| HS Code | 195484 |
| Product Name | NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin |
| Polymer Type | Hexene Linear Low-Density Polyethylene (LLDPE) |
| Comonomer | Hexene |
| Melt Index I2 | 1.0 g/10 min |
| Density | 0.919 g/cm³ |
| Melt Flow Ratio I21 I2 | 28 |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Yield Td | 10.3 MPa |
| Tensile Strength At Break Md | 34.5 MPa |
| Tensile Strength At Break Td | 31.0 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| 1 Secant Modulus Md | 207 MPa |
| 1 Secant Modulus Td | 234 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 10% |
| Gloss 45 | 70 |
| Vicat Softening Point | 100 °C |
| Melting Point | 124 °C |
As an accredited NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin is supplied in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet; bulk trucks/railcars available. |
| Container Loading (20′ FCL) | Typically loads 20–22 MT in 25 kg bags, floor-loaded or palletized, shrink-wrapped, and securely stowed in 20′ FCL. |
| Shipping | NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin is typically supplied in 25 kg PE bags, stacked on pallets, stretch-wrapped, or in bulk railcars/trucks. Ship in clean, dry, covered transport; protect from moisture, heat, and sunlight. Not classified as dangerous goods. |
| Storage | Store Novapol TF-0119-FP in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers tightly closed, off the floor, and palletized. Prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Rotate stock first-in, first-out. Consult the SDS for specific storage requirements. Do not stack excessively; follow supplier recommendations. |
| Shelf Life | Shelf life is typically 12 months from date of manufacture when stored in original packaging, dry, cool, and below 50°C. |
Hexene linear low density polyethylene film resin NOVA Chemicals Novapol® TF-0119-FP is specified at a nominal density of 0.919 g/cm³ when tested to ISO 1183-1, with a nominal melt index of 1.0 g/10 min at 190 °C/2.16 kg when tested to ISO 1133-1:2022 Method A. In heavy-duty industrial sack conversion, the hexene branch length produces a higher tie-molecule population than butene LLDPE of equivalent density, which directly influences slow puncture energy dissipation in filled sacks and polymer evacuation bags. A three-layer A/B/A coextrusion structure positions the TF-0119-FP resin in the two skins at 70–85 wt% blended with low-density polyethylene at 15–30 wt%; the core carries post-industrial reclaim at up to 35 wt% only when haul-off sag and dart impact requirements permit. The LDPE fraction widens the bubble stability window on a grooved-feed extruder with a 30:1 L/D screw and a 200 mm spiral mandrel die. The die gap is held between 1.8 mm and 2.5 mm, with a blow-up ratio between 2.2:1 and 2.8:1. Melt temperatures are limited to 190–220 °C; excursions above 225 °C generate oxidative gels that appear as unmelted inclusions in the film web and weaken drop impact performance. The sacks are filled with resin pellet loads, carbon black masterbatch, or mineral fillers at 10–25 kg fill weights and are qualified under ASTM D5276 drop impact, ISO 6383-2 trouser tear, and warehouse stack retention protocols. A recurring line failure is die lip solids accumulation at high output, which is controlled with fluoropolymer processing aid at 200–800 ppm and a screen pack sequence of 20/40/60 mesh. Film thickness for this conversion typically ranges from 120 µm to 250 µm depending on fill weight and expected transport abuse.
The lower melt temperature limit of 190 °C is set by screw torque and melt pressure on the grooved bushing; below this temperature, extruder amp-load rises and the frost line drops below the stabilizing cage, causing uneven gauge. The upper limit of 220 °C is constrained by oxidative gel accumulation in the die mandrel. Film gels are counted by inline optical detection and correlated to a melt pressure delta of 30–50 bar across the screen pack. Addition of reclaim above 35 wt% creates a property cliff-edge in dart impact and trouser tear, so converters qualify each reclaim lot by testing the finished sack under ISO 7765-1 and ISO 6383-2 before release to fill stations. The terminal product is further converted by bottom gusseting and side gusseting equipment running in a linear speed envelope of 60–100 m/min, with seal bar temperature controlled between 150 °C and 180 °C.
