| HS Code | 661824 |
| Productname | NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Hexene |
| Meltindex | 0.8 g/10 min |
| Density | 0.922 g/cm³ |
| Meltflowratio | 30 |
| Tensilestrengthatyieldmd | 1500 psi |
| Tensilestrengthatyieldtd | 1500 psi |
| Tensilestrengthatbreakmd | 4500 psi |
| Tensilestrengthatbreaktd | 4000 psi |
| Elongationatbreakmd | 600 % |
| Elongationatbreaktd | 700 % |
| Dartimpactf50 | 250 g |
| Elmendorftearmd | 250 g/mil |
| Elmendorfteartd | 500 g/mil |
| Haze | 12 % |
| Gloss45 | 55 |
| Coefficientoffriction | 0.20 |
| Vicatsofteningpoint | 100 °C |
| Meltingpoint | 124 °C |
As an accredited NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | The resin is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL: NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin in 25 kg bags, palletized, stretch-wrapped, and secured for ocean shipment. |
| Shipping | NOVA Chemicals Novapol® TF-Y822-CP is shipped as non-hazardous polyethylene resin pellets in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars. Keep packages dry, clean, and away from heat and contamination. It is not regulated for transport under DOT, IMDG, or IATA. Handle with care to avoid bag damage. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed, on pallets, off the floor, and protect from moisture, dust, and contamination. Avoid prolonged high temperatures, UV exposure, and static buildup. Use first-in, first-out rotation and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 12 months from manufacture when stored in unopened original packaging in a cool, dry, well-ventilated area. |
On high-speed cast film lines producing 12–23 µm machine stretch web, the hexene comonomer branch distribution in Novapol® TF-Y822-CP reduces the melt’s tendency to draw-resonant oscillation compared with butene LLDPE at equivalent melt index, allowing a stable chill-roll window at air gaps between 60 mm and 100 mm. Compliance documentation for this segment is aligned to FDA 21 CFR 177.1520(c) 3.1a for olefin polymers and EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² when the film is supplied as a direct food-contact wrap or as a primary packaging component; mechanical release and load retention are tested under ASTM D5458 for peel cling, ASTM D5748 for protrusion puncture resistance, and ASTM D882 for tensile elongation at break. In monolayer machine-film formulation, TF-Y822-CP is introduced at 70–85 wt% as the load-bearing phase, with 10–25 wt% metallocene LLDPE for machine-direction tear uniformity and 1.0–3.5 wt% cling masterbatch for controlled cling force; in three-layer A/B/C structures, the TF-Y822-CP-rich core can carry 65–80 wt% of the total web while the skins contain slip and cling packages to separate unwind and cling surfaces. Downstream conversion uses a single-screw extruder with L/D ≥ 30:1, a barrier screw, and a low-shear Maddock mixer; barrel set points range from 190°C in the feed zone to 245°C at the metering zone, with melt temperature held at 232–260°C, die gap set at 0.55–0.70 mm, chill-roll temperature maintained at 18–25°C, and winding tension taper controlled at 10–40% to prevent roll blocking. Field observations from cast film lines show that melt temperature excursions above 260°C accelerate die-lip buildup and cling force drift, while air gaps above 100 mm can increase edge neck-in and reduce transverse gauge consistency. Published production-scale data for 23 µm machine film at pre-stretch above 275% remain limited; the stated operating bands are therefore drawn from industrial hexene LLDPE cast-film lines with equivalent melt-index and density envelopes. Terminal product types include machine stretch film, power pre-stretch film, and hand pallet wrap in thicknesses from 8 µm to 30 µm.
