Nova Chemicals Novapol Tf Y826 Cp Hexene Lldpe Film Resin

NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 908139
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Melt Index 0.8 g/10 min (ASTM D1238, 190°C/2.16 kg)
    Density 0.926 g/cm³ (ASTM D792)
    Melting Point 124 °C (DSC)
    Vicat Softening Point 100 °C (ASTM D1525)
    Brittleness Temperature < -70 °C (ASTM D746)
    Tensile Strength At Yield Md 10.5 MPa (ASTM D882)
    Tensile Strength At Yield Td 10.5 MPa (ASTM D882)
    Tensile Strength At Break Md 35 MPa (ASTM D882)
    Tensile Strength At Break Td 32 MPa (ASTM D882)
    Elongation At Break Md 600% (ASTM D882)
    Elongation At Break Td 700% (ASTM D882)
    1 Secant Modulus Md 234 MPa (ASTM D882)
    1 Secant Modulus Td 255 MPa (ASTM D882)
    Dart Drop Impact 200 g (ASTM D1709)
    Elmendorf Tear Md 250 g (ASTM D1922)
    Elmendorf Tear Td 400 g (ASTM D1922)
    Puncture Resistance 60 J/cm (ASTM D5748)
    Haze 10% (ASTM D1003)
    Gloss 60 (ASTM D2457, 45°)
    Coefficient Of Friction 0.2 (ASTM D1894)
    Blocking 50 g (ASTM D3354)
    Heat Seal Initiation Temperature 110 °C

    As an accredited NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin typically comes in 25 kg polyethylene bags or 1,000 kg bulk bags, palletized.
    Container Loading (20′ FCL) 20′ FCL: 20 pallets of 25 kg polyethylene bags, NOVA Chemicals Novapol TF-Y826-CP Hexene LLDPE Film Resin, stretch-wrapped and braced.
    Shipping NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin ships as a non-hazardous solid in 25 kg multiwall bags or 1,000 kg bulk bags on pallets. Transport by truck or rail in dry, covered equipment. Store away from heat, moisture, and UV. Not DOT/IMDG/IATA regulated.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original bags or containers sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Stack securely to prevent package damage. Use first-in, first-out inventory practices and maintain good housekeeping. Keep away from strong oxidizers. Suitable for normal storage of polyethylene resin pellets.
    Shelf Life 12 months from date of manufacture when stored in original packaging at ambient temperatures, away from direct sunlight.
    Application of NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin

    On three-layer blown-film lines producing heavy-duty sacks in the 80–150 µm thickness range, Novapol® TF-Y826-CP is dry-blended at the feed hopper with 20–30 wt% high-pressure LDPE having a melt index of 0.20–0.35 g/10 min at 190°C under 2.16 kg load per ISO 1133-1:2022. The skin layers are extruded through 45–65 mm grooved-feed screws with length-to-diameter ratios of 25:1 to 30:1, barrel temperature profiles rising from 175°C to 215°C, and die zones held at 210–225°C; the core layer carries 70–80 wt% TF-Y826-CP at melt temperatures of 215–230°C. Die gaps are set between 1.8 mm and 2.4 mm with dual-lip air rings and internal bubble cooling, yielding a frost line height of 450–850 mm at output rates of 8–14 kg/h per die circumference centimetre. When the blow-up ratio is kept at 2.2:1 to 3.0:1, film flat width control remains within ±5 mm on a 250 mm spiral mandrel die; excursions above 3.2:1 induce low-frequency bubble wave unless the LDPE fraction is raised to 30 wt% or the frost line is lowered below 400 mm. Conditioning for 40 h at 23°C ± 2°C and 50% ± 10% relative humidity is required before destructive testing. Dart drop impact by ASTM D1709/A for 100 µm film commonly sits between 300 g and 600 g depending on the LDPE fraction and frost line; puncture resistance by ASTM D5748-18 generally falls in the 40–80 N range for 100 µm specimens. The end product is used for resin pellet sacks, dry chemical packaging, and construction aggregate bags where stack-loading at 45°C for 48 h must not produce creep rupture.

    How Does Hexene Short-Chain Branching Affect Seal Integrity in Frozen Food Pouch Layers?

