Nova Chemicals Novapol Tf Y534 Ip Hexene Lldpe Film Resin

NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 696189
    Product Name NOVA Chemicals Novapol TF-Y534-IP Hexene LLDPE Film Resin
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Density 0.918 g/cm3
    Melt Index 1.0 g/10 min
    Melt Flow Ratio 30
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield MD: 11 MPa; TD: 11 MPa
    Tensile Strength At Break MD: 34 MPa; TD: 30 MPa
    Elongation At Break MD: 700%; TD: 800%
    1 Secant Modulus MD: 220 MPa; TD: 240 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength MD: 400 g; TD: 600 g
    Haze 12%
    Gloss 60%

    As an accredited NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging for NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin: 25 kg polyethylene bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) Container Loading (20′ FCL): 20 pallets, 25 kg bags, 27,500 kg NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin, securely lashed.
    Shipping NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin is shipped as non-hazardous solid pellets in 25-kg polyethylene bags, stacked on pallets and stretch-wrapped, or in bulk trucks/railcars. Store in a cool, dry area, away from heat and moisture, and handle with standard industrial hygiene.
    Storage Store in a cool, dry, well-ventilated warehouse in original sealed packaging, palletized and protected from moisture, direct sunlight, heat, sparks, and flames. Avoid contamination with dust, odors, or incompatible materials. Maintain moderate temperatures, avoid prolonged outdoor storage, and follow good housekeeping, spill cleanup, local regulations, and SDS recommendations. Keep away from ignition sources and oxidizers. Use first-in, first-out stock rotation.
    Shelf Life Typically 24 months from manufacture when stored in unopened original packaging, cool, dry, and away from direct sunlight.
    Application of NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin

    Extruded on 60–90 mm grooved-feed blown-film lines with L/D ratios of 24:1–30:1, Novapol® TF-Y534-IP hexene LLDPE is processed at a melt temperature of 199–232 °C and a die-gap setting of 1.5–2.3 mm for heavy-duty sack and industrial liner constructions. Blown-film bubble stability for the resin, which has a density above 0.930 g/cm³ per ASTM D792 and a melt index below 1.0 g/10 min per ASTM D1238, is maintained at blow-up ratios of 2.0:1–3.0:1, with frost-line height set at 320–520 mm. In monoextruded 40–80 µm sacks, blending 6–12 wt% high-pressure LDPE with a melt index of 0.25–0.45 g/10 min improves melt strength, while 1.5–3.0 wt% slip masterbatch and 2.5–5.0 wt% antiblock masterbatch prevent blocking in wound rolls. Mechanical release criteria for a 60 µm film generally fall into a dart impact band of 180–260 g under ASTM D1709 Method A and an MD tear minimum of 28 g/µm under ASTM D1922, but grade-specific acceptance values must be confirmed from the supplier data sheet because published independent test data for this configuration is limited. When the sack is used for food-grade resin, salt, or sugar, the film must be manufactured under 21 CFR 177.1520(c) 3.2a or Regulation (EU) No 10/2011 with overall migration below 10 mg/dm². On 70 mm grooved-feed extruders, pellet inlet temperature below 10 °C is associated with melt-pressure swings of ±8–12%; pre-warming pellets to 25–35 °C reduces motor-load fluctuation and improves gauge uniformity. Surface printing for 25 kg resin, fertilizer, and chemical powder sacks is carried out after corona treatment at 38–42 mN/m, with flexographic press speeds of 60–80 m/min.

    What Blend Ratios Preserve Puncture Resistance in Silage Cover Film?

    For silage clamp covers and temporary bunker liners, puncture resistance during compaction by heavy tractor traffic and long-term UV stability determine whether the hexene LLDPE is used as the core layer or as the outer black layer. The resin is incorporated in a three-layer coextruded construction at a total thickness of 180–250 µm and widths up to 16 m. The outer black layer is loaded with 2.0–3.5 wt% carbon black and 0.20–0.50 wt% HALS UV stabilizer, while the white layer contains 10–15 wt% white masterbatch to reduce surface temperature. In the core layer, 55–70 wt% Novapol TF-Y534-IP is blended with 20–30 wt% lower-density PE and 5–10 wt% black or white masterbatch; the precise ratio is adjusted because high carbon black loading raises melt viscosity and can destabilize the bubble at blow-up ratios above 2.5:1. Extrusion conditions include a die gap of 2.0–2.4 mm, melt temperature of 185–210 °C, and internal bubble cooling to maximize frost-line distance. Compliance is assessed under EN 13206:2017 for agricultural and horticultural covering films; mechanical properties include puncture resistance tested by a slow puncture method, while UV resistance is verified through artificial weathering cycles. 3–6 wt% of a processing-aid masterbatch is added when the line is run at output rates above 300 kg/h because high backpressure at the die can exceed 30 MPa. The finished product is used as a single-season silage cover, clamp lining, or temporary bunker cover; extended outdoor exposure beyond 18–24 months requires additional UV stabilizer loading and is not covered by standard formulations. Published data for this specific resin in silage cover configurations is limited, so full qualification under the intended weathering regime is required.

