Nova Chemicals Sclair 11d1 Butene Lldpe Film Resin

NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 886354
    Product Name NOVA Chemicals Sclair 11D1 Butene LLDPE Film Resin
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.919 g/cm³
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Melt Flow Ratio I21 I2 30
    Tensile Strength At Yield 9.65 MPa
    Tensile Strength At Break 33.1 MPa
    Elongation At Break 750%
    Tensile Modulus 0.207 GPa
    Dart Drop Impact 110 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Haze 12%
    Gloss 55%
    Coefficient Of Friction 0.2
    Vicat Softening Point 100°C
    Melting Point 122°C

    As an accredited NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin is typically supplied in 25 kg polyethylene bags or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg polyethylene bags of NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin, palletized and stretch-wrapped.
    Shipping NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin is non-hazardous and not DOT/IMDG regulated. It is shipped in 25 kg polyethylene bags, stretch-wrapped pallets, or bulk trucks/railcars. Keep dry, clean, and away from heat and contamination. Transport in closed, dry containers. No special dangerous-goods placards required.
    Storage Store Sclair 11D1 LLDPE resin indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Place on pallets, avoid excessive stacking and physical damage, and use first-in, first-out rotation. Limit prolonged UV exposure. Ensure good housekeeping and follow supplier guidance.
    Shelf Life Typically 2 years from date of manufacture when stored in original unopened packaging in a cool, dry, well-ventilated area.
    Application of NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin

    Blown and cast film conversion data for Sclair® 11D1 indicate that the resin is processed either neat or as the major constituent of a dry blend. The nominal density of 0.920 g/cm³ and melt flow rate of 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg define a butene LLDPE film grade whose dart impact and tear propagation are more strongly affected by die gap, bubble geometry, and chill roll temperature than by screw speed fluctuations. Published line-specific data for certain configurations is limited; the following ranges reflect typical industrial practice for butene LLDPE of this density and melt flow class.

    On a cast film line with a 2,800 mm slot die and a three-layer feedblock, Sclair® 11D1 is allocated to the core layer because the butene comonomer distribution maintains extensional viscosity during the draw from die to chill roll. Core-layer addition of 70–85 wt% Sclair® 11D1 is typical; the balance comprises 10–25 wt% metallocene VLDPE and 0–15 wt% LDPE, while skin layers may carry 20–40 wt% LDPE to modify cling and release. Tackifier addition in the skin layer ranges from 0.5–1.5 wt% for machine wrap; higher loadings are limited by roll blocking. The cast stretch film sector is covered by ASTM D5458 for peel cling and ASTM D4649 for selection and use of stretch wrap materials. Films sold for palletising food-contact packaging in the EU fall under EU 10/2011 when a functional barrier is not present, and in the US under FDA 21 CFR 177.1520(c) for olefin polymers provided the film meets the extractable fraction specifications. Processing on high-output lines sets melt temperature at 240–280 °C, die gap at 0.4–0.8 mm, and air gap at 50–150 mm; chill roll temperature is held at 20–35 °C. Thin-gauge terminal products include hand stretch wrap at 15–23 µm, machine stretch film at 20–35 µm, and pre-stretched wrap at 8–15 µm final thickness. A processing boundary appears at air gaps above 150 mm, where neck-in reduces edge trim recovery and disturbs final roll hardness.

    What Limits Frost Line Height When 11D1 Is Blown on High-Stalk Film Lines?

    Frozen food packaging converters running high-stalk bubbles with die diameters of 300–500 mm use Sclair® 11D1 at 70–90 wt% in blends with LDPE at 10–30 wt% to increase bubble stability. Slip masterbatch is added at 0.05–0.10 wt% active slip, and antiblock masterbatch at 0.10–0.30 wt% synthetic silica or equivalent. Compliance for direct food contact is evaluated under FDA 21 CFR 177.1520(c) for the olefin polymer base resin and under EU 10/2011 with testing according to EN 1186 migration protocols for aqueous and fatty food simulants; for frozen storage conditions, OM2 simulant exposure is applied. Blown-film process parameters include die gap 1.8–2.4 mm, blow-up ratio 2.0–2.5, and melt temperature 180–220 °C. Frost line height is maintained between 6× and 10× die diameter; below 6×, bubble cooling is insufficient for dart impact, while above 10×, gauge variation and tear anisotropy become measurable. Electronically controlled internal bubble cooling and gauge control rings are specified because butene LLDPE film exhibits lower melt tension than hexene copolymer grades under comparable ASTM D1238 flow conditions. Terminal products include frozen vegetable pouches at 40–70 µm, bag-in-box liners at 80–150 µm, and VFFS freezer bags at 50–90 µm.

