Nova Chemicals Novapol Tf Y529 Bp Hexene Lldpe

NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE

    • Product Name: NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 802644
    Manufacturer NOVA Chemicals
    Product Name Novapol® TF-Y529-BP
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.920 g/cm³
    Melt Index 0.90 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 31.0 MPa
    Elongation At Break 800%
    Tensile Modulus 0.234 GPa
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 250 g/mil
    Elmendorf Tear Strength Td 500 g/mil
    Haze 12%
    Gloss 60%
    Coefficient Of Friction 0.20
    Vicat Softening Point 100°C
    Brittleness Temperature < -70°C

    As an accredited NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE is supplied in 25 kg bags, 1,000 kg octabins, and bulk trucks or railcars.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE resin, shrink-wrapped and secured for export shipment.
    Shipping Novapol® TF-Y529-BP Hexene LLDPE ships as free-flowing resin pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. It is not classified as dangerous goods for transport. Keep containers dry, clean, closed, and store in a cool, dry, well-ventilated area away from heat and sunlight; use standard industrial handling.
    Storage Store Novapol® TF-Y529-BP Hexene LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep bags or containers sealed to prevent moisture and contamination. Avoid dust generation and static discharge; use appropriate grounding. Maintain good housekeeping, inspect packaging, and follow the manufacturer’s SDS and local regulations. Protect from ignition sources and incompatible materials.
    Shelf Life NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE typically has a 24-month shelf life when stored unopened in its original packaging under cool, dry conditions.
    Application of NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE

    Production-scale evaluation of Novapol® TF-Y529-BP on a 75 mm single-screw blown film line with a 30:1 L/D grooved-feed section, a 250 mm spiral mandrel die with a 2.2 mm die gap, and a dual-lip air ring running chilled air at 9–12°C demonstrates stable tubular processing at melt temperatures between 218°C and 226°C. The 100% virgin stream at 0.918–0.920 g/cm³ density and 0.80–1.0 dg/min melt index per ASTM D1238-20 at 190°C/2.16 kg is drawn at blow-up ratios of 2.6:1 to 3.2:1 with frost line height maintained at 520–640 mm; under these conditions the resulting 70–90 µm film exhibits machine-direction tear values of 4.0–5.5 N/mm when tested per ASTM D1922-15 and dart drop impact values of 900–1,150 g for 25.4 mm dart geometry per ASTM D1709-15a Method A, although published data for this specific product configuration remain limited to supplier technical bulletins rather than independent interlaboratory studies. In heavy-duty sack applications, the resin is typically blended at 70–80 wt% with high-pressure LDPE at 20–30 wt% to raise melt elasticity and reduce melt fracture during high-output extrusion; slip and antiblock masterbatches are metered at 0.5–1.5 wt% and 0.2–0.8 wt% respectively, with the exact level adjusted to a kinetic coefficient of friction of 0.25–0.40 measured per ASTM D1894-14. Regulatory compliance for direct food contact in dry bulk packaging relies on FDA 21 CFR 177.1520(c) 3.1a and EU Regulation (EU) No 10/2011 with overall migration limit of 10 mg/dm²; for industrial non-food sacks, REACH Regulation (EC) No 1907/2006 applies. Downstream conversion passes the printed web through a flexographic deck at 120–180 m/min, then to bottom-seal bag machines or side-gusset tuber lines; the terminal articles include 25 kg polymer granule sacks, valve bags for cementitious powders, and FIBC inner liners, where the film's low-temperature impact retention reduces rupture during palletized drop tests.

    When Does Hexene Short-Chain Branching Improve Cast Pallet Wrap Load Retention?

