    Specifications
    HS Code 740667
    Comonomer Hexene
    Polymer Type Linear Low-Density Polyethylene (LLDPE)
    Density 0.919 g/cm³
    Melt Index 0.9 g/10 min
    Melt Flow Ratio I21 I2 30
    Tensile Strength At Yield Md 11 MPa
    Tensile Strength At Yield Td 11 MPa
    Tensile Strength At Break Md 38 MPa
    Tensile Strength At Break Td 30 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Drop Impact 180 g
    Elmendorf Tear Md 250 g
    Elmendorf Tear Td 350 g
    Haze 8%
    Gloss 45 75
    Coefficient Of Friction 0.20
    Blocking 50 g
    Vicat Softening Point 100 °C
    Melting Point 124 °C

    As an accredited NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin is supplied in 25 kg bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) NOVA Novapol TF-0119-D LLDPE: 20′ FCL holds 10 pallets, 550 × 25 kg bags, 13,750 kg net, shrink-wrapped and secured.
    Shipping NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin is shipped as non-hazardous plastic pellets in 25 kg bags, stretch-wrapped pallets, or bulk trucks/railcars. Keep packaging sealed and dry; avoid excessive heat, moisture, and UV. Store in a cool, dry area. Not regulated for transport under DOT, IMDG, or IATA.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, open flames, and static discharge. Keep original bags closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking, prolonged UV exposure, and temperature extremes. Use first-in, first-out inventory, inspect containers regularly, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original packaging in a cool, dry, well-ventilated area.
    Application of NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin

    In frozen food pillow pouch and ice bag applications, NOVA Chemicals Novapol TF-0119-D is processed as a hexene-copolymer linear low-density polyethylene film resin with a nominal density of 0.919 g/cm³ and a melt mass-flow rate of 1.0 g/10 min under ISO 1133-1:2022 conditions of 190 °C/2.16 kg. Food-contact compliance rests on FDA 21 CFR 177.1520(c) for olefin polymers in direct food contact and on EU Regulation (EC) No 10/2011, which imposes an overall migration limit of 10 mg/dm² and specific migration limits for the additives used in the sealant layer. The sealant formulation is typically compounded at 70–85 wt% TF-0119-D, 15–30 wt% high-pressure LDPE with a melt index between 0.7 g/10 min and 2.0 g/10 min, 0.3–1.0 wt% synthetic silica antiblock masterbatch, and 0.1–0.3 wt% erucamide slip concentrate to control coefficient of friction during high-speed filling. On a commercial blown-film line using a grooved-feed single-screw extruder with 30:1 L/D and a 250–350 mm spiral-mandrel die, the process typically runs at a die gap of 1.8–2.5 mm, blow-up ratio 2.0–2.5:1, melt temperature 190–225 °C, and frost line height 8–12 die diameters; corona treatment is maintained at 38–42 dyn/cm for lamination or print adhesion. The finished product types include side-seal and bottom-seal pillow pouches for frozen vegetables, ice cube bags, and bag-in-box liners for chilled liquids. Pre-drying is not required under normal ambient storage, but if warehouse relative humidity exceeds 60% RH and the resin is transferred into a humid feed zone, hopper condensation can introduce pinholes and bubble instability.

    What Blown Film Parameters Govern Puncture Resistance in Silage Wrap?

    The puncture resistance of agricultural silage wrap and greenhouse cover film depends on the interaction of blow-up ratio, frost line height, and die gap rather than resin selection alone. Agricultural silage film is assessed under EN 13206:2001 or equivalent national specifications for thermoplastic stretch films for bale wrapping; greenhouse and mulch films are further placed on the market under REACH Regulation (EC) No 1907/2006, with Annex XVII restrictions applying to certain UV stabilizer decomposition products. A typical UV-stabilized compound for silage wrap or greenhouse film contains 80–95 wt% TF-0119-D, 3.0–6.0 wt% HALS-based UV masterbatch, 1.0–2.5 wt% titanium dioxide or carbon black masterbatch, and 0.5–1.5 wt% LDPE processing-modifier concentrate to stabilize the bubble under high-blow conditions. Extrusion on a 300 mm spiral-mandrel die with internal bubble cooling and a dual-lip air ring operates at a die gap of 1.6–2.2 mm, blow-up ratio 2.5–3.0:1, melt temperature 200–230 °C, and frost line height 1.2–1.8 m. Finished products are silage wrap rolls for round balers, greenhouse covering film, and low-tunnel mulch film. The operational boundary is the frost line: at blow-up ratios above 3.0:1, a low frost line height below 1.0 m produces excessive transverse-direction shrinkage and can reduce puncture resistance when tested by ISO 7765-1; above 6.0 wt% UV masterbatch, die-lip plate-out increases cleaning frequency on long production runs.

