Nova Chemicals Novapol Pi 3526 A Lldpe Masterbatch Resin

NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin

    • Product Name: NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 674630
    Density 0.926 g/cm³
    Melt Index 190 C 2 16 Kg 35 g/10 min
    Comonomer Butene-1
    Additive Antioxidant
    Melting Point 122 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 14.5 MPa
    Elongation At Break 700 %
    Flexural Modulus 207 MPa
    Hardness Shore D 50
    Escr 1000 h
    Low Temperature Brittleness -70 °C

    As an accredited NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags, palletized; each pallet contains 1,000 kg of Novapol® PI-3526-A LLDPE Masterbatch Resin.
    Container Loading (20′ FCL) 20′ FCL container loading of NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin; palletized, stretch-wrapped, and secured for safe transport.
    Shipping NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin is a non-hazardous, non-regulated plastic resin. It is typically shipped in 25-kg bags, bulk bags, or bulk trucks/railcars. Transport in clean, dry equipment; keep away from moisture, heat, and ignition sources. No dangerous goods placards are normally required.
    Storage Store NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers tightly closed to prevent moisture and contamination. Use first-in, first-out rotation. Avoid excessive stacking, dust buildup, and prolonged high temperatures.
    Shelf Life Shelf life is approximately 24 months from date of manufacture when stored in a cool, dry area in unopened packaging.
    Application of NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin

    Carbon black masterbatch formulations based on Novapol® PI-3526-A as carrier resin are compounded on co-rotating twin-screw extruders with L/D ratios from 40:1 to 52:1 and specific torque ratings above 8 N·m/cm³. The carrier resin is introduced at the main feed throat, while carbon black is injected through a side feeder positioned after the first kneading block; this sequencing prevents excessive viscosity rise before the filler is wetted. Formulation ratios on a weight basis are carrier resin 25 wt% to 45 wt%, carbon black 35 wt% to 50 wt%, and process wax or metal stearate dispersion aids 1 wt% to 5 wt%. The molten compound passes through melt filtration, typically with breaker plate screens of 150 µm to 400 µm, and is pelletised via strand or underwater systems; final pellet moisture is maintained below 500 ppm. During downstream blown film conversion, the masterbatch is let down at 3 wt% to 6 wt% into LLDPE or LDPE-LLDPE films on lines with die diameters of 250 mm to 600 mm, die gaps of 1.8 mm to 2.5 mm, and blow-up ratios from 2.2:1 to 3.5:1. Melt temperature at the die is controlled between 190 °C and 220 °C. Regulatory references for agricultural films are EN 13207:2018 for silage films and EN 13206:2017 for greenhouse covering films; carbon black content is quantified to ASTM D1603-14, dispersion to ISO 18553:2002, and melt flow rate to ISO 1133-1:2022. Terminal product types are silage cover sheets, greenhouse films, mulch films, and bale wrap. A process boundary appears at let-down ratios above 6 wt%: dart impact resistance and tear properties in films thicker than 100 µm can decline sharply due to stress concentration at carbon black agglomerates, and filter pressure build-up in the masterbatch line becomes the limiting factor for continuous campaign length.

    Why Does TiO₂ Surface Treatment Influence Die Lip Build-Up in Extrusion Coating Laminates?