Agricultural silage covers and greenhouse cladding converted from TF-0119-FP are processed on internally cooled blown film lines where the frost line is held at 1.0–1.5 times die diameter to reduce transverse direction tension imbalance. The hexene comonomer concentration controls the tie-chain population that resists slow crack growth in wet, UV-stressed environments; thinner cover sections of 150–200 µm still pass ISO 7765-1 puncture testing when the die gap is maintained below 2.2 mm and the bubble is not quenched too rapidly. Hindered amine light stabilizers are compounded at 0.4–1.2 wt% in the outer layer to protect post-industrial recyclate content in the middle layer; a nonionic antifog/antidust additive at 0.5–1.0 wt% is concentrated on the inner surface to control water film condensation without reducing solar transmission. The film is tested according to EN 13206 and ISO 4892-2 for weathering; tensile elongation after exposure is measured under ISO 527-3. A processing conflict in this sector is the need for high melt temperature to disperse UV masterbatch versus the risk of reducing molecular weight and destabilizing the bubble; the resin is therefore run at 195–210 °C, with a maximum of 210–220 °C on the outermost die zone.
Coextruded greenhouse side films add low-density polyethylene skin layers and a UV absorber package; the core layer remains TF-0119-FP. Silage film and bale wrap must not be overdosed with migratory slip agents because silage contact film friction must remain stable on wrap applicators. Terminal products include silage clamp covers, round bale wrap film, and greenhouse gable sheets; all are evaluated for hail impact perforation and wind-induced tear propagation. Published data for long-term silage film performance in this specific reclaim-rich blend is limited.
| Application segment | Primary performance methods | Major regulatory or specification boundary |
|---|---|---|
| Heavy-duty sacks | ASTM D5276, ISO 6383-2, ISO 7765-1 | End-user stack-load retention specification |
| Agricultural silage covers | EN 13206, ISO 4892-2, ISO 527-3, ISO 7765-1 | EN 13206 weathering classes for service life |
| Stretch hood/pallet | ASTM D4649, ASTM D882, ASTM D880 | Warehouse storage temperature below 35 °C |
| Frozen food laminations | ASTM F88/F88M, ASTM F1921, ISO 7765-1, ASTM F392 | FDA 21 CFR 177.1520(c), EU Regulation (EC) No 10/2011 |
| Liquid liners | ASTM F1140, ASTM F392, ISO 527-3 | UN dangerous goods transport protocol for specific liquid classes |
Pallet unitization films made from TF-0119-FP are converted on cast stretch wrap lines with a 150 mm screw and on blown stretch hood lines with internal bubble cooling. In cast stretch wrap with a thickness of 35–80 µm, the hexene LLDPE is compounded with a metallocene plastomer or an octene LLDPE at 20–30 wt% to modify elastic recovery and allow the film to hold irregular loads without necking excessively. A low-molecular-weight polyisobutylene tackifier is dosed at 0.5–1.5 wt% to generate cling force; however, migration to the film surface can reduce coefficient of friction on the unwind side of the roll. The film is tested for cling using ASTM D4649 and for tensile stress at 200% elongation using ASTM D882. In blown stretch hood film of 50–100 µm, the resin is blended with low-density polyethylene at 10–20 wt% to stabilize the large bubble, and a silica antiblock at 2,000–4,000 ppm prevents film-to-film blocking during roll storage. The critical manufacturing risk is blocking at warehouse temperatures above 35 °C; converters are advised to store rolls below 30 °C and to rotate stock within 12 weeks. End users evaluate hood durability with an incline impact test based on ASTM D880. Terminal pallet covers are supplied to chemical drum shipments, white goods, and beverage tray unitization; no direct food contact standard is required unless the pallet sheet is used as a temporary cover for unpackaged produce.
In frozen food laminate sealant webs, TF-0119-FP is converted at 20–40 µm thickness and then adhesive-laminated to biaxially oriented PET or biaxially oriented polypropylene. The low seal initiation temperature is critical for vertical form-fill-seal lines because dwell time is short; a laboratory VFFS machine establishes a seal window between 105 °C and 130 °C with jaw pressure at 45 psi and dwell between 0.4 s and 0.8 s. Seal strength after 24 h conditioning at 23 °C and 50% RH is measured per ASTM F88/F88M. Hot tack strength is determined by ASTM F1921, which is a better predictor of burst-open failures in gusseted pouches and vertical form-fill-seal applications than room-temperature seal strength alone. The die gap is deliberately maintained below 2.0 mm because thicker die gaps produce a less oriented and more crystalline sealant that requires higher sealing temperature and can cause pleats at the side seals. Melt temperatures above 220 °C increase the probability of oxidative gel inclusions that register as defects during post-lamination inspection.
