Nova Chemicals Novapol Td 9022 C Superhexene Lldpe

NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE

    • Product Name: NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 370684
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.920 g/cm³
    Meltindex 0.80 g/10 min
    Meltflowratio 27
    Tensilestrengthatyieldmd 10.3 MPa
    Tensilestrengthatyieldtd 9.7 MPa
    Tensilestrengthatbreakmd 33.1 MPa
    Tensilestrengthatbreaktd 29.0 MPa
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Dartdropimpact 120 g
    Elmendorftearstrengthmd 250 g
    Elmendorftearstrengthtd 400 g
    Haze 12%
    Gloss45degree 55%
    Vicatsofteningpoint 100°C
    Meltingpoint 122°C

    As an accredited NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, stacked on pallets and stretch-wrapped; bulk truck or railcar options may also be available.
    Container Loading (20′ FCL) 20′ FCL loading: 22 MT NOVA Chemicals Novapol TD-9022-C Superhexene LLDPE in 25 kg bags, 880 bags, palletized.
    Shipping Novapol® TD-9022-C Superhexene LLDPE ships as non-hazardous polyethylene pellets, typically in 25 kg bags, 500–1000 kg bulk bags, or bulk trucks and railcars. It is not classified as dangerous goods for transport. Store dry, cool, away from ignition sources, and follow SDS and local regulations.
    Storage NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE should be stored in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep bags or containers sealed to prevent moisture, odor, and contamination. Avoid prolonged UV exposure. Use clean handling equipment, follow manufacturer/SDS guidance, and practice first-in, first-out inventory rotation.
    Shelf Life Novapol® TD-9022-C Superhexene LLDPE shelf life: two years from manufacture when stored unopened in original packaging under normal conditions.
    Application of NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE

    On three-layer blown-film lines for heavy-duty industrial sacks and FIBC liners, Novapol® TD-9022-C Superhexene LLDPE is processed at a melt temperature of 195–230°C, a spiral mandrel die gap of 1.8–2.5 mm, and a blow-up ratio of 2.0:1–2.8:1. The resin’s nominal density is 0.918 g/cm³ and its melt index is 0.9 g/10 min under ASTM D1238 at 190°C/2.16 kg. The superhexene comonomer reduces melt fracture relative to butene LLDPE at equivalent viscosity, but line operators report bubble side-to-side flutter when the high-pressure LDPE fraction exceeds 35 wt% or when the frost line is moved above the air ring exit by more than 200 mm. For sack structures, the resin is dosed at 65–90 wt% in the core layer and 0–35 wt% high-pressure LDPE in the skin layers to stabilize the bubble, with 1.0–2.0 wt% fluoroelastomer processing aid and 0.5–1.5 wt% slip/antiblock masterbatch added when extrusion output exceeds 300 kg/h. Finished sack compliance is tested under ISO 7965:2018 drop testing and ISO 21898 for FIBC liners, while film tear and tensile properties are measured under ASTM D882-18 and ASTM D1922-15; gauge variation across the film web is held to ≤±5% to prevent weak spots at bottom gussets. Downstream conversion includes corona treatment to 38–42 mN/m, bottom sealing by heat or ultrasonic welding, and insertion into woven PP outer sacks. End products are 25 kg fertilizer and petrochemical sacks, FIBC inner liners, hazardous-goods packagings where UN drop-test certification is required, and mineral powder bags with capacity up to 50 kg.

    What Limits Low-Temperature Puncture Performance in Silage Film After Anaerobic Fermentation?