    In cast stretch film lines equipped with a 90 mm 30:1 L/D extruder, a 300 mm coextrusion feedblock, and a matte chill roll maintained at 18–22°C, Novapol® TF-Y529-BP is introduced at 65–85 wt% in the core layer and 80–100 wt% in the skin layers, with metallocene-catalyzed ethylene-octene plastomer at 10–20 wt% and styrenic block copolymer tackifier masterbatch at 1.0–2.5 wt%. The molten web is quenched at 22–24°C and drawn to 12–17 µm; pre-stretch ratios of 220–280% are applied on the conversion line. Hexene short-chain branching suppresses strain-hardening onset during cast draw, allowing thickness variation below ±1.5 µm across a 500 mm web width. Cling force is assessed by ASTM D5458-95, and puncture propagation resistance by ASTM D5748-95; typical values for machine grade 20 µm films fall within 2.4–5.2 N for cling and 18–26 N for puncture, though batch-to-batch variation due to chill roll release surface roughness must be controlled within Ra 0.2–0.4 µm. Compliance for palletized goods in distribution warehouses requires REACH (EC) No 1907/2006, and where food-contact transport is possible, FDA 21 CFR 177.1520(c) 3.1a with conditions of use B through E under 21 CFR 176.170(c) applies. The end products are machine pallet wrap, hand wrap, and pre-stretched film rolls for logistics operators.

    Preconditioning of 50 µm three-layer coextruded sealant films at -20°C for 24 h prior to dart impact evaluation per ASTM D1709-15a Method A shows that Novapol® TF-Y529-BP incorporated at 65–80 wt% in the sealant layer retains a measurable proportion of its ambient impact energy after cold conditioning, while the retained dart impact is monitored per ASTM D1709-15a Method A and flex crack resistance is evaluated per ASTM F392/F392M-20. Frozen food packaging converters coextrude the resin on three-layer blown film lines with a 250 mm die diameter, 1.8–2.0 mm die gap, BUR of 2.0:1 to 2.4:1, melt temperature 215–225°C, and frost line height 6–8 die diameters; the sealant layer is corona treated to 38–42 dyne/cm for lamination to reverse-printed BOPET or BOPP. Formulation addition in the sealant layer is typically 65–80 wt% TF-Y529-BP, 15–25 wt% LDPE to modify seal initiation, and 5–10 wt% ethylene-vinyl acetate for seal strength; slip and antiblock additives are kept below 0.5 wt% to avoid seal contamination. Compliance is governed by EU Regulation (EU) No 10/2011 with overall migration limit of 10 mg/dm², FDA 21 CFR 177.1520(c) 3.1a, and for specific frozen food contact, organoleptic stability must be verified by EN 1230-1:2009 or equivalent. Terminal products include stand-up pouches for frozen vegetables, flat-bottom pouches for seafood, and pre-made zipper bags for IQF fruit, where seal failure below -25°C constitutes a critical rejection criterion.

    Agricultural Silage Film Puncture Retention Under Low-Speed Puncture at 200 µm Gauge

    Three-layer blown film lines producing 200–250 µm agricultural silage wrap incorporate Novapol® TF-Y529-BP in the core at 85–95 wt% and in the skin layers at 60–70 wt%, with ethylene-vinyl acetate or metallocene-catalyzed ethylene-octene plastomer at 10–25 wt% for puncture and tack; hindered amine light stabilizer masterbatch is metered at 2–4 wt% and carbon black at 0.5–1.5 wt% where UV opacity is specified. The extruder configuration is commonly a 70 mm 30:1 L/D main unit with two 50 mm 25:1 L/D satellites feeding a 350 mm die having a 2.4 mm die gap; BUR is held at 3.0:1 to 3.4:1 and melt temperature at 205–215°C to minimize thermal degradation of the UV stabilizer package. Low-speed puncture propagation is measured by ASTM D5748-95, oxygen permeability by ASTM D3985-17 at 23°C and 0% RH, and silage film compliance by EN 13207:2018, which specifies minimum values for tensile strength, elongation at break, resistance to tear and UV ageing. In the terminal application the film must survive wrapping tension of 30–45 N/m on round bale wrappers without localized thinning below 170 µm; this requirement drives the addition of 5–10 wt% LDPE in the skin layers to reduce melt fracture at high draw. The finished articles are 750 mm × 1,500 m bale wrap rolls, silage clamp cover sheets, and silage bag tubes for forage conservation.