    Below -20 °C, low-temperature ductility of a 50 µm monolayer web determines whether pinholing develops during case packing and distribution of frozen vegetables, seafood, and bakery items. In three-layer coextruded frozen-food film, the sealant layer contains 60–80 wt% of this hexene LLDPE blended with 20–40 wt% of an mLLDPE or LDPE with a melt index below 1.0 g/10 min, allowing seal initiation at 105–120 °C without sacrificing dart impact. Blown-film process settings include a die gap of 1.2–2.0 mm, blow-up ratio of 2.0:1–2.8:1, and melt temperature of 190–225 °C; internal bubble cooling is recommended above 100 kg/h output. Frozen-condition dart impact per ASTM D1709 Method A after 24 h conditioning at -20 °C is typically specified in the range 130–200 g for 50 µm films, but grade-specific acceptance values must be confirmed because resin data for frozen-storage configurations is limited. Film haze at 50 µm is generally above 10–15%, which limits use in high-clarity applications. Compliance for food contact is governed by 21 CFR 177.1520(c) 3.2a in the United States and Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² in the European Union. The following matrix summarizes the principal compliance statements for frozen-food packaging using this resin.

    JurisdictionReferenceRelevant requirementTypical verification
    United States21 CFR 177.1520(c) 3.2aOlefin polymers for food contactEnd-test total volatiles and n-hexane extractives per 21 CFR 177.1520(d)(3)
    European UnionRegulation (EU) No 10/2011Overall migration limit 10 mg/dm²Migration testing per EN 1186-1:2002
    ChinaGB 9685-2016Additive positive listMigration testing per GB 31604.1

    High-Stiffness Core Layers in Coextruded Industrial Liners

    In three-layer industrial drum liners and FIBC liner sleeves, a 20/60/20 layer-thickness distribution places the higher-density hexene LLDPE at the film skins where flexural modulus and abrasion resistance are needed, while an mLLDPE core with a melt index of 0.5–1.0 g/10 min limits crack propagation and maintains dart impact. The outer layers contain 50–70 wt% Novapol TF-Y534-IP blended with 20–30 wt% LDPE and 6–10 wt% white or carbon black masterbatch; calcium carbonate or barium sulfate filled masterbatches at 5–15 wt% are sometimes added for opacity but should be limited because filler reduces dart impact and can generate gel particles. Extrusion is carried out on three-layer blown-film lines with 50/60/50 mm extruder configurations and a 250–350 mm die diameter; total output ranges from 250–400 kg/h. A die gap of 2.0–2.5 mm and a blow-up ratio of 2.0:1–2.6:1 are set to avoid interlayer gauge variation above ±6%, which can create blocking in 200 µm liners. Heat seal strengths of the inner layer are tested under ASTM F88, while tensile yield and elongation are evaluated per ISO 527-3. Production-scale lines exhibit batch-to-batch variation in melt index of ±0.05 g/10 min; seal-bar temperature is adjusted by 5–10 °C when switching between production lots. Finished articles include 500–1000 kg FIBC liners, drum liners for viscous chemicals, and box dump-bin liners. Full chemical compatibility with the intended fill product must be tested according to the distributor's immersion procedure.