    Silage bale wrap and clamp sheets using TD-9022-C are specified for puncture resistance after months of contact with acidic silage effluent and exposure to ultraviolet radiation. In a three-layer coextruded construction, the outer layers carry 85–95 wt% TD-9022-C and 5–15 wt% high-pressure LDPE, while the core carries 70–90 wt% TD-9022-C; a UV-stabilized carbon black masterbatch is metered into all layers at 4–8 wt% overall, with the final carbon black concentration in the film controlled to the EN 13207 light transmission and weathering requirements. Processing uses a grooved-feed extruder with 25–30 L/D barrier screw and spiral mandrel die at melt temperature 200–220°C, and die gap is maintained at 1.6–2.4 mm because deviations greater than ±0.05 mm create thick lanes that resist stretching on baler films. The critical process window for bubble stability with high carbon black loading is ±5°C around the frost line temperature; below that window, bubble diameter oscillation produces helical gauge bands and finished roll hardness variations. Film is tested for dart drop at −20°C after 48 h conditioning under ASTM D1709, and tear resistance under ASTM D1922. Downstream conversion includes edge trimming, surface treatment, slitting to 500 mm or 750 mm rolls, and winding on baler-compatible cores. End products are round-bale silage wrap, silage clamp covering sheets, greenhouse side films, and mulch film where multi-season UV resistance is validated by ISO 4892-2 weathering and EN 13207 field exposure. Published data for this specific grade under high-UV, multi-season agricultural service is limited; converters typically run field trials before substituting the grade into existing agricultural constructions.

    On cast film lines with polished chill rolls at 18–24°C and die widths from 1,500 mm to 2,000 mm, TD-9022-C is used in the core layer of machine stretch wrap at 65–85 wt% to maximize machine-direction toughness while the skin layers carry metallocene-catalyzed LLDPE or ULDPE at 15–35 wt% for high on-machine pre-stretch and controlled cling. A polyisobutylene tackifier masterbatch is dosed into the cling skin layer at 0.5–3.0 wt%; a slip/antiblock package is added to the opposite skin at 0.5–1.0 wt% to produce one-side cling film. If the tackifier masterbatch drops below 0.3 wt%, cling force falls below the minimum level required for pallet stabilization, and if chill roll temperature exceeds 28°C, residual heat causes blocking and telescoping on the winder. The cast process runs at 400–600 m/min, with die lip gaps between 0.5 mm and 0.9 mm and air gap adjusted so that melt web neck-in remains below 3% of die width. Compliance for stretch wrap is assessed using ASTM D5748 for cling and stretch retention, and ASTM D882 for machine-direction elongation at break; load containment is verified on finished pallets by ASTM D5331 for load stability. End products include machine-grade pallet wrap from 15 µm to 50 µm, hand-wrap film, and pre-stretched film.

    Three-layer cast stretch film construction using TD-9022-C in the core layer
    LayerLayer thickness shareTD-9022-C content in layerFunctional additiveTest method
    Core60–80%65–85 wt%Processing aid 0.5–1.0 wt%ASTM D882
    Cling skin10–20%0–20 wt%Tackifier masterbatch 0.5–3.0 wt%ASTM D5748
    Slip skin10–20%0–20 wt%Slip/antiblock 0.5–1.0 wt%ASTM D1894

    Frozen Food Sealant Webs and Cold-Temperature Seal Integrity

    Frozen food sealant webs made from TD-9022-C are coextruded or laminated to PET, BOPP, or metallized PET and are evaluated for seal strength at −20°C after package filling and frozen distribution. The sealant layer formulation contains 70–100 wt% TD-9022-C with 0–30 wt% high-pressure LDPE to shift seal initiation temperature; slip and antiblock masterbatches are kept at 1.0–2.0 wt%, and no amine-based additives are incorporated because they can interfere with sealant-layer adhesion and organoleptic performance. The blown film process uses a 30:1 L/D barrier screw with die temperatures between 180–210°C and die gaps of 1.5–2.0 mm, producing sealant films from 20 µm to 35 µm that are then solventless-laminated to printed barrier substrates. Heat seal performance is measured according to ASTM F88/F88M at 0.3–0.5 MPa seal pressure and 0.5–1.0 s dwell time, with seal initiation temperatures recorded over a 60–120°C range to identify the lower operational boundary. Compliance for direct food contact in the United States is evaluated under FDA 21 CFR 177.1520(c) and in the European Union under Regulation (EU) No 10/2011, with overall migration testing performed according to EN 1186 and specific migration of selected additives according to applicable annexes. Downstream processes include extrusion lamination, adhesive lamination, printing, and pouch-making with vertical or horizontal form-fill-seal machines. End products are frozen vegetable bags, ice cream pouches, seafood packaging, and frozen poultry bags where needle-puncture resistance and cold-temperature seal integrity are required.