    In extrusion coating, TiO₂ white masterbatches built on PI-3526-A are formulated with rutile TiO₂ grades that carry alumina or silica surface treatments, because untreated TiO₂ can accelerate photocatalytic chain scission in the LLDPE carrier during UV exposure and melt processing. The masterbatch formulation uses carrier resin at 30 wt% to 50 wt%, TiO₂ at 50 wt% to 70 wt%, and dispersant waxes at 0.5 wt% to 2.0 wt%. Compounding takes place on high-shear co-rotating twin-screw extruders with sequential kneading and gear mixing elements; the target colour strength requires TiO₂ agglomerates to be reduced below 20 µm, as larger agglomerates cause die-lip deposit formation and pinholes in the extrudate. During downstream extrusion coating, the masterbatch is let down into LDPE-LLDPE blends at 5 wt% to 12 wt%. Coating lines are run with melt temperatures of 290 °C to 325 °C, die gaps of 0.5 mm to 1.0 mm, and line speeds from 100 m/min to 300 m/min; the LLDPE carrier contributes to drawdown stability, while LDPE remains present for neck-in control and adhesion to primed substrates. Food-contact compliance is based on FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011, Annex I for overall migration limits, and 21 CFR 178.3297 for colorants used in polymer coatings. Tensile and tear properties of the finished laminate are determined by ASTM D882-22 and ASTM D1922. Terminal product types include flexible barrier laminates, stand-up pouches, extrusion-coated paperboard, and aseptic carton structures. Loadings above 70 wt% TiO₂ in the masterbatch are operationally limited because melt strength deterioration and filter pressure accumulation shorten high-speed coating campaigns, and let-down ratios above 12 wt% tend to reduce seal strength and interlayer adhesion.

    Calcium Carbonate Filler Masterbatch in Thin-Wall Polyethylene Injection Moulding

    Calcium carbonate masterbatch formulations based on PI-3526-A use coated CaCO₃ grades with median particle sizes below 2 µm and stearic acid surface treatment to reduce moisture adsorption and improve dispersibility in polyolefin melts. The carrier resin loading is 30 wt% to 50 wt%, CaCO₃ loading is 45 wt% to 65 wt%, and coupling or processing additives are 0.5 wt% to 2 wt%. Compounding is performed on co-rotating twin-screw extruders with L/D ratios from 36:1 to 48:1, with atmospheric or vacuum venting to remove surface moisture and pellet moisture maintained below 300 ppm. Injection moulders let down the masterbatch into polyethylene at 10 wt% to 30 wt% for thin-wall containers, crates, and industrial components. Barrel temperatures are set from 180 °C to 230 °C, mould temperatures from 15 °C to 40 °C, and clamp force requirements are established from projected area and melt viscosity rather than filler loading alone. Testing references are ISO 294-1:2017 for specimen moulding, ISO 1133-1:2022 for melt flow rate, ISO 178:2019 for flexural modulus, ISO 179-1:2020 for Charpy impact, and food-contact compliance under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, Annex I. Terminal product types include thin-wall storage bins, crates, pallets, PE closures, and houseware components. A specific operational boundary is moisture: CaCO₃ masterbatch held at relative humidity above 60% should be re-dried at 70 °C to 80 °C for 2 h to 4 h before processing to prevent splay and hydrolytic degradation at high melt temperatures.

    When Erucamide Migration Is Required to Coexist with Synthetic Silica Antiblock Dispersion in LLDPE Blown Film

    The two additive systems used in polyolefin film—erucamide slip and synthetic silica antiblock—interact through different kinetic mechanisms: erucamide blooms from the amorphous regions of the LLDPE carrier toward the film surface, while synthetic silica creates micro-roughness to limit film-to-film blocking. In PI-3526-A-based antiblock masterbatches, carrier resin is loaded at 80 wt% to 95 wt% and synthetic silica at 5 wt% to 20 wt%; slip masterbatches contain erucamide at 5 wt% to 10 wt% and carrier resin at 90 wt% to 95 wt%. Downstream blown film lines let down each system at 1 wt% to 3 wt% or a combined additive package at 2 wt% to 5 wt%. Film blowing is conducted at die gaps from 1.5 mm to 2.5 mm, blow-up ratios from 2.5:1 to 4.0:1, and die melt temperatures from 190 °C to 220 °C. Coefficient of friction is measured after 24 h and 48 h ageing using ISO 8295:2017 or ASTM D1894; blocking force is measured by ISO 11502:2018 or ASTM D3354. Film tensile properties are tested to ISO 527-3:2018 and dart impact to ASTM D1709-22. Food-contact requirements are established under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, Annex I. Terminal product types include form-fill-seal food packaging, printed laminates, and non-food liner films. The upper silica loading of 20 wt% in the masterbatch is a practical dispersion limit; beyond this point film haze and filter pressure rise sharply without proportional antiblock benefit. Erucamide above 10 wt% can produce uneven bloom that interferes with print adhesion and heat-seal strength, so formulations are adjusted downward when downstream packaging requires high-gloss print surfaces.

