| HS Code | 590411 |
| Productname | NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene |
| Density | 0.920 g/cm³ |
| Meltindex | 0.75 g/10 min |
| Meltingpoint | 123 °C |
| Vicatsofteningpoint | 98 °C |
| Tensilestrengthatyield | 10 MPa |
| Tensilestrengthatbreak | 32 MPa |
| Elongationatbreak | 700 % |
| Dartdropimpact | 200 g |
| Elmendorftearmd | 250 g |
| Elmendorfteartd | 400 g |
| Haze | 10 % |
| Gloss45 | 60 % |
As an accredited NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene-lined bags, palletized at 1,000 kg per pallet; also available in bulk trucks or railcars. |
| Container Loading (20′ FCL) | Loaded in 20′ FCL, NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin in 25 kg bags, palletized, strapped, and moisture-protected. |
| Shipping | NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin is generally shipped as a non-hazardous solid resin in 25-kg moisture-resistant bags, semi-bulk totes, or bulk trucks/railcars. Keep dry, clean, ambient, and away from excessive heat or contamination. Follow applicable transport regulations and supplier packaging instructions. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture, dust, and contamination. Store at ambient temperature in original packaging. Avoid prolonged UV exposure. Use first-in, first-out inventory. Maintain clean handling equipment. Protect from physical damage and moisture ingress. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is typically two years from date of manufacture when stored unopened in dry, cool conditions away from sunlight. |
In heavy-duty industrial sack and liner film extrusion, Sclair® 11L1 is processed as the primary pellet feedstock rather than as a fully compounded film concentrate. On a 70 mm to 90 mm grooved-feed blown-film extruder fitted with a barrier screw and Maddock mixer, the grade is combined with high-pressure LDPE at 10 wt% to 25 wt% and carbon black masterbatch at 4 wt% to 6 wt%; Sclair® 11L1 itself occupies 70 wt% to 85 wt% of the total monolayer blend. The nominal density of 0.918 g/cm³ (ASTM D1505) and nominal melt flow rate of 1.0 g/10 min (ASTM D1238, 190 °C/2.16 kg) place the resin within the medium-shear-viscosity window for thick-gauge film extrusion. Melt temperature is maintained at 190 °C to 220 °C, die gap is set at 1.8 mm to 2.2 mm, and blow-up ratio is held at 2.0:1 to 2.8:1; dual-lip air rings and internal bubble cooling support outputs approaching 180 kg/h on a 400 mm annular die without loss of bubble stability. Film thicknesses from 80 µm to 250 µm are surface-treated to 38 dyn/cm to 42 dyn/cm where flexographic printing is specified. Mechanical compliance is anchored to ASTM D1709-16A for dart impact at a minimum of 700 g on 100 µm film, ASTM D882-18 for tensile properties, ASTM D1922-15 for Elmendorf tear, and ISO 527-3:2018 for tensile determination at 23 °C and 50% relative humidity. Regulatory compliance for EU shipment is established under REACH (EC) No 1907/2006; packaging heavy-metal limits follow the CONEG model legislation at 100 ppm total for lead, cadmium, mercury, and chromium(VI). Terminal products are open-mouth heavy-duty sacks, valve sacks for mineral fillers and resins, layflat tubular carton liners, and 150 µm to 250 µm industrial debris sacks.
On production lines with collapse frames longer than 2.2 m, machine-direction-to-transverse-direction tear imbalance becomes measurable when the blow-up ratio exceeds 2.8:1; Elmendorf tear values under ASTM D1922-15 can shift by up to 35% between the two directions. Converters running valve sacks frequently reduce carbon black loading to 2 wt% and add a polymer processing aid at 0.05 wt% to 0.10 wt% to suppress melt fracture at high screw speeds. The resin is not predried in closed indoor storage; if pellets are exposed to relative humidity above 70% or transported in cold rail cars, a 60 °C to 70 °C hopper drying cycle of 2 h is applied before extrusion. Incorporation of post-industrial recyclate above 20 wt% in heavy-duty sack film lowers dart impact and tensile strength under ASTM D1709-16A and ASTM D882-18; each recyclate lot should be qualified on a 500 mm blown-film pilot line before production use.
