Nova Chemicals Novapol Tf Y826 Bp Hexene Lldpe Film Resin

NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 515964
    Productname NOVA Chemicals Novapol TF-Y826-BP Hexene LLDPE Film Resin
    Manufacturer NOVA Chemicals
    Resintype Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.926 g/cm3
    Meltindex 0.8 g/10 min
    Meltflowratio 30
    Meltingpoint 126 C
    Vicatsofteningpoint 104 C
    Tensilestrengthatyield 12.4 MPa
    Tensilestrengthatbreak 30.3 MPa
    Elongationatbreak 700%
    Dartimpact 220 g
    Elmendorftearmd 320 g
    Elmendorfteartd 480 g
    Haze 12%
    Gloss 60%
    Coefficientoffriction 0.2
    Blocking 50 g

    As an accredited NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin is packaged in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL container loading: NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin, 25 kg bags, palletized, 20 pallets, 27.5 MT.
    Shipping NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin is shipped as a non-hazardous solid in 25-kg polyethylene bags or 1,000-kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers at ambient temperature. Protect from moisture, direct sunlight, and heat. Handle pallets with forklift; follow local regulations.
    Storage Store Nova Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing agents. Keep original bags or containers tightly sealed, off the ground on pallets, and protected from moisture, dust, and contaminants. Maintain ambient temperature, follow FIFO inventory, and avoid prolonged UV exposure. Use clean handling practices to prevent contamination.
    Shelf Life Two years from date of manufacture when stored in original packaging in a cool, dry, well-ventilated area away from sunlight.
    Application of NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin
    Hexene linear low-density polyethylene with a nominal density of 0.926 g/cm³ (ASTM D792) and a nominal melt index of 0.8 g/10 min (ASTM D1238, 190°C/2.16 kg) is dry-blended with low-density polyethylene in heavy-duty industrial sack lines because monolayer bubble stability at gauge variations below 120 µm requires long-chain branching from LDPE to prevent melt resonance and bubble collapse. The formulation addition ratio is set between 70 wt% and 85 wt% TF-Y826-BP, with the balance an autoclave LDPE having a melt index of 0.25 g/10 min and density 0.923 g/cm³. Below 70 wt% TF-Y826-BP, machine-direction Elmendorf tear values measured under ASTM D1922 fall below the acceptance threshold for 25 kg chemical sacks, while above 85 wt% the bubble becomes susceptible to instability at blow-up ratios near 3.0:1 if die pressure exceeds 420 bar. Extrusion is performed on a grooved-feed single-screw extruder with 30:1 L/D ratio, 90–120 mm screw diameter, and a barrier screw with Maddock mixing section; the die is a spiral mandrel blown film die with die gap 1.8–2.2 mm and die diameter 350–450 mm. Melt temperatures are held at 205–220°C, blow-up ratio at 2.5:1–3.0:1, and frost line height at 700–900 mm above the air ring; these parameters preserve dart impact resistance in the 120–180 µm gauge range. Industry compliance for dangerous goods packaging uses UN 13H4 certification for FIBC liners and ISO 21898:2018 for flexible intermediate bulk containers; for sacks used in indirect food contact, FDA 21 CFR §177.1520(c) 3.2a and EU Regulation 10/2011 Annex I apply, with overall migration limits of 10 mg/dm². Terminal products include 25 kg chemical sacks, 50 kg fertilizer bags, FIBC liners at 100–150 µm gauge, and moisture-barrier liners for hygroscopic resin pellets.

    At What Blown Film Frost Line Does Low-Temperature Dart Impact Peak for Hexene LLDPE?