    Frozen food pouch structures with 45–70 µm total thickness are coextruded with a sealant layer based on TF-Y826-CP or blends containing 80–90 wt% TF-Y826-CP and 10–20 wt% metallocene LLDPE having a melt index of 0.5–1.0 g/10 min. The sealant layer is positioned on the inside of the bubble at die temperatures of 215–225°C, while the outer skin is a high-stiffness HDPE or MDPE to provide heat resistance during sealing. Vertical form-fill-seal machines operate with jaw temperatures of 115–135°C, dwell times of 0.3–0.8 s, and jaw pressures of 0.3–0.6 MPa; seal initiation temperature is typically 95–105°C for the neat hexene LLDPE layer, rising by 3–5°C when the formulation contains secondary amide slip additives. Hexene short-chain branching in TF-Y826-CP distributes crystalline lamellae more heterogeneously than butene LLDPE, which limits low-temperature brittleness and maintains hot tack at sealing temperatures where the outer HDPE skin has not yet melted. Seal strength is measured by ASTM F88/F88M-21 at 200 mm/min jaw separation, with acceptable values of 10–20 N/25 mm for 50 µm films after sealing at 120°C and 0.4 MPa. Frozen storage at -25°C for 48 h followed by a 1 m drop test onto concrete is a standard distribution check; pouches with dart impact below 200 g at -20°C per ASTM D1709/A exhibit corner punctures in unrestrained drops.

    Standard / RegulationScopePass Criterion / Operating Limit
    FDA 21 CFR 177.1520(c)Ethylene/1-hexene copolymer for food contact, Conditions of Use A–HCompliant as olefin polymer; migration confirmed through end-use extraction testing under 21 CFR 176.170(c) Table 2
    EU Regulation 10/2011, Annex I and IIPlastic material in contact with foodOverall migration <10 mg/dm² under OM2, 60°C for 10 days
    REACH EC 1907/2006, Article 33SVHC declarationNo SVHC above 0.1 wt% in supplied resin or formulation
    ASTM F88/F88M-21Seal strength of flexible barrier materials10–20 N/25 mm for 50 µm sealant layer after 120°C seal
    ASTM F1921-18Hot tack seal strength4–8 N/25 mm at 0.5 s dwell, 0.3 MPa

    Agricultural silage covers and greenhouse films utilizing TF-Y826-CP are compounded on twin-screw lines at 30:1 L/D with intensive mixing elements because UV stabilizer masterbatches containing 20–25 wt% hindered amine light stabilizer and 10–15 wt% benzotriazole must be dispersed without exceeding 240°C melt temperature. Film thickness of 150–200 µm is typical for silage bags, with blow-up ratios of 2.5:1 to 3.2:1 and a die gap of 2.0–2.6 mm to preserve tear resistance in the machine direction. After 4000 h of QUV-A accelerated weathering under ASTM G154-16 Cycle 1, elongation retention above 70% is expected for film containing 8–12 wt% of the stabilizer masterbatch; failure below 50% indicates inadequate HALS dispersion or hot spots above 250°C during extrusion. Silage films are exposed to lactic acid condensate at pH 4.0–4.5 during fermentation, and additive packages must keep calcium stearate below 1200 ppm to avoid surface bloom that reduces surface friction and hinders unfolding. Puncture resistance measured by ASTM D5748-18 is controlled to 60–120 N for 180 µm film, while dart drop by ASTM D1709/A should exceed 800 g at 23°C. Greenhouse applications require the opposite additive profile: anti-fog and anti-drip surfactants are incorporated at 1.5–3.0 wt% in the inner layer, but these additives migrate and can reduce interfacial tension at the seal; therefore, greenhouse film is normally anchored with aluminium lock profiles rather than heat-sealed seams.

    Cast Stretch Film Neck-In and Cling Bloom During High-Speed Slitting

    Cast stretch film lines processing TF-Y826-CP at 15–23 µm thickness operate with 75–100 mm barrier screws, 2.2–2.8 m slot dies, die gaps of 0.45–0.75 mm, and chill roll temperatures of 18–25°C. Neat hexene LLDPE exhibits neck-in between 80 mm and 120 mm at 750 m/min line speed; blending 15–20 wt% metallocene LLDPE with a melt index of 0.5–1.0 g/10 min reduces neck-in to 55–75 mm while preserving pre-stretch retention. Air knife velocity is maintained at 5–10 m/s to pin the melt curtain before the chill roll, and edge trim is recycled at 5–15 wt% in the core layer without exceeding a melt pressure fluctuation of ±8% across the screen changer. Cling agents based on polyisobutylene are added at 2–4 wt%, with erucamide slip at 0.2–0.5 wt% to modify unwind tension; cling force measured by ASTM D5458-20 on 25 mm wide specimens after 24 h aging typically falls in the 1.0–2.0 N range. Pre-stretch at 200–250% requires a stretch retention of at least 80% after relaxation for 10 s to maintain pallet load stability; above 300% pre-stretch, residual stress causes core deformation and the film fails in creep at ambient temperatures above 30°C. Film is slit at 450–500 m/min and wound on 76 mm paper cores with taper tension of 0.2–0.5 N/mm; winding hardness above 85 Shore A causes blocking in warm warehouses.