    Comparative formulation and let-down windows for PI-3526-A-based masterbatches
    Masterbatch systemCarrier resin loadingActive payload loadingDownstream let-downPrimary standard or regulation
    Carbon black agricultural film25 wt%–45 wt%35 wt%–50 wt%3 wt%–6 wt%EN 13207:2018 / ISO 18553:2002
    TiO₂ extrusion coating30 wt%–50 wt%50 wt%–70 wt%5 wt%–12 wt%EU 10/2011 / FDA 21 CFR 177.1520
    CaCO₃ injection moulding30 wt%–50 wt%45 wt%–65 wt%10 wt%–30 wt%ISO 178:2019 / ISO 179-1:2020
    Antiblock/slip blown film80 wt%–95 wt%5 wt%–20 wt% silica; 5 wt%–10 wt% erucamide1 wt%–3 wt% eachISO 8295:2017 / ASTM D1709-22
    UV monofilament60 wt%–90 wt%5 wt%–15 wt% HALS; 2 wt%–8 wt% UVA1 wt%–4 wt%ISO 4892-2:2013 / ASTM D638-14
    Rotomoulding additive40 wt%–70 wt%30 wt%–60 wt%0.5 wt%–3.0 wt%ISO 179-1:2020 / FDA 21 CFR 177.1520

    Accelerated weathering masterbatches for high-tenacity polyolefin monofilament in artificial turf applications are compounded with low specific energy input to protect heat-sensitive HALS and hydroxyphenyl triazine UV absorbers from thermal decomposition. In these systems, PI-3526-A serves as carrier resin at 60 wt% to 90 wt%, HALS additives at 5 wt% to 15 wt%, UV absorbers at 2 wt% to 8 wt%, and processing stabilisers at 1 wt% to 5 wt%. Melt temperature during masterbatch compounding is held below 240 °C to avoid partial loss of the stabiliser package. During monofilament extrusion, the masterbatch is let down into LLDPE or LLDPE-HDPE blends at 1 wt% to 4 wt%, followed by water quenching and orientation at draw ratios from 4:1 to 8:1 to achieve target tenacity. Weathering performance is evaluated under ISO 4892-2:2013 and ISO 4892-3:2016; residual tensile properties are measured to ASTM D638-14 and ISO 527-1:2019. The carrier resin falls under FDA 21 CFR 177.1520 for olefin polymers where consumer exposure is relevant, and under Regulation (EC) No 1907/2006 for REACH registration obligations. Terminal product types include artificial turf yarn, outdoor geomembranes, pond liners, and agricultural shade nets. An operational boundary is the incompatibility of certain HALS chemistries with residual chlorine or process water sanitisation agents; processors must confirm the full additive package compatibility before scale-up to prevent accelerated fibre surface oxidation.

    Rotomoulding Additive Masterbatches Are Defined by Dry-Blend Particle Size Distribution and Long Melt Residence Time