| Property | Test method | Typical specification window |
|---|---|---|
| Tensile elongation at break, machine direction | ASTM D882 | ≥ 400% |
| Protrusion puncture force | ASTM D5748 | ≥ 3.0 kg |
| Peel cling force | ASTM D5458 | 100–250 g |
| Dart impact, Method A | ASTM D1709 | ≥ 150 g |
The freezer-grade packaging sector evaluates the sealant web after vacuum and zipper conversion under ASTM F88/F88M for seal strength and ISO 527-3:2018 for tensile properties, while the resin’s olefin-polymer compliance is reviewed under FDA 21 CFR 177.1520(c) 3.1a and EU Regulation 10/2011 when the film contacts fatty foods at sub-zero temperatures. The hexene branch length in TF-Y822-CP disrupts short-chain regularity, lowering the brittle temperature and preserving dart impact in frozen storage without requiring an excessive slip package. In three-layer blown-film formulations, TF-Y822-CP is introduced at 55–75 wt% in the core or outer skins, blended with 15–25 wt% high-pressure LDPE for melt strength and 10–20 wt% mLLDPE for low-temperature dart impact; slip and antiblock masterbatches are maintained at 500–1500 ppm to prevent blocking without contaminating seal initiation. The downstream process is blown-film coextrusion through a 1.8–2.5 mm die gap at a blow-up ratio of 2.5:1–3.5:1, with melt temperature held between 190°C and 220°C and frost-line height controlled to balance quench rate and MD/TD dart impact; internal bubble cooling is necessary when line output exceeds 200 kg/h on 70–80 mm extruders. Amide slip above 1500 ppm in the sealant layer can raise seal initiation temperature and contaminate zipper anvils; sealant-layer slip is therefore limited to 1200 ppm maximum in most frozen-food constructions. Terminal products include frozen vegetable pouches, ice bags, seafood pouches, and poultry packaging with zipper closures in the 40–100 µm gauge range.
Agricultural silage and bale wrap conversion requires a hexene comonomer distribution that maintains dart impact and tear resistance after repeated mechanical stretching over irregular bale surfaces. Compliance in this sector is less dependent on direct food-contact regulation but is anchored to EN 13207:2018 for silage films and REACH Regulation (EC) No 1907/2006 for UV stabilizer masterbatch registration. The formulation places TF-Y822-CP at 80–95 wt% in monolayer or five-layer film structures, with 5–15 wt% high-pressure LDPE for bubble stability, 1–3 wt% UV stabilizer masterbatch, and 1–2 wt% carbon black or white colorant masterbatch depending on solar exposure. Blown-film conversion for silage wrap uses 70–90 mm extruders with a 200–300 mm die, blow-up ratio of 2.0:1–3.0:1, melt temperature 205–235°C, and film gauge 25–50 µm; the high dart impact and tear resistance at field wrap speed are checked by ASTM D5748 for puncture and ASTM D1922 for propagation tear. Post-consumer recyclate should be avoided in this segment because inconsistent UV packages can create split propagation in the stretched wrap and compromise bale sealing. Terminal product types include round-bale silage wrap, bale net replacements, silage clamp top covers, and greenhouse side sheets where puncture resistance against hail and mechanical handling is the dominant specification.
In heavy-duty blown film, the film web’s dart impact and tear resistance are governed more by die gap and frost-line geometry than by resin selection alone, and production-scale trials on 80 mm grooved-feed extruders indicate that a die gap below 2.0 mm can produce orientation-induced pinholes in the film because the hexene LLDPE has lower melt elasticity than high-pressure LDPE. Compliance for this segment is anchored to ASTM D4976 for polyethylene molding and extrusion materials, ASTM D1709 Method B for dart impact, ASTM D1922 for Elmendorf tear, ISO 527-3:2018 for film tensile properties, and EN 13592:2017 for plastics sacks for waste collection. TF-Y822-CP is the primary resin at 85–100 wt% in monolayer structures, with 0–15 wt% high-pressure LDPE for melt stability and 2–4 wt% carbon black masterbatch for UV and light shielding; closed-loop edge trim at 5–15 wt% is used only when the trim is from the same product family to avoid incompatible recycle contamination. Blown-film conversion uses a 70–90 mm extruder with L/D 24–30, die gap 2.0–3.0 mm, blow-up ratio 2.2:1–3.0:1, melt temperature 200–225°C, and film thickness 60–125 µm; line output typically ranges from 150 kg/h to 250 kg/h depending on die diameter and internal bubble cooling. Die-gap settings below 1.8 mm are not recommended for gauge levels above 90 µm because the reduced relaxation time in the bubble cone can create localized thickness thinning and dart impact loss. Terminal product types include construction debris bags, industrial can liners, heavy-duty agricultural sacks, and box liners for FIBC-grade transport.