    With grooved-feed extruders of 30:1 to 36:1 L/D and barrier screw geometries, FIBC liner and heavy-duty sack production from Sclair® 11D1 proceeds at melt temperatures below 220 °C because excessive compression ratio would raise shear heat and degrade impact strength. Addition of 60–100 wt% neat resin is common; process scrap from the same film line is reintroduced at 10–20 wt% when melt filtration through 100–150 µm screen packs is available. For packaging of dangerous goods, the assembled FIBC is certified under UN 13H4 or equivalent flexible IBC performance tests; the liner film contributes tear resistance measured according to ASTM D1922 and puncture resistance measured according to ASTM D5748. Extrusion uses die gaps of 2.0–3.0 mm, blow-up ratios of 1.8–2.4, and melt temperatures of 190–230 °C. Terminal products include construction debris sacks at 80–120 µm, plastic resin packaging liners at 60–100 µm, and FIBC inner liners at 100–150 µm.

    Silage Wrap Ultraviolet Stabiliser Loading and Peel Cling After Ageing

    Agricultural bale wrap made with Sclair® 11D1 is formulated with a UV masterbatch containing hindered amine light stabiliser and benzotriazole UV absorber. Total UV masterbatch addition of 1.0–2.5 wt% is typical for 12–24 month outdoor storage; below 1.0 wt%, tensile elongation at break after UV aging can fall below the 50% retained elongation commonly required for bale wrap under EN 13206:2017. Tackifier addition ranges from 0.5–1.0 wt% to maintain peel cling after ageing. Blown film processing uses three-layer lines with die gap 1.8–2.4 mm, blow-up ratio 2.5–3.2, and melt temperature 200–240 °C. The film is typically produced at 25 µm nominal thickness, with minimum thickness of 20 µm; the more severe drawing on the bubble edge can produce gauge variation above ±8%, which is controlled by reversing die lip air rings. Terminal products include bale wrap film, silage cover sheets at 100–150 µm, and greenhouse films at 150–200 µm when a heavier gauge profile is selected.

    Extrusion Lamination Sealant Webs on Aluminium Foil Require a Coextruded Tie Layer

    Lamination structures for pouch packaging combine Sclair® 11D1 in the sealant web with LDPE or plastomer to lower seal initiation temperature. A sealant layer formulation of 40–70 wt% Sclair® 11D1 and 30–60 wt% LDPE is used when heat seal strength must remain above 15 N/25 mm after ASTM F88 testing; film structures with high seal integrity are specified under FDA 21 CFR 177.1520(c) and EU 10/2011 for food contact. The extrusion lamination process runs a tandem line at melt temperature 290–315 °C, die gap 0.5–0.8 mm, and air gap 120–180 mm before nip; melt curtain instability increases at air gaps above 180 mm. Substrates include aluminium foil at 6–9 µm, PET at 12 µm, and oriented polyamide at 15 µm; without an adhesion promoter or printed primer, direct foil adhesion is insufficient, so a tie layer is coextruded. Terminal products are stand-up pouches, foil lidding, sachet laminates, and aseptic overpack, with sealant layer thickness between 15–40 µm.

    At cycle rates above 80 packs/min, personal care and hygiene overwrap lines running high-speed VFFS equipment use Sclair® 11D1 in the sealant layer at 50–80 wt%, with 20–50 wt% LDPE to broaden the heat-seal window. Slip additive is introduced at 400–800 ppm and antiblock at 2,000–4,000 ppm according to film gauge and static charge. The film is converted from blown or cast stock and evaluated under FDA 21 CFR 177.1520(c) for skin-contact packaging migration limits, with EU compliance assessed under EU 10/2011 using EN 1186 test cells. Processing on VFFS requires a seal initiation temperature below 95 °C at 0.5 s dwell time; seal bar temperature above 120 °C can cause burn-through on reverse-printed laminates. Terminal products include tampon overwrap, nappy liner film, wet wipe refill pouches, and protective film for absorbent pads.