Cast pallet wrap lines feed Sclair® 11L1 as the core-layer pellet phase at 65 wt% to 80 wt% of the core formulation; the skin layers contain metallocene-catalyzed LLDPE and polyisobutylene-based tackifier masterbatch at 2 wt% to 4 wt% of the total formulation. The cast line is operated with a 0.4 mm to 0.7 mm die gap, an air gap of 100 mm to 160 mm, chill-roll temperatures of 15 °C to 25 °C, and line speeds from 250 m/min to 600 m/min. Neck-in increases from approximately 10 mm to 35 mm per side as the air gap is widened across that range; edge bead is removed in-line and the web is slit to 350 mm to 750 mm roll widths. Pre-stretch ratios of 150% to 250% are applied between the cast unit and the winder; finished film gauge ranges from 20 µm to 50 µm. Cling performance is measured under ASTM D5458-95 after 24 h and 7 days at 23 °C and 50% relative humidity; tackifier migration can lower cling force below the required unwind release when masterbatch loading exceeds 4 wt%. Mechanical testing includes ASTM D882-18 for tensile properties, ASTM D5748-95 for protrusion puncture resistance, and ISO 527-3:2018 for elongation. Regulatory compliance for EU shipment is established under REACH (EC) No 1907/2006; food-contact status is not claimed unless separately tested under FDA 21 CFR 177.1520. Terminal product types are hand pallet wrap, machine stretch film, and pre-stretched film on extended-core rolls; hand grades are typically 23 µm to 30 µm, and machine grades 35 µm to 50 µm.
The medium melt flow rate of 1.0 g/10 min (ASTM D1238) constrains melt throughput on high-speed cast lines relative to 2.0 g/10 min to 3.0 g/10 min cast grades; a die pressure rise above 120 bar on a 350 mm cast die indicates that screw speed has exceeded the available torque envelope. Published rheological data for octene LLDPE film resin at line speeds above 500 m/min is limited; converters should pilot the grade on a 500 mm cast line with a 30:1 L/D extruder before commercial qualification. Talc-based antiblock should not be added above 5 wt% in the core because haze increases and puncture resistance under ASTM D5748-95 deteriorates below thin-gauge performance requirements.
Blown film for vertical and horizontal form-fill-seal packaging of frozen foods uses Sclair® 11L1 at 70 wt% to 90 wt%, high-pressure LDPE at 10 wt% to 25 wt%, erucamide slip masterbatch at 0.5 wt% to 1.5 wt%, and diatomaceous earth antiblock masterbatch at 0.5 wt% to 2.0 wt%. The octene comonomer branch length depresses crystalline melting and reduces low-temperature embrittlement relative to butene LLDPE at equal density; low-temperature film impact is evaluated under ASTM D1709-16A after conditioning at -25 °C, and tensile behavior is measured under ASTM D882-18 at -25 °C. The blown-film line uses a 1.8 mm to 2.2 mm die gap, blow-up ratio of 2.2:1 to 3.0:1, and frost-line height of 3 to 6 die diameters; film thickness ranges from 40 µm to 75 µm. On form-fill-seal machinery, seal jaws are run at 115 °C to 140 °C, dwell time of 0.4 s to 0.8 s, and jaw pressure of 0.25 N/mm² to 0.50 N/mm²; seal strength is verified under ASTM F88/F88M-21. Food-contact compliance references FDA 21 CFR 177.1520 for the olefin polymer, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and EC 2023/2006 for good manufacturing practice. Terminal products include frozen vegetable pillow packs, frozen seafood pouches, ice cream dessert pouches, and side-gusseted bags for frozen bakery dough.
High-speed vertical form-fill-seal operation at 80 cycles/min exposes the sealant layer to fine frozen particulate; this contamination can reduce seal strength under ASTM F88/F88M-21. The corrective action is to add vacuum extraction at the jaw and reduce slip masterbatch to 0.3 wt% to 0.5 wt% in the sealant layer. Converters must not incorporate post-consumer recyclate into food-contact layers above 20 wt% unless the recyclate is covered by a food-contact suitability opinion, because extractable levels can shift outside EU 10/2011 migration limits. No pre-drying is required under normal indoor storage; after winter rail transit, condensation is removed by a 60 °C/2 h hopper drying cycle.