    For seamless industrial drum and bin liners in 100–250 µm thickness, TD-9022-C is dosed at 90–100 wt% with 0–10 wt% LDPE for melt strength adjustment and 1.0–2.0 wt% slip/antiblock masterbatch; antistatic masterbatch is added at 0.5–2.0 wt% only where liners are used to protect combustible powder filling operations. The liner is produced on a downward-extrusion blown-film line with die diameter 400–600 mm, die gap 1.8–2.5 mm, and melt temperature 190–220°C, then is aged 24 h before welding to remove residual stress. Chemical resistance is screened according to ASTM D543 for 30-day contact with aliphatic hydrocarbons, mild acids, and aqueous salt solutions; mechanical integrity after chemical exposure is confirmed by ASTM D882 tensile retention above 90% of original yield strength. End products include drum liners for lubricants, additive powders, and resins, FIBC liners for food powders, and corrugated box liners for high-fat dry mixes. The process boundary is gauge variation below ±8%; greater variation causes bottom seal failure when the liner is drop-filled with 25 kg product.

    Stretch Hood Extrusion Requires Thermal Homogeneity Across the Die Gap

    Stretch hood film produced from TD-9022-C is designed for insertion on pallet hooding machines that stretch the film over the top corners of a loaded pallet and allow it to recover onto the load. The formulation is 70–85 wt% TD-9022-C, 15–30 wt% high-pressure LDPE, and 1.0–2.0 wt% slip/antiblock masterbatch; the LDPE fraction is not increased beyond 30 wt% because corner-holding force decreases when the film loses recovery tension after stretching. The blown-film process runs with a die gap of 1.8–2.5 mm, blow-up ratio 2.5:1–4.0:1, and melt temperature 195–225°C; thermal homogeneity across the die gap is held within ±3°C to avoid lane orientation differences that show up as uneven corner stretch at the hooder. On-line thickness scanning is set to reject film with gauge variation exceeding ±5%, because thin lanes fail under the 3–8% stretch applied at the pallet hooding station. Compliance for stretch hood films references ASTM D4649 for selection and use of stretch wrap materials and ASTM D882 for tensile properties; load stability under transport is validated by ASTM D5331. End products are pallet hoods for appliances, bagged building materials, beverage multipacks, and cold-chain distribution loads where a sealed dust-proof cover is required.

    Free Quote

    Competitive NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Novapol® TD-9022-C Superhexene LLDPE is a linear low density polyethylene resin manufactured by NOVA Chemicals Corporation using 1-hexene as the primary alpha-olefin comonomer. The material is defined for cast film processing, with a nominal melt index of 2.0 g/10 min determined by ASTM D1238 at 190°C under 2.16 kg load and a nominal density of 0.918 g/cm³ determined by ASTM D792. These two parameters position the resin in the lower-crystallinity segment of the linear polyethylene range, where hexene-derived short-chain branching decreases lamellar thickness and increases the number of amorphous tie-chain segments relative to butene-based LLDPE of the same nominal density. Typical commercial uses include monolayer and coextruded cast stretch wrap, heavy-gauge shipping sacks, industrial liners, and lamination layers. The pelletized product is compatible with standard polyolefin vacuum conveying, gravimetric feeding, and melt filtration equipment; no special drying is required at normal warehouse humidity.

    The term “superhexene” identifies a resin family based on 1-hexene rather than 1-butene or 1-octene. In the ethylene copolymer crystal, 1-hexene contributes C4 branches that are more strongly excluded from the polyethylene orthorhombic lattice than the ethyl branches contributed by 1-butene. This exclusion depresses density and creates broader amorphous regions where polymer chains can participate in multiple crystallites. The resulting tie-molecule population improves the film’s resistance to crack propagation and dart impact when compared at equivalent density and melt index, but the effect is not uniform across all test temperatures and strain rates. The exact molecular weight distribution and comonomer sequence distribution are not disclosed in typical product literature; converters should not rely solely on melt index and density to estimate melt processing behavior or final film properties.