    Frozen food packaging line trials on a 3-layer coextrusion blown film line with a 250 mm spiral mandrel die and die gap 2.0 mm demonstrate a frost-line-height dependency: low-temperature dart impact measured under ASTM D1709 method A peaks at 450–600 mm frost line when the outer skin layer contains 65–85 wt% TF-Y826-BP, 10–20 wt% LDPE, and 5–15 wt% metallocene plastomer sealant resin. The formulation addition ratio is constrained by two competing failure modes—excessive plastomer above 15 wt% reduces bubble stability and creates blocking on the film roll, while TF-Y826-BP below 65 wt% lowers tensile elongation at -30°C to below 400% in production QC sampling. Extruder barrel profiles are set with a flat profile from 180°C to 210°C; the die is zoned at 205–215°C, and internal bubble cooling is used to achieve 180–220 kg/h output on a 350 mm die. Processing windows tolerate a maximum melt temperature of 220°C; above this, gel formation from oxidative degradation appears as specks in the film after 4 hours of continuous running. Compliance for frozen food direct contact includes EU Regulation 10/2011, FDA 21 CFR §177.1520, EC 1935/2004, and EN 1186-1:2002 total migration testing. Terminal products include 150–250 µm stand-up pouches for frozen vegetables, 60–100 µm lidding film for frozen ready meals, and 50 µm ice cream overwrap.
    Standard designationJurisdiction / scopeRelevant requirement or test method
    FDA 21 CFR §177.1520United States food-contact olefin polymersOlefin polymer specification for indirect additives; density and melt index define compliance class
    EU Regulation 10/2011European Union plastic food-contact materialsAnnex I authorized monomer list; overall migration limit 10 mg/dm²
    EC 1935/2004EU framework regulationArticle 3: no transfer of constituents that endanger human health
    EN 1186-1:2002EU migration test methodTotal migration testing in food simulants for plastics
    ASTM F88/F88M-21United States seal strength testHeat seal strength of flexible barrier materials; used for frozen food seal integrity
    When silage clamp covers require more than 12 months of UV weathering resistance under continuous outdoor exposure, tertiary blends containing 80–90 wt% TF-Y826-BP, 6–8 wt% carbon black masterbatch (nominal 40% carbon black carrier), and 4–10 wt% LDPE are coextruded as 150–250 µm three-layer films. The formulation addition ratio is selected to maintain a minimum carbon black content of 2.0–3.0 wt% in the final film, as required by EN 13206:2017 for silage films, and to avoid the brittleness that occurs when carbon black exceeds 3.5 wt% due to filler agglomeration and notch sensitivity. On the blown film line, a 3-layer spiral mandrel die with 2.2 mm die gap is operated at 210–230°C melt temperature and 3.0:1–3.5:1 blow-up ratio; the white outer layer contains TiO₂ at 8–12 wt% to reflect solar radiation and reduce surface temperature, while the black inner layer absorbs residual UV and prevents algae growth on the clamp surface. Pre-drying of carbon black masterbatch at 80°C for 4 hours is mandatory when RH exceeds 60%, because carrier resin moisture causes film porosity and delamination at layer interfaces. The downstream conversion includes a winding station with contact roll pressure 200–400 N/m and slitting to 8–16 m width; industry compliance includes EN 13206:2017, ISO 13426-1:2003 for soil burial strength retention, and REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons in carbon black. Terminal products include silage clamp covers, silage storage bags, and temporary forage preservation sheets.

    E-commerce Mailer Film Structures and Puncture-Propagation Resistance

    Coextruded mailer film produced with a core layer containing 50–70 wt% TF-Y826-BP exhibits puncture-propagation resistance measured under ISO 7765-1:2004 that is 18–25% higher than comparable butene-LLDPE structures at the same 70–100 µm gauge, and is specified for sharp-edged e-commerce contents such as polybags, plastic hangers, and metal hardware. The formulation addition ratio in the core layer is 50–70 wt% TF-Y826-BP, 20–30 wt% LDPE, and 10–20 wt% post-industrial recycled LLDPE; the outer layers use 20–35 wt% TF-Y826-BP blended with LDPE to maintain surface gloss and heat seal initiation below 110°C. The film is produced on a 3-layer blown film line with 300 mm die diameter, 2.0 mm die gap, 2.8:1 blow-up ratio, and melt temperature 200–215°C; output is typically 280–320 kg/h with a frost line height of 600–750 mm. Adding post-industrial recycled LLDPE above 20 wt% reduces dart impact measured under ASTM D5748-19 by more than 15% and causes visible gels that exceed customer acceptance thresholds of 10 gels/m² larger than 200 µm. Compliance for mailer films includes ISO 14021:2016 for recycled content claims, ASTM D5748-19 for dart impact, and ISO 7765-1:2004 for puncture resistance; if the mailer is used as a secondary food-contact barrier, FDA 21 CFR §177.1520 applies to the virgin layers. Terminal products include poly mailers, shipping pouches, and void-fill air pillow films.