    Free Quote

    Competitive NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Designated as a butene-comonomer linear low density polyethylene film resin, NOVA Chemicals Sclair® 11D1 is supplied as pelletized feedstock for cast film and selected blown film operations. The manufacturer’s published nominal density is 0.920 g/cm³ when measured by ASTM D792, and the melt index is 1.0 g/10 min when measured under ASTM D1238 at 190 °C with 2.16 kg. These values place the grade in the medium-molecular-weight, low-to-moderate-density segment of the butene LLDPE class. The short-chain branching derived from 1-butene copolymerization reduces crystallinity relative to high-pressure LDPE of comparable density; the peak melting endotherm is reported in the range 121–124 °C under ASTM D3418. The resin is used in cast stretch film, industrial liners, fresh produce packaging, frozen food bags, and lamination sealant webs. Converters familiar only with branched LDPE should note that the linear backbone of Sclair® 11D1 requires higher motor load at equivalent melt index; barrel temperature profiles must be raised or the screw design must include high-shear mixing elements to avoid pressure spikes and melt fracture.

    Which Conversion Conditions Are Reported for Cast Film Extrusion of Sclair® 11D1?

    On cast film lines equipped with 75 mm or 90 mm single-screw extruders with 30:1 L/D and barrier screws, the material is processed through a reverse-temperature profile from 180 °C in the feed zone to 225–240 °C at the adapter and flat die. Melt temperature measured at the die lip is typically 232–246 °C. Screen packs of 100–120 mesh are recommended to trap incidental gels; die gaps between 0.5 mm and 0.8 mm are standard. The chill-roll temperature is maintained at 15–25 °C to control crystallinity and optical clarity. Because the melt strength of butene LLDPE is lower than that of high-pressure LDPE, the air gap is reduced to 25–50 mm to limit neck-in and prevent gauge thinning at the web edges. At line speeds of 120–250 m/min, film thickness can be drawn to 10 µm on cast film equipment; the primary limitation at thin gauges is transverse tear rather than drawdown. If melt fracture appears as sharkskin on the film surface, the first corrective action is to raise the adapter and die temperatures by 5–10 °C or to reduce output by 10–15%. The resin is moisture-insensitive and does not normally require pre-drying; however, when storage conditions exceed 60% relative humidity, condensation on cold pellet surfaces can introduce water to the feed throat and produce surface defects. In such cases, hopper air at 50–60 °C is applied.

    Rheological measurements on a capillary rheometer at 190 °C indicate that the apparent shear viscosity of Sclair® 11D1 follows the expected shear-thinning profile for a linear polyethylene with 1.0 g/10 min melt index. At an apparent shear rate of 100 s⁻¹, the viscosity is approximately 300–500 Pa·s; at 1000 s⁻¹, it falls to 80–120 Pa·s. The activation energy for viscous flow is approximately 28–32 kJ/mol for linear polyethylenes in this density range. These values explain why increasing die temperature by 10 °C reduces die pressure without substantially changing melt strength. For extrusion lines equipped with gear pumps, suction pressure at the gear pump inlet should be maintained above 0.5 MPa to avoid cavitation; discharge pressure upstream of the screen changer is typically 15–25 MPa depending on throughput and screen pack condition. Filter pressure rise above 8 MPa across the screen pack indicates gel accumulation and requires screen replacement.

    Film property data derived from cast film at 25 µm thickness and conditioned for 40 h at 23 °C and 50% relative humidity are summarized in the tables below. The values are typical, not specification limits; they vary with die gap, air gap, chill-roll temperature, output rate, and orientation. Machine-direction tensile values exceed transverse values because of preferential machine-direction orientation on the chilled roll. Dart impact and Elmendorf tear reflect the short-chain branching distribution of butene copolymerization.

