–70% pre-stretch before wrapping; this step is adjusted to avoid whitening at the film edges, which indicates excessive orientation.

    Terminal products include silage bale wrap, horticultural greenhouse covers, and short-service mulch films. The grade is also used in black silage pit covers where high puncture resistance against corn stover is required.

    Differential scanning calorimetry of the coextruded sealant web shows a seal initiation plateau when Sclair 11L4B is present at 60–90 wt% in the sealant layer; this plateau allows horizontal form-fill-seal lines to reduce sealing temperature from 145 °C for a standard LDPE sealant to 110–130 °C without reducing seal strength. The remaining 10–30 wt% is LDPE to raise bubble stability during blown-film conversion. Slip masterbatch is metered at 0.1–0.3 wt%, antiblock at 0.1–0.4 wt%, and a fluoroelastomer processing aid at 0.02–0.05 wt% to suppress die lip buildup.

    Food-contact compliance follows 21 CFR 177.1520(c) and EU 10/2011 Annex I. For dry foods, overall migration must remain below 10 mg/dm²; for fatty foods, the converter must verify the finished pouch under the relevant food simulant in EU 10/2011 Annex III. Seal strength tests are conducted under ASTM F88/F88M and burst strength under ASTM F2054.

    The blown-film process uses a three-layer die with a die gap of 1.5–2.0 mm, total film thickness of 35–80 µm, and a sealant layer thickness of 15–25 µm. Corona treatment is held at 38–42 mN/m; over-treatment above 48 mN/m shifts heat-seal initiation upward and is avoided on high-speed pouch lines. Seal jaws are set at 1.2–2.5 bar pressure with 0.3–0.8 s dwell; below 0.3 s intermittent cold-spot failures occur in the transverse seal at production speeds above 80 cycles/min.

    Terminal formats include snack food pouches, dry mix pouches, frozen seafood pouches, and sachet applications where low seal initiation temperature is required on thin-gauge sealant webs.

    Free Quote

    Competitive NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Sclair 11L4B is a linear low-density polyethylene film resin manufactured with 1-octene as the alpha-olefin comonomer. The nominal melt index is 1.0 g/10 min tested under ASTM D1238 at 190 °C with a 2.16 kg load, and the nominal density is 0.918 g/cm³ tested under ASTM D1505 or ASTM D792. The grade is supplied in pellet form and is intended primarily for blown-film extrusion rather than cast-film conversion. The octene-derived short-chain branches contain 6 carbon atoms, while butene-derived branches contain 2 carbon atoms; this difference in branch length is a primary structural variable governing low-temperature toughness, tear resistance, and drawability. The resin-level density and melt index do not predict final film performance. Film performance must be measured using film-specific methods such as ASTM D1709 for dart impact, ASTM D1922 for Elmendorf tear, ASTM D882 for tensile properties, ASTM D1003 for haze, and ASTM D2457 for gloss. The product is selected for heavy-duty sacks, industrial liners, shipping sacks, agricultural films, and high-performance blown-film structures where improved impact-strength-to-gauge relationships are required.

    Nominal resin-level specification values for NOVA Chemicals Sclair 11L4B
    PropertyTest methodNominal value
    Melt indexASTM D12381.0 g/10 min
    DensityASTM D15050.918 g/cm³
    ComonomerMaterial composition1-octene
    Primary conversion routeProcess specificationBlown-film extrusion

    What separates 11L4B from butene LLDPE at the same density and melt index?

    The principal difference is branch length. At an equivalent density of 0.918 g/cm³, an octene-copolymerised LLDPE requires a lower molar fraction of comonomer than a butene-copolymerised LLDPE to achieve the same amorphous-phase disruption. The longer hexyl branch in 11L4B is more effective at creating intercrystalline tie molecules during crystallisation, and those tie molecules reduce low-temperature brittle failure. The practical result is measurable under ASTM D1709 dart impact and ASTM D1922 Elmendorf tear: at the same gauge, the octene-based film typically exhibits higher dart impact energy and higher tear propagation resistance than a butene-based film of the same density. Tensile yield strength measured under ASTM D882 is less sensitive to branch length because yield is controlled primarily by density and orientation state; therefore a comparison of yield stress alone will not reveal the toughness difference. The property gap widens below 5 °C, where butene LLDPE loses ductility more rapidly than octene LLDPE. That difference matters in cold-storage packaging, frozen-food distribution, and outdoor agricultural films subjected to wind and abrasion.

    Butene LLDPE is not uniformly inferior. On the extrusion side, butene-copolymer LLDPE often gives lower melt pressure and can be processed on lower-torque extruders. The shift to an octene grade such as 11L4B may require a higher drive load on a single-screw blown-film extruder with a 24:1 to 30:1 L/D barrier screw because the longer branch and broader molecular weight distribution change the shear-viscosity curve. The processing trade-off is generally accepted when the end-use specification requires a minimum dart impact or tear value that butene film cannot meet without increasing gauge.

