| HS Code | 235385 |
| Resintype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene |
| Density | 0.919 g/cm³ |
| Meltindex | 0.8 g/10 min |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 29.6 MPa |
| Elongationatbreak | 750 % |
| Dartdropimpact | 120 g |
| Elmendorftearmd | 250 g |
| Elmendorfteartd | 400 g |
| Haze | 11 % |
| Gloss45 | 55 % |
| Coefficientoffriction | 0.20 |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 100 °C |
As an accredited NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin is supplied in 25 kg bags, palletized for handling. |
| Container Loading (20′ FCL) | NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin: 20′ FCL: 25 kg bags, 55 bags/pallet, 20 pallets, 27.5 MT net. |
| Shipping | NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin is shipped as non-hazardous solid pellets in 25 kg bags, 500–1000 kg octabins, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from direct sunlight and ignition sources; handle carefully to prevent package damage. Resin should remain sealed until use. |
| Storage | Store Sclair® 11F2 Butene LLDPE Film Resin in a cool, dry, well-ventilated area out of direct sunlight. Keep original bags or boxes closed and palletized off the floor to prevent moisture pickup and contamination. Avoid heat, flames, and strong oxidizers. Maintain good housekeeping; follow supplier SDS and local regulations. Use first-in, first-out stock rotation. |
| Shelf Life | Typically two years from manufacture when stored unopened in a cool, dry, well-ventilated area, away from sunlight, heat, and contaminants. |
Blown film conversion of NOVA Chemicals Sclair® 11F2 begins with the nominal resin parameters that define the processing envelope. Melt flow rate is typically 1.0 g/10 min when measured at 190°C under 2.16 kg load according to ASTM D1238 / ISO 1133-1, and solid-state density is typically 0.920 g/cm³ according to ASTM D1505 or ASTM D792. These two values locate the grade in the linear low-density polyethylene range where short-chain branching from butene comonomer disrupts crystallinity and lowers flexural modulus while retaining ductile tear behaviour. On single-screw blown film lines with barrier screws of L/D 24:1 to 30:1, a barrel profile from 170°C at the feed throat to 230°C in the metering zone, with die set points of 215°C to 240°C, is ordinarily sufficient. The die gap should be held between 1.6 mm and 2.5 mm for film thicknesses from 25 µm to 150 µm; narrower gaps can increase shear stress at the die lip and trigger sharkskin melt fracture, while wider gaps may reduce shear-induced homogenization and lower optical clarity. Pellets do not require desiccant drying under normal closed-warehouse conditions below 80% RH, but surface condensation from outdoor silo storage must be removed by hopper-air sweeping at 50°C to 60°C for a minimum of 30 min before extrusion. Output-rate increases on lines without internal bubble cooling are typically limited not by motor load but by bubble instability and frost-line height oscillation; the frost-line should be maintained at 1.5 to 2.5 die diameters above the air ring for gauges above 50 µm. Because butene LLDPE has lower melt strength than hexene- or octene-based grades, the addition of 10 wt% to 30 wt% high-pressure LDPE is frequently used to stabilise the bubble and raise elongation viscosity. Fluoroelastomer processing aids must be pre-dispersed as masterbatch at let-down ratios not exceeding 1:20; otherwise die-lip build-up can transfer to film surfaces as visible specks. These operating boundaries form the basis for the downstream usage scenarios described below.