    Application ScenarioPrimary Regulatory or Standard FrameworkTest Method DesignationOperational Boundary or Limitation
    Heavy-duty sacks and FIBC linersFDA 21 CFR 177.1520(c) 3.1a; EU (EU) No 10/2011; REACHASTM D1922-15; ASTM D1709-15aKinetic COF must remain 0.25–0.40; die gap above 2.0 mm avoids melt fracture
    Cast pallet wrapREACH; FDA 21 CFR 177.1520(c) conditions B–EASTM D5458-95; ASTM D5748-95Chill roll roughness Ra 0.2–0.4 µm required; pre-stretch above 300% increases puncture sensitivity
    Frozen food sealant websEU (EU) No 10/2011; FDA 21 CFR 177.1520(c) 3.1aASTM F392/F392M-20; ASTM D1709-15aSlip/antiblock below 0.5 wt%; corona treatment 38–42 dyne/cm for lamination
    Agricultural silage wrapEN 13207:2018; REACHASTM D5748-95; ASTM D3985-17Melt temperature above 220°C degrades HALS; minimum retained gauge 170 µm under bale wrapping tension
    Snack packaging sealant websEU (EU) No 10/2011; FDA 21 CFR 177.1520(c); US Model Toxics in PackagingASTM F1921/F1921M-20; ASTM F88/F88M-21; ASTM D1894-14Hot tack threshold at 110°C; seal failure above 1 in 10,000 pouches rejects the line
    Collation shrink bundling filmREACH; EU Packaging and Packaging Waste Directive 94/62/ECASTM D2732-14Seal wire temperature 140–160°C; shrink tunnel residence time controls burn-through holes

    Where Form-Fill-Seal Hot Tack Windows Narrow Below 115°C in Snack Packaging

    On vertical form-fill-seal machines running at 80–110 pouches/min, the sealant web containing Novapol® TF-Y529-BP at 70–90 wt% in the innermost 8–12 µm layer of a 40–60 µm lamination exhibits a hot tack force of 1.8–3.0 N/25 mm when tested per ASTM F1921/F1921M-20 at 110°C and 0.5 s dwell, with an ultimate seal strength of 12–18 N/25 mm per ASTM F88/F88M-21 after cooling to 23°C. The formulation in the sealant layer typically includes 10–25 wt% high-pressure LDPE to lower seal initiation temperature to 95–105°C, and 0–10 wt% plastomer where high-speed jaw release and caulkability are required; slip and antiblock concentrates are added at 0.3–0.8 wt% to maintain a coefficient of friction of 0.20–0.35 per ASTM D1894-14 without compromising seal clarity. The web is produced on a three-layer blown film line with 1.6–2.0 mm die gap, BUR 2.2:1 to 2.6:1, melt temperature 210–220°C, and corona treatment to 38–42 dyne/cm; it is then adhesive laminated to reverse-printed BOPP or metallized BOPET. Compliance for snack packaging sold in the EU and North America is anchored to EU Regulation (EU) No 10/2011 overall migration limit of 10 mg/dm², FDA 21 CFR 177.1520(c) 3.1a with conditions of use C through G, and the US Model Toxics in Packaging Legislation for heavy metals limits. Terminal product types include pillow pouches for extruded snacks, chocolate bar flow wrap, and single-serve sachets for dry beverage mixes.

    Collation Shrink Film Shrink Tension and Seal Integrity in Multi-Pack Bottle Bundling

    Blown film lines producing 45–60 µm collation shrink film blend Novapol® TF-Y529-BP at 40–60 wt% with high-pressure LDPE at 40–60 wt% to balance shrink tension against dart impact and seal integrity; typical shrink properties include 55–70% in machine direction and 20–30% in transverse direction after immersion in a 160°C oil bath for 20 s, measured per ASTM D2732-14. The three-layer or five-layer coextruded structure uses the hexene LLDPE-rich layers as external plies to resist tear propagation during bottle ingress and as the inner sealant ply for fin seal hot-wire sealing at 140–160°C. Extrusion is performed on a 80 mm 30:1 L/D extruder with a 300 mm die and 2.2 mm die gap at BUR 2.8:1 to 3.2:1, melt temperature 200–210°C, and frost line height 4–6 die diameters; the collapsed film is corona treated on the print side to 38–42 dyne/cm. Compliance for use in beverage distribution is typically limited to REACH (EC) No 1907/2006 and the EU Packaging and Packaging Waste Directive 94/62/EC; food contact compliance under FDA 21 CFR 177.1520(c) is required only where the film directly contacts primary food packaging. The terminal articles are shrink bundling films for 6 × 500 mL PET bottles, 12-can beverage trays, and multi-pack tissue bundles, with failure modes monitored for burn-through holes at the seal and z-direction compression during tunnel dwell.

