| HS Code | 934096 |
| Comonomer | Hexene-1 |
| Melt Index 190 C 2 16 Kg | 0.90 g/10 min |
| Density | 0.919 g/cm³ |
| Peak Melting Point | 124 °C |
| Vicat Softening Point | 104 °C |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Yield Td | 10.3 MPa |
| Tensile Strength At Break Md | 38 MPa |
| Tensile Strength At Break Td | 34 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Dart Impact Strength | 150 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12% |
| Gloss 45 | 55% |
| Coefficient Of Friction | 0.20 |
As an accredited NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL container typically loads 20 metric tons of NOVA Novapol® TF-0119-F Hexene LLDPE Film Resin in 25 kg bags. |
| Shipping | NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin is shipped as non-hazardous polymer pellets. It is not regulated for transport by DOT, IMDG, IATA, or ADR. Typical packaging includes 25 kg bags, bulk bags, or bulk trucks/railcars. Keep dry, clean, and away from excessive heat, sunlight, and ignition sources. |
| Storage | Store in a cool, dry, well-ventilated area. Keep containers sealed and palletized off the floor. Protect from direct sunlight, moisture, excessive heat, and ignition sources. Avoid contamination with other materials, dust, or odors. Maintain good housekeeping and follow local regulations. Refer to the SDS and supplier guidance for specific storage and shelf-life requirements. |
| Shelf Life | Stable under normal storage; store cool, dry, well-ventilated away from heat, sunlight, and ignition sources. No specific shelf life established. |
Monolayer and three-layer food-contact webs produced from hexene-linear grades on blown-film lines with 250 mm to 450 mm die diameters are typically formulated around Novapol® TF-0119-F at 70–90 wt% in the core and sealing surface layers, with the balance supplied by high-pressure LDPE at 10–30 wt% to restore bubble stability and reduce neck-in during bubble expansion. Where slip and antiblock performance is specified, a silica or talc antiblock masterbatch is introduced at 2–5 wt% and an erucamide slip masterbatch at 0.5–2.0 wt%, although the exact addition is adjusted to maintain kinetic coefficient of friction below 0.30 as measured by ASTM D1894-14. The nominal resin parameters used for screw-speed and temperature modeling are melt index 1.0 g/10 min under ISO 1133-1:2022 and density 0.919 g/cm³ under ASTM D792-20. FDA 21 CFR 177.1520(c) applies to the olefin polymer base, and Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² under test condition OM2 governs the finished food-contact structure; specific migration for any additive concentrates must be verified against the individual additive limits in the European positive list. Processing is performed on three-layer coextrusion blown-film platforms with barrel temperatures rising from 180 °C in the feed section to 210–230 °C at the die, die gaps between 1.8 mm and 2.4 mm, blow-up ratios of 2.2:1–2.8:1, and an internal bubble cooling system to bring the frost line down to 2–4 die diameters above the air ring. On lines without internal bubble cooling, operators have observed bubble flutter and gauge variation when output exceeds 300 kg/h, especially when the hexene resin content exceeds 85 wt% because the hexene branches lower melt tension relative to high-pressure LDPE. Terminal products include printed bread bags, snack pouches, stand-up pouch sealant webs, and converted flow-wrap films where hot-tack strength is the critical control parameter.
On vertical form-fill-seal lines used for quick-frozen vegetables, seafood, and meat, the seal layer is usually a 60–85 wt% blend of TF-0119-F with 15–40 wt% high-pressure LDPE, a 0.5–1.5 wt% antiblock masterbatch, and no high-slip additive unless an outer layer requires coefficient of friction below 0.20 for downstream case packing. Compliance for frozen food packaging is assessed under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, while low-temperature mechanical integrity is evaluated against ASTM D746-20 for brittleness temperature and ASTM F88/F88M-21 for seal strength at 23 °C and after conditioning at −25 °C for 48 h. The converting process is usually a 2.5 mil tri-layer coextruded blown film run at melt temperatures of 190–215 °C, die gap 2.0 mm, blow-up ratio 2.0:1–2.4:1, with a frost line held below 3 die diameters so that molecular orientation does not produce a splitty film at freezer temperatures. Form-fill-seal equipment uses flat sealing jaws at 100–130 °C and 350–600 kPa jaw pressure, with dwell times of 0.20–0.40 s; the hexene comonomer distribution supports hot-tack over a wider sealing-temperature range than butene copolymers, but the upper temperature boundary must be constrained because excessive seal temperatures create chain scission at the seal interface and reduce cold peel fracture resistance. Terminal products include frozen shrimp bags, IQF vegetable pouches, and meat-packaging liners where puncture, not gas barrier, governs the shelf-life failure mode. The film is not an oxygen barrier; use in vacuum skin packaging for oxygen-sensitive products requires coextrusion with EVOH or PVDC and is outside the resin’s single-layer performance envelope.
