| HS Code | 309460 |
| Productname | NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin |
| Manufacturer | NOVA Chemicals |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene |
| Application | Blown Film |
| Meltindex | 0.9 g/10 min (190°C/2.16 kg) |
| Density | 0.919 g/cm³ |
| Meltingpoint | 124°C |
| Vicatsofteningpoint | 100°C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 27.6 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 241 MPa |
| Dartdropimpact | 150 g |
| Elmendorftearmd | 300 g |
| Elmendorfteartd | 500 g |
| Haze | 10% |
| Gloss45degree | 70% |
| Coefficientoffriction | 0.2 |
As an accredited NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 11L2B resin is supplied in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL: 20 pallets double-stacked, 55 × 25 kg bags per pallet; total 1,100 bags, 27.5 MT, securely wrapped. |
| Shipping | NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin is typically shipped as dry, free-flowing pellets in 25 kg polyethylene bags, bulk bags, or bulk railcars/trucks. Palletized loads are stretch-wrapped and labeled. Store in a cool, dry, clean area away from moisture, heat, and contaminants. It is generally non-hazardous for transport. |
| Storage | Store NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and oxidizing agents. Keep packages closed to prevent moisture, dust, and contamination. Place on pallets, off the floor, and rotate stock. Maintain ambient temperature and follow the SDS and local regulations. Avoid prolonged UV exposure. |
| Shelf Life | No specific shelf life assigned; stable under normal storage conditions. Store in a cool, dry, well-ventilated area away from heat and ignition sources. |
On a three-layer coextrusion blown-film line with a 75 mm grooved-feed extruder and 450 mm spiral mandrel die, Sclair® 11L2B is processed as the skin and core resin for stretch-hood pallet unitization films. The octene branch distribution provides lower crystalline orientation in the transverse direction than a butene LLDPE of equivalent density, which reduces localized thinning at pallet corners during TD stretch. Typical die gap is held at 2.0–2.5 mm, blow-up ratio between 2.2:1 and 2.6:1, and melt temperature at 205–220°C at the die lip. A 5-layer structure may place the resin in the core with 0.5–1.5 wt% polypropylene homopolymer in the skins to balance directional elongation; addition of polypropylene above 2 wt% causes a measurable loss in Elmendorf tear at 25 µm gauge. The finished pallet hood is typically 120–180 µm in thickness and is specified by end users for construction blocks, beverage pyramids, and chemical bag stacks.
Stretch-hood pre-stretch ratios are set between 30% and 60% depending on pallet load stability; at pre-stretch above 60%, the film develops transverse striations that concentrate stress at gusset folds and can reduce retained holding force after 72 h. Converters evaluate retained load force using a constant-strain pallet-load simulation, not a resin test. A dual-lip air ring with internal bubble cooling is recommended for gauge uniformity; without IBC, output rates above 180 kg/h on a 75 mm extruder typically produce frost-line oscillation and lower MD tear. The primary process boundary is condensation on pellets transferred from outdoor silos at relative humidity greater than 60%. Polyethylene does not require hydrolytic drying, but surface moisture above 0.02 wt% can generate bubble pinholes and die lip deposit. A hopper dryer set at 40°C for 2 h is the standard corrective action. Acceptable mechanical performance is verified at the converter's incoming QC through ASTM D882-18 tensile elongation and ASTM D1922-15 tear resistance; the resin alone cannot be certified against a finished-web specification without confirming layer structure and stretch ratio. For EU distribution, REACH Annex XVII and RoHS substance restrictions apply; food-contact clearance is not required for this non-food logistics track.
The transition from butene LLDPE to octene LLDPE in vertical form-fill-seal lines for IQF vegetables and seafood pouches is driven by seal-through-contamination performance and cold-temperature impact. Sclair® 11L2B at the 0.918 g/cm³ density class gives longer comonomer short-chain branches, producing higher tie-molecule concentration in the amorphous region; this reduces seal initiation to the lower end of the conventional LLDPE window and improves dart impact at −20°C when measured per ISO 7765-1:2004. In a typical 3-layer coextruded structure, the sealant skin comprises 100% Sclair® 11L2B with a silica antiblock masterbatch at 5,000–10,000 ppm active synthetic silica and erucamide slip at 600–1,200 ppm. The core layer may contain 5–10 wt% LDPE for bubble stability, but LDPE addition in the sealant skin above 20 wt% degrades hot tack measured by ASTM F1921-18 and is avoided.