    In heavy-duty sack extrusion, the hexene comonomer branch architecture improves dart impact and tear resistance relative to butene LLDPE at equivalent melt index, which allows film downgauging for filled-sack applications without sacrificing drop performance. Heavy-duty sack compounds are typically specified under ASTM D4976 for polyethylene feedstock and tested for impact and tear by ASTM D1709 and ASTM D1922; export sacks for polymer granules are further assessed for filled-bag drop resistance under ISO 7965-1 or equivalent national transport packaging codes. The formulation range for 100–250 µm thick film is 65–85 wt% TF-0119-D, 10–25 wt% butene-LLDPE or high-pressure LDPE, 5–15 wt% post-industrial repellets with melt filtration at 100 µm or finer, and 1.0–2.5 wt% anti-slip masterbatch. Blown-film production uses a 200–350 mm spiral-mandrel die with die gap 2.0–2.8 mm, blow-up ratio 1.8–2.2:1, melt temperature 195–220 °C, internal bubble cooling, and gusseting at 100–150 mm. Terminal finished goods include form-fill-seal heavy-duty sacks for polymer granules, fertilizer sacks, FIBC liners, and protective sheeting for geomembrane transport. If the TF-0119-D fraction drops below 65 wt%, the film typically no longer retains the dart impact margin required by ASTM D1709 for 200 µm heavy-duty sacks; end-user specifications commonly require a minimum of 350 g, but published values for this exact formulation are limited. If regrind exceeds 15 wt% without adequate gel filtration, pinhole-induced burst failures increase on the filling line.

    When Hexene LLDPE Is Extruded as a Pallet Stretch Hood Layer

    Stretch hood palletization lines demand a balance of puncture resistance, elastic recovery, and film-to-film cling during high-speed automatic application. Stretch hood film for industrial load containment is characterized under ASTM D882 for tensile properties and ISO 7765-1 for impact resistance; when the film is used in export packaging, national packaging waste and hazardous substance requirements such as EU Packaging and Packaging Waste Directive 94/62/EC may apply to overall heavy metal content. Coextruded structures typically run 60–80 wt% TF-0119-D in the outer and core layers for puncture resistance, 20–40 wt% metallocene-catalyzed ethylene-hexene or ethylene-octene copolymer with melt index 0.5–1.5 g/10 min to increase elongation at break, and 0.5–1.0 wt% cling agent masterbatch in the outer surface layer. Cast film production offers higher line speeds, while blown-film production of stretch hood uses a 250–400 mm die, die gap 2.0–2.5 mm, blow-up ratio 1.8–2.2:1, melt temperature 210–240 °C, and edge trim recycled at 5–10 wt% if approved. Terminal types include stretch hood film rolls for automatic pallet wrapping machines, pallet covers, and weather protection shrouds for tall loads. At melt temperatures above 250 °C, oxidative gel formation increases and tear initiation resistance can decline; at metallocene copolymer addition above 40 wt%, blocking strength may increase to levels that impede film opening on automated equipment.

    Adhesive lamination for stand-up pouches and liquid packaging often uses a blown LLDPE sealant web rather than a hot-melt coating; the resin’s low seal initiation temperature supports fast jaw-cycle speeds. The sealant web is placed on the food-contact side and must comply with FDA 21 CFR 177.1520(c) and EU Regulation (EC) No 10/2011; in pharmaceutical or medical pouch structures, ISO 11607-1:2019 may govern converted package integrity. The sealant layer formulation is commonly 55–75 wt% TF-0119-D, 20–30 wt% high-pressure LDPE or ethylene vinyl acetate with vinyl acetate content 4–9 wt%, and 0.5–1.5 wt% antiblock masterbatch; the middle and outer layers may use the same resin at higher concentration to preserve stiffness. Blown-film coextrusion on a 200–300 mm die with die gap 1.6–2.0 mm, blow-up ratio 2.0–2.4:1, and melt temperature 190–215 °C is followed by adhesive lamination to reverse-printed 12–23 µm PET or 15–20 µm BOPP webs at 150–250 m/min. Finished goods are stand-up pouches for liquids, sachets, lidding film, and modified-atmosphere packaging laminates. On packaging lines exceeding 40 cycles/min, hot-tack strength should be characterized by ASTM F1921; if the sealant layer falls below 55 wt% of this resin, the hot-tack force may drop below 1.5 N/25 mm, causing seal failure during continuous vertical form-fill-seal operation. Published industrial data for this exact film structure is limited; line trials remain the standard method for setting sealant-layer dilution limits.