    When E-Commerce Mailer Structures Need Sub-Zero Puncture Resistance Without Sealant Density Increases

    E-commerce mailers and padded envelopes with total thickness of 40–80 µm are produced as three-layer blown film with an outer skin of HDPE or MDPE containing 15–30 wt% post-consumer recycled material, a core of TF-Y826-CP at 50–70 wt%, and an inner sealant layer of metallocene LLDPE or plastomer. The structure is intended to survive automated packing, air pillow insertion, and courier sorting without punctures at -20°C. Dart impact at -20°C measured by ASTM D1709/A for 60 µm film generally falls between 250 g and 450 g, while Elmendorf tear in the machine direction measured by ASTM D1922-21 is 6–14 N; films that fall below 6 N MD tear exhibit envelope corner tearing on high-speed mail insertion lines running above 120 cycles/min. Sealant layer density is kept below 0.910 g/cm³ per ISO 1183-1:2019 to avoid increasing the overall structure density and to allow low seal initiation at 85–95°C, while the core layer provides the abuse resistance. The outer skin with recycled HDPE must not exceed 30 wt% because gel quantification per DIN 53765-1:1998 should remain below 20 gel counts per 1000 cm² above 0.2 mm; higher recycle levels create surface roughness that reduces flexographic print density and increases coefficient of friction above 0.45 per ASTM D1894-14.

    Stress Crack Resistance Screening in Geomembrane Blown Film Joins Output Stability to Weld Compatibility

    Landfill liner and temporary containment films produced at 200–500 µm thickness from TF-Y826-CP require a 24 h conditioned tensile test per ISO 527-3 and an environmental stress crack resistance test per ASTM D1693-15 in 10 wt% Igepal CO-630 at 50°C; published data for this specific configuration is limited, but hexene LLDPE geomembranes typically require 1000 h to failure for 2 mm notched specimens. Blown film lines with 90–120 mm grooved feed and 300–400 mm spiral mandrel dies run at melt temperatures of 210–230°C and die gaps of 2.5–3.5 mm; bubble cooling must be controlled to avoid residual thermal stress that lowers weld shear strength. Wedge welding at 350–400°C and 0.8–1.2 m/min produces seams whose peel and shear strength should exceed 80% of parent material yield strength per ASTM D6392-12. Field seaming is intolerant of moisture; surface exposure to relative humidity above 70% for more than 2 h before welding reduces weld peel strength by 10–20%.

    Free Quote

    Competitive NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Resin grade NOVA Chemicals Novapol® TF-Y826-CP is a linear low-density polyethylene based on hexene-1 comonomer. It is supplied as cylindrical pellets and positioned for slot-die cast film lines, including stretch film and industrial surface-protection structures. The grade is not formulated with reactor-introduced slip or antiblock packages, which transfers surface-function control to the converter. Nominal melt index is 2.8 g/10 min at 190°C/2.16 kg by ASTM D1238; nominal density is 0.925 g/cm³ by ASTM D1505. Differential scanning calorimetry gives a peak melting endotherm near 123°C when tested according to ASTM D3418. These values describe a hexene-copolymer architecture: the longer comonomer side chain reduces crystallinity more effectively than butene at equivalent mole fraction and increases the probability of intercrystalline tie-chain formation. Because the extrusion envelope is specified for cast film, published data for this same product in high-stalk blown-film operation is limited.

    PropertyTest methodNominal value
    Melt indexASTM D12382.8 g/10 min
    DensityASTM D15050.925 g/cm³
    Peak melting endothermASTM D3418123 °C
    Comonomer—hexene-1
    Slip/antiblock package—none intentionally added

    How Does Hexene-1 Short-Chain Branching Influence Tear and Impact Response?