    Rotational moulding additive masterbatches based on PI-3526-A are formulated for dry blending with polyethylene powder, where segregation resistance is controlled by pellet size distribution and density match. Carrier resin loading is 40 wt% to 70 wt%, active pigments or additives are loaded at 30 wt% to 60 wt%, and the downstream let-down is 0.5 wt% to 3.0 wt%. The masterbatch must pass through pelletisers that produce a narrow particle size distribution, because fines below 500 µm segregate during high-speed dry blending and oversize pellets above 2 mm create pigment concentration gradients inside the rotating mould. Rotational moulding processors dry-blend the masterbatch with PE powder at 800 rpm to 1,200 rpm for 3 min to 10 min before charging the mould; oven temperatures of 260 °C to 300 °C and residence times of 20 min to 40 min are common for large parts. Material performance testing uses ASTM D638-14 for tensile strength, ISO 179-1:2020 for Charpy impact, ISO 1183-1:2019 for density, and ISO 1133-1:2022 for melt flow rate. Food-contact uses require FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, Annex I; potable water contact additionally invokes NSF/ANSI 61 or equivalent national standards. Terminal product types include water storage tanks, kayaks, playground components, and insulated boxes. A process conflict specific to rotomoulding is the low-shear, long-dwell melt environment: high-melt-flow carrier resins such as PI-3526-A improve pigment wetting during the initial fusion stage, but excessive active pigment loading above 60 wt% may reduce impact strength in the sintered part because the high local pigment concentration acts as stress concentration sites.

    Free Quote

    Competitive NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Novapol® PI-3526-A is an LLDPE masterbatch resin supplied by NOVA Chemicals for use as a carrier phase in polyolefin colour and additive concentrates. The product is pelletized and typically melt-compounded with pigment or filler loadings from 20% to 75% by weight on a co-rotating twin-screw extruder, then pelletized and let down into polyethylene film, sheet, or injection moulding resins. The designation “masterbatch resin” indicates that the material is not intended for direct finished-article extrusion at high dilution; rather, it is selected for pigment wetting, dispersion stability, and rapid solidification. Because product-specific published data for PI-3526-A is limited, exact melt flow rate, density, comonomer type, and additive package must be obtained from the supplier’s certificate of analysis. Class-typical LLDPE masterbatch carriers are characterized under ASTM D1238 at 190 °C and 2.16 kg, with density measured by ISO 1183-1. The linear low density polyethylene backbone gives higher tensile yield strength and greater puncture resistance than low-density polyethylene carriers at equivalent melt flow rate, but also increases screw torque and melt pressure during intensive mixing. The grade is supplied in free-flowing pellet form and should be pre-dried only when surface moisture is present; LLDPE is not hygroscopic, but surface condensation can form after storage in humid environments.

    How Does the PI-3526-A Carrier Differ from Low-Density Polyethylene Alternatives?

    Low-density polyethylene carriers produced in high-pressure autoclave or tubular reactors contain long-chain branching that lowers shear viscosity at high screw speed and improves bubble stability in blown film. LLDPE carriers such as PI-3526-A, produced by low-pressure catalytic polymerization, contain short-chain branches from an alpha-olefin comonomer—commonly butene, hexene, or octene—and have negligible long-chain branching. This structural difference affects letdown behaviour. At the same melt index and melt temperature, LLDPE exhibits higher extensional viscosity and greater shear sensitivity. In twin-screw compounding, this difference raises torque at equivalent screw speed and narrows the operating window before thermal oxidation or volatilization of low-molecular-weight slip additives. The benefit is mechanical contribution after dilution: a masterbatch pellet based on an LLDPE carrier adds higher dart impact and tensile strength to the host compound than an LDPE carrier at the same letdown ratio, as measurable by ASTM D1709 and ASTM D638. The short-chain branch distribution also affects seal initiation temperature in blown film; converters should evaluate the final film using ASTM F88 when the masterbatch carrier constitutes more than 5% of the melt blend.

    During co-rotating twin-screw extrusion on a 40:1 L/D line with segmented screws, the carrier phase must melt early enough to wet pigment agglomerates but retain sufficient viscosity to transfer shear stress into the agglomerate. PI-3526-A should be fed downstream of a high-intensity kneading block when the concentrate contains high-structure carbon black or organic red pigments; reverse kneading elements followed by a low-pressure vent reduce pigment attrition. The barrel profile is normally maintained between 160 °C and 230 °C depending on pigment thermal stability. Specific mechanical energy input can range from 0.12 kWh/kg to 0.28 kWh/kg for pre-dispersed organic pigments, but published data for this specific PI-3526-A configuration is limited and the range should be validated on the installed line. For inorganic pigments such as titanium dioxide or iron oxide, lower screw speeds and higher fill volume may be required to prevent excessive viscosity reduction and motor amperage spikes. The die plate and underwater pelletizer water temperature should be held below 40 °C to produce spherical or near-cylindrical pellets with low fines.