Under ensiling conditions, the film is exposed to UV radiation, silage leachate acids, and repeated abrasion from bale wrappers and pit cover trampling, so the formulation is built around TF-0119-F at 90–97 wt% with 3–7 wt% carbon black masterbatch and a hindered amine light stabilizer package at 0.5–2.0 wt% to achieve a service life of 12–18 months. The relevant seasonal-use standard is EN 13207:2018 for thermoplastic silage films, with weathering verification under ISO 4892-2:2013 and tensile retention under ISO 527-3:2018; carbon black loading is tied to UV screening, and any reduction below 3 wt% lowers the surface resistivity and accelerates oxidation at fold points. Film production is executed on a three-layer blown-film line with die diameter 250–400 mm, die gap 2.0–2.4 mm, blow-up ratio 2.5:1–3.0:1, and melt temperatures 190–220 °C; black masterbatch concentrates at 30–40 wt% carbon black can raise melt pressure and necessitate more frequent screen pack changes than natural film runs. Finished gauge ranges from 25–45 µm for bale-wrap constructions to 100–150 µm for pit-cover sheet; downstream bale wrappers apply 55–75% pre-stretch, and the film must retain enough elastic recovery to hold bale density without tearing at the overlap points. Terminal products are round-baled haylage film, maize silage pit covers, and stretch-banded silage bags; the film is not intended for use as a structural greenhouse covering where multi-year UV warranties are required.
Machine-grade stretch films are typically cast on three-layer slot-die lines with die widths of 1.5–3.0 m, air gaps of 20–80 mm, and chilled roll temperatures of 15–30 °C. The core layer contains 75–85 wt% TF-0119-F, with 15–25 wt% metallocene linear low-density polyethylene to add dart impact and tear resistance, while the cling layers use 5–15 wt% cling agent masterbatch and 1–3 wt% antiblock/anti-tack additive in a carrier resin; overall film thickness is typically 8–23 µm. Compliance is validated using ASTM D5458-95 for peel cling and ASTM D638-14 for tensile properties, with elongation at break generally exceeding 300% in the machine direction when the resin is cast in the core; pre-stretch retention is monitored on the converting line because residual stress after film winding dictates pallet load stability. The hexene backbone gives higher dart impact and slow-puncture resistance than a butene-linear film at comparable gauge, but it also shifts the cling migration curve: at warehouse temperatures below 10 °C, peel cling can drop below the 50 g/25 mm threshold needed for secure pallet wrap unless the cling additive is reformulated for low-temperature bloom. Converting on cast-film equipment requires careful edge trim handling, because the cling masterbatch increases tack at the edge-trim refeed block and can cause screw feed bridging when edge material exceeds 20 wt% of the core layer feed. Terminal products include hand stretch wrap, machine stretch wrap for rotary and turntable wrappers, powered pre-stretch film, and dust-suppression wrap for logistics centres.
In protective void-fill and air-cushion converting, the film must survive high-speed inflation and snap-back flexing without pinhole formation. Three-layer cast coextrusion runs with a core at 80–95 wt% TF-0119-F, 5–20 wt% metallocene LLDPE, and 1–2 wt% polymer processing aid to reduce die lip buildup over long campaigns. The packaging compliance baseline is EU Directive 94/62/EC Annex II, with total concentration of lead, cadmium, mercury, and hexavalent chromium not exceeding 100 mg/kg in the package; if electronics goods are shipped, REACH SVHC screening and RoHS 2011/65/EU Annex II restrictions may additionally apply to the finished inflated cushion. Film production uses a cast coextrusion line with slot die gap 0.5–1.0 mm, chill roll temperature 20–35 °C, gauge 45–70 µm, and gauge variation held within ±2% to avoid local thinning at inflation seals. Downstream inflation machines seal the two plies at 120–160 °C on heated rotary sealing jaws and then inflate with compressed air; the hexene copolymer’s high slow-puncture resistance reduces pinhole formation when heavy cartons shift during transport. Terminal products are air pillows, void-fill cushions, air-chamber wrap-around sleeves, and mixed-carton stabilizing air bags. Static charge build-up is a known processing issue at relative humidity below 20%, so antistatic masterbatch or ionizing bars on the slitter are often required.