High-speed vertical form-fill-seal lines operating at 60–120 packs/min impose a short seal dwell that may drop below 0.3 s. Under these conditions, hot tack measured by ASTM F1921-18 at 115–135°C seal temperatures is the controlling variable; the octene LLDPE sealant retains acceptable hot tack at lower seal bar temperatures than butene grades with the same density and melt index. Converters frequently set the seal jaw temperature at 125–150°C and maintain the cooling jaw below 35°C to prevent seal creep. Any addition of recycled trim in the sealant layer above 10 wt% broadens seal initiation variability and is rejected for frozen-food structures because of seal-through-contamination risk.
Regulatory compliance for EU and US frozen-food contact falls under FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation 10/2011; compliance requires overall migration no greater than 10 mg/dm² in the specified food simulant. Converters should request the supplier's food-contact declaration and confirm that slip and antiblock masterbatch carriers are also compliant. Slip bloom from erucamide reduces surface energy below 38 dyn/cm within 24 h of winding; corona treatment is therefore applied in-line at the blown-film line, and the converter should not store sealed rolls beyond the treated-shelf-life guarantee without retesting wetting tension per ASTM D2578-23. Terminal products include frozen vegetable bags, shrimp pouches, and ice cream overwrap; all are high-speed VFFS formats where seal bar temperature must not exceed 170°C to avoid seal-stringing caused by low-molecular-weight additives.
Because heavy-duty sack converters routinely blend Sclair® 11L2B with 5–15 wt% HDPE to raise stiffness without sacrificing the tearing resistance required for valve sacks, the resin is commonly specified in unsupported liners and multi-wall constructions. On a 90 mm grooved-feed extruder with 24:1 L/D and a barrier screw with moderate Maddock mixing, the extruder barrel is set from 180°C to 210°C, the adapter at 210°C, and the die at 210–220°C. A die gap of 2.0 mm and blow-up ratio of 2.0:1–2.8:1 are typical; frost-line height must remain below 7 die diameters, otherwise transverse direction gauge control widens beyond ±15% and bubble movement introduces edge creasing. At 100–200 µm gauge, the converted sack body is tested for dart impact by ASTM D1709-16A Method A and for slow puncture by ASTM D5748-19. Conformant sacks carry polymer pellets, mineral fillers, and chemical feedstocks; the resin's octene fraction provides resistance to split propagation along heat-sealed bottom creases.
Antistatic performance for FIBC liners is achieved by adding an amine-free antistat masterbatch at 1.0–3.0 wt%, targeting surface resistivity between 10^8 and 10^11 ohm per IEC 61340-2-3. Alkylamine-based antistats are excluded from liners used for fine mineral fillers and hygroscopic chemical powders because migratory amine species can contaminate the packed product and reduce surface resistivity stability during warehousing. The process boundary for high-carbon-black formulations is de-mixing in the feed throat; a forced side-feeder or pre-letdown masterbatch is required above 3 wt% carbon black loading. Published data for this specific resin grade in long-distance container drop tests is limited; final sack certification is always conducted on the finished structure rather than the resin alone.
At silage cover thicknesses of 180–220 µm, the principal formulation variables are hindered amine light stabilizer concentration, antifog droplet control, and the resin's inherent dart impact retention after weathering. Sclair® 11L2B is compounded with a HALS masterbatch at 1.0–3.0 wt% active HALS, a fluoropolymer processing aid at 0.1–0.3 wt%, and an antifog concentrate at 0.5–1.5 wt% for low-tunnel interior moisture control. The film is blown on a 120 mm extruder with internal bubble cooling and a die gap of 2.0 mm; blow-up ratio is kept between 2.0:1 and 3.0:1 to balance MD tear and field handling. Terminal products include silage clamp covers, bale wraps, and low-tunnel greenhouse covers. EU agricultural film is subject to EN 13206:2017 for covering thermoplastic films, which requires declaration of duration class and mechanical retention after artificial weathering.
