| HS Code | 783018 |
| Product | NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Hexene |
| Melt Index | 0.8 g/10 min |
| Density | 0.918 g/cm³ |
| Tensile Strength At Yield | 10.5 MPa |
| Tensile Strength At Break | 28 MPa |
| Elongation At Break | 800% |
| Dart Drop Impact | 220 g |
| Elmendorf Tear Strength | 400 g |
| Haze | 8% |
| Gloss At 45 | 70 |
| Coefficient Of Friction | 0.20 |
| Melting Point | 125 °C |
| Vicat Softening Point | 100 °C |
As an accredited NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene-lined bags, 1,000 kg bulk bags, or bulk railcar/truck shipments. |
| Container Loading (20′ FCL) | 20′ FCL: 20 pallets, 40 x 25 kg bags, 20,000 kg net, stretch-wrapped; NOVA Novapol® TF-Y826-D hexene LLDPE film resin. |
| Shipping | NovaPol® TF-Y826-D Hexene LLDPE Film Resin is shipped as a non-hazardous solid resin, typically in 25 kg polyethylene bags on stretch-wrapped pallets. Transport in clean, dry trucks or containers at ambient temperatures; protect from moisture, direct sunlight, and excessive heat. Not regulated for DOT/IMDG/IATA. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep resin in original, sealed packaging or bags, palletized off the ground to prevent moisture uptake and contamination. Store indoors at moderate ambient temperature. Protect from prolonged direct sunlight and weather. Avoid excessive stacking, sharp objects, and dust generation. Follow manufacturer’s SDS and local regulations. |
| Shelf Life | No specific shelf life; stable indefinitely under normal storage when sealed, dry, cool, away from direct sunlight, heat, and contaminants. |
In heavy-duty industrial sack packaging, the resin is converted into mono-layer or coextruded blown film where side-gusseted sacks are filled with 25 kg to 50 kg of granular or powdered product; the film must resist tear propagation during drop cycles rather than fail through tensile yield. Novapol® TF-Y826-D carries a typical density of 0.918 g/cm³ and typical melt index of 0.80 g/10 min under ISO 1133-1:2022, which supports the blend calculation. A typical industrial formulation uses 80 wt% of the resin with 20 wt% of a high-pressure LDPE homopolymer having a melt index of 0.25 g/10 min; carbon black masterbatch is optional at 2–3 wt% where extended UV resistance is required for outdoor storage. Compliance references include ISO 21898:2004 for industrial sack performance, ASTM D4976-12a for polyethylene film, and, where the sack enters food-adjacent distribution, 21 CFR 177.1520(c) for the olefin base polymer. Production on a 90 mm single-screw extruder with 30:1 L/D, a barrier screw and a 350 mm annular die requires a die gap of 1.8–2.2 mm, melt temperature 205–220 °C, blow-up ratio 2.2–2.5:1, and frost-line height 7–9 die diameters. Below 10 wt% LDPE, bubble instability and surging are observed on lines with die gap above 2.0 mm; beyond 2.5 mm die gap, MD tear strength loses the orientation balance needed for drop resistance. Terminal products include outer bag liners for woven polypropylene sacks, FIBC liners, fertilizer sacks, resin pellet sacks, and construction-material sacks.
| Property / Parameter | Standard or reference | Typical control range for 100 µm sack liner film |
|---|---|---|
| Melt index of blend | ISO 1133-1:2022 | 0.60–0.80 g/10 min |
| Dart drop impact | ASTM D1709-16a Method A | >200 g |
| Elmendorf tear, MD / TD | ASTM D1922-15 | >15 N / >25 N |
| Puncture resistance | ASTM D5748-95 | >40 N |
| Filled-bag drop test | ISO 21898:2004 | No rupture at 1.2 m on 25 kg sack |
| Visual gel limit | ASTM D4976-12a | < 10 gels/0.5 m² above 0.5 mm |
Agricultural bale-wrap film is produced from formulations in which Novapol® TF-Y826-D is used at 85–90 wt% with 10–15 wt% metallocene LLDPE, while a black or white UV-stabilized masterbatch is introduced at 4 wt% let-down. An external cling concentrate containing 20 wt% polyisobutylene is dosed at 2–3 wt% of total film weight to control unwind tension. The applicable product standard is EN 14932:2018 for thermoplastic stretch films for bale wrapping; puncture resistance is checked with ASTM D5748-95, tensile properties with ISO 527-3:2018, and UV retention is qualified by cumulative irradiance testing rather than visual inspection. Production on a 65 mm cast or blown line with 28:1 L/D typically uses die gap 1.2 mm, melt temperature 210–220 °C, and blow-up ratio 2.5–3.0:1 for blown variants; frost-line height is held at 6 die diameters to develop transverse orientation and improve tear propagation resistance. Masterbatch loading above 5 wt% depresses dart drop and creates gel streaking; storage above 35 °C accelerates PIB migration and can cause roll blocking before the film reaches the baler. Terminal products are round-bale wrap, square-bale wrap, pit cover, and tube film for ensiled grains.