    Collation Shrink Overwrap and Machine-Direction Shrink Force

    Collation shrink overwrap relies on controlled machine-direction orientation to hold bottled goods, cans, and cartons in a tight bundle through the distribution chain. Shrink film for this application is characterized by unrestrained linear thermal shrinkage under ASTM D2732 and shrink force under ISO 14616; regulatory status for packaging waste falls under EU Directive 94/62/EC, Annex II for heavy metal concentration limits. The blown-film formulation commonly contains 70–90 wt% TF-0119-D, 10–30 wt% high-pressure LDPE with high melt strength, and 0.5–1.5 wt% antistatic or antifog masterbatch only where end-use line conditions require static dissipation; antiblock is generally avoided because surface friction is needed for bundle stability. Extrusion at a die gap of 1.8–2.2 mm, blow-up ratio 1.8–2.0:1, and melt temperature 195–225 °C is followed by machine-direction orientation at draw ratios between 4:1 and 6:1; the shrink tunnel operates at 150–180 °C for 1.5–3.0 s. Terminal products include bottled water collation bundles, canned food shrink wraps, aerosol can multipacks, and industrial bundle overwrap. At draw ratios above 6:1, machine-direction tear propagation along perforation lines can cause splitting; if high-pressure LDPE content falls below 10 wt%, bubble instability during the orientation step may create uneven shrink force and loose bundle corners.

    Free Quote

    Competitive NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Novapol® TF-0119-D is a 1-hexene linear low-density polyethylene film resin characterized by a nominal density of 0.919 g/cm³ and a melt index of 1.0 g/10 min, the latter determined according to ASTM D1238 at 190 °C and 2.16 kg. Density is determined according to ASTM D792. The resin is supplied in pellet form and is intended for blown-film and cast-film conversion in monolayer and coextruded structures. It does not include a UV stabilizer or antimicrobial package as supplied; those additives require separate masterbatch incorporation.

    In production-scale cast-film operations, the resin is extruded through slot dies with gap settings from 0.5 mm to 0.8 mm and chill-roll surface temperatures from 18 °C to 25 °C. In blown-film conversion, reference conditions on a 50 mm grooved-feed extruder with 24:1 L/D screw have included melt temperatures of 204 °C to 216 °C, blow-up ratios from 2.0:1 to 2.5:1, and frost-line heights from 200 mm to 400 mm. These process coordinates are industrial reference points rather than resin specification limits.

    Which Standards Govern the Olefin Compliance Profile of Novapol TF-0119-D?

    Compliance of the unmodified polymer with food-contact requirements is evaluated under U.S. FDA 21 CFR 177.1520(c), which applies to olefin polymers used in contact with food. The resin is expected to meet the olefin polymer specifications; however, final articles containing colorants, slip, antiblock, or processing aids must be tested in their final formulation. For European applications, the governing framework is Regulation (EU) No 10/2011, with overall migration measured according to EN 1186 and specific migration of substances such as 1-hexene-derived oligomers assessed under EN 13130 when applicable. The resin is not formulated with restricted phthalates or hazardous heavy metals, but justification for RoHS compliance under RoHS Directive 2011/65/EU requires analysis of the final compound.

    PropertyTest methodTypical value
    Melt index (190 °C/2.16 kg)ASTM D12381.0 g/10 min
    DensityASTM D7920.919 g/cm³
    Comonomer—1-hexene
    Melting point (DSC)ASTM D3418122 °C
    Vicat softening pointASTM D1525102 °C

    Table 1 lists published nominal resin properties. These values are typical and are not specification limits; the current certificate of analysis governs lot-to-lot variation.

    Regulatory referenceScopeTest method
    U.S. FDA 21 CFR 177.1520(c)Olefin polymer food-contactEnd-use extraction
    Regulation (EU) No 10/2011Plastic food-contact migrationEN 1186, EN 13130
    RoHS Directive 2011/65/EUHazardous substance restrictionMaterials analysis

    Table 2 lists regulatory references applicable to the unmodified base resin; certification of a fabricated article must account for all additives and layer constituents.

    The primary technical distinction between TF-0119-D and butene-based LLDPE grades of the same density and melt index is the longer short-chain branch length of 1-hexene relative to 1-butene. The C6 branch is more effective at creating interlamellar tie chains, which increases the crack-propagation resistance of the semicrystalline network. This difference is measured in fabricated film as higher dart impact under ASTM D1709 and higher Elmendorf tear under ASTM D1922. When compared with LDPE of the same density, the hexene LLDPE has superior tensile elongation under ASTM D882 but lower melt strength; converters without internal bubble cooling often blend 10 wt% to 30 wt% LDPE to maintain bubble stability.