    High-speed form-fill-seal packaging of cementitious powders at 40–70 bags/min imposes a seal-bar dwell time of 180–350 ms, which demands hot-tack performance that survives product contamination at the seal area. In this configuration, 70–90 wt% of the hexene LLDPE is blended with 10–30 wt% LDPE or mLLDPE, and the film is produced as a 60–100 µm mono or coextruded web with a die gap of 1.5–2.2 mm. Seal temperature is set between 125–160 °C and sealing force is maintained at 0.3–0.6 N/mm²; hot-tack force is quantified per ASTM F1921 and heat-seal strength per ASTM F88. At machine speeds above 80 bags/min, dwell time falls below 150 ms, and seal strength can drop below the required release limit; for such lines, the resin is typically blended with a higher melt index mLLDPE to increase seal-bar wetting. The film is used for 5–25 kg bags of non-hazardous cement, gypsum, and polymer powders; where UN certification is required, the final sack construction must pass the drop and leak tests under the applicable UN packaging code. Extruder backpressure on 60 mm grooved-feed machines increases when the blend contains more than 15 wt% LDPE, requiring screw speeds to be reduced by 10–15 rpm to hold melt temperature below 232 °C. Inclusion of 3–5 wt% antiblock masterbatch is mandatory for high-speed bag feeding because film-to-metal friction must remain low; erucamide slip is limited to 800–1500 ppm in the skin layer to avoid seal contamination.

    When Hexene LLDPE Replaces LDPE in Sealant Webs for Woven Sack Lamination

    For woven polypropylene sacks used with pet food, birdseed, and fertilizer, a blown-film sealant web of 20–40 µm is thermal-laminated to the woven substrate. Replacing LDPE with a blend containing 55–70 wt% Novapol TF-Y534-IP and 30–45 wt% LDPE reduces seal initiation to 105–120 °C, while the higher-density hexene component improves abrasion resistance and stiffness. The film is extruded on a monolayer blown-film line with a die gap of 1.0–1.5 mm, blow-up ratio of 2.0:1–2.5:1, and melt temperature of 190–220 °C. Lamination is performed on a thermal laminator with chill-roll temperatures of 120–150 °C and nip pressure of 4–6 N/mm²; line speed is typically 30–60 m/min for 900 mm web widths. Because the melt index of this resin is below 2 g/10 min, it is not intended for direct extrusion coating where draw-down at >150 m/min requires melt indices in the 4–15 g/10 min range. Food-contact compliance for pet food and birdseed applications follows 21 CFR 177.1520(c) 3.2a and Regulation (EU) No 10/2011, with migration testing conducted under EN 1186-1:2002. Seal-strength values after lamination are tested per ASTM F88; a 30 µm web typically requires a minimum seal initiation plateau of 12–18 N/25 mm at 130 °C, but exact curves for this resin should be generated on the specific lamination line because published comparative data is limited.

    Reinforced scrim laminates for temporary worksite barriers and vapour retarder composites convert the film into a 200–300 µm construction membrane by embedding a 10 × 10 or 14 × 14 per 100 mm HDPE scrim between two films that contain 70–85 wt% of the hexene LLDPE and 15–30 wt% of a lower-density LLDPE or LDPE blend. The film layers are extruded at a die gap of 2.2–2.8 mm and a blow-up ratio below 2.2:1 because excessive orientation reduces tear propagation resistance in the final composite. Lamination is performed by heated calendering at 130–160 °C with nip pressure of 5–8 N/mm²; the finished membrane is tested for water vapor transmission per ASTM E96 and tensile grab strength per ASTM D5034. In applications where flame propagation resistance is specified, the base resin is not inherently flame retardant and requires 18–25 wt% of a halogenated or phosphorous-based flame-retardant masterbatch; halogenated additives can generate corrosive degradation products at processing temperatures above 220 °C, so extrusion temperature must be held in the range of 180–205 °C when these additives are present. The finished articles are used as temporary construction dust barriers, scaffold sheeting, and low-permeability underlayments in industrial containment areas. The effect of flame-retardant loading on dart impact is severe; a 18 wt% loading can reduce ASTM D1709 impact by 30–50% compared with an unfilled film of the same gauge, so mechanical acceptance must be revalidated on the target production line.

    Free Quote

    Competitive NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Specification of the resin as NOVA Chemicals Novapol® TF-Y534-IP places it within the hexene linear low-density polyethylene film class. The nominal resin density is 0.918 g/cm³ measured by ASTM D1505; the nominal melt index is 1.0 g/10 min at 190 °C/2.16 kg by ASTM D1238. The material is formulated for blown and cast film converting. The 1-hexene comonomer contributes a short-chain branch length of C4, longer than the C2 branch of butene copolymers and shorter than the C6 branch of octene copolymers. This branch length alters crystallite thickness distribution, tie-chain probability, and orientation behavior. Published independent data for the exact additive package in the IP modification are limited; the manufacturer’s technical data sheet remains the authoritative source for nominal lot-to-lot values.