Film structures for IQF vegetables and seafood are produced as three-layer coextrusions in which the sealant layer contains 70 wt% Novapol® TF-Y826-D and 30 wt% metallocene LLDPE with melt index 1.0 g/10 min; the outer skin includes 5 wt% silica-based antiblock masterbatch. Compliance references include 21 CFR 177.1520(c) for the olefin polymer base, EU Regulation No 10/2011 Annex I for overall migration limits of 10 mg/dm², EC 2023/2006 for good manufacturing practice, and ASTM F88/F88M-21 for seal strength. The coextrusion line usually runs a 250 mm die with 1.5 mm die gap, melt temperature 200–210 °C, blow-up ratio 2.0:1, and frost-line height not exceeding 5 die diameters; this suppresses crystalline development and preserves hot tack. Seal initiation is controlled between 115 °C and 130 °C with a dwell of 0.5–1.0 s. Slip-agent concentration above 1000 ppm in the sealant layer contaminates the seal bar and reduces burst strength of frozen pouches. Published data for dart drop on this exact sealant architecture is limited; converting sites typically qualify through ASTM D1709-16a Method A after a 48-hour -20 °C conditioning cycle. Terminal products include pouches for IQF vegetables, seafood bags, pre-formed freezer bags, and frozen bakery overwrap.
Machine-grade stretch film converting uses a five-layer cast line in which Novapol® TF-Y826-D is allocated asymmetrically to exploit its tear and puncture characteristics. The core layer contains 55–60 wt% of the total film thickness; the cling layer contains 90–95 wt% TF-Y826-D plus 3–5 wt% PIB masterbatch and 1–2 wt% high-melt-index LLDPE; the release layer is formulated with 85–90 wt% TF-Y826-D and 10–15 wt% LDPE. The relevant standards are ASTM D4649-20 for evaluation of stretch wrap performance, ISO 527-3:2018 for tensile modulus, and ASTM D1894-14 for coefficient of friction. A 2,000 mm cast die with 0.6–0.7 mm die gap is used; melt temperature is 250–265 °C, chill roll temperature 15–20 °C, air gap 5–10 cm, and line speed 400–600 m/min. PIB addition above 5 wt% in the cling layer generates roll blocking at ambient storage, while a chill roll below 10 °C causes condensation marks and transverse thickness bands. Terminal products are machine film, hand film, pre-stretched pallet wrap, and bundling film.
| Layer | Mass fraction of total film | Resin formulation | Evaluation reference |
|---|---|---|---|
| Cling skin | 10–15% | TF-Y826-D 90–95 wt% + PIB masterbatch 3–5 wt% | ASTM D1894-14 |
| Intermediate | 15–20% | TF-Y826-D 80 wt% + mLLDPE 20 wt% | ISO 527-3:2018 |
| Core | 55–60% | TF-Y826-D 100 wt% | ASTM D5748-95 |
| Intermediate | 15–20% | TF-Y826-D 80 wt% + mLLDPE 20 wt% | ISO 527-3:2018 |
| Release skin | 10–15% | TF-Y826-D 85–90 wt% + LDPE 10–15 wt% | ASTM D1894-14 |
Extrusion lamination with Novapol® TF-Y826-D is specified when converters require a low-gauge sealant layer against aluminum foil or polyester in liquid pouches without adding solvent-borne adhesive. The extrudate is 100 wt% TF-Y826-D for full-width coating; for narrow web lanes, up to 15 wt% of a high-melt-index LDPE is blended to reduce neck-in and improve adhesion. Compliance is governed by EU Regulation No 10/2011 Article 3 and Annex I for specific migration limits, 21 CFR 177.1520(c) for food-contact olefin polymers, REACH Regulation EC 1907/2006 for inventory compliance, and RoHS Directive 2011/65/EU where applicable for electrical and electronic associated packaging. A 90 mm extruder with 32:1 L/D, die gap 0.6–0.8 mm, melt temperature 315–325 °C, air gap 80–150 mm, and coat weight 12–20 g/m² is typical; line speed varies from 100 m/min to 200 m/min depending on substrate thermal stability. Moisture on the substrate at relative humidity above 80% produces pinholes; pre-drying of paper-based substrates is required at 70–80 °C before coating. Terminal products are laminated pouches for liquid dairy, juice, detergent refill packs, and single-serve condiment sachets.