The operational boundary for sulfur-producing environments is explicit. Sclair® 11L2B films stabilized with HALS are resistant to UV oxidation under ASTM G154-23 Cycle 1 accelerated weathering, but sulfur dioxide generated by combustion heaters can form acid deposits on the film surface, which may accelerate loss of HALS efficacy and reduce service life; direct contact with organosulfur fumigants must be avoided. Conversely, films with only UV absorbers and no HALS embrittle within a single season in regions with annual global irradiance above 2,000 kWh/m². Published data for this specific resin grade after 24-month field aging is limited; accelerated laboratory data cannot be linearly extrapolated to service life. Converters should conduct south-exposure trials in the target climate before issuing a multi-season warranty.
| Application Track | Regulatory / Standard Reference | Boundary Condition |
|---|---|---|
| Frozen food sealant web | FDA 21 CFR 177.1520(c); EU 10/2011; ASTM F88-21 | Overall migration ≤ 10 mg/dm² |
| Agricultural silage cover | EN 13206:2017; REACH Annex XVII | HALS package REACH-registered; duration class declared |
| Heavy-duty sack / FIBC liner | ASTM D1709-16A; IEC 61340-2-3 | Surface resistivity 10^8–10^11 ohm |
| Pallet hood | ASTM D882-18; ASTM D1922-15 | Directional elongation and tear measured on finished hood |
| Void-fill air pillow | ISO 7765-1:2004 | Puncture at 20 µm caliper; pillow leak test per converter |
A sealant web laminated to 12 µm aluminum foil and a PET print web is exposed to repeated flexural strain during stand-up pouch filling and distribution. In that structure, Sclair® 11L2B delivers the low-temperature crack resistance that cannot be obtained from butene-copolymer LLDPE at equivalent melt index. The film is converted as a 30–60 µm blown web, corona-treated in-line to 38–42 dyn/cm, and adhesive-laminated within 24 h before slip migration can reduce surface energy. Seal strength is evaluated with ASTM F88-21 using a 25 mm strip width, 0.5 s dwell, 0.3 MPa jaw pressure, and a seal bar temperature of 150°C. These settings are commonly specified for dry-food and pet-care stand-up pouches, where heat-seal inspection rejects channels and edge de-wetting below the laminate's minimum seal force.
Food-contact compliance for this structure is upstream of the lamination process; the resin must comply with FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 at the overall migration limit. The operational boundary is heat resistance: Sclair® 11L2B alone is not suitable for retort pouches above 121°C because the sealant web loses dimensional stability and may delaminate under steam-pressure cycles. For hot-fill applications up to 95°C, a converter may specify Sclair® 11L2B in the sealant layer with a higher-density LLDPE or HDPE backing layer to limit creep; the grade's octene fraction suppresses brittle seal failure at freezer temperatures after long distribution cycles.
Machine-direction tear control at 20 µm caliper is the principal production constraint in void-fill air pillow conversion. The pillow film is blown on high-output lines with a die gap of 1.8–2.0 mm, a blow-up ratio of 2.5:1–3.0:1, and a frost-line height set for balanced MD/TD strength. Sclair® 11L2B's octene comonomer permits down-gauging to 18–25 µm while retaining inflation seal integrity; below 18 µm, gauge variation outside ±2 µm causes random seal failure and deflation in continuous pillow lines. Antiblock is added at 3,000–6,000 ppm active synthetic silica, and slip is limited to 300–600 ppm erucamide because excessive slip reduces film-to-film friction needed for stable bubble collapse and pillow tracking. Terminal products are air pillows, bubble cushioning sleeves, and continuous void-fill tubes for electronics and pharmaceutical parcel distribution.
Puncture resistance is characterized with ISO 7765-1:2004 instrumented impact at 20 µm, and MD tear with ASTM D1922-15. The processing boundary is melt fracture at narrow die gap: if the converter pushes melt temperature above 230°C to eliminate sharkskin, gel formation from high-molecular-weight tails becomes a risk in long runs; a fluoropolymer processing aid at 0.1–0.3 wt% is preferred over temperature increase. No food-contact clearance is required for non-food protective packaging, but REACH and RoHS substance restrictions remain applicable for EU import. The resin should be evaluated on the converter's inflation line at minimum gauge before commercial release because seal bar geometry and pillow inflation pressure are machine-specific variables not governed by a universal standard.