    Resin PropertyTest StandardTypical ValueUnit
    Nominal densityASTM D7920.920 g/cm³g/cm³
    Melt indexASTM D12381.0 g/10 ming/10 min
    Peak melting endothermASTM D3418121–124 °C°C
    Vicat softening pointASTM D152595–100 °C°C
    Brittle temperatureASTM D746< -60 °C°C
    Film Property at 25 µmTest StandardTypical ValueUnit
    Tensile strength at break, machine directionASTM D88235–45 MPaMPa
    Tensile strength at break, transverse directionASTM D88230–35 MPaMPa
    Elongation at break, machine/transverse directionASTM D882600–800%%
    Elmendorf tear resistance, machine directionASTM D1922150–250 gg
    Elmendorf tear resistance, transverse directionASTM D1922300–450 gg
    Dart drop impact, F50ASTM D170990–140 gg
    HazeASTM D10034–8%%
    Gloss at 45°ASTM D245770–85dimensionless

    Water vapor transmission rate for a 25 µm film is approximately 15–20 g/(m²·day) at 38 °C and 90% relative humidity under ASTM F1249. Oxygen transmission rate is approximately 4000–5000 cm³/(m²·day·atm) under ASTM D3985. These values are similar to other polyethylenes of equal thickness and density; barrier performance is determined primarily by crystallinity, thickness, and orientation.

    When Sclair® 11D1 Replaces High-Pressure LDPE in Lamination Sealant Webs

    Lamination structures using Sclair® 11D1 as the sealant layer are processed on solventless adhesive lines and extrusion lamination lines. Heat-seal initiation temperature is lower than that of a high-pressure LDPE of matched melt index; measurable seal strength appears at 95–105 °C, and plateau seal strength is reached between 120 °C and 140 °C. Seal strengths of 8–12 N/15 mm are typical after 0.5 s dwell and 0.3 MPa jaw pressure when measured under ASTM F88. The resin is used in frozen food bags because low-temperature flexibility and impact resistance remain adequate at −30 °C; the brittle temperature of the resin is below −60 °C under ASTM D746. In form-fill-seal operations running 30–80 packages/min, jaw temperatures of 110–130 °C are used. Operators converting from LDPE usually increase barrel temperature setpoints by 10–15 °C because of the higher shear viscosity of the linear backbone. The motor load may increase by 10–20% at equivalent output; therefore, extruders with less than 15% available torque reserve may require a reduction in screw speed.

    Comparative performance against octene LLDPE of matched density and melt index is governed by short-chain branch length. The 1-butene comonomer produces ethyl branches, whereas 1-octene produces hexyl branches; the shorter ethyl branches are less effective at forming tie molecules between lamellar crystals. As a result, film produced from Sclair® 11D1 exhibits lower dart impact and Elmendorf tear than an octene LLDPE of identical density. Published data for this specific configuration is limited; however, broader polymer science literature indicates that replacing butene with octene at equivalent density can raise dart impact by 20–40% and transverse Elmendorf tear by 30–50%. The butene grade typically shows slightly higher tensile modulus and lower resin cost, which makes it suitable for lamination layers and industrial liners where tear resistance is not the primary requirement. Against metallocene LLDPE, Sclair® 11D1 generally has a broader molecular weight distribution and lower optical quality; however, cast film haze values below 8% are still attainable with chilled-roll temperatures at 15–20 °C.

    Within the butene LLDPE class, grade selection is primarily governed by melt index and additive package. Higher melt index grades provide better drawdown but lower dart impact and tensile strength. A grade with melt index greater than 2.0 g/10 min is generally specified for very thin cast film below 12 µm, while Sclair® 11D1 is selected for converters requiring a balance of tear resistance, stiffness, and stable processing at 25–50 µm film thickness. Lower melt index grades may offer improved toughness but require elevated melt temperature and increase extruder motor load. The specific additive package of Sclair® 11D1 must be confirmed on the supplier technical data sheet because slip and antiblock levels influence coefficient of friction, blocking, and heat-seal behavior.

    Regulatory and Safety Boundaries for Food-Contact Converting

    Food-contact status for Sclair® 11D1 is generally covered by FDA 21 CFR §177.1520(c) 3.1a and §177.1520(c) 3.2a, depending on food type and use temperature; the converter must verify end-use compliance for the finished article. European packaging compliance is assessed under Regulation (EU) No 10/2011, and the supplier provides REACH registration documentation in the safety data sheet. The grade is not designed for prolonged contact with strong oxidizing agents, aromatic hydrocarbons, or chlorinated solvents; these media can swell the surface and extract low-molecular-weight fractions. Processing at melt temperatures above 260 °C is not recommended because thermal degradation can generate aldehydes and reduce optical quality. At melt temperatures exceeding 280 °C, measurable reductions in molecular weight occur, and gel formation may increase. The resin is not designed for retort applications above 121 °C; sustained exposure at higher temperatures causes creep, loss of seal integrity, and deformation.