High-clarity bakery film uses a blend of 70 wt% Novapol® TF-Y826-D with 30 wt% high-clarity metallocene LLDPE; a silica-based antiblock masterbatch is added at 2–3 wt%, and erucamide slip is controlled at 500–800 ppm. The applicable compliance references for bread and pastry contact are 21 CFR 177.1520(c), EU Regulation No 10/2011 Annex I for overall migration 10 mg/dm², and EC 2023/2006 for GMP. Production on a mono-layer or three-layer blown line with die gap 1.0 mm, melt temperature 195–210 °C, blow-up ratio 1.8–2.0:1, and frost-line height 5 die diameters yields a 25 µm film with haze typically below 8% when line speed exceeds 150 m/min; slower rates permit surface roughness from antiblock to scatter light. Antiblock masterbatch above 3 wt% raises haze beyond 8% and reduces gloss below 60 GU at 20°; slip below 500 ppm causes sticking on bag-fill lines. Terminal products are sliced-bread bags, baguette sleeves, bun bags, and light produce bags.
Competitive NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® TF-Y826-D is a hexene-copolymer linear low-density polyethylene film resin intended primarily for cast-film conversion. The grade is characterized by a nominal melt index of 2.0 g/10 min when tested under 190 °C and 2.16 kg load according to ASTM D1238, and a nominal density of 0.926 g/cm³ according to ASTM D1505. Equivalent melt flow classification under ISO 1133-1:2022 uses the same 190 °C, 2.16 kg condition. The 1-hexene comonomer introduces short-chain branching that increases the population of load-bearing tie molecules relative to butene-copolymer LLDPE at equivalent density and melt index. End-use sectors include cast stretch film, food-packaging overwrap, lamination sealant webs, industrial liners, and thin-gauge protective film, where puncture resistance, tear propagation energy, and drawability on chill-roll lines dominate the selection decision. TF-Y826-D is not classified as a blown-film grade; its melt-curtain stability on cast-film equipment defines the practical processing envelope.
Table 1 summarizes incoming quality-control parameters and the relevant test designations.
| Parameter | Nominal value | Test method |
|---|---|---|
| Melt index | 2.0 g/10 min | ASTM D1238 at 190 °C, 2.16 kg |
| Density | 0.926 g/cm³ | ASTM D1505 at 23 °C |
Film property values—dart impact by ASTM D1709A, Elmendorf tear by ASTM D1922, puncture force by ASTM D5748, haze by ASTM D1003, and 45° gloss by ASTM D2457—are determined on fabricated film and therefore vary with gauge, draw ratio, chill-roll temperature, and additive content. Published data for this specific configuration is limited; converters should generate product-specific data on the intended cast-film line rather than transfer values from different hexene LLDPE grades. The additive package associated with the suffix should be confirmed against the supplier’s current technical data sheet because slip and antiblock concentrations affect surface migration, coefficient of friction, and seal performance.
At equivalent density and melt index, a 1-hexene LLDPE generally provides higher dart impact and machine-direction tear resistance than a 1-butene LLDPE when tested by ASTM D1709A and ASTM D1922. The longer C6 short-chain branch increases the probability of tie-chain formation between adjacent crystallites, improving resistance to slow crack growth and impact-induced fibril fracture. This difference becomes more pronounced in films below 25 µm and under high-strain-rate loading. Compared with 1-octene LLDPE, hexene grades occupy an intermediate toughness/processability position; octene may offer greater impact at similar density, but the specific molecular weight distribution and additive package can reverse that ordering. The comparison is not absolute and must be measured on the final film because extrusion thermal history, draw ratio, and quench rate alter crystal morphology and tie-chain concentration.
Processing of this resin is carried out on single-screw extruders with barrier-screw geometry and Maddock mixing sections. A representative configuration is a 45 mm diameter barrel, 30:1 L/D, with a water-cooled feed throat held at 40–60 °C. Barrel set points are ramped from 180 °C in the feed zone to 235 °C in the metering zone, with adapter and die zones maintained between 240 °C and 250 °C. Melt temperature, measured with a flush-mounted resistance probe, should remain between 220 °C and 250 °C. Below 220 °C, the viscosity increase may raise wall shear stress above the critical threshold near 0.14 MPa, producing sharkskin melt fracture on the web. Above 250 °C, thermal-oxidative scission can create gel particles, increase neck-in, and destabilize the melt curtain. A die gap of 0.5–0.8 mm is typical for cast film, with chill-roll surface temperature maintained at 18–25 °C. The quench rate from the chill roll controls haze development measured by ASTM D1003 and affects the amount of surface-additive migration that governs coefficient of friction.