Competitive NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 11L2B is a 1-octene linear low-density polyethylene film resin produced by NOVA Chemicals. The grade is characterized in supplier technical literature by a melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load, determined by ASTM D1238-20 Procedure A and ISO 1133-1:2022, and a nominal density of 0.918 g/cm³, determined by ASTM D1505-18 or ISO 1183-1:2019. The 1-octene comonomer is incorporated during solution polymerization, generating hexyl short-chain branches that disrupt regular packing of the polyethylene chain and increase the volume fraction of mobile amorphous phase. This molecular architecture affects large-strain tensile behavior, puncture resistance, and tear resistance differently from short-chain branching produced by butene. The resin is intended for blown film extrusion and is used in heavy-duty sacks, industrial liners, agricultural silage film, and stretch-wrap formulations. Film performance depends on gauge, die gap, blow-up ratio, frost line height, and cooling-air conditions; a single set of mechanical values is not transferable across unrelated film lines.
Additive content in Sclair® 11L2B is formulation-specific. Current supplier documentation should be consulted for exact slip, antiblock, and process stabilizer concentrations because these additives control coefficient of friction, winding behavior, and organoleptic properties. Food-contact status is not automatic: if the film is intended for food packaging, the finished article must comply with FDA 21 CFR 177.1520 in the United States or Regulation (EU) No 10/2011 in the European Union. Compliance depends on additive selection, overall migration testing under EN 1186-1, and specific migration limits for any stabilizers or processing aids. The resin is a hydrocarbon polymer; it is not hygroscopic in the same manner as polyamide or polyester, but surface condensation on pellets exposed to high humidity can introduce water into the extruder feed throat and cause surging at high screw speeds.
Selecting 1-octene rather than butene changes the distribution of short-chain branches from ethyl to hexyl repeat units in the amorphous and interfacial regions. The longer branch is less readily excluded from the lamellar core after cooling, increasing the probability of interlamellar tie chains that transmit load between adjacent crystals. Under ASTM D1709-16a dart impact, films produced at equivalent thickness generally show higher F50 values than butene-based LLDPE; the magnitude is not constant because frost line height changes the amount of co-crystallization and tie-chain relaxation. Comparative runs on a 55 mm, 30:1 L/D blown film line at a 2.5:1 blow-up ratio and 1.2 mm die gap indicate that octene-based film can maintain the same dart impact at roughly one gauge step lower than butene film; however, published data for this specific resin across all gauge ranges is limited, and line trials should be used to establish downgauging limits.
Elmendorf tear, measured under ASTM D1922-15 after conditioning for 24 h at 23 ± 2 °C and 50 ± 5 % RH, is typically asymmetric in blown film. For Sclair® 11L2B, transverse-direction tear is generally higher than machine-direction tear, a common pattern in LLDPE tubular orientation. The difference is useful for sacks and liners that fail by seam or edge tear rather than puncture.
| Comparison dimension | Sclair® 11L2B / octene LLDPE | Butene LLDPE at equal melt index and density | Reference method |
|---|---|---|---|
| Short-chain branch structure | hexyl branches from 1-octene | ethyl branches from 1-butene | — |
| Dart impact | higher F50 at equal gauge; downgauging often possible | lower impact threshold | ASTM D1709-16a |
| Elmendorf tear | balanced to transverse-direction-biased tear | more anisotropic tear envelope | ASTM D1922-15 |
| Tensile elongation at break | larger strain to rupture | reduced terminal elongation | ASTM D882-18 |
| Seal initiation temperature | approximates density-equivalent LLDPE | similar nominal seal initiation temperature | ASTM F88/F88M-21 |
| Film haze | generally above high-clarity metallocene LLDPE but acceptable for industrial film | similar for conventional Ziegler-Natta LLDPE | ASTM D1003-13 |
Extrusion behavior on conventional blown film lines follows octene LLDPE viscosity and pressure characteristics. Barrel temperature profiles may be set from hopper to adapter at 180 °C, 200 °C, 210 °C, 220 °C, and 220 °C, with die zones held between 210 °C and 225 °C. Actual melt temperatures are usually close to the adapter setting but can rise at high screw speeds due to shear heating. Screw speed, back pressure, and motor load on a grooved-feed extruder respond strongly to feed throat temperature and pellet bulk density. If feed throat temperature rises above 45 °C, bridging and irregular feed can occur; water-cooled feed throats are commonly used to maintain stable solids conveying.