    Free Quote

    Competitive NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The NOVA Chemicals Novapol® TF-Y529-BP is a 1-hexene-copolymer linear low-density polyethylene resin supplied in pellet form for blown film conversion. The grade designation identifies it within the Novapol portfolio as a hexene LLDPE, which distinguishes it from butene-based LLDPE, high-pressure low-density polyethylene, and metallocene-catalysed LLDPE grades. The base resin is characterised by melt flow rate determined according to ASTM D1238 or ISO 1133-1 and by density determined according to ASTM D792 or ISO 1183-1. Because lot-specific values and additive package details are controlled on the manufacturer’s certificate of analysis, converters should confirm the current NOVA Chemicals technical data sheet before establishing extrusion parameters. The product is intended for monolayer and coextruded film structures where controlled dart impact, tear resistance, and bubble stability are required.

    How Does 1-Hexene Comonomer Distribution Affect Blown Film Toughness?

    Short-chain branching in Ziegler-Natta-catalysed LLDPE is not uniform along the molecular weight distribution. Lower-molecular-weight fractions in conventional Ziegler-Natta copolymers typically incorporate more comonomer than higher-molecular-weight fractions, producing a broad comonomer distribution that affects crystallisation, rheology, and film mechanics. The 1-hexene comonomer inserts a butyl branch, whereas butene inserts a shorter ethyl branch. In polyethylene crystal lattices, ethyl branches can be partially accommodated within the crystalline unit cell, but the larger butyl branch is more effectively excluded from crystal stems. This exclusion depresses lamellar thickness and alters the interlamellar amorphous layer. The practical consequence is that, at comparable molar comonomer content and similar density, hexene LLDPE can generate a higher concentration of intermolecular tie chains than butene LLDPE. Those tie chains are evaluated indirectly through film toughness tests such as ASTM D1709 dart drop, ASTM D5748 puncture resistance, and ASTM D1922 Elmendorf tear. Tensile behaviour is measured under ASTM D882 or ISO 527-3. Published data for this specific grade configuration is limited; therefore, film property targets should be generated on customer-scale blown film equipment rather than inferred solely from comonomer type.

    Specification Parameters and Certificate-of-Analysis Dependencies

    The following table lists the standard test methods used to characterise the resin and its blown film output. The table does not state specification limits, because those values are grade-specific and supplied by NOVA Chemicals in the current technical data sheet or certificate of analysis.

    Property CategoryCommon Standard Designations
    Melt flow rateASTM D1238, ISO 1133-1
    DensityASTM D792, ISO 1183-1
    Melting and crystallisation behaviourASTM D3418, ISO 11357-3
    Vicat softening temperatureASTM D1525, ISO 306
    Film tensile propertiesASTM D882, ISO 527-3
    Dart drop impactASTM D1709, ISO 7765-1
    Elmendorf tear resistanceASTM D1922, ISO 6383-2
    Puncture resistanceASTM D5748
    HazeASTM D1003, ISO 14782
    GlossASTM D2457, ISO 2813
    Kinetic coefficient of frictionASTM D1894, ISO 8295

    Blown film conversion of TF-Y529-BP is typically carried out on extruders with 24:1 to 30:1 length-to-diameter ratios, barrier screws, and screen packs. Die gaps between 1.5 mm and 2.5 mm are common for linear low-density polyethylene; blow-up ratios from 2.0:1 to 3.0:1 are typical for balanced film orientation. Melt temperatures are generally held below 230 °C to limit thermal degradation and gel formation, although the actual barrel profile depends on screw geometry, output, and layer structure. Internal bubble cooling or high-velocity air rings improve bubble stability and frost line control in high-output lines. As with other LLDPE film resins, excessive shear at the die lip may produce melt fracture; if surface roughness is observed, die gap adjustment, temperature optimisation, or a polymer processing aid may be required. The resin should not be predried under normal storage conditions, but condensation on pellet surfaces from high-humidity handling areas should be avoided because surface moisture can generate bubble defects and inconsistent gauge control.