At line start-up, draw ratio between die exit and chill roll is commonly 2:1 to 4:1. The resin’s 2.0 g/10 min melt index provides a moderate degree of shear thinning in the die land. However, TF-Y826-D does not possess the long-chain branching of high-pressure LDPE; therefore, strain-hardening and melt-curtain stiffness are lower. Neck-in must be controlled by die-width margin and edge encapsulation, not by excessive melt temperature. A die-bolt profile should be adjusted before changing melt temperature, because a temperature adjustment of more than 5 °C across the die width can create gauge variation and edge-bead instability. On a 75 mm line for multi-layer structures, melt-curtain wander is minimized when the air-knife pressure and vacuum-box extraction are operated to maintain a curtain length of 10–15 mm.
Field experience on production-scale cast-film lines with similar hexene LLDPE grades indicates that edge-bead formation becomes pronounced when the adapter temperature is raised above 255 °C or when the chill-roll temperature exceeds 30 °C. These observations are process-specific; a 1 °C change in chill-roll inlet water can shift web flatness on a 1.2 m line with a 0.6 mm die gap. The surface of the chill roll, whether polished or matte, determines film optical contact and therefore haze and gloss values measured by ASTM D1003 and ASTM D2457. Reclaimed edge trim may be re-fed after grinding, but the re-feed level should be kept below 5 wt%; higher levels introduce double-shear history that can reduce melt-index retention and affect cast-web uniformity.
Seal initiation for TF-Y826-D is not supplied as a fixed value because it depends on film quench rate, thickness, seal-bar dwell time, and the migration of slip and antiblock additives to the surface. The relevant heat-seal strength method is ASTM F88, and hot-tack behavior is measured by ASTM F1921. For hexene LLDPE cast film in the density range 0.925–0.930 g/cm³, laboratory hot-tack transitions are frequently observed at jaw temperatures between 115 °C and 125 °C under short dwell conditions, but this range is indicative only and must be verified on the specific film. The difference from butene-copolymer LLDPE is most evident at high line speeds, where the shorter available dwell time favors a broader hot-tack plateau and less crystalline perfection in the sealing interface. The sealant web should therefore be tested on the packaging line at the intended speed, with seal-bar pressure and dwell time recorded; otherwise, laboratory seal curves cannot be reliably transferred.
Substituting this resin into a 20 µm cast stretch-film structure from a 35 µm butene LLDPE film requires mechanical re-qualification by ASTM D882 tensile testing and ASTM D1709A impact testing. The downgauging potential of hexene LLDPE is based on higher energy absorption during deformation, but the converter must measure machine-direction elongation at break, transverse-direction tear by ASTM D1922, and stretch force at 200% elongation to confirm that the film retains load-holding capacity. In pre-stretch equipment operating at 70–100% elongation, transverse-direction edge tears are often the limiting failure mode; C6 short-chain branching generally delays that tear propagation relative to C4, but only when the chill-roll quench is rapid enough to limit excessive crystallinity. If the film is run too slowly on a hot chill roll, the resulting crystal morphology can offset the comonomer advantage. Compared with high-clarity metallocene hexene grades, this resin may show different shear-thinning and surface-additive behavior, so the packaging line’s coefficient-of-friction specification should be re-checked using ASTM D1894 before final substitution.
| Standard or regulation | Scope | Relevant condition |
|---|---|---|
| ASTM D1238 | Melt mass-flow rate | 190 °C, 2.16 kg |
| ASTM D1505 | Density | 23 °C |
| 21 CFR 177.1520(c) | US FDA olefin polymer clearance | Food-contact use under specified extractives limits |
| EU 10/2011 | Plastic food-contact materials | Overall migration and specific migration limits |
Storage of the resin in 25 kg bags or bulk containers follows standard polyolefin handling. Condensation on granule surfaces is not a hydrolysis concern, but cold resin transferred into a warm production hall at relative humidity above 60% can introduce surface moisture that appears as splay or small bubbles in the cast web. In such cases, the hopper should be purged with dehumidified air, and the resin should be allowed to reach ambient temperature before opening. Prolonged storage above 65 °C should be avoided, as should contact with unsaturated oils, solvents, or amine-based additives that can swell the granule surface or generate odor at processing temperatures.