    The hexene-1 comonomer inserts a 4-carbon side branch into the ethylene backbone; by comparison, butene-1 inserts a 2-carbon side branch and octene-1 inserts a 6-carbon side branch. The longer side branch disrupts lamellar folding more efficiently at equivalent comonomer content, shifting the crystal thickness distribution downward and increasing the amorphous tie-chain concentration. This morphological change is not directly measured in film production, but it appears in standard mechanical tests: Elmendorf tear values measured per ASTM D1922 and dart drop impact values measured per ASTM D1709 are generally higher for hexene LLDPE than for butene LLDPE of the same nominal density and melt index. The improvement is thickness-dependent. At 25 µm cast film, published hexene LLDPE comparisons commonly report dart impact gains of 20 to 45% over butene LLDPE, but exact values vary with chill-roll temperature, air-gap distance, line speed, and masterbatch loading. The grade should therefore be evaluated in the target structure and at the target gauge; blown-film data or compression-moulding data should not be substituted for cast-film performance. Machine-direction orientation increases tensile strength but reduces machine-direction tear; transverse-direction tear generally remains higher because of the preferential alignment of polymer chains in the machine direction.

    When TF-Y826-CP Replaces Butene LLDPE in a Three-Layer Cast Stretch Line

    In a three-layer A/B/A cast stretch film line, replacement of a butene LLDPE core with TF-Y826-CP changes the viscosity ratio between core and skin layers. The nominal melt index of 2.8 g/10 min is typically higher than conventional butene LLDPE core grades; this reduces melt pressure at a fixed screw speed and may lower screw torque. However, lower melt elasticity can shift the onset of draw resonance to a lower line speed. If oscillating gauge variation exceeds ±5% at 200 m/min, the process response is mechanical: reduce the die-to-roll air gap from 15 cm to 8 cm or increase chill-roll temperature from 18°C to 25°C to stabilise the web. The absence of slip and antiblock in the core grade means that surface coefficient of friction is governed by the skin layers, so the change in core resin should not be used to adjust film-to-film friction. On a 75 mm 33:1 L/D single-screw extruder running at 120 rpm, die inlet pressure should remain between 8 MPa and 30 MPa; below 8 MPa mixing may be insufficient, and above 30 MPa shear heating can initiate melt fracture at the die lip. Published data for this specific grade in 8 µm cast stretch film is limited; converter trials are required to define the minimum gauge at the intended winder tension.

    Extruder Screw Design, Melt Pressure, and Draw Resonance Windows

    TF-Y826-CP is processed on a conventional polyethylene single-screw extruder with 30:1 to 36:1 L/D and a barrier-flighted screw with a Maddock mixing section. Typical temperature set points from feed throat to die are 40°C, 180°C, 210°C, 230°C, 240°C, adapter 250°C, and flat die 255°C. Melt temperature should not exceed 280°C; at 260°C the melt residence time should remain below 15 min to avoid phenolic antioxidant depletion and gel generation. Extrusion backpressure in cast film is typically 12 to 25 MPa at 300 kg/h on a 90 mm extruder; values outside this band should prompt a check of screw wear, screen pack condition, or die deckle geometry. Screen packs finer than 120 mesh are generally unnecessary and may add 6 MPa pressure drop at high throughput. Polyethylene is not hydrolytically sensitive, but if pellets are transferred from cold storage into a high-humidity processing hall, surface condensation can be removed by hopper drying at 70°C for 2 to 4 h when ambient relative humidity exceeds 60%. Draw resonance in cast film is controlled by reducing the air gap and increasing electrostatic pinning force; thin gauges below 10 µm require tighter die-bolt temperature control.

    Slip and Antiblock Are Not Reactor-Introduced; Surface Functionality Must Be Added by the Converter

    Because TF-Y826-CP contains no reactor-introduced slip or antiblock package, the film surface is not fixed by the base resin. Erucamide or oleamide masterbatch is typically added to the skin layer at 1 to 3 wt% to reduce kinetic coefficient of friction below 0.20 after 48 h aging at 23°C when measured by ASTM D1894. Silica or synthetic antiblock masterbatch at 5000 to 10,000 ppm controls blocking at roll pressures above 0.5 MPa. The antiblock particle size distribution must be controlled; particles larger than 6 µm can produce visible surface defects in film below 12 µm. Optical property shifts after additive addition are measured by ASTM D1003 for haze and ASTM D2457 for gloss. Because additive migration occurs over time and depends on film temperature, initial coefficient of friction after winding is not equivalent to coefficient of friction after 48 h at ambient or after heat exposure. Published data for this grade with specific commercial masterbatch formulations is limited; each converter must establish additive loading against the actual film structure, roll dimension, and storage temperature.