    From a processing-control standpoint, the resin is normally introduced into cast film extruders as a neat resin or as a dry blend with additive masterbatches. Gravimetric feeding accuracy of ±0.5% is recommended when blending antiblock, slip, or process aid masterbatches into the film formulation because additive concentration affects surface friction, blocking, and seal behavior. The material is not recommended for high-temperature coatings or for continuous exposure to strong oxidizing agents without additive stabilization. When the resin is stored in humid environments, surface moisture may be absorbed onto the pellets; drying at 80°C for 2 h to 4 h in a desiccant dryer with a dew point below -40°C prevents steam bubbles and surface roughness in the extrudate.

    Why Does 1-Hexene Comonomer Distribution Alter Elmendorf Tear and Dart Impact?

    The comonomer architecture of a linear low density polyethylene directly influences the probability that polymer chains traverse the amorphous region between adjacent crystalline lamellae. In a butene copolymer, the ethyl branch is small enough to be partially accommodated at the crystal surface, which raises the critical thickness of the amorphous layer but produces fewer load-bearing tie chains at a given density. In contrast, the C4 branch from 1-hexene is excluded more strongly from the crystal, so a lower molar concentration of comonomer is required to achieve the same 0.918 g/cm³ density. The remaining amorphous fraction contains longer chain segments that are more likely to be embedded in two or more crystalline regions. When the film is subjected to dart impact according to ASTM D1709, these tie molecules transfer stress across the lamellar structure and delay catastrophic fracture. Under Elmendorf tear testing according to ASTM D1922, the same tie-chain network retards crack growth even after the initial tear is initiated, producing higher tear resistance in the machine direction of cast films than a butene-based resin of equivalent density.

    This mechanistic difference is not limited to impact and tear. A hexene-based LLDPE at this density generally retains a higher secant modulus than a butene-based resin that has been compounded to the same dart impact level, because the butene resin must be reduced in density, sacrificing modulus. The standard test methods used to quantify these effects include tensile testing according to ASTM D882, secant modulus at 1% strain according to ASTM D882, puncture resistance according to ASTM D5748, and instrumented impact tests that record force-displacement curves during the piercing event. Film specimens should be conditioned at 23°C ± 2°C and 50% ± 5% relative humidity for 40 h under ASTM D618 before testing, because polyethylene mechanical properties are sensitive to temperature and conditioning time. The actual measured values for Novapol TD-9022-C vary with film gauge, draw ratio, chill roll temperature, and additive package; the manufacturer’s product data sheet provides nominal resin properties, while the certificate of analysis and line-specific capability data should be used for incoming inspection.

    On cast film lines equipped with 90 mm to 150 mm single-screw extruders having 30:1 to 36:1 L/D ratios, the resin is processed with a general-purpose polyolefin screw containing a barrier section and a Maddock mixer. Barrel temperature profiles are typically set from 180°C in the feed section to 240°C in the metering section, with screen changer and adapter temperatures maintained between 230°C and 260°C. The melt temperature measured at the die entrance should be kept in the 220°C to 260°C range; operation above 280°C promotes oxidative degradation that becomes visible as gel particles, die-lip deposit, and lower dart impact values. Die gap settings of 0.8 mm to 1.2 mm are appropriate for final film gauges from 12 µm to 50 µm, although thinner gauges may require a narrower die gap to maintain web stability. The molten film is quenched on a chill roll held at 15°C to 30°C, with higher temperatures reducing quench-related haze but increasing blocking unless an antiblock masterbatch is present. Air gap length controls uniaxial draw in the machine direction; longer air gaps increase machine direction orientation and machine direction tear but reduce transverse direction tear. Extruder head pressure at a given throughput depends on the resin’s molecular weight distribution and melt temperature. A production-scale observation on a 120 mm cast film extruder running at 300 kg/h suggests that melt pressures above 350 bar at the gear pump inlet are indicative of excessive shear heating or insufficient melt temperature, but published data for this specific configuration is limited. Continuous melt pressure monitoring is recommended above 60% of maximum screw speed.