| Property | Method | Key conditions | Reported unit |
|---|---|---|---|
| Melt flow rate | ASTM D1238 / ISO 1133-1 | 190°C, 2.16 kg | g/10 min |
| Solid-state density | ASTM D1505 / ASTM D792 | 23°C | g/cm³ |
| Tensile properties | ASTM D882 / ISO 527-3 | 500 mm/min | MPa |
| Elmendorf tear | ASTM D1922 / ISO 6383-2 | Pendulum tear, conditioned at 23°C | gf or N |
| Dart drop impact | ASTM D1709 / ISO 7765-1 | Phenolic dart head, clamped specimen | g |
| Puncture resistance | ASTM D5748 | Test speed per method | N |
| Haze | ASTM D1003 / ISO 14782 | Integrating sphere | % |
| Coefficient of friction | ASTM D1894 / ISO 8295 | Metal sled, conditioned film | dimensionless |
| Oxygen transmission rate | ASTM D3985 / ISO 15105-2 | 23°C, 0% RH | cm³/(m²·d·atm) |
| Water vapour transmission rate | ASTM F1249 / ISO 15106-2 | 38°C, 90% RH | g/(m²·d) |
Industrial sacks for free-flowing construction powders, resins, and minerals are typically converted at final thicknesses between 80 µm and 150 µm. The main process conflict occurs when the line is pushed above 180 kg/h on a 90 mm grooved-feed extruder, because the low melt strength of butene LLDPE makes the bubble susceptible to helical instability at blow-up ratios above 2.8:1. In this regime, the die gap is held at 2.0 mm to 2.5 mm and the BUR is reduced to 2.2:1 to 2.6:1 while frost-line height is increased to 2.0 to 2.5 die diameters to stabilise the melt web. Sack toughness is assessed by ASTM D1709 dart drop and ASTM D1922 Elmendorf tear; butene-based films at 100 µm typically exhibit lower puncture energy than comparable octene LLDPE films, so converters blend Sclair® 11F2 with 15 wt% to 25 wt% LDPE and sometimes 5 wt% to 10 wt% HDPE to raise modulus and creep resistance. Surface slip is controlled with erucamide masterbatch added at 0.5 wt% to 1.0 wt%, but blocking force should be verified after 48 h at 50°C using ASTM D3354 because excessive slip migration can weaken subsequent lamination bonds. Sealing on bottom-seal sack lines requires jaw temperatures of 150°C to 175°C and dwell times of 0.5 s to 1.0 s at 0.3 MPa seal pressure; seal initiation temperature should be confirmed per ASTM F1921. For export packaging, compliance with REACH Annex XVII and CONEG model legislation is maintained by ensuring the sum of lead, cadmium, mercury, and hexavalent chromium does not exceed 100 ppm in the finished film, measured by EPA 3052 digestion and ICP-OES. Die-lip build-up from low-quality recycled trim can be managed by adding a fluoropolymer processing-aid masterbatch at 0.5 wt% to 1.0 wt% rather than by raising die temperature, which may increase odour and gel formation.
Agricultural silage and bunker cover films are produced in thicknesses from 100 µm to 200 µm, with width often exceeding 8 m on high-stalk blown film lines. The critical processing limitation is maintenance of a uniform frost line across the die circumference; deviations larger than ±5% of average lay-flat width produce thick bands that fail oxygen-barrier verification under ASTM D3985 at 23°C and 0% RH. Published grade-specific oxygen transmission data for Sclair® 11F2 at 150 µm is limited, so converters are required to qualify each film structure against the target OTR established for fermenting silage rather than relying on nominal resin permeability values. Typical stabiliser packages for temperate and subtropical exposure combine hindered amine light stabiliser at 0.3 wt% to 0.8 wt% concentrate with a UV absorber at 0.2 wt% to 0.5 wt%; both must be pre-compounded into LDPE or LLDPE carrier resin, not dry-blended into the hopper, to avoid concentration gradients that reduce service life. Blown film lines for this application are often operated at BUR values of 2.0:1 to 3.0:1, but high-stalk bubbles above 2.5 die diameters are avoided because butene LLDPE tends to sag and form gauge bands. Puncture resistance is measured by ASTM D5748; film intended for maize silage should be evaluated at final gauge on the production line because cooling-air temperature and film orientation dominate this property. Repair tape adhesion after surface oxidation requires corona discharge at 38 mN/m to 42 mN/m dyne level, checked by ASTM D2578, because untreated butene LLDPE surfaces can fall below 32 mN/m within 72 h of extrusion.