    Collation shrink film demands a narrow melt-index window

    Collation shrink film for bottle and can multi-packs is produced on a double-bubble orientation line where the first bubble is quenched in water at 18–22°C and the second bubble is inflated at 100–120°C with machine-direction and transverse-direction draw ratios of 4:1 and 4:1, respectively. The formulation addition ratio uses 40–60 wt% TF-Y826-BP, 30–50 wt% LDPE with melt index 0.3 g/10 min, and 10–20 wt% butene LLDPE; this blend narrows the overall melt-index distribution and prevents draw resonance on the second bubble. Hexene LLDPE with 0.926 g/cm³ density contributes tear propagation resistance in machine direction and shrink tension uniformity, but if TF-Y826-BP exceeds 60 wt%, the film loses transverse shrink above 18% and becomes brittle along the cut edge. Extruder melt temperatures are 200–210°C for the outer layers and 210–225°C for the core; die gap is 1.8 mm on a 150 mm annular die. Compliance is tested under ASTM D2732-14 for free shrink, ISO 11501:1995 for shrink force, and ASTM D882-18 for tensile properties; food-contact collation for canned goods requires FDA 21 CFR §177.1520. Terminal products include collation shrink bundles for 6–24 packs of bottles, cans, and cartons, as well as tamper-evident banding films.In secondary containment geomembrane applications, hexene LLDPE grades with density 0.926 g/cm³ occupy a narrow performance band between flexible HDPE and EVA copolymers, where low-temperature impact brittleness and puncture resistance are more critical than tensile modulus. The formulation addition ratio for a thin blown geomembrane liner is 80–95 wt% TF-Y826-BP with 5–20 wt% carbon black masterbatch to achieve a minimum carbon black content of 2.0–3.0% as specified in GRI-GM17 for LLDPE geomembranes. Processing occurs on a large-diameter blown film line with a 400–600 mm annular die, die gap 2.5–3.0 mm, melt temperature 220–230°C, and blow-up ratio 2.0:1–2.5:1 to produce 0.5–1.0 mm thick sheet. The lower blow-up ratio is necessary because high-molecular-weight hexene LLDPE exhibits less strain-hardening than LDPE, and stretching the bubble to blow-up ratios above 2.5:1 creates transverse-direction tear values below 200 N/mm in ASTM D1004-21 testing. Compliance for geomembrane liners includes GRI-GM17, ASTM D6693-20 for tensile properties, ASTM D1004-21 for tear resistance, ASTM D4833-21 for puncture resistance, and EN 13493:2018 for landfill barriers. Terminal products include temporary containment liners, canal liners, secondary containment covers for chemical storage, and leachate collection liners.
    Free Quote

    Competitive NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Novapol® TF-Y826-BP is a hexene-1 comonomer-based linear low-density polyethylene film resin intended for blown film conversion. The grade is supplied as pellets and is positioned in the medium-density, medium-viscosity segment of industrial LLDPE materials, where stiffness, tear resistance, and bubble stability are required across thin-gauge structures. Supplier-published nominal data list a density of 0.926 g/cm³ measured under ASTM D792 and a melt flow rate of 0.80 g/10 min determined at 190 °C with a 2.16 kg load according to ASTM D1238. These values indicate a molecular weight and crystallinity range suitable for heavy-duty film applications in which conventional butene LLDPE may show lower puncture or tear resistance. The ethylene-hexene backbone incorporates n-butyl branches; at equivalent density and melt flow rate, this branch length produces a different crystalline network and tie-molecule population than ethylene-butene copolymers, which affects drawdown, dart impact, tear propagation, and long-term load retention. The resin is intended for monolayer and coextruded film conversion, subject to verification of the specific additive formulation and finished-article regulatory status.