    Die-lip deposit formation on cast film lines often results from low-molecular-weight species migrating to the die surface and oxidizing. When processing TD-9022-C, die-lip buildup is managed by maintaining the die adapter temperature at or below 260°C, using a die-lip cooling air flow, and adding a fluoropolymer process aid if the line is not already running one. Melt fracture can appear as alternating matte and glossy streaks in the film when the shear stress at the die lip exceeds the critical shear stress of the resin. In a 0.8 mm die gap at 260°C, raising the melt temperature by 5°C to 10°C can remove melt fracture, but only up to the point where oxidation begins. Draw resonance, a periodic thickness variation in the machine direction, is controlled by adjusting the air gap, the draw ratio, and the melt temperature; an unstable web at high draw ratios often requires a narrower die gap or a lower line speed.

    Dart Impact, Puncture, and Elmendorf Tear Values at 25 µm Gauge

    Mechanical evaluation of cast film is often performed at 25 µm gauge because this thickness is used in industrial liners and light stretch wrap. Dart impact under ASTM D1709 Method A records the mass at which a 38 mm dart with a 26 in drop height causes sufficient film failure to produce a visible rupture. The test result is influenced by the film’s gauge variability, surface defects, and conditioning history. Puncture resistance under ASTM D5748 measures the peak force and energy absorbed when a probe penetrates the film at a controlled rate; this test is more representative of contact with sharp load surfaces than dart impact alone. Elmendorf tear under ASTM D1922 reports the force required to propagate a pre-initiated tear; in cast film, the orientation introduced by the chill roll generally causes machine direction tear values to exceed transverse direction tear values. A comparison between TD-9022-C and conventional butene LLDPE at the same 0.918 g/cm³ density and 2.0 g/10 min melt index should be performed on films of identical gauge, additive package, and thermal history, because these variables can mask the effect of the hexene comonomer. Product literature for similar superhexene cast film grades indicates that the selection of 1-hexene as comonomer produces a measurable increase in machine direction Elmendorf tear and dart impact relative to butene LLDPE, but exact values for TD-9022-C must be taken from the manufacturer’s certificate of analysis or generated by the converter on the target production line.

    Rheological measurements for incoming resin quality control are usually performed with a capillary rheometer using ASTM D3835 or a rotational rheometer with a 25 mm parallel plate fixture. At 190°C, the melt index of 2.0 g/10 min is a single-point test that does not capture the full shear-thinning behavior. A shear viscosity curve over 10 s⁻¹ to 1000 s⁻¹ is more relevant to cast film extrusion because the melt experiences high shear rates in the die lip region. Broad molecular weight distribution resins of this class typically show strong shear thinning, which lowers die pressure at high throughput but may also produce higher die swell. Die swell affects the effective draw ratio and film gauge; chill roll positioning and air gap must compensate for the swelling of the extrudate. Product literature for Novapol TD-9022-C does not typically provide a complete viscosity curve, so converter characterization is required for precise process simulation.

    When High-Speed Pre-Stretch Demands Uniform Yield and Load Retention

    In pallet-wrapping operations, the cast film is elongated by power pre-stretch equipment at ratios commonly between 200% and 300%. The film must deform uniformly without forming broad transverse bands of thinned material, known as “smile” defects, which cause localized weakness when the pallet is transported. The yield behavior of TD-9022-C is influenced by the 1-hexene comonomer distribution, which reduces the sharp yield point associated with higher-crystallinity polyethylene and permits a more uniform drawing process. Load retention after stretching is measured under ASTM D5459, which specifies a load cell and clamp arrangement; the standard does not provide a universal pass/fail threshold because the required retention depends on pallet weight, film thickness, and pre-stretch ratio. Puncture resistance during wrapping is assessed under ASTM D5748, and film tensile properties under ASTM D882, with secant modulus at 1% strain used as a predictor of load containment stiffness. The nominal density of 0.918 g/cm³ positions the film to balance stiffness and stretch: lower densities increase elongation capacity but reduce penetration resistance, while higher densities increase modulus but promote film splitting under high pre-stretch. In a high-speed cast stretch line, on-line gauging systems record thickness variation across the web; variation above ±3% is generally considered undesirable because it correlates with inconsistent stretch and local failure. Published data for TD-9022-C in specific pre-stretch equipment configurations is limited; converters should qualify the film on the intended wrapping machine using actual pallet profiles.