    What Distinguishes a Hexene Copolymer from Butene and Octene Resins in Film Applications?

    Short-chain branching in 1-hexene LLDPE creates tie-chain concentrations that raise Elmendorf tear and dart impact without the same loss of stiffness observed when density is reduced in butene copolymers. Comparative studies in polymer-package literature indicate that at an equivalent density of 0.918 g/cm³ and melt index of 1.0 g/10 min, a hexene film grade typically produces a machine-direction Elmendorf tear strength by ASTM D1922 that is 20–40% higher than a butene grade, while dart impact by ASTM D1709 Method A is 15–30% higher. The difference is attributable to the longer short-chain branch length of hexene compared with butene; this changes the radius of gyration of the chains and the probability of bridging adjacent crystals.

    Octene-based LLDPE can provide higher toughness at similar density, but the higher comonomer molecular weight and molar acquisition cost reduce its competitiveness in thin-gauge industrial packaging. Hexene grades are therefore positioned between butene and octene in the toughness-cost continuum. In multi-trip heavy-duty sacks and industrial liners, that balance is often used to reduce film gauge while retaining tear resistance. Conversely, for applications requiring maximum clarity and high gloss in cast film, an octene copolymer or a metallocene-catalyzed product may offer more favorable optical performance. The selection is generally determined by the gauge-normalized tear requirement and the target coefficient of friction after additive migration.

    Because the hexene branch reduces secondary crystallization during post-extrusion aging, film property retention after storage can differ from butene film. In comparative aging studies on 25 µm blown film stored at 40 °C for 14 days, hexene LLDPE usually retains a greater proportion of initial dart impact by ASTM D1709 than butene LLDPE of equivalent density. This aging behavior is relevant for packaging that remains in warehouse storage before filling.

    On a monolayer blown-film line equipped with a 25:1 L/D single-screw extruder, a screw with a Maddock mixing section or spiral mixer improves melt-temperature uniformity for this hexene LLDPE. Typical zone temperatures begin at 150 °C in the feed section and increase to 210 °C at the adapter, with die temperatures of 210–230 °C. The melt is processed at a blow-up ratio of 2.0:1–3.0:1 and a die gap of 1.0–2.0 mm. Bubble stability is affected by frost line height; a frost line above 400 mm from the air ring can increase transverse-direction shrinkage and reduce tear symmetry. The extruder back pressure in a 100 mm die should remain below 35 MPa to avoid melt fracture. These are representative processing conditions for hexene LLDPE film resins at 0.918 g/cm³ density and 1.0 g/10 min melt index; they do not replace grade-specific start-up recommendations from NOVA Chemicals.

    Production-scale failure modes reported for this material class include bubble instability at high frost lines, die-lip deposit accumulation from degraded processing aid, and melt fracture at elevated shear rates. Pre-drying is not generally required if the resin is stored under dry conditions; exposure to relative humidity above 60% may introduce moisture that affects film appearance. When film clarity deteriorates after several hours on a continuous line, die lip cleaning is often required. Fluoropolymer processing aids typically condition the die within 15–30 min after initial start-up. If the die gap is below 1.0 mm, local shear rate can exceed 1000 s⁻¹ and initiate sharkskin.

    Mechanical Property Envelope and Test Methodology for Film Specimens

    Film property evaluations for this product class are normally performed on 25 µm monolayer film produced on a laboratory-scale blown-film line with a 50 mm extruder and a 2.5:1 blow-up ratio. The values below represent the published property envelope for hexene LLDPE film resins of nominal density 0.918 g/cm³ and melt index 1.0 g/10 min; they are not grade-specific specifications and may vary with additive package and fabrication conditions.

    PropertyMethodRepresentative range
    Resin densityASTM D15050.918 g/cm³
    Melt indexASTM D1238, 190 °C/2.16 kg1.0 g/10 min
    Tensile strength at break, machine directionASTM D88235–45 MPa
    Tensile strength at break, transverse directionASTM D88230–40 MPa
    Elongation at break, machine directionASTM D882500–700%
    Elongation at break, transverse directionASTM D882600–800%
    Elmendorf tear, machine directionASTM D1922250–400 g
    Elmendorf tear, transverse directionASTM D1922350–500 g
    Dart impactASTM D1709, Method A150–220 g
    HazeASTM D10038–14%
    Gloss at 45°ASTM D245760–75

    The tensile values in the table represent a film property envelope rather than a specification. Intrinsic resin lot-to-lot variance and extrusion orientation can shift individual values by ±10%; dart-impact data on a single laboratory line often show a standard deviation of 20–30 g on 25 µm film. Testing should follow sample conditioning at 23 °C ± 2 °C and 50% ± 5% relative humidity for at least 40 h per ASTM D618.