    When 11L4B moves through a spiral mandrel die on a high-output blown-film line

    Extrusion conditions for 11L4B are typically set within a melt-temperature range of 190–230 °C. Lower temperatures increase melt viscosity and head pressure; higher temperatures may reduce bubble stability and accelerate oxidative gel formation. The grade is compatible with conventional smooth-bore and grooved-feed single-screw extruders using barrier or Maddock mixing sections. Die gaps from 1.0 mm to 2.5 mm are used in blown-film conversion, with the wider gap preferred for thicker films above 50 µm to reduce melt fracture and improve bubble stability. Blow-up ratio is normally held between 2.0:1 and 3.0:1. A value near 2.5:1 is common for balanced machine-direction and transverse-direction tear, but the optimum is dependent on die gap, frost line height, and film gauge. Frost line height is typically set from 1 to 8 die diameters, depending on cooling-air velocity and output rate.

    On lines with a spiral mandrel die and a dual-lip air ring, bubble instability with 11L4B is most often observed as low-frequency bubble breathing or as high-side draw resonance. Raising the frost line height or reducing cooling-air velocity generally corrects the breathing mode. Melt fracture, appearing as surface roughness on the film, may occur at low melt temperature or narrow die gaps. In that case, increasing the die gap or raising the melt temperature within the specified window reduces the instability. Compared with metallocene-catalysed LLDPE of similar density, 11L4B tends to have a broader shear-response window, which improves bubble stability across a wider range of extruder speeds but can produce higher haze. The broader molecular weight distribution also reduces melt fracture sensitivity at high output rates on large-diameter dies.

    Blending with butene LLDPE or recycled polyethylene is performed on-line by dry blending pellets or by melt blending in a compounding step. Addition levels of 11L4B from 10 wt% to 50 wt% are commonly used to raise dart impact and tear strength of lower-performance scrap streams. Above 50 wt%, the blend begins to take on the processability and property profile of the octene resin. The exact addition level must be validated by film testing under ASTM D1709 and ASTM D1922 at the target gauge because the relationship between blend ratio and film toughness is non-linear.

    Die-gap, frost-line, and tear-balance control in 11L4B film

    Tear balance in 11L4B film is controlled by molecular orientation frozen during bubble cooling. Machine-direction tear strength measured under ASTM D1922 decreases as the film is drawn more strongly in the machine direction, while transverse-direction tear strength increases. A narrow die gap combined with a low frost line height generally intensifies machine-direction orientation and depresses machine-direction tear. A wider die gap or a higher frost line height allows greater relaxation before solidification and shifts the tear balance toward the transverse direction. This interaction is not linear and must be established on the production line because the same-grade specification can produce different tear results when die gap changes from 1.5 mm to 2.5 mm at constant blow-up ratio.

    Dart impact under ASTM D1709 is less sensitive to orientation than tear but is gauge-dependent. Thicker 11L4B films show higher dart impact energy because more material participates in deformation before puncture. For example, a film gauge increase from 25 µm to 50 µm does not simply double dart impact; the relationship is non-linear and is influenced by cooling rate and frost line height. Converters should generate a gauge-series dataset on their specific line rather than relying on a single gauge from a technical data sheet. Published data for this specific configuration may be limited, particularly for coextruded films where 11L4B is used in a core or toughness layer.

    For food-contact constructions, 11L4B may be suitable for direct food contact under FDA 21 CFR 177.1520(c) when the final article meets extractive limits and end-use restrictions for olefin polymers. The converter must obtain the current NOVA Chemicals regulatory statement for the purchased lot because additive package and lot-specific compliance can vary. For European Union food-contact use, migration testing of the finished article under Regulation (EU) No 10/2011 is required; the resin alone does not guarantee compliance of the final multi-material article. REACH registration for the polymer substance is managed by the supplier or importer, but downstream users remain responsible for communicating their uses under REACH Article 37 and for Article 33 communication if a Candidate List substance is present in an article above 0.1% w/w.

    Storage life for LLDPE pellets is typically 6–12 months from the date of manufacturing when stored at ambient temperature and relative humidity below 60%; prolonged exposure to direct sunlight should be avoided. Purging from butene LLDPE, metallocene LLDPE, or recycled polyethylene should use a compatible LLDPE or LDPE purge compound, not vinyl-based or acetate-based purge materials, to avoid thermal degradation residues. The grade is not recommended for high-clarity shrink film where haze below 3% is required by specification, nor for cast-film extrusion where the melt curtain stability and cooling rate are better matched to lower-viscosity polyolefins. Published data for cast-film use of 11L4B is limited, and blown-film equipment remains the appropriate conversion route for this resin.

    Top