Extrusion lamination of woven polypropylene substrates at line speeds above 120 m/min brings a separate process boundary: neck-in and draw resonance restrict the thickness reduction that can be achieved with a pure hexene LLDPE melt, so processors blend TF-Y822-CP with high-pressure LDPE to raise elongational viscosity and stabilize the melt curtain. The food-contact status for laminated woven sacks follows 21 CFR 177.1520 for the polyolefin layer and the overall migration requirements of EU Regulation 10/2011 when the lamination is the food-contact surface; adhesion performance is tested by T-peel on ASTM D1876 and seal strength by ASTM F88/F88M. Formulation ratios for this segment place TF-Y822-CP at 60–85 wt%, high-pressure LDPE at 15–40 wt%, and optionally 2–5 wt% adhesion promoter masterbatch for metallized or coated substrates; coat weight is maintained at 15–25 g/m². Downstream conversion uses a 90–120 mm extruder with L/D 30:1, melt temperature 260–300°C, die gap 0.5–0.8 mm, air gap 150–250 mm, and corona treatment of the woven substrate at 38–42 dyn/cm before lamination. Chlorinated primers should be avoided with this polyolefin film because adhesion loss can occur under tropical storage conditions. Terminal products include coated woven fertilizer sacks, pet food bags, mineral and cement sacks, and tarpaulin lamination webs.
When pallet loads are consolidated for long-haul distribution, a blown-film stretch hood must retain elastic recovery in the transverse direction after being stretched over the load corners; TF-Y822-CP is compounded in a three-layer blown film with 70–85 wt% in the core, 10–20 wt% mLLDPE in the skins for tear resistance, 5–10 wt% high-pressure LDPE for process stability, and slip/antiblock masterbatch at 500–1200 ppm. Compliance is evaluated under ASTM D5459 for machine direction and cross-machine direction elastic recovery and permanent deformation, and ISO 7765-1 for free-falling dart impact resistance. Blown-film conversion uses high-stalk bubble geometry with a 2.0–2.5 mm die gap, blow-up ratio 2.5:1–3.5:1, melt temperature 210–230°C, internal bubble cooling, and automatic gauge control to maintain thickness consistency across the hood circumference. Slip loading above 1200 ppm is not recommended because the reduced coefficient of friction can allow pallet load shifting during transportation. Terminal product types include stretch hoods for beverage pallets, building materials, appliances, and bagged chemical goods.
Competitive NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® TF-Y822-CP is a hexene-based linear low-density polyethylene film resin with a nominal melt index of 0.80 g/10 min when tested under ASTM D1238 at 190 °C with a 2.16 kg load and a nominal density of 0.922 g/cm³ when tested under ASTM D792. The resin is produced via solution-phase ethylene-hexene copolymerization, and the hexene comonomer introduces short-chain branches of 4 carbon atoms along the polyethylene backbone. This branch length is the first structural variable separating the grade from butene-based LLDPE, because a C4 branch interrupts lamellar crystallization more effectively than a C2 branch. The resulting changes in tie-molecule population, crystalline thickness, and melt relaxation behavior control tear, puncture, and gauge uniformity in finished film. The values cited are supplier-published representative data points and are not contractual release limits.