Monolayer and coextruded frozen-food packaging in the 25 µm to 50 µm gauge band depends on low-temperature impact resistance and seal integrity after contact with moisture and fat. The film is processed at a die temperature of 210°C to 230°C with a BUR of 2.5:1 to 3.0:1 to balance transverse-direction tear. Low-temperature ductility is characterised by ASTM D1709 at -18°C after conditioning samples for 48 h; if the dart-drop value falls below 80 g at 25 µm, converters typically increase gauge to 35 µm or blend 10 wt% to 20 wt% of an octene LLDPE or plastomer, because butene comonomer distribution in Sclair® 11F2 provides less effective tie-chain density than higher α-olefin grades for sub-freezing puncture events. Heat-seal performance must satisfy ASTM F88/F88M-21 seal-strength testing with a minimum seal bar temperature of 120°C and 0.3 s dwell at 0.3 MPa; the actual seal initiation temperature should be generated on the line rather than inferred from resin crystallinity. For direct food contact, compliance is assessed under FDA 21 CFR 177.1520 and EU Regulation 10/2011 with overall migration below 10 mg/dm² using simulant D1 or D2 as applicable to frozen fatty food types. Additives used in this layer must not include phthalate-based plasticisers or primary aromatic amines; slip and antiblock loadings above 1.5 wt% total can create visible haze and reduce print adhesion on surface-printed lidding film. The use of reclaimed post-industrial trim in food-contact layers is permitted only if the re-feed fraction is kept below 20 wt% and the trim is generated from the same food-compliant structure without external contamination, in accordance with the site’s hazard analysis under 21 CFR 117.
| Regulation / Standard | Scope | Verification parameter |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers in direct food contact | Extraction tests, end-use conditions A–H, extractable limits per subpart B |
| EU Regulation 10/2011 | Plastic food-contact materials | Overall migration 10 mg/dm²; SML values for authorised additives |
| REACH 1907/2006 | SVHC communication, Annex XVII restrictions | Article 33 compliance; restricted phthalates below 0.1 wt% |
| CONEG model legislation | Heavy metals in packaging | Sum of Pb, Cd, Hg, Cr(VI) 100 ppm |
| RoHS Directive 2011/65/EU | Electrical/electronic packaging components if applicable | Homogeneous material limits for Pb, Hg, Cd, Cr(VI), PBB, PBDE |
Coextrusion of Sclair® 11F2 as the sealant layer in three-layer or five-layer barrier structures introduces viscosity-matching constraints that are not present in monolayer extrusion. The melt index of 1.0 g/10 min at 190°C/2.16 kg is lower than many LDPE sealant grades, so the adjacent tie layer and polyolefin skin layers should be selected within ±0.5 g/10 min of the Sclair® 11F2 value to avoid interfacial flow instabilities at layer ratios from 10% to 20% of total structure thickness. A five-layer line with L/D 30:1 extruders and flat dies of 750 mm to 1,500 mm width may run the sealant layer at 200°C to 220°C; raising the sealant melt temperature above 240°C to reduce viscosity is not recommended for structures containing EVOH, because residence-time decomposition of EVOH can generate gels and odour. Sealant thickness is typically held at 5 µm to 15 µm in a total film of 60 µm to 120 µm, and the final laminate must pass a 1.5 kg to 2.5 kg / 25 mm heat-seal strength threshold per ASTM F88/F88M-21. Peelable behaviour is not a native attribute of butene LLDPE; easy-open seals require blending with polybutene or ionomer at 10 wt% to 30 wt%, which alters the seal plateau and must be re-qualified for food contact. Optical haze in the sealant layer after coextrusion is measured by ASTM D1003 and should remain below 15% for clear barrier pouches; haze increases non-linearly when the layer thickness exceeds 12 µm or when melt-temperature deviation across the die exceeds ±3°C. The use of Sclair® 11F2 in retortable structures is not typical because butene LLDPE lacks the high-temperature seal integrity required after 121°C retort exposure.