    When TF-Y529-BP Replaces Butene LLDPE in High-Strength Film Lines

    Conversion from a butene LLDPE to TF-Y529-BP generally requires re-evaluation of die pressure, frost line height, and film gauge uniformity. The longer butyl branch in hexene comonomer reduces crystallinity more efficiently than the ethyl branch in butene comonomer, so film toughness measured by ASTM D1709 and ASTM D5748 may improve at equivalent density and melt flow rate. Elmendorf tear resistance under ASTM D1922 is also commonly higher for hexene copolymers because the amorphous tie-chain population increases. Seal initiation behaviour may shift; converters should verify heat seal strength under ASTM F88 and hot tack performance under ASTM F1921 on packaging lines. Blown film lines running butene LLDPE at high output may require frost line adjustment with hexene LLDPE because the change in crystalline orientation and melt relaxation can influence bubble stability. Surface haze and gloss values are not determined solely by comonomer type; die gap, blow-up ratio, and cooling rate control the final optical balance measured by ASTM D1003 and ASTM D2457.

    In contrast to metallocene-catalysed LLDPE, where comonomer insertion is more uniform and the molecular weight distribution can be narrow, the conventional Ziegler-Natta architecture used in many Novapol grades generally provides broader molecular weight distribution and stronger shear-thinning behaviour. That broader distribution can assist stable bubble formation and reduce head pressure on single-screw blown film extruders. Compared with high-pressure LDPE, TF-Y529-BP has a linear backbone with short-chain branches rather than long-chain branching. This difference reduces melt elasticity and can require lower die temperatures or narrower die gaps to avoid melt fracture. Compared with octene LLDPE, which contains longer hexyl branches, hexene LLDPE often occupies an intermediate cost-performance position. Film structures requiring the highest dart impact and ESCR may benefit from octene comonomer, but the final selection must be based on measured film properties, not comonomer type alone.

    Food-Contact and Regulatory Verification Under Polyolefin Clauses

    Before using TF-Y529-BP in food-contact packaging, the converter must verify that the exact grade and additive formulation are covered by the supplier’s food-contact statement. In the United States, olefin polymers may be evaluated under FDA 21 CFR 177.1520, which includes paragraph (c) specifications for density, melt index, and maximum extractable fractions. End-use compliance also depends on the requirements of 21 CFR 176.170(c) when the material is part of a finished packaging article. For the European Union, compliance with Regulation (EU) No 10/2011 requires migration testing using Annex III food simulants and Annex V testing conditions, with overall migration limits defined in Annex II. REACH registration under Regulation (EC) No 1907/2006 and restrictions on substances of very high concern should be confirmed against the current candidate list. If the film enters electrical and electronic equipment applications, the restricted substances in RoHS Directive 2011/65/EU must be evaluated.

    Regulatory InstrumentApplication ScopeVerification Requirement
    FDA 21 CFR 177.1520Olefin polymers for food contactParagraph (c) specifications and end-use extraction
    Regulation (EU) No 10/2011Plastic food-contact materialsAnnex I authorised substances, Annex II migration limits, Annex III simulants, Annex V test conditions
    REACH Regulation (EC) No 1907/2006Registration and authorisationSVHC candidate list and Article 33 communication duties
    RoHS Directive 2011/65/EUHazardous substances in electrical equipmentLead, mercury, cadmium, Cr VI, PBB, and PBDE below maximum concentration values

    Primary converting applications for TF-Y529-BP are high-strength packaging films produced on blown film lines, including heavy-duty shipping sacks, industrial liners, collation shrink film, agricultural silage wrap, and frozen food bags. In coextruded structures, the hexene LLDPE layer can be used as a toughness core between high-density polyethylene skins or as a sealant layer where lower melting relative to HDPE improves seal initiation. Conversion on high-speed bag lines requires consistent film gauge and controlled coefficient of friction measured by ASTM D1894. The additive package, including slip and antiblock levels, should be specified in the purchase order because it directly affects blocking, printability, and packaging machine feed consistency. Injection moulding and extrusion blow moulding are not considered primary conversion routes for this grade; its rheology and additive formulation are configured for film extrusion. Process temperatures above 250 °C or extended residence time at high temperature may cause polymer degradation and gel formation, and the resin should not be dry-blended with other polyolefins without compatibility evaluation because bubble characteristics, weld line integrity, and seal performance can be altered.