At an equivalent density, a hexene-based LLDPE contains a lower molar fraction of comonomer than a butene-based resin of the same crystallinity, because the longer C4 branch excludes more backbone contour length from the growing lamella. The tie-molecule probability increases when chains cannot easily fold into one crystal and are instead incorporated into adjacent lamellae; this is the structural basis for the improvement in dart impact and slow tear propagation often observed in hexene grades. The effect is not a fixed material constant. It is influenced by molecular weight distribution, comonomer distribution, cooling rate, and film gauge. In a 25 µm film, the dart impact result under ASTM D1709 Method A can change substantially when the same resin is run at a different frost-line height or die gap. Published data for this specific configuration is limited; therefore, a converter should generate film-property data on the target line rather than relying on a single datasheet value. The density of 0.922 g/cm³ also places the resin at the denser end of the conventional LLDPE film range, so the film’s secant modulus, bag stiffness, and water vapor transmission rate must be evaluated at the gauge at which the converter intends to run.
In blown film conversion, the 0.80 g/10 min melt index class is typically run on single-layer or coextruded air-cooled lines with die gaps between 1.5 mm and 2.5 mm and blow-up ratios between 2.0:1 and 2.5:1. Melt temperatures between 200 °C and 240 °C are commonly used, but the barrel profile must be set to avoid upstream solids-conveying starvation and downstream overheating in the spiral mandrel die. The resin is not hygroscopic, so desiccant drying is generally unnecessary for the neat pellet; however, at relative humidity above 60%, condensation on cold pellet surfaces drawn from outdoor silos should be avoided because localized surface moisture can affect film optics and feed consistency. Screen packs around 80/120/80 mesh are used on many general-purpose polyolefin lines, but the pressure drop is line-specific. When switching from a butene grade, the pressure at the breaker plate may shift even if the melt index is unchanged, because the longer branch can alter shear viscosity at the same low-shear flow. Operators should monitor gear pump inlet pressure, die pressure, motor load, and bubble frost-line height as indirect indicators of viscosity differences.
The practical difference between a conventional Ziegler-Natta hexene LLDPE and a metallocene ethylene-hexene LLDPE is not fully visible in a melt index or density table. Ziegler-Natta resins often possess a broader composition distribution and a broader molecular weight distribution, which can produce greater shear thinning and lower head pressure through a long spiral mandrel die. Metallocene resins typically distribute comonomer more uniformly along the polymer chain, which can improve clarity and reduce the heat-seal initiation temperature but may raise torque and make the bubble more sensitive to air-ring instability. If a converter replaces a metallocene grade with TF-Y822-CP, the line must be re-profiled rather than simply adjusted at the haul-off. The die-lip heater setpoints, screen pack, and winder tension are all part of the conversion envelope. Conversely, if a converter replaces a butene grade with this hexene resin, the modified melt relaxation may require a slightly higher frost line to reduce differential MD/TD shrink and to prevent periodic gauge oscillation. These are production-scale equipment interactions, not inherent defects of the resin.
For an unbiased comparison among butene, hexene, and octene LLDPE, the evaluation should be performed at a fixed film gauge, typically 25 µm or 50 µm, using the same die, same blow-up ratio, same frost-line position, and same masterbatch. Under those conditions, hexene grades usually show higher dart impact and Elmendorf tear values than butene grades of equivalent density and melt index, but the magnitude is influenced by the concentration and distribution of the comonomer. Octene grades, with a 6-carbon branch, generally extend the impact resistance further, but they are processed at a different economics and may exhibit lower melt strength in some film towers. The difference between hexene and octene is not simply twice the butene-to-hexene increment, because lamellar exclusion, tie-molecule formation, and melt-state stress relaxation are nonlinear functions of branch length. A converter should therefore run a minimum of 30 dart drops per condition under ASTM D1709 and 30 tear specimens per direction under ASTM D1922 before assigning a final ranking. Without that level of repeated measurement, the natural scatter in blown film data can exceed the expected comonomer advantage.