Blown stretch-hood film for pallet load stabilisation is a lower-volume but technically demanding application for butene LLDPE because the resin must combine elastic recovery with puncture resistance during manual or automatic hood deployment. In blown-film gauge bands of 50 µm to 80 µm, Sclair® 11F2 can be processed at a BUR of 3.0:1 to 4.0:1 to increase transverse-direction extensibility, but the bubble becomes more sensitive to collapsing-frame chatter at these higher blow-up ratios. Stretch force and ultimate elongation should be measured by ASTM D5458 or the specific end-user’s stretch-hood protocol; published data for Sclair® 11F2 in this specific configuration is limited, so line qualification on the target palletizer is required before export shipment. Cling is normally generated by incorporation of polyisobutylene or ultra-low-density ethylene copolymer at 3 wt% to 8 wt%, but excess cling additive above 10 wt% can foul collapsing frames and create roll-blocking during ocean freight in containers above 40°C. Blocking resistance after accelerated ageing is assessed by ASTM D3354; rolls should be wrapped with a low-slip core and stored at 30°C or below. Retention-force loss over 24 h must be measured per ASTM D5458 rather than assumed, because butene LLDPE does not share the elastic recovery of metallocene-catalyzed octene grades. If the converter observes cling transfer to film surfaces after 7 days, the additive masterbatch carrier resin should be changed to a low-melting EVA or ULDPE rather than increasing dilution, which reduces cling uniformity.
Standard refuse sacks and light-duty can liners in the 25 µm to 40 µm range are converted from Sclair® 11F2 on conventional monolayer lines at a BUR of 2.0:1 to 3.0:1 without special additive packages beyond normal slip/antiblock, and the converter’s primary control points are melt temperature and frost-line stability rather than complex formulation design.
Competitive NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Sclair® 11F2 is a butene comonomer linear low-density polyethylene film resin supplied for cast film and blown film conversion. The resin is produced through a Ziegler-Natta polymerization route and is characterized by a solid-state density of 0.919 g/cm³ when measured by ASTM D792/ISO 1183-1 and a melt flow index of 1.0 g/10 min at 190 °C/2.16 kg when measured by ASTM D1238/ISO 1133-1. The 1.0 g/10 min melt flow rate places the grade in the medium-molecular-weight LLDPE range used for film structures requiring a measurable balance of melt strength, drawdown, and impact toughness. The butene comonomer generates short-chain branches that reduce crystallinity relative to high-pressure LDPE and alter the lamellar morphology, which influences tear, dart impact, and heat-seal response. The resin is normally supplied as pellets with antioxidant stabilization; any slip or antiblock additive package must be verified from the supplier’s certificate of analysis because additive type and concentration directly affect film coefficient of friction and seal performance.
| Property | Test method | Typical value |
|---|---|---|
| Solid density | ASTM D792 / ISO 1183-1 | 0.919 g/cm³ |
| Melt flow rate | ASTM D1238 / ISO 1133-1 at 190 °C/2.16 kg | 1.0 g/10 min |
The values in Table 1 are not release limits. They are supplier-published typical values obtained under laboratory conditions. Batch-to-batch variation may occur within the manufacturer’s specification band, and incoming resin should be evaluated for melt flow rate and density before large-scale trials. Published data for additional film properties generated at specific gauges and process settings is limited; direct qualification on the target converting line is required.
Processing of Sclair 11F2 is not defined by a single setpoint; the operating window is constrained by melt temperature, shear history, and cooling rate. Because the resin has a relatively low melt flow index of 1.0 g/10 min, the apparent viscosity at the die is higher than that of a 2.0 g/10 min butene LLDPE. This raises melt pressure and motor load at the same screw speed, and the extruder may become torque-limited before the intended output is reached. Melt flow ratio, sometimes calculated as the ratio of melt index at 10 kg to melt index at 2.16 kg, is used as an approximate measure of polydispersity. For a Ziegler-Natta butene LLDPE, the melt flow ratio is generally higher than that of a metallocene LLDPE, indicating broader molecular weight distribution and stronger shear thinning; the specific value for Sclair 11F2 should be taken from the current datasheet.