A five-layer barrier film positions TF-0119-FP in the sealant skin, an ethylene vinyl alcohol copolymer in the barrier core, and tie resins at the interlayers; the structure is tested for cold-temperature dart impact at -20 °C according to ISO 7765-1 and for flex crack resistance according to ASTM F392. Frozen food contact compliance rests on FDA 21 CFR 177.1520(c) for olefin polymers and on EU Commission Regulation (EC) No 10/2011 for overall migration. Converters must confirm with the resin supplier that the product is covered by the applicable food-contact compliance certificate before using this grade in direct food contact packaging. The sealant layer is not combined with high levels of migratory slip agents because excessive slip migration can reduce seal strength below the minimum specified value for freezer-graded pouches.
Bulk liquid liners and flexible intermediate bulk container liners convert TF-0119-FP into 100–300 µm multi-ply blown films with a flex-crack-resistant laminate structure. The hexene LLDPE is used in the sealant and outer layers; the center layer may contain a polyolefin elastomer or low-density polyethylene to reduce pinhole propagation at welded seams. The liner seams are welded by thermofusion at 150–180 °C; burst strength is evaluated by ASTM F1140 and flex durability by ASTM F392. The terminal liners are filled with water treatment chemicals, urea ammonium nitrate, and non-flammable industrial fluids; the resin is not recommended for long-term immersion in aromatic solvents or strong oxidizer streams without independent chemical compatibility testing. A known operational boundary is the use of post-industrial reclaim in the middle layer above 30 wt%, which increases the incidence of microvoids at the weld corner during repeated flexing. Converters reduce this risk by restricting the center layer reclaim content to 20–30 wt% and by adding a coextruded low-density polyethylene skin that accommodates seam compression without cracking. The film is measured for pinhole formation using a pressure-decay test after 200 flex cycles. End users in drum and flexitank applications require the form-fill-seal seam to retain burst pressure of at least 0.5 bar; this value is determined by the liner specification and is not a universal limit for all liquid classes. Published data for long-term immersion testing of this specific resin with aromatic hydrocarbons is limited.
For e-commerce mailer film production, TF-0119-FP is converted at 50–80 µm gauge on compact blown film lines with single-lip air rings, where a 5–15 wt% LDPE addition is used to control bubble chatter at high air flow. The web is corona treated to 38–44 mN/m surface tension before flexo printing, and incoming inspection uses ASTM D1922 for tear strength and ISO 7765-1 for dart impact. This segment represents a shallow conversion zone: the technical requirements are fully established, and no proprietary adjustment beyond blend ratio and chilling air temperature is required.
Competitive NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin is an ethylene/1-hexene linear low-density polyethylene film resin manufactured as a pelletized blown film extrusion grade. The hexene-1 comonomer produces butyl branches along the polyethylene backbone, distinguishing the resin from butene-1 LLDPE and from high-pressure LDPE. At the nominal lot-release level, the melt mass-flow rate is 0.75 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg load, and the density is 0.918 g/cm³ under ASTM D792. These values place the grade in a low-melt-index, low-density segment used for thin-gauge blown films requiring high dart impact and tear propagation resistance.
The product is specified for monolayer and coextruded blown film applications, including food-contact packaging, industrial liners, heavy-duty shipping sacks, and agricultural films. The low melt index supports bubble stability at low gauge, but the exact processing response is governed by die geometry, frost-line height, blow-up ratio, cooling-air temperature, and the thermal stabilizer package. Converters should obtain the current manufacturer’s technical data sheet for lot-specific additive information and film property values generated under the supplier’s standard extrusion conditions.
Because published data for this specific configuration is limited, any substitution or downgauging program should be validated on the target blown film line using the actual die gap and feedblock configuration. The product should not be characterized solely by its density and melt index, because film failure under abuse loading is also a function of molecular weight distribution, comonomer distribution, processing history, and film thickness variation across the web.