For heavy-duty shipping sacks and box liners carrying dry-flowable powders, films are typically 100–250 µm thick and formed on blown-film lines with die diameters of 300–500 mm, die gaps of 2.4–3.0 mm, blow-up ratios of 1.8:1–2.2:1, and output rates of 400–650 kg/h using barrier screws with L/D ratios of 30:1 or 36:1. Formulation addition is 80–100 wt% TF-0119-F, 0–20 wt% high-density polyethylene to raise modulus, 1–3 wt% carbon black or white masterbatch, and 0.5–2 wt% slip/antiblock masterbatch. Industry performance standards are ASTM D1709-16a for falling dart impact, ASTM D882-18 for tensile properties, and ISO 527-3:2018 for film tensile testing; where liners contact food-grade dry powders, FDA 21 CFR 177.1520(c) applies, and where used as an inner liner in UN-rated packaging the relevant 49 CFR or ADR/RID requirements govern the assembled sack. Downstream conversion includes in-line gusseting, bottom sealing, and heat-seal or sewn closure, with slit widths up to 1.8 m depending on die geometry. Terminal products are flexible intermediate bulk container liners, box liners, gusseted heavy-duty sacks, and valve sacks for mineral powders or resins. The resin is not recommended for direct contact with aromatic solvents or strong oxidizers; long-term service above 60 °C reduces tear resistance and should be revalidated before use.
Competitive NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® TF-0119-F is a linear low-density polyethylene film resin produced with hexene-1 as the primary α-olefin comonomer. The designation identifies a hexene copolymer within the Novapol® film resin portfolio; the nominal density is 0.919 g/cm³ when determined by ASTM D792 or ISO 1183-1:2019, and the nominal melt index is 1.0 g/10 min at 190 °C under a 2.16 kg load as measured by ASTM D1238 or ISO 1133-1:2022. These values place the grade in the medium-stiffness film extrusion segment used for cast and blown packaging structures.
From a compositional standpoint, the material falls within the olefin polymer class. The hexene-1 comonomer introduces short-chain branches of six carbon atoms, in contrast to the four-carbon branches introduced by 1-butene. This structural difference is not apparent from density or melt index readings alone, but it affects melt rheology, orientation behaviour, and film toughness. The resin is supplied as free-flowing pellets, and the supplier’s current technical data sheet remains the controlling document for release limits, additive package, and lot-to-lot variation.
| Property | Nominal value | Test method |
|---|---|---|
| Melt index at 190 °C, 2.16 kg | 1.0 g/10 min | ASTM D1238, ISO 1133-1:2022 |
| Density at 23 °C | 0.919 g/cm³ | ASTM D792, ISO 1183-1:2019 |
| Comonomer type | Hexene-1 | Manufacturer designation |
| Physical form | Free-flowing pellets | Visual inspection |
In cast film extrusion, the melt index of 1.0 g/10 min is a pivotal variable because it influences both screw back pressure and the critical draw ratio. Draw resonance is observed as periodic gauge oscillation and is triggered when the take-up speed exceeds a critical value for a given die gap, air gap, melt temperature, and extensional rheology. On conventional single-screw lines with L/D ratios from 24:1 to 30:1 and coat-hanger dies with a die gap of 0.4 mm to 1.0 mm, hexene LLDPE grades in this melt-index class are typically processed at melt temperatures between 210 °C and 260 °C. Published data for this specific configuration is limited to supplier processing guides and line-specific trials.
To control draw resonance, the chill-roll temperature is typically maintained between 15 °C and 30 °C, with the air gap reduced to the shortest setting that avoids web instability. A longer air gap generally increases molten web sag and lowers the critical draw ratio, whereas a shorter gap accelerates quench and can preserve optical properties. The 0.919 g/cm³ density should not be interpreted as indicating the behaviour of high-pressure LDPE; hexene LLDPE has lower melt strength and therefore requires stricter control of die-to-roll distance and air gap than a branched LDPE of similar density.
Moisture uptake is not normally a processing constraint for polyethylene pellets stored in closed packaging. If pellets are exposed to high relative humidity or surface condensation, pre-drying at 70 °C to 80 °C for 2 h using a desiccant-air dryer is sufficient to remove trapped surface moisture. Extended exposure above 80 °C should be avoided to prevent pellet agglomeration in the hopper.
Where blown film is used, stable bubble configuration is governed by blow-up ratio, frost line height, and melt temperature. Blow-up ratios of 2.0:1 to 3.0:1 and frost line heights of 5 to 10 die diameters are common for linear low-density polyethylene film lines; these are process variables rather than product specifications and must be tuned to the die and air ring. The absence of long-chain branching in linear hexene polyethylene reduces bubble stability compared with LDPE, so processors may need to blend with 10–20 wt% LDPE or use grooved-barrel extruders to manage output and melt pressure.
Film tensile properties are typically determined according to ASTM D882 or ISO 527-3 on strips cut parallel and transverse to the machine direction. For a 25 µm cast film, commercial hexene LLDPE resins of 0.919 g/cm³ density generally exhibit higher secant modulus values than comparable butene copolymers; however, exact values for TF-0119-F are not reproduced here because film properties depend on quench rate, gauge variation, and additive bloom. The manufacturer’s technical data sheet provides the current typical film data generated under defined laboratory processing conditions.