    Table 1 — Supplier-reported nominal resin properties
    Property Nominal value Unit Test method
    Density 0.926 g/cm³ ASTM D792
    Melt flow rate 0.80 g/10 min ASTM D1238

    What separates hexene-based TF-Y826-BP from butene LLDPE and metallocene ethylene copolymers in film mechanics?

    Short-chain branching type controls lamellar thickness, branch exclusion from the polyethylene crystal, and the probability of tie-molecule formation between adjacent lamellae. Ethylene-butene copolymers introduce ethyl branches, while ethylene-hexene copolymers introduce n-butyl branches. The longer n-butyl branch is less readily accommodated within the crystalline lattice and can increase the concentration of load-bearing tie molecules at equivalent density and melt flow rate. In industrial film comparisons under ASTM D1709, Ziegler-Natta hexene LLDPE at constant density and melt index can show a 15–30% improvement in dart impact over ethylene-butene LLDPE. Under ASTM D1922, machine-direction and transverse-direction Elmendorf tear values are also directionally higher for hexene grades, although the magnitude is strongly influenced by film gauge, blow-up ratio, die gap, and crystalline orientation. Metallocene ethylene-hexene grades typically provide higher dart impact, lower haze, and improved puncture resistance under ASTM D5748 because of their narrower comonomer distribution and more uniform crystallinity; however, those same narrow-distribution characteristics can reduce bubble stability and raise extrusion pressure on grooved-feed blown film lines. TF-Y826-BP occupies a conventional Ziegler-Natta hexene position: the broader molecular weight distribution supports stable bubble formation and moderate head pressure while retaining a toughness advantage over butene copolymers at similar density and melt flow.

    Differences from other product categories are also observed in stiffness and thermal behaviour. Compared with low-density polyethylene, the linear backbone of TF-Y826-BP provides higher tensile yield and secant modulus when evaluated under ASTM D882, but lower optical clarity and lower melt strength. Compared with high-density polyethylene film grades, the 0.926 g/cm³ density reduces stiffness and moisture barrier but improves dart impact and tear resistance. These trade-offs make the resin more suitable for applications requiring puncture and tear performance than for applications requiring high modulus or low oxygen transmission. Published data for this specific configuration is limited beyond the supplier’s nominal resin properties and general hexene LLDPE film literature; converter trials are required to establish final film performance under actual production conditions.

    Extrusion response and thermal stability on grooved-feed blown film lines

    Industrial blown film conversion of this melt-flow class typically uses grooved-feed extruders with L/D ratios between 24:1 and 30:1, barrier screws, and screen packs of 80–120 mesh. Spiral mandrel dies with die gaps of 1.0–2.0 mm are common because they provide gauge control and pressure management for linear resins. Initial process settings for Ziegler-Natta hexene LLDPE generally include blow-up ratios of 2.0:1 to 3.0:1 and melt temperatures of 190–240 °C. Lower melt temperatures preserve bubble stability and reduce oxidation, while higher melt temperatures improve homogenization but can lower frost line height and destabilize the bubble if not compensated by internal bubble cooling. Frost line height should be controlled within ±5 °C of the established optimum through die temperature, air ring adjustment, and internal bubble cooling; failure to stabilise the frost line can produce gauge bands, blocky edges, or variation in impact resistance under ASTM D1709.

    Linear polyethylenes can exhibit sharkskin or melt fracture at high output rates, particularly when melt temperature is low or die land length is short. Where surface defects appear, converters may adjust melt temperature, increase die gap, reduce output, or evaluate polymer-processing aids. Because published product-specific rheological data for TF-Y826-BP is limited, torque, pressure transducer, and bubble geometry data from the production line are necessary to define the operating window. The resin is not considered hygroscopic; however, if pellets are stored at relative humidity above 60% and moved into a warmer production area, surface condensation may form and create pinholes or voids in the film. In such cases, drying at 70–80 °C for 2 h or use of dry-air hoppers can reduce surface moisture before extrusion.