In polyethylene, the short-chain branch length determines the efficiency with which polymer chains can form interlamellar tie molecules at a given crystallinity. Butene-1 introduces ethyl branches, while hexene-1 introduces butyl branches. At equal density and equal melt index, the longer butyl branch is less readily incorporated into the lamellar crystal and therefore produces a more effective tie-chain network. The consequence in blown film is typically an increase in dart impact F50 measured by ASTM D1709, higher Elmendorf tear propagation resistance in both machine and transverse directions under ASTM D1922, and greater puncture energy to break under ASTM D5748 when compared with a butene-1 LLDPE of identical density and melt index. This behavior is well documented in polymer physics literature and is not specific to a single converter’s film line.
The hexene-based architecture occupies an intermediate position between butene-1 and octene-1 LLDPE. Octene-1 introduces hexyl branches, which can further improve low-temperature toughness and tie-chain density at equivalent crystallinity, but may require higher comonomer incorporation to reach the same density and can have different melt fracture behavior. Hexene-1 copolymers often provide a practical combination of toughness and processability on standard monolayer lines. Compared with metallocene-catalyzed LLDPE resins of similar density, a Ziegler-Natta hexene grade such as TF-0119-FP generally has a broader molecular weight distribution. That distribution increases shear sensitivity, lowers melt viscosity at high screw speed, and improves melt strength for bubble stability, while reducing optical clarity relative to a narrow-distribution metallocene grade when haze is evaluated by ASTM D1003.
Compared with autoclave or tubular LDPE, the resin has higher tensile strength at break and higher dart impact at equivalent gauge, but lower melt strength and less shear thinning. For that reason, many converters blend a minor fraction of LDPE into the film to improve bubble stability and to broaden the heat-seal window. Compared with HDPE film grades of density above 0.940 g/cm³, TF-0119-FP provides lower stiffness and lower upper service temperature, but substantially higher puncture resistance and dart impact; it is therefore directed toward flexible packaging rather than rigid or high-modulus film structures.
Processability of a 0.75 g/10 min LLDPE on monolayer blown film equipment requires attention to extruder mixing, die pressure, and melt temperature. Single-screw extruders with a length-to-diameter ratio of at least 24:1 and a barrier-type screw or high-performance mixing section are recommended. On a spiral mandrel die, die gaps from 1.5 mm to 2.5 mm and blow-up ratios between 2.0:1 and 3.0:1 are common for similar hexene LLDPE film resins. Higher blow-up ratios increase transverse orientation and can improve impact balance but may challenge bubble stability on low-MI materials. Frost-line height should be set within the range that balances mechanical orientation and optical quality; an excessively low frost line increases haze and can raise film blocking tendency, while an excessively high frost line reduces bubble stability and may produce gauge bands at the nip.
Melt temperature measured at the die is typically maintained between 190 °C and 230 °C for LLDPE film conversion. Temperatures above 240 °C are not recommended because they may accelerate oxidative degradation and shift film color. The onset of sharkskin or melt fracture is not a single resin property; it is a function of shear stress in the die land, die geometry, melt temperature, and the processing aid package. On lines with short feed sections or simple general-purpose screws, pressure fluctuations and melt temperature differences can generate gel-like defects even when the resin is within specification. A grooved feed throat or reverse-taper barrier screw improves solids conveying and reduces melt heterogeneity when throughput is increased. Nitrogen blanketing in the feed throat and minimization of hopper residence time during line stops reduce oxidation and lot-to-lot variability.
Film physical properties are strongly dependent on cooling air and web handling. For example, dart impact may decrease if the film is wound with excessive tension or if the collapsing frame creates uneven contact pressure. Therefore, incoming resin certificates should not be used as the sole predictor of finished film toughness; the fabricated film must be tested after steady-state extrusion using the specified gauge, blow-up ratio, and back-sheet treatment. Standard film conditioning at 23 °C and 50% RH for at least 40 h before testing per ASTM D618 is generally required to obtain reproducible dart and tear results.