Dart impact is measured by ASTM D1709, Method B, or ISO 7765-1; Elmendorf tear is measured by ASTM D1922 or ISO 6383-2. These toughness indicators are sensitive to film gauge and orientation. In blown film, increasing blow-up ratio from 2.0:1 to 3.0:1 shifts the balance between machine-direction and transverse-direction tear. The hexene branch length influences the tie-molecule concentration and therefore tear propagation resistance more than the density value alone would suggest.
Optical properties, including haze and clarity, are evaluated by ASTM D1003; gloss is evaluated by ASTM D2457. On cast film lines, rapid quench achieved at chill-roll temperatures of 15 °C to 25 °C reduces spherulite size and improves clarity, but insufficient quench or excessive melt temperature can raise haze. Industrial cast film lines often monitor these optical responses as indirect indicators of quench uniformity and die-lip cleanliness. Coefficient of friction, when specified, is measured by ASTM D1894; slip and antiblock additive packages can alter this value significantly, so the grade’s additive formulation must be verified before converting line trials.
For packaging films in which machine-direction tear and dart impact define the specification, replacing a 1-butene LLDPE with a hexene-1 LLDPE of equivalent density and melt index often moves the property balance toward higher toughness. The six-carbon short-chain branch in hexene copolymers is more effective than the four-carbon butene branch in promoting tie-molecule formation between crystal lamellae; this effect is supported by solid-state NMR, small-angle X-ray scattering, and Raman crystallization studies. The practical consequence is generally improved Elmendorf tear and slower crack propagation under impact, as measured by ASTM D1922 and ASTM D1709.
The comparison is not unconditional. Differences in molecular weight distribution, catalyst type, comonomer distribution, and film orientation can reverse the expected ranking. A solution-process hexene LLDPE may show better dart impact than a gas-phase butene LLDPE of the same density, while a high-clarity butene grade with a narrow comonomer distribution may still offer lower haze. Selection of TF-0119-F should therefore rest on pilot-line film data generated at the intended gauge and draw ratio, not on comonomer identity alone.
Compared with 1-octene LLDPE, industry experience generally indicates that octene copolymers can provide higher puncture and tear toughness at similar density because the longer C8 branch further increases tie-molecule mobility. Hexene LLDPE often represents a balance of toughness, stiffness, and processability for cast stretch film and high-strength liners. Published direct comparative data for TF-0119-F versus octene grades is limited; the manufacturer’s technical data sheet should be consulted for current typical values and for any new lot-specific data.
At the line-trial level, three process responses distinguish TF-0119-F from butene-based grades of similar density. First, web tear at the winder may show fewer oriented fractures because the hexene branch reduces yield stress anisotropy in the cast web. Second, the film may tolerate a smaller air gap before draw resonance occurs, consistent with the melt strength characteristics of linear hexene copolymers. Third, the quenched film may exhibit higher gloss retention when the chill roll is run at lower temperatures, provided die-lip buildup is controlled with a clean resin stream. These observations require confirmation on the actual production line because slip and antiblock packages alter surface friction and tear.
| Region | Reference | Relevant criterion |
|---|---|---|
| United States | 21 CFR 177.1520(c) | Olefin polymer food-contact clearance; article must meet density, extractive, and end-use conditions |
| European Union | Regulation (EU) No 10/2011 Annex I | Overall migration ≤ 10 mg/dm²; 60 mg/kg for infant food applications |
| Characterisation | ASTM D1238, ASTM D792, ISO 1133-1:2022, ISO 1183-1:2019 | Resin melt index and density determination standards |
Food-contact status is not a single resin property; it is an article-level fitness-for-use determination. In the United States, polyolefin resins may be evaluated under 21 CFR 177.1520(c), which covers olefin polymers for use in contact with food, provided the finished article meets extractive and end-use limitations. In the European Union, plastic food-contact articles must comply with Regulation (EU) No 10/2011 Annex I, including the overall migration limit of 10 mg/dm² or 60 mg/kg for infant food applications. Converters must obtain a food-contact statement from NOVA Chemicals for TF-0119-F and verify that printing inks, tie resins, and lamination layers do not compromise final compliance.
Storage should follow the resin supplier’s recommendation for polyolefin film resins. Keep unopened packaging in a dry, well-ventilated area at temperatures below 50 °C, away from direct sunlight and ultraviolet sources. Although polyethylene does not require drying, recondensation on cold pellets moved into a humid area can introduce surface moisture into the hopper; if this occurs, dry-air purging is preferred. No post-arrival blending with other resins should be performed without verifying additive compatibility, because slip and process stabilizer packages can interact with other materials and change the measured coefficient of friction or colour stability.