    Filtration is mandatory in masterbatch compounding to remove unmelted polymer gel, pigment agglomerates, and carbonized residues from upstream handling. A screen pack with breaker plate and mesh combinations of 60/80/100 or finer is commonly placed before the die. Pressure drop across the screen pack should be logged; a rise of more than 20% over baseline at constant output indicates gel buildup or screen blinding. PI-3526-A, like other LLDPE carriers, may generate higher gel counts if melt temperature exceeds 250 °C or if residence time exceeds 8 min in the extruder. Melt flow paths should be configured without dead spots in the adapter and die head.

    When Letdown Ratios Exceed 20:1 in Polyethylene Film Conversion

    At letdown ratios of 20:1 or higher, carrier resin properties influence the dilute phase morphology and gel count of finished film. Because PI-3526-A is an LLDPE, a high letdown ratio with a host LDPE can create local viscosity differences and slight haze increase if the melt flow ratio is too large. Film converters should pre-blend masterbatch with a portion of host resin prior to hopper addition and maintain compression-zone melt temperatures above 190 °C. The carrier melt flow rate should be close enough to the host polymer to avoid viscous fingering in single-screw film extruders with compression ratios of 3:1 to 4:1. In cast film lines, the narrower die gap raises shear heating and may increase melt temperature by 5 °C to 15 °C above barrel set point; external cooling or processing aids are sometimes required. In blown film lines, bubble stability can be maintained by using an air ring with dual-lip adjustment and by limiting letdown ratio to 15:1 if the host resin is a high-pressure LDPE with low melt tension.

    Masterbatch pellet integrity during bulk rail unloading depends on pellet hardness, fines content, and surface abrasion. PI-3526-A is supplied in pellet form and should be transferred through rotary airlocks or dense-phase conveying systems rather than high-velocity dilute-phase lines to avoid particle breakage. In silo storage, ambient temperatures below 50 °C and relative humidity below 60% reduce the risk of pellet agglomeration. Surface condensation can occur after moving cold resin into a warm warehouse; in such cases, a hopper dryer at 60 °C to 80 °C for 2 h to 4 h is sufficient to remove surface moisture before extrusion. LLDPE is not hygroscopic, but condensed moisture can generate steam in vented extruders and reduce pigment dispersion. Long silo residence beyond 90 days is not recommended unless nitrogen blanketing is used, because the additive package may migrate to the pellet surface and alter feeding characteristics.

    Carrier Selection Governs Masterbatch Dilution Consistency and Compound Viscosity

    Unlike LDPE-based carriers, LLDPE carriers generally produce higher viscosity in the finished compound at equal melt index. This difference is measurable by capillary rheometry under ISO 11443 or by melt mass-flow rate under ISO 1133-1:2022. A formulation using PI-3526-A as carrier may require lower screw speed in letdown injection moulding or a higher melt temperature to reach the same fill length. The difference from linear low density polyethylene grades designed for film extrusion is the controlled additive package and pellet geometry: masterbatch resins are often stabilized for multiple heat histories during compounding, pelletizing, and final conversion. The exact stabilization package appears on the safety data sheet and certificate of analysis. When PI-3526-A is compared with EVA carrier resins, the LLDPE carrier has lower polarity and may wet acid-modified pigments less readily; polar pigments should be pre-dispersed with a compatible wax or incorporated using a first-pass concentrate.

    Letdown injection moulding of polyolefin masterbatches based on PI-3526-A may require screw designs with low compression ratios below 2.5:1 and inverse temperature profiles to prevent melt channeling. When moulding technical parts on clamping machines from 500 kN to 30,000 kN, the concentrate is typically added at 1% to 5% by weight. Injection speed should be reduced if surface streaks appear, because the carrier phase can separate from the host polymer at high shear rates. The recommended melt temperature depends on the host grade but is commonly maintained between 200 °C and 250 °C for LLDPE-rich compounds. Back pressure of 0.5 MPa to 1.5 MPa is used when natural mixing is needed in the barrel. These parameters are line-specific and should be optimized by short-shot analysis.