Processability of Sclair 11F2 is governed by the balance between melt residence time and shear heating. In a single-screw extruder with L/D between 24:1 and 30:1, the recommended screw uses a barrier section and a dispersive mixing element to prevent unmelted granules from reaching the die. Barrel profiles for blown film commonly begin at 150–170 °C in the feed zone and increase to 190–220 °C in the metering zone. Cast film lines may use slightly higher melt temperatures but should not exceed 250 °C, above which oxidative degradation of the polyethylene backbone can generate gel particles and die-lip deposit. Melt temperature at the adapter is a better control parameter than barrel temperature. Adapter and die pressure should be recorded because pressure instability is an early indicator of melt fracture, degraded material accumulation, or a progressively clogging screen pack. Screen packs of 20/40/80 mesh are often used to trap gels, but finer screens increase pressure drop and may reduce output. The use of a melt pump can reduce extruder pulsation and improve gauge uniformity, but adds shear history and requires closer temperature monitoring.
The resin does not require pre-drying for absorbed water because LLDPE is non-hygroscopic. However, cold pellets exposed to humid air can collect surface condensation. If pellets are moved from an outdoor storage area into a warm plant at RH > 60%, surface moisture can cause splay and bubble pinholes. In such conditions, use of a dry-air hopper purge is recommended. The resin should not be processed at melt temperatures above 250 °C without inert gas blanketing, because oxidative gel formation and yellowing become increasingly probable at extended residence times.
In blown film, the die gap, blow-up ratio, and frost line height determine the balance between machine-direction and transverse-direction orientation. Because Sclair 11F2 is a butene LLDPE with a melt flow index of 1.0 g/10 min, bubble pressure and motor torque are typically higher than in a 2.0 g/10 min grade. A die gap between 0.8 and 1.2 mm is a common starting point for 25–75 µm films. Narrower gaps raise shear rate and die pressure, reducing melt residence time but potentially increasing die-lip deposit. Frost line height should be set by observing bubble stability and film haze; a short frost line increases output but raises quench stress and can reduce tear resistance in the transverse direction. A blow-up ratio between 2.0:1 and 3.5:1 is typical for general-purpose LLDPE film; values outside this range may distort thickness uniformity and cause bubble instability. Published data for the precise frost-line response of this specific grade is limited, so start-up trials should bracket frost-line settings in 50 mm increments.
In cast film conversion, Sclair 11F2 is processed through a flat die onto a polished chill roll. The melt temperature at the die lip is typically higher than in blown film because the draw-down step requires low melt tension. The chill roll surface temperature is maintained between 15 and 35 °C depending on film gauge and line speed; lower temperatures increase film gloss and reduce blocking, but may cause condensation if the dew point in the plant exceeds the roll surface temperature. Air-knife or vacuum box settings are adjusted to minimize edge neck-in and motor striping, which are common failure modes on high-output cast lines. Gauge uniformity is controlled with an automatic die bolt system; manual dies are generally inadequate for films thinner than 30 µm because thickness variation in the web translates directly into variation in ASTM D882 tensile energy to break.
Film performance is not defined by resin density alone. The relevant properties are measured on finished film after conditioning at 23 °C and 50% RH for at least 40 h unless the test standard specifies otherwise. Tensile properties are measured by ASTM D882/ISO 527-3; the test reports tensile strength at break, yield strength, elongation at break, and secant modulus. For blown film, orientation in the transverse direction is usually lower than in the machine direction, so tear and tensile values are anisotropic. Elmendorf tear is measured by ASTM D1922/ISO 6383-2, and for a butene LLDPE the machine-direction tear is typically lower than transverse-direction tear at a given gauge. Dart impact is measured by ASTM D1709/ISO 7765-1 and is expressed as the impact weight that ruptures 50% of test specimens. Because dart impact is highly sensitive to gauge, frost line, and comonomer type, it should not be compared across films unless both gauge and processing conditions are stated.