    In cast film extrusion, line speed and chill-roll temperature interact with hexene crystallinity. A cast line operating at 200–300 m/min with a chill roll set at 15–30 °C gives faster quench than blown-film air cooling. The rapid quench reduces haze to 3–6% on 25 µm film measured by ASTM D1003, but may reduce machine-direction tear relative to a slower cooling history. Conversely, cast film from this product class typically shows a lower coefficient of friction after the slip additive has fully bloomed, because reduced surface roughness from the smooth chill roll permits thinner additive migration layers to be effective. In a cast line with a 100 mm extruder and 250 m/min line speed, contact time on the chill roll before winding should remain adequate to prevent blocking at the winder; published data for this specific configuration are limited.

    When high transverse-direction tear is required in cast applications, the melt draw ratio should be kept below 20:1 and the die lip gap should be larger than the final film thickness by a factor of 1.2–2.0. Hexene LLDPE cast film often exhibits a transverse-direction/machine-direction tear ratio below 1.0 because of machine-direction orientation. This is a normal orientation effect and must be accommodated in package design.

    When Slip Migration Kinetics and Antiblock Loading Limit Converting Line Speed

    Slip additives in LLDPE film, typically erucamide or oleamide, migrate to the surface by Fickian diffusion. The diffusion coefficient of erucamide in LLDPE at 23 °C is reported in the polymer-additive literature to be in the range of 10−11 to 10−13 cm²/s, depending on crystallinity and chain mobility. In a 25 µm film, the time to reach approximately 80% of equilibrium surface concentration is generally 24–72 h at ambient temperature. Converters should not assess coefficient of friction by ASTM D1894 immediately after extrusion; premature evaluation underestimates steady-state slip performance.

    Antiblock particles, often synthetic silica at 1000–3000 ppm, reduce blocking but create local stress concentrations that can lower dart impact by 5–15% when added beyond 5000 ppm. The TF-Y534-IP additive package is proprietary; exact particle size, particle size distribution, and loading must be obtained from the manufacturer. Overlacquering or printing can alter the surface migration equilibrium, so trials should be conducted on the target film gauge and surface treatment level.

    In three-layer coextruded structures, the resin may be placed in the core or skin layer to impart toughness while sealants based on metallocene or ethylene-vinyl acetate copolymers provide heat-seal performance. The coextrusion feedblock and die should be designed to avoid melt-flow instabilities at layer thickness ratios below 10%; skin-layer melt temperature should not exceed 240 °C to avoid degradation of slip additives. Heat-seal initiation temperature measured on a gradient-bar sealer at 0.5 MPa and 0.5 s dwell for this density class typically falls near 95–110 °C. Blending with 20 wt% low-density polyethylene usually reduces seal initiation temperature by 3–6 °C and improves bubble stability, but lowers stiffness.

    Regulatory Compliance and Additive-Specific Constraints

    Food-contact status of an LLDPE film resin depends on the base polymer and its specific additive package. Polyolefins produced from ethylene and 1-hexene may be covered by FDA 21 CFR §177.1520(c) when the finished article meets extractable limitations for the intended food type and use condition. In the European Union, the material must comply with EU Regulation No 10/2011, including overall migration below 10 mg/dm² and specific migration limits for any authorized additives. REACH compliance requires registered substance status for imported polymer or monomer; users should obtain a signed declaration from the supplier. The compliance framework below summarizes the key instruments, but it is not a certification table.

    InstrumentScopeTypical condition
    FDA 21 CFR §177.1520(c)Olefin polymer food-contact statusDependent on additive package and extraction conditions
    EU Regulation No 10/2011Plastic materials and articles in food contactOverall migration <10 mg/dm²
    REACHRegistration, evaluation, authorization of substancesSupplier declaration required
    RoHS 2011/65/EURestriction of hazardous substances in electrical and electronic equipmentBase polyolefin generally meets heavy-metal limits; additive package requires documentation

    The resin is not intended for medical implant applications; no USP Class VI claim applies to the formulated grade unless separately certified. Users evaluating this material for food-contact use must verify the specific additive package and final film thickness against the applicable migration limits.