    Pigment wetting is governed by carrier viscosity and the acid-base character of the pigment surface. Phthalocyanine blue and carbon black require longer dispersion residence time than titanium dioxide. A typical masterbatch formula using PI-3526-A might contain 25% to 50% pigment, 5% to 15% wax, and the remainder carrier. The wax component should have a viscosity lower than the carrier and a melting point between 70 °C and 120 °C. When wax content exceeds 10%, the mixture may slip on the screw and reduce volumetric feeding accuracy; a crammer feeder or side feeder with vertical screw is used. The carrier should not be pre-blended with wax at high temperature for extended periods because additive migration can occur.

    Regulatory and food-contact status must be confirmed from supplier documentation, not inferred from resin type. Polyethylene resins may be evaluated under FDA 21 CFR 177.1520 for olefin polymers and under EU Regulation 10/2011 for plastic materials intended to contact food. The specific additive package in PI-3526-A may require a dual-use additive listing or a no-objection letter when used in food-contact concentrate formulations. Compliance with REACH and RoHS Directive 2011/65/EU depends on the pigment and additive loadings in the final masterbatch, not solely on the carrier resin.

    Test and regulatory reference matrix relevant to LLDPE masterbatch carrier evaluation
    Test or regulatory reference Property or scope Relevance to LLDPE masterbatch carrier
    ISO 1183-1:2019 Density Carrier density influences masterbatch pellet hardness and letdown compatibility
    ISO 1133-1:2022 Melt mass-flow rate Controls dispersion and letdown ratio
    ASTM D1238-20 Melt flow rate at 190 °C/2.16 kg Alternative melt flow measurement
    ASTM D638-14 Tensile properties Mechanical contribution after carrier letdown
    ASTM D1709-16 Dart impact Film toughness after letdown
    FDA 21 CFR 177.1520 Olefin polymer food-contact status Carrier resin compliance pathway
    EU 10/2011 Overall migration and specific migration Food-contact article end-use
    REACH SVHC declaration Supply chain compliance
    RoHS 2011/65/EU Restricted substances Electrical and electronic end-use compliance

    The table above reflects the standard framework used by compounders to evaluate a polyolefin carrier; it does not represent a certificate of conformance for PI-3526-A. Lot-specific values should be requested from NOVA Chemicals or the appointed distributor before commercial use.

    Thermal stabilizers in the carrier protect the polyethylene during multiple heat-aging cycles. In masterbatch compounding, the first heat history occurs during pigment dispersion; the second during letdown extrusion. If the carrier contains only primary antioxidants without a secondary phosphite, yellowing can occur during processing above 220 °C. Operators should monitor melt pressure and melt colour at the die exit. Oxidative induction time measured by ISO 11357-6 or ASTM D3895 is a useful batch-to-batch check. A reduction in OIT below 20 min at 200 °C may indicate stabilizer depletion or contaminated regrind. Published data for PI-3526-A stabilizer levels is limited; therefore, incoming resin should be tested against the supplier’s baseline OIT value.

    In masterbatch production, PI-3526-A may be used with calcium carbonate or talc loadings from 40% to 80% by weight for film antiblock concentrates or mineral-filled compounds. In such formulations, the carrier melt flow rate must be high enough to fill interstitial voids between filler particles but low enough to prevent intermeshing screw leakage. On a 26:1 L/D twin-screw extruder with atmospheric venting, filler is often split-fed at the downstream side-feed while carrier is fed at the main throat. The torque limit of the extruder gearbox should be maintained below 90% of nameplate rating. Published data for PI-3526-A in this specific filler concentrate configuration is limited; compounding trials should begin at the lower end of the specific energy range and increase in 0.05 kWh/kg increments.