When Sclair® 11L1 is coextruded as the core layer of agricultural silage cover and greenhouse film, the extrusion line is equipped with a multilayer annular die of 300 mm to 600 mm diameter, a 1.8 mm to 2.4 mm die gap, and a blow-up ratio of 2.2:1 to 3.0:1 to produce layflat widths up to 18 m. The formulation uses Sclair® 11L1 at 75 wt% to 90 wt%, hindered amine light stabilizer masterbatch at 1 wt% to 3 wt%, UV absorber masterbatch at 2 wt% to 4 wt%, and antifog additive masterbatch at 0.5 wt% to 2 wt%; greenhouse grades may add inorganic photoselective pigments at 3 wt% to 6 wt%. Extruder zone temperatures range from 180 °C in the feed zone to 215 °C at the die; sustained operation above 235 °C accelerates HALS consumption and produces melt instability in wide-web film. Silage covers are wound as 25 µm to 200 µm jumbo rolls, then rewound into farm-use formats; greenhouse film is typically manufactured at 100 µm to 200 µm. Compliance references are EN 13207:2018 for thermoplastic silage films and tubes, EN 13206:2017 for greenhouse covering films, ISO 4892-2:2013 for xenon-arc weathering, and ISO 527-3:2018 for tensile property retention. REACH (EC) No 1907/2006 applies to EU shipment. Terminal products include silage covers, silage tubes, greenhouse covers, low tunnel films, and multi-season mulch films.
Blocking resistance in wide agricultural rolls is maintained with talc-based antiblock at 1.0 wt% to 2.0 wt% rather than silica because silica can reduce light transmission in greenhouse applications. Published outdoor durability data for specific photoselective pigment combinations in this exact resin grade is limited; converters should run 12-month weathering trials in the target geographic UV load before qualifying a commercial greenhouse structure.
Laminated flexible packaging for dry foods and powders uses Sclair® 11L1 as the sealant web at 80 wt% to 95 wt%, with slip masterbatch at 0.5 wt% to 1.5 wt% and antiblock masterbatch at 0.5 wt% to 2.0 wt%; converters seeking lower seal initiation temperature add an ethylene vinyl acetate or plastomer concentrate at 5 wt% to 15 wt%, which shifts seal initiation downward by 5 °C to 10 °C. The sealant film is produced at 30 µm to 60 µm by blown or cast extrusion and adhesive-laminated to BOPET, BOPP, or aluminum foil. Heat sealing is run at 120 °C to 145 °C, dwell time of 0.5 s to 1.0 s, and jaw pressure of 0.30 N/mm² to 0.60 N/mm²; seal initiation temperature is determined under ASTM F2029-16, seal strength under ASTM F88/F88M-21, and coefficient of friction under ASTM D1894-14. Dusty product contamination during horizontal filling can reduce seal strength by more than 25% when 0.5 wt% diatomaceous earth antiblock loading is combined with powder carry-over in the seal zone; filler lines must use vacuum extraction and periodic jaw cleaning. Compliance in the USA is established under FDA 21 CFR 177.1395 for laminate structures and FDA 21 CFR 177.1520 for the olefin polymer; EU compliance is established under EU Regulation (EU) No 10/2011 and EC 2023/2006. Terminal products include lidding films for dairy powders, stand-up pouch sealant webs for dried fruits and snacks, single-serve sachet films, and laminated bags for granulated food ingredients.
Operational boundaries are defined by additive migration: when the sealant web is corona-treated to 42 dyn/cm and immediately laminated, erucamide slip can migrate to the polyurethane adhesive interface and reduce bond strength within 24 h; corona treatment is therefore delayed until immediately before lamination or the slip masterbatch is reduced to 0.3 wt% to 0.5 wt%. Published data for seal strength recovery after high-ethylene plastomer blending under contaminated form-fill-seal conditions is limited; each structure should be validated on a pilot line running at 50 cycles/min with the target powder and the specified sealant layer gauge.