| Film property | Test standard | Primary process variable affecting result |
|---|---|---|
| Dart impact | ASTM D1709 / ISO 7765-1 | Gauge, frost line height, comonomer type |
| Elmendorf tear | ASTM D1922 / ISO 6383-2 | Orientation, film thickness, blow-up ratio |
| Tensile properties | ASTM D882 / ISO 527-3 | Gauge, draw ratio, cooling rate |
| Haze | ASTM D1003 | Frost line height, die gap, cooling rate |
| Seal strength | ASTM F88 / ASTM F1921 | Seal temperature, dwell pressure, dwell time |
| Coefficient of friction | ASTM D1894 | Slip additive migration, aging time, surface roughness |
Optical properties are measured by ASTM D1003 for haze and ASTM D2457 for gloss; coefficient of friction is measured by ASTM D1894. For LLDPE films containing slip and antiblock additives, the measured coefficient of friction is time-dependent because slip additives migrate to the surface over 24–72 h after extrusion. Seal initiation temperature is measured using ASTM F88 or ASTM F1921. Sealed specimens are produced with a laboratory heat sealer at controlled pressure and dwell time; for general-purpose LLDPE, seal initiation typically falls between 80 °C and 110 °C. The exact value for Sclair 11F2 depends on film thickness, additive composition, and seal-pressure settings.
The resin is selected for liner films, industrial packaging, can liners, and coextruded seal layers where the butene LLDPE toughness envelope is adequate. It is not the first choice for applications requiring maximum low-temperature dart impact or high tear resistance at heavy gauge, because hexene and octene copolymers at the same density and melt index provide higher tie-chain concentration. The material may be blended with metallocene LLDPE or LDPE to modify bubble stability, heat-seal performance, or film modulus; the blend ratio is a converting-line decision and should be validated by the film property test methods in Table 2.
Substitution of Sclair 11F2 for a hexene or octene LLDPE is not a drop-in exchange in all lines. The butene comonomer provides a short-chain branch length of 2 carbon atoms, whereas hexene provides 4 and octene provides 6. At a fixed density of 0.919 g/cm³, the branch content required to reach that density is not identical across comonomer types. A butene LLDPE generally requires a higher molar fraction of short-chain branches than an octene LLDPE to produce the same decrease in crystal density because the 2-carbon butene branch is shorter and less efficient at disrupting the crystal lattice. The higher branch count in butene LLDPE may increase surface segment mobility and lower the seal initiation temperature, but it does not produce the same tie-chain population as a smaller number of longer octene branches. As a result, the butene grade tends to show lower impact strength and lower tear resistance at equivalent density and melt index. Direct comparisons require film samples extruded on the same line at the same gauge.
The extrusion conditions must be re-tuned for the target gauge. The lower melt strength of butene LLDPE may necessitate a shorter frost line, narrower die gap, or lower blow-up ratio to maintain bubble stability. Die pressure and motor torque typically change when the comonomer changes, even at the same melt flow index, because molecular weight distribution and shear thinning behavior differ. Published data for this specific substitution on a fixed converting line is limited; a controlled trial using the test methods in Table 2 is required before production conversion.
Compliance with food-contact regulations must be confirmed in writing for the specific grade and lot. Polyethylene olefin copolymers of this type are generally addressed by FDA 21 CFR 177.1520 and EU 10/2011, but actual suitability depends on additive composition and migration testing. The supplier should provide a certificate of compliance, a safety data sheet, and a REACH registration statement where applicable. The material is not intended for medical implant use or for packaging of strong oxidizing agents without prior compatibility testing. Storage should be in sealed original packaging at temperatures below 40 °C, away from direct sunlight and ignition sources. Polyethylene dust generated by pellet handling is combustible and must be controlled under NFPA 654 and local fire codes. Avoid storage near organic peroxides, strong acids, or chlorinated solvents.
On production lines, the main failure modes to monitor are torque-limited extruder operation, die-lip deposit, bubble instability, gauge bands, and low seal strength caused by excessive surface slip migration. These are operational limits rather than resin defects; they can be corrected through screw design, melt temperature, and cooling settings. If a converter observes consistent gel formation, the first diagnostic step is to verify melt temperature at the adapter and screen pack condition, not to assume resin contamination.