    When the resin is compared with a butene-copolymer LLDPE of the same 2.0 g/10 min melt index, the hexene grade provides a different balance of modulus and toughness. A butene-based resin can achieve the same 0.918 g/cm³ density with a higher molar comonomer concentration, but the shorter ethyl branches are less effective at creating tie molecules. To match the dart impact and tear resistance of TD-9022-C, a butene resin often must be formulated to a lower density, which reduces secant modulus and load containment. Conversely, a metallocene-catalyzed LLDPE of similar density and melt index may exhibit better optical properties and lower seal initiation temperature because of its narrower composition distribution, but it often requires more precise control of melt pressure and die gap due to higher melt elasticity. TD-9022-C is positioned as a Ziegler-Natta superhexene cast film resin that retains sufficient melt strength for high-speed draw-down while avoiding the extreme back pressure sometimes observed with metallocene grades. The differentiation is not absolute; film property rankings depend on the coextruded layer structure, the additive package, and the thermal history of the web. In blown film equipment, the resin may require lower melt temperatures and larger die gaps than butene LLDPE because the higher elongational viscosity associated with hexene-based chains can improve bubble stability but reduce ease of drawdown. In cast film, the principal adjustments are die gap, air gap, and chill roll temperature, since these factors control the orientation state that governs mechanical properties. The converter should use gel permeation chromatography and dynamic rheological data when available to compare molecular weight distribution and long-chain branching between candidate resins, but the typical public data sheet does not include these measurements.

    Compared with 1-octene-based LLDPE, a 1-hexene-based resin at the same density and melt index is generally expected to have slightly lower toughness because octene branches are longer and more effective at tie-molecule formation. However, 1-hexene copolymers are often preferred in cast films when processability and cost are weighted alongside mechanical performance. The specific advantage of TD-9022-C lies in the superhexene platform’s combination of 2.0 g/10 min melt index and 0.918 g/cm³ density, which suits thin-gauge cast film lines that require moderate extensibility and puncture resistance without excessive back pressure. A direct comparison with an octene-based LLDPE should use the same film structure and test standards; published data for this specific configuration is limited.

    In lamination structures, TD-9022-C may serve as a sealant or tie layer when compounded with appropriate additives. Heat seal performance is evaluated on a gradient heat sealer with temperature increments of 5°C and dwell times of 0.5 s to 1.0 s; seal initiation is typically lower than that of HDPE but higher than some metallocene LLDPE grades. The resin’s optical properties are influenced by chill roll temperature and surface finish; a higher gloss chill roll improves clarity but may increase blocking. Slip and antiblock masterbatches are added to adjust coefficient of friction measured under ASTM D1894, with typical target values of 0.1 to 0.3 for high-speed packaging lines. These additive-containing films require aging to allow the slip agent to migrate to the surface; migration kinetics depend on storage temperature and film crystallinity. Because TD-9022-C contains no intentionally added slip or antiblock in the base resin, the final formulation is under the converter’s control and must be validated for the specific packaging machine.

    Regulatory Compliance Matrix for Food-Contact Cast Film Structures

    Compliance for the final film structure must be established by the converter because additives, coextruded layers, printing inks, and processing aids alter the regulatory status of the package. The base resin is typically covered by a manufacturer’s food-contact declaration, but the declaration is not a substitute for final compliance testing.

    Regulatory references relevant to polyethylene cast film
    Regulatory areaStandard or regulationAssociated test procedure
    United States food contactFDA 21 CFR 177.1520(c)Extractives limits specified by the regulation
    European Union food contactCommission Regulation (EU) No 10/2011, Annex IOverall migration under EN 1186-1; specific migration under EN 13130
    European packaging and packaging wasteDirective 94/62/ECSum of lead, cadmium, mercury, and chromium(VI) under the directive
    REACH registrationRegulation (EC) No 1907/2006Safety data sheet and registration dossier
    RoHS restrictionsDirective 2011/65/EUHomogeneous material analysis for restricted substances
    Top