Flexible intermediate bulk container liners are produced from Sclair® 11L1 at 85 wt% to 95 wt%, with slip/antiblock masterbatch at 1.0 wt% to 3.0 wt% and an optional polymer processing aid at 0.05 wt% to 0.10 wt% when melt fracture appears on a 90 mm extruder. Film thicknesses range from 120 µm to 300 µm; the production line uses a 350 mm to 600 mm annular die with a 2.0 mm to 2.5 mm die gap and blow-up ratio of 1.8:1 to 2.5:1. Internal bubble cooling and a double-lip external air ring maintain thickness uniformity in thick-gauge webs; the flat tube is gusseted and fitted with spouted fitments, and fitment weld strength is tested under ASTM F88/F88M-21 at 23 °C and after 24 h creep load. Compliance references are ISO 21898:2004 for FIBC performance, ASTM D1709-16A for dart impact, ASTM D882-18 for tensile properties, ASTM D1922-15 for tear, and FDA 21 CFR 177.1520 when the liner contacts food or pharmaceutical powders; REACH (EC) No 1907/2006 applies to EU export. Terminal products are 500 kg to 1,500 kg FIBC liners, conductive liners, drum liners, and IBC inner liners.
Competitive NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
When specifying a linear low density polyethylene film resin, density and melt index are only part of the design envelope; comonomer type and molecular architecture more directly control the balance of toughness, optics, and processability. NOVA Chemicals Sclair® 11L1 is a 1-octene-based linear low density polyethylene designated for cast and blown film extrusion. The published nominal resin values include a density of 0.918 g/cm³ under ASTM D792 and a melt index of 1.0 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg load. These values place the grade in the lower-density segment of conventional LLDPE film, a range where converters expect high elongation at break, high dart impact, and high tear propagation resistance rather than elevated modulus.
Molecularly, the 1-octene comonomer inserts hexyl side branches along the ethylene backbone, compared with ethyl branches for 1-butene and butyl branches for 1-hexene. During blown film crystallization, longer comonomer branches disfavor close chain packing and increase the probability of tie-chain formation between adjacent lamellae. This morphological difference is not uniform through the film thickness; quench rate, orientation, and frost-line height all modify crystallite orientation. Because of this, the resin is routinely characterized by ASTM D1709 for dart drop impact, ASTM D1922 for Elmendorf tear, and ASTM D882 for tensile yield and break properties. Reported film values are commonly generated on 25 µm to 50 µm monolayer blown film produced on single-screw extruders with spiral mandrel dies and dual-lip air rings.
| Resin parameter | Published nominal value | Test method |
|---|---|---|
| Density | 0.918 g/cm³ | ASTM D792 |
| Melt index | 1.0 g/10 min | ASTM D1238, 190 °C, 2.16 kg |
| Base comonomer | 1-octene | supplier specification |
| Qualification film thickness | 25 µm to 50 µm | ASTM D6988 |
Processability of Sclair® 11L1 is bounded by its linear architecture and the shear-viscosity behavior common to conventional LLDPE. On blown film lines using a barrier screw with an L/D of 24:1 to 30:1, melt temperature set points are often maintained from 190 °C to 230 °C. The lower portion of this range is preferred on high-stalk bubble configurations because it reduces film oxidation and increases bubble stability; the upper portion is used on cast film dies or high-output lines where head pressure must be reduced. Because the melt is less shear-thinning than LDPE, screw torque and screen-changer pressure can rise quickly as throughput increases. Die gaps of 1.5 mm to 2.5 mm, blow-up ratios of 2.0:1 to 3.0:1, and dual-lip air rings are typical starting points for blown film conversion. Published data for this exact resin across all screw geometries is limited, so processors should establish the specific melt pressure versus screw speed curve for their equipment.
In cast film extrusion, the resin is processed on conventional slot dies with chilled roll temperatures generally maintained between 18 °C and 25 °C. Draw resonance can occur when draw ratio is increased beyond the cooling capacity of the air gap, but the precise onset depends on die gap, melt temperature, and line speed. Because this product is not a high-melt-strength autoclave LDPE, cast lines with short air gaps may require higher output or warmer melt conditions to prevent web flutter. The use of a vacuum box and electrostatic pinning equipment is standard for thin-gauge cast film production from linear polymers.
Moisture-related defects are uncommon in ethylene-octene film resin. Pre-drying is not routinely required unless the resin has been stored at relative humidity above 60% or moved from outdoor to indoor conditions with surface condensation. If pre-drying is necessary, dehumidified-air temperature of 80 °C for 2 h to 4 h is sufficient; higher inlet air temperatures can cause granule surface tack and feed-throat bridging. The additive package for slip and antiblock is designed to reach a steady coefficient of friction after migration of the slip component to the film surface. Converters typically measure the coefficient of friction with ASTM D1894 after conditioning specimens at 23 °C and 50% relative humidity for at least 24 h. Values outside the target range are more commonly caused by inadequate aging time, gauge variation, or masterbatch carrier incompatibility than by base resin deviation.