Butene comonomer yields a C2 branch, hexene yields a C4 branch, and octene yields a C6 branch. A longer branch is more strongly excluded from the orthorhombic polyethylene lattice, so the crystalline lamella is thinner at the same density and the distribution of tie molecules is altered. However, catalyst and reactor design determine whether the comonomer is placed in the lower- or higher-molar-mass fractions. A conventional Ziegler-Natta hexene resin may have a different intermolecular composition distribution than a metallocene hexene resin, which is why the branch length alone does not establish a performance hierarchy. The nominal density of 0.922 g/cm³ in TF-Y822-CP gives a higher room-temperature modulus and a lower water vapor permeability than a 0.918 g/cm³ film resin, but it also places greater demand on impact resistance. The melt index class is selected to maintain bubble stability at useful output rates; fractional-melt resins can produce higher impact but require excessive head pressure, while high-melt-index resins lose bubble strength. This is the central processing trade-off for this grade.
Film property translation from resin data to a specific package requires a production-scale trial at the target gauge and line speed. A typical qualification protocol includes tensile measurements under ASTM D882, dart impact under ASTM D1709, and Elmendorf tear under ASTM D1922, plus haze and gloss measurements under ASTM D1003 and ASTM D2457. Because the same resin can produce different dart impact values on two air-cooled lines with identical melt temperatures but different die mandrel diameters and air-ring geometries, the conversion line is part of the performance equation. The resin’s density of 0.922 g/cm³ and melt index of 0.80 g/10 min define a starting window; they do not replace a statistically symmetrical split-run evaluation.
| Property | Unit | Test method | Supplier-listed value |
|---|---|---|---|
| Melt index | g/10 min | ASTM D1238 | 0.80 |
| Density | g/cm³ | ASTM D792 | 0.922 |
| DSC peak melting endotherm | °C | ASTM D3418 | 120–124 |
Compliance for a polyethylene film resin is not established by the polymer backbone alone. The supplier must provide a written declaration for the specific grade and additive package, and the converter must carry the final article through the applicable end-use extraction or migration assessment. In the United States, olefin polymers are commonly evaluated under 21 CFR 177.1520(c), but the paragraph includes extraction limits and formulations that must be confirmed for the final article. In the European Union, plastic food-contact materials are assessed under (EU) 10/2011, where the overall migration limit is 10 mg/dm² for most film and sheet geometries, or 60 mg/kg for certain container applications. Additives such as slip agents, antiblock minerals, antioxidants, and neutralizers require separate specific migration limits. REACH under EC 1907/2006 does not apply registration duties to the polymer itself, but monomers and other substances above threshold may require registration or notification. A converter’s addition of color concentrates or processing aids not covered by the resin supplier’s declaration creates a new food-contact compliance obligation for the final package.
Downstream converting operations add another layer of qualification. If the film is printed, the surface treatment level and the slip/antiblock package affect ink adhesion and coefficient of friction. If the film is used in a form-fill-seal machine, the heat-seal dwell time, temperature, and jaw geometry, not the resin density alone, determine the seal window. For lamination, the interaction between the film’s low-molecular-weight extractables and the adhesive or solvent must be assessed. These application-specific demands sit outside the base resin certificate of analysis and require converter-owned data. Published data for this specific configuration is limited.
| Regulatory or standard reference | Scope | Converter data request |
|---|---|---|
| 21 CFR 177.1520(c) | Olefin polymers in U.S. food-contact articles | Supplier compliance statement for the grade and listed additives; extraction limitations. |
| (EU) 10/2011 | Plastic food-contact materials and articles in the EU | Overall migration verification; specific migration limits for additives; conditions of use. |
| EC 1907/2006, Article 33 | REACH communication of SVHCs in articles | SVHC concentration declaration for substances above 0.1% w/w. |
| 2011/65/EU | RoHS electrical and electronic equipment scope | Base polyolefin usually outside scope; verify additives and colorants. |
Substitution of this hexene resin into a structure previously made from a butene grade should therefore be treated as a conversion engineering change rather than a drop-in replacement. The appropriate response is a controlled split run at constant die gap, blow-up ratio, and frost-line height, followed by film testing above the minimum statistical sample size. Any performance statement has meaning only when it is tied to that specific film line, the measured film thickness profile, and the exact test method designation.