    Metallocene-Catalysed Hexene LLDPE Offers Different Optical and Rheological Boundaries

    Compared with metallocene-catalysed hexene LLDPE of similar density and melt index, TF-Y826-CP is generally described in converter practice as a conventional-catalysis grade with a broader molecular weight distribution. This broader distribution improves screw pressure stability and reduces melt-pressure fluctuation on older cast-film extruders with shallow screw designs. The trade-off is typically lower gloss and higher haze than a narrow-distribution metallocene resin, measured by ASTM D2457 and ASTM D1003. In coextruded structures, TF-Y826-CP can be used in the core or machine-side skin while metallocene hexene LLDPE is placed in the external skin to maintain optical quality. The two resin classes should not be assumed interchangeable at the same melt index; the metallocene grade may have a different critical shear rate for melt fracture and may require a different die-lip set point. Compared with octene-1 LLDPE, hexene-1 LLDPE provides an intermediate branch length and impact performance; octene-1 generally has a longer 6-carbon side branch and can give higher dart impact at equivalent density under ASTM D1709, but cost and supplier availability often differ. Published data for the optical properties of TF-Y826-CP in monolayer cast film is limited because the grade is usually combined with additive masterbatch that dominates surface haze.

    Thermal Degradation Pathways in Hexene-Copolymer Melt Processing

    Hexene LLDPE undergoes oxidative degradation through radical chain scission and crosslinking. The rate depends on oxygen partial pressure in the feed throat, melt temperature, and residence time. The phenolic stabiliser system in TF-Y826-CP is consumed slowly under normal processing but depletes rapidly above 280°C. On a 45 mm 30:1 L/D extruder running at 100 rpm, gel count can increase after 30 min of intermittent hot idle if the screw is not purged. A nitrogen blanket on the hopper and vacuum venting at -0.08 MPa reduce oxygen entrainment and stabilise melt quality. If gel counts measured by ASTM D2765 exceed 100 gels per m² in 25 µm film, melt temperature and screw speed should be reduced, and the screen pack should be inspected. Published data for TF-Y826-CP under extended run conditions is limited; the stated gel limit is derived from general hexene LLDPE cast-film processing practice rather than a manufacturer-reported failure threshold for this specific grade.

    If Regrind Ratios Exceed 20%, Oxidative Stability and Additive Partitioning Shift

    Post-industrial edge trim and roll scrap can be reintroduced into the core layer. At regrind ratios up to 20 wt%, melt index and density typically remain within lot-to-lot variation if the scrap is ground at low temperature and has low gel content. Repeated heat histories consume the residual antioxidant; the regrind fraction should be checked by melt flow rate after 3 passes. If the melt index increases by more than 15% relative to the virgin pellet, chain scission has occurred and the regrind should be rejected from critical film structures. When the scrap includes previously compounded skin layers, the regrind may carry slip or antiblock into the core; this changes interlayer adhesion and coefficient of friction in ways that are not captured by virgin resin data. Gravimetric blending with ±0.5% dosing accuracy is necessary to avoid layer-to-layer fluctuation. Published data for this specific grade under high-regrind conditions is limited; the allowable regrind ratio must be validated on the production line with final film property testing.

    Regulatory suitability for food contact must be confirmed against the supplier’s current compliance statement. Polyolefin films of this class are commonly evaluated under FDA 21 CFR 177.1520 and EU Regulation 10/2011; specific migration limits depend on the final film structure, food simulant, and contact time-temperature. The base resin does not contain a UV stabiliser package or antistatic additives; those functions require additional masterbatches. TF-Y826-CP should not be melt-blended with high-acid ionomers or high-level maleic anhydride grafted resins above 10 wt% because phase incompatibility can produce melt instabilities and reduce film toughness. The documented processing envelope is slot-die cast film; published data for blown-film and biaxially oriented film using this exact product is limited. Lot-to-lot variation in melt index, density, and additive residuals should be reviewed on the certificate of analysis before changing screw speed, die gap, or winder tension.

    Top