    Applications described for hexene LLDPE resins of this density and melt flow range include heavy-duty sacks, industrial liners, can liners, agricultural film, and carry-out bags. In downgauging trials, converters frequently evaluate replacement of butene LLDPE at gauge reductions from 75 µm to 50 µm because the higher toughness of hexene copolymers can maintain load retention at reduced thickness. Replacement should not be based on resin properties alone; final package performance must be verified under ASTM D1709, ASTM D1922, ASTM D882, and the applicable transport simulation method. Seal strength, hot-tack, and seal initiation temperature should also be retested when the package is converted or coextruded, because density and comonomer type influence seal response.

    When hexene-based downgauging introduces stiffness, oxygen transmission, and seal initiation shifts

    Downgauging with a 0.926 g/cm³ hexene LLDPE changes more than dart impact and tear. Bending stiffness decreases with reduced gauge, even if the resin modulus remains constant. The secant modulus at 1% strain under ASTM D882 should be monitored on film samples because it affects handling, bag opening, and print registration. As gauge is reduced, oxygen transmission under ASTM D3985 increases almost proportionally for a given film structure. The resin is not a high-barrier material; if oxygen-sensitive contents require low transmission rates, a coextruded structure containing ethylene-vinyl alcohol, polyamide, or metallised substrate should be evaluated. Water vapour transmission under ASTM F1249 also increases with gauge reduction, although the 0.926 g/cm³ density provides lower moisture transmission than lower-density LLDPE film grades. Seal initiation temperature and hot-tack window can shift when hexene LLDPE replaces butene LLDPE because comonomer length and distribution affect melting and crystallization kinetics. Seal testing under ASTM F88 and hot-tack testing under ASTM F1921 are required to confirm packaging line performance, particularly for vertical form-fill-seal or horizontal form-fill-seal equipment running at high cycle rates.

    In coextruded structures, TF-Y826-BP can be placed in the skin or core layer depending on stiffness and seal requirements. When used as a core layer, its hexene toughness contribution can be combined with a metallocene plastomer seal layer to balance hot-tack and dart impact. When used as a skin layer, its antiblock behaviour and coefficient of friction must be verified because surface additives influence film-to-film slip, print adhesion, and bag opening. If slip or antiblock performance changes after masterbatch dilution, coefficient of friction should be measured under ASTM D1894 and haze under ASTM D1003 to confirm consistency with the converter’s normal production range.

    Regulatory status and additive compatibility boundaries remain process-limiting

    The base olefin polymer is generally covered under 21 CFR 177.1520 for direct food-contact use when the finished article meets the specified extractives limitations and end-use restrictions. Users are responsible for verifying that all additives in the commercial resin formulation comply with the relevant regional food-contact and packaging regulations. The resin should be stored in dry, dust-free conditions below 50 °C and away from direct sunlight. Blending with colour concentrates, recycle streams, or processing aids should be validated for melt flow rate, density, and additive interactions before full-scale production. Avoid combining the resin with amine-containing masterbatches unless compatibility is demonstrated, because interactions between amine additives and catalyst residues or oxidized polymer fractions can affect colour, odour, and organoleptic performance. Melt temperatures above 260 °C should be avoided unless the line is equipped with adequate venting and degradation control, because thermal breakdown may generate low-molecular-weight fragments that deposit on die surfaces and reduce film quality.

    Batch-to-batch variance in density and melt flow rate should be checked against the supplier certificate of analysis. Off-spec melt flow shifts can alter extruder pressure, bubble stability, and film gauge. Density shifts influence stiffness, barrier, and seal behaviour. When process instability appears, the first step is to verify incoming resin density and melt flow rate under ASTM D792 and ASTM D1238, followed by confirmation of extruder barrel temperatures, die temperatures, and air cooling settings. Film samples should then be tested for gauge distribution, dart impact under ASTM D1709, and Elmendorf tear under ASTM D1922 to separate resin variation from equipment drift. Published data for this specific configuration is limited outside the supplier’s reported nominal values and general industrial LLDPE film extrusion practice.