Transitioning from a butene-1 LLDPE to a hexene-1 grade on an existing blown film line will alter die pressure, motor load, and melt temperature even when both resins have the same nominal melt index and density. The hexene grade can exhibit higher melt strength and may support lower gauge without immediate bubble instability, but the die pressure may shift upward. Before the transition, operators should record the baseline die pressure, screw speed, motor load, and melt temperature for the butene grade. A purge resin, often a fractional-melt LDPE or a general-purpose LLDPE, should be used to displace the prior material. The purge quantity is equipment-specific and should be determined by the mass of the extruder, adapter, and die.
After the transition, the line should not be evaluated until the resin feed system has achieved steady state. Transient melt blends are not representative of TF-0119-FP film properties. If die pressure approaches the equipment-specific alarm limit, the rear barrel temperature profile may be adjusted upward in 5 °C increments while staying below the maximum recommended melt temperature. Screw speed should not be increased into an overload region. Film samples for dart impact, tear, and seal strength should be collected after the die pressure and motor load have stabilized for a time equivalent to at least three complete residence-time turnovers of the extrusion system.
Compared with a butene-1 product at the same density, the hexene-1 grade may permit some gauge reduction while maintaining comparable dart impact and tear resistance, but published data for this specific configuration is limited and the reduction must be validated on the target line. Heat-seal initiation temperature and hot-tack performance are also line-dependent and should be characterized by ASTM F88 and ASTM F1921, respectively, across the intended seal-bar temperature range. The presence of LDPE in the blend, the corona discharge level, and the slip/antiblock masterbatch all affect final seal and friction behavior.
Regulatory status for food-contact applications should be confirmed from the supplier’s product-specific statement of compliance. The base olefin polymer in this grade is generally covered under FDA 21 CFR 177.1520(c) 3.2a or 3.2b, subject to end-use conditions of use and food type. For European Union food-contact use, the finished film must comply with the overall migration and specific migration limits of Regulation (EU) No 10/2011, and the converter is responsible for verification under the intended time, temperature, and food-simulant matrix. REACH obligations under Regulation (EC) No 1907/2006 apply to the legal entity placing the resin or finished article on the market; a declaration of SVHC content should be obtained from the supplier when required. RoHS Directive 2011/65/EU applies to the finished electrical or electronic article and to any intentionally added restricted substances above threshold values, not to the thermoplastic resin as supplied in bulk form.
Storage constraints must be observed to protect film quality. The resin should remain in the original sealed packaging, protected from UV radiation and protected from ambient humidity above 60% RH. If pellet moisture is visible or packaging has been opened for prolonged periods, drying at 80 °C for 2 h to 4 h with a desiccant dryer is a conservative pre-processing step. Prolonged storage above 50 °C may promote additive migration, pellet agglomeration, and slip-agent bloom. Regrind addition above the level validated by the converter can reduce dart impact and tear resistance; regrind should be clean, uniform in melt index, and limited to the percentage consistent with the finished film specification.
| Reference | Test or compliance scope | Application condition |
|---|---|---|
| ASTM D1238 | Melt mass-flow rate | Lot release at 190 °C, 2.16 kg |
| ASTM D792 | Density | Lot release at 23 °C |
| ASTM D1709 | Dart impact F50 | Film validation; gauge and preconditioning dependent |
| ASTM D1922 | Elmendorf tear | Film validation; MD and TD anisotropy |
| ASTM D5748 | Puncture energy | Film validation; fixture geometry dependent |
| FDA 21 CFR 177.1520(c) | Olefin polymer food contact | Supplier statement of compliance required |
| (EU) No 10/2011 | Plastic materials in food contact | Converter final article verification |
| (EC) No 1907/2006 | REACH SVHC | Supplier confirmation |
| 2011/65/EU | RoHS restricted substances | Finished article if applicable |
Film qualification programs should include steady-state dart impact, tear, and seal-strength measurements after line startup. A common failure mode in heavily downgauged films is not low tensile yield but rather local thickness variation at the frost line, which reduces impact resistance at the thinnest web points. On converting lines, film samples collected near the edge of the layflat may show different orientation and lower dart impact than center samples; sampling plans should account for this spatial variability. Because the product is designed for blown film, flat-die cast extrusion is not the primary processing route and may require different thermal stabilizer considerations. There is no single property specification that predicts all film performance; conformance to melt index and density specifications is necessary but not sufficient for fitness for use.