    When Hexene Short-Chain Branching Shifts Tear and Impact Balance

    In three-layer coextruded packaging films, placing TF-0119-D in the skin layers instead of the core shifts the balance of machine-direction and transverse-direction tear. At a 2.5:1 blow-up ratio and a 300 mm frost-line height, the orientation state of the skin layers is altered; this can reduce machine-direction tear as measured by ASTM D1922. Manufacturer-published data for this specific configuration is limited; tear values must be generated on the target line because die gap, blow-up ratio, and cooling rate modify orientation and cocrystallization.

    Seal initiation and hot-tack performance are evaluated according to ASTM F1921 and ASTM F88. Hexene LLDPE generally develops seal strength at lower temperatures than butene LLDPE at equivalent density and melt index, but the actual seal window depends on film gauge, additivation, and coextruded sealant-layer composition. The resin is not recommended for bake-in-bag service above 100 °C without verification of antioxidant migration and organoleptic performance under final-use conditions.

    Compared to octene-based LLDPE produced in solution processes, TF-0119-D may exhibit a broader molecular weight distribution that improves bubble stability but can detract from optical clarity. In high-clarity packaging applications where haze is measured by ASTM D1003, metallocene LLDPE grades are often preferred; TF-0119-D is selected when puncture resistance, gouging resistance, and downgauging capability govern the technical specification.

    The anisotropic tear profile of blown films produced from TF-0119-D is influenced by the ratio of machine-direction draw to transverse-direction expansion. At a 2.0:1 blow-up ratio, machine-direction orientation is stronger, and the film often exhibits lower machine-direction tear and higher transverse-direction tear under ASTM D1922. At 2.5:1, the transverse-direction orientation increases, narrowing the difference. The frost-line height controls the amount of stress relaxation available before crystallization; a frost-line position too high permits excessive molecular relaxation and can reduce tensile modulus under ASTM D882. A frost-line position too low freezes in orientation and can embrittle the film. These interactions are primary process-control levers in high-stalk extrusion.

    Film Extrusion Equipment Conditions and High-Stalk Bubble Stability Boundary

    High-stalk blown-film lines place greater demand on melt tension than low-stalk configurations. The resin’s molecular weight distribution and comonomer distribution control the draw-resonance stability and the maximum attainable blow-up ratio. On a 45 mm extruder with 24:1 L/D, 2.0 mm die gap, and 40 µm screen pack, a melt temperature above 220 °C lowers extensional viscosity and can destabilize the bubble, while operation below 195 °C raises die pressure and reduces throughput. The practical processing window is therefore bounded by melt temperature, die pressure, and frost-line height; these boundaries vary with screw design, die geometry, and internal bubble cooling.

    Severe gel formation is observed when melt temperature exceeds 250 °C or when residence time in the extruder exceeds 10 min in stagnant flow regions. Gels larger than 200 µm degrade film appearance and reduce tear strength under ASTM D1922. The resin should not be pre-dried unless stored at relative humidity above 60%; if surface moisture is present, a desiccant dryer at 60 °C for 2 h is sufficient to condition the pellet surface.

    In high-output cast-film lines, the onset of sharkskin and melt fracture is governed by wall shear stress at the die lip. For linear low-density polyethylene, the critical shear stress is often reported between 0.10 MPa and 0.20 MPa; die gap and melt temperature are adjusted to keep shear stress below the critical value. The 0.5 mm to 0.8 mm die gaps used for TF-0119-D in cast-film production are consistent with that shear-stress control. Maintaining the melt below the critical shear stress reduces die-lip buildup and optical defects.

    Published data for the melt flow ratio and full molecular weight distribution of TF-0119-D is limited; converters relying on rheometer data should obtain the supplier’s current lot-specific curve before designing a die or screw. The nominal melt index alone does not fully predict shear thinning, melt curvature, or bubble stability.

    Typical film structures include heavy-duty sacks, agricultural film, and laminating film. In heavy-duty sacks, the resin is coextruded with high-density polyethylene core layers to improve puncture resistance measured by ASTM D5748 and tear resistance measured by ASTM D1922. In agricultural film, the resin may be blended with metallocene LLDPE to modify tear-propagation resistance; the final formulation requires a separate UV-stabilizer masterbatch because the base resin does not contain UV stabilization. Published data for this specific configuration is limited.

    Slip and antiblock masterbatches based on erucamide or oleamide modify the film coefficient of friction under ASTM D1894. Typical letdown ratios are 1 wt% to 3 wt%, and the final static coefficient of friction for form-fill-seal conversion is often controlled between 0.20 and 0.35. Higher slip loadings can increase haze and reduce hot-tack performance under ASTM F1921; formulation development must balance these results.

    The material is not recommended for injection molding or for applications requiring continuous service above 80 °C without additional heat stabilizers. It is not formulated for potable-water pipe extrusion. These limitations reflect the standard thermal-oxidative envelope of linear low-density polyethylene film grades and do not replace end-use qualification under the applicable application-specific standards.

    Top