The resin can be processed without predrying when pellet surface moisture is below 0.02% by weight. If storage conditions cycle below dew point or relative humidity exceeds 80%, surface condensation may require predrying at 60 °C for 2 h in a desiccant dryer. Drying above 80 °C should be avoided because pellet agglomeration may occur in the hopper.
The usable melt temperature range is bounded at the lower end by high melt viscosity and at the upper end by oxidative gel formation. Below 190 °C melt temperature, the resin may not homogenize adequately in short extruders, producing melt pressure fluctuations and visible gauge bands. Above 235 °C and at residence times exceeding 5 min, oxidized gel defects can form and appear as translucent or discolored particle inclusions in the film. The critical time depends on oxygen ingress at the feed throat and screw design; vacuum venting is not required for standard blown film processing but can reduce volatiles when recycling edge trim.
Bubble stability depends on die gap, blow-up ratio, and internal bubble cooling. Stable operation is usually reported at blow-up ratios between 2.0:1 and 3.0:1, with a frost line height set between 600 mm and 1,000 mm on conventional air-ring lines. Frost line movement of more than ±20 mm can alter machine-direction/transverse-direction tear balance and optical uniformity; closed-loop frost line control is preferred for continuous heavy-gauge production. Narrow die gaps below 1.0 mm may increase melt shear and reduce dart impact, while die gaps above 2.5 mm may reduce haul-off stability and require longer cooling lengths.
Regulatory status is application-specific and cannot be assumed from the resin design alone. In the United States, olefin polymers may be regulated under FDA 21 CFR 177.1520, which covers olefin polymers used in contact with food and specifies extractable fractions in n-hexane or xylene depending on end-use temperature. In the European Union, Regulation (EU) No 10/2011 as amended requires overall migration testing under EN 1186-1 and specific migration testing for additives. Sclair® 11L2B may be used in food packaging when the formulated film meets the applicable conditions, but the converter must obtain current lot-specific documentation from NOVA Chemicals. The resin is not intended for medical implant use; no ISO 10993 biocompatibility statement should be inferred from food-contact status.
| Regulatory area | Applicable designation | Film-specific note |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520 | olefin polymer; extraction limits depend on end use |
| EU food contact | Regulation (EU) No 10/2011 | overall migration and specific migration limits apply |
| REACH | Regulation (EC) No 1907/2006 | polymer is exempt from registration as a substance, but monomers and additives require registration |
| RoHS heavy metals | Directive 2011/65/EU | typically below restriction thresholds; not the primary compliance driver for polyolefin film |
Optical haze in Sclair® 11L2B is influenced by crystalline morphology, surface roughness from antiblock, and film gauge. Heavy-duty film formulations generally exhibit haze values above 8% at 25 µm under ASTM D1003-13; this is a consequence of light scattering at spherulitic boundaries and at antiblock-induced surface asperities. The grade is therefore less suited to high-clarity display packaging than metallocene-catalyzed LLDPE or LDPE blends, where haze below 5% is often required. Seal initiation temperature is controlled mainly by density and short-chain branching; at 0.918 g/cm³, Sclair® 11L2B seals below the initiation temperature of higher-density LLDPE and has a broad hot-tack range under ASTM F1921-12. Seal strength measured by ASTM F88/F88M-21 is sensitive to slip additive migration to the seal interface; high slip concentrations can reduce hot-tack strength even when cold seal strength remains acceptable.
Observed use patterns include heavy-duty shipping sacks, agricultural silage cover, collation shrink film, and liners for dry bulk packaging. In heavy-duty sacks, the resin is often blended with LDPE at 10–20% by weight to improve melt strength and bubble stability on low-pressure air rings. In agricultural silage film, ultraviolet stabilizers are introduced by masterbatch; compatibility with hindered amine light stabilizers should be confirmed because acidic species from oxidized process residues can deactivate certain amine stabilizers and shift color during long outdoor exposure. In stretch-wrap, the octene comonomer contributes high ultimate elongation but requires a tackifier package designed for LLDPE migration kinetics to avoid blocking on the roll after storage at elevated temperature. These applications exploit the grade’s tear resistance and drawability rather than optical clarity or high-temperature dimensional stability.