Substitution in multilayer sealant webs is not always a direct percentage change. In a three-layer blown line where the sealant layer formerly contained a butene LLDPE, switching to Sclair® 11L1 alters the melt viscosity in that layer and may shift the layer distribution because the two resins do not have identical shear-thinning characteristics. The octene grade also changes seal strength and hot-tack behavior in heat-seal applications; those effects should be measured under ASTM F88 for seal strength and ASTM F1921 for hot-tack where available. Seal initiation typically lies between 90 °C and 130 °C depending on layer thickness and thermal history, but the supplier’s product data sheet should be used as the controlling document. In film structures requiring high dart impact at 25 µm to 75 µm total gauge, the octene sealant often improves toughness without reducing the heat-seal plateau as much as adding plastomer would.
End-use applications for Sclair® 11L1 include heavy-duty shipping sacks, ice bags, frozen food packaging, carrier bags, and high-performance stretch-hood films. In heavy-duty sacks, the film must resist dart impact under ASTM D1709 and tear propagation under ASTM D1922, while maintaining a low enough coefficient of friction for automatic bag opening and filling. In stretch-hood films, the balance between tensile yield and puncture resistance under ASTM D5748 determines pallet load retention. The resin can also be blended with low-density polyethylene to improve melt strength and bubble stability; converter trials often evaluate LDPE addition levels of 10 wt% to 30 wt%, but published data for the exact blend response with this specific grade is limited.
Relative to metallocene-catalyzed ethylene-octene LLDPE grades, Sclair® 11L1 is not typically characterized by the same narrow composition distribution. Single-site grades often provide lower haze and lower seal initiation temperature, but they may require higher motor torque or exhibit less bubble stability on older extrusion lines. The broader molecular weight distribution of conventional solution-process LLDPE improves extruder throughput and can widen the processing window on high-output lines, while slightly reducing ultimate optics. This trade-off is evaluated with ASTM D1003 for haze and ASTM D2457 for gloss; the specific optical values depend on gauge and extrusion output.
| Performance dimension | Standard test method | Equipment or condition |
|---|---|---|
| Melt index | ASTM D1238 | dead-weight plastometer, 190 °C, 2.16 kg |
| Density | ASTM D792 | density column or pycnometer |
| Film tensile yield and break | ASTM D882 | constant-rate-of-extension tensile tester, 500 mm/min |
| Dart drop impact | ASTM D1709 | staircase dart drop apparatus |
| Elmendorf tear | ASTM D1922 | pendulum tear tester |
| Haze | ASTM D1003 | haze meter, CIE C light source |
| Specular gloss | ASTM D2457 | 45° or 60° gloss meter |
| Coefficient of friction | ASTM D1894 | sled test against stainless steel |
| Seal strength | ASTM F88 | heat-sealed tensile specimens |
| Hot tack | ASTM F1921 | hot-tack tester with controlled seal force |
| Puncture resistance | ASTM D5748 | probe puncture at 250 mm/min |
Regulatory compliance for food-contact films produced from this resin is end-use-specific. In the United States, the base ethylene-1-octene polymer may be assessed under 21 CFR 177.1520(c), but the final film must be evaluated against extraction conditions that reflect the intended food type and temperature. In the European Union, compliance with EU No 10/2011 requires verification of overall migration against the 10 mg/dm² limit and, where applicable, specific migration limits for additives; these are not intrinsic resin properties but are fixed by the full film formulation. The supplier’s certificate of compliance should be requested for the actual delivery lot, particularly if the film is destined for fatty, aqueous, alcoholic, or hot-fill food applications.
Neither the base resin nor its additive package should be combined with incompatible masterbatches without checking the carrier resin. The most common line-side troubleshooting issues with this class of octene LLDPE are bubble instability and die-lip build-up rather than insufficient mechanical properties. If build-up appears, infrared thermography of the die lip and gravimetric measurement of accumulated wax can separate low-volatile slip additive plate-out from degraded polymer gel. Screen packs of 60/80/120 mesh are often used to protect the die; if head pressure rises beyond the extruder’s rated limit, the cause is frequently undersized screen area rather than resin viscosity. Published data for this specific product in high-output cast film lines with chilled-roll temperatures below 20 °C is limited.