Nova Chemicals Novapol Pi 2024 A Lldpe Masterbatch Resin

NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin

    • Product Name: NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 289864
    Density 0.924 g/cm³
    Melt Index 20 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 9.7 MPa
    Tensile Strength At Break 12.4 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Vicat Softening Point 93°C
    Melting Point 121°C
    Hardness Shore D 47
    Thermal Conductivity 0.33 W/m·K
    Brittleness Temperature < -70°C
    Specific Heat Capacity 2.3 J/g·°C
    Coefficient Of Linear Thermal Expansion 1.5E-4 cm/cm/°C

    As an accredited NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin is packaged in 25 kg bags, with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL: 18.75 MT of NOVA Novapol PI-2024-A in 25 kg bags, securely loaded and strapped for ocean transport.
    Shipping NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin is shipped as non-hazardous solid pellets, typically in moisture-resistant 25 kg bags, bulk sacks, or railcars/trucks. Not classified as dangerous goods. Transport in cool, dry conditions, away from heat, moisture, and contaminants. Secure loads and follow local regulations plus supplier handling instructions.
    Storage NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin should be stored indoors at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers sealed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged high temperatures and UV exposure. Do not stack excessively; use first-in, first-out rotation and follow the manufacturer’s SDS.
    Shelf Life Shelf life: 12 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin

    White Masterbatch Carrier Performance in Monolayer Blown Film

    In monolayer blown film lines running at die gaps of 1.2–2.0 mm and blow-up ratios of 2.5:1–3.0:1, the carrier phase in a white masterbatch governs both pigment dilution and melt-pressure stability. When Nova Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin is evaluated as the LLDPE carrier resin, the masterbatch formulation is typically built with 35–50 wt% carrier resin, 50–65 wt% rutile TiO₂, and 0.5–1.5 wt% structural processing aid; the finished masterbatch is then let down into natural film resin at 8–15 wt%. A co-rotating twin-screw compounding line with screw L/D of 44:1–52:1 is operated with side feeding of TiO₂, screw speed 350–600 rpm, and melt temperature 200–230 °C. A screen changer with 150–250 mesh pack retains undispersed pigment aggregates; pressure rise across the screen pack exceeding 0.8 bar/kg/h indicates poor dispersion. On the film line, the let-down blend is extruded through a spiral mandrel die with die gap 1.5–2.3 mm, barrel profile 170–210 °C, and die temperature 210–225 °C. Terminal products include white opaque frozen food bags, dairy film, bread bags, hygiene overwrap, and agricultural mulch; food-contact grades require olefin polymer compliance with FDA 21 CFR 177.1520 and EU Regulation 10/2011, with pigment purity verified under relevant national positive lists. Published data for this specific configuration is limited; therefore, line trials at the target let-down ratio remain mandatory before commercial approval.

    Why Does Carbon Black Dispersion Deteriorate Above 40 wt% in Injection Moulding Carriers?

    Injection moulding grades of carbon black masterbatch place the carrier resin under two simultaneous demands: wetting of high-surface-area furnace black and preservation of sufficient flow to fill thin-wall moulds. In a starting formulation, carbon black is charged at 30–45 wt%, PI-2024-A carrier resin at 50–65 wt%, a polar dispersant at 1–3 wt%, and a hindered phenolic antioxidant at 0.1–0.5 wt%; the resulting masterbatch is let down at 2–4 wt% into natural HDPE or LLDPE injection moulding resin. Deterioration above 40 wt% carbon black is observed as a non-linear increase in melt viscosity, higher screen-pack pressure, and generation of undispersed agglomerates that reduce notched impact strength. High-torque co-rotating twin-screw compounding at L/D of 48:1 is specified with a side feeder positioned after the primary melting zone, screw speed 450–700 rpm, specific energy input 0.22–0.30 kWh/kg, and melt temperature 220–250 °C. A water ring pelletizer is preferred to strand pelletizing because low-viscosity masterbatch melt can sag during strand haul-off. Injection moulding of the let-down compound uses barrel temperatures of 190–235 °C, mould temperatures of 15–35 °C, injection velocities of 80–120 mm/s, and hold pressures of 600–1,000 bar. Terminal parts include agricultural crates, automotive wheel-arch liners, refuse containers, industrial pails, and closures; automotive applications additionally require compliance with REACH and RoHS 2011/65/EU, while black masterbatch suppliers may be asked to provide heavy-metal and PAH declarations under relevant OEM specifications.

    Compliance and test matrix for carbon black masterbatch in injection moulding applications
    RequirementStandard / regulationMethod / clause
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kg
    DensityISO 1183-1:2019Gradient column method
    Tensile yield strengthASTM D638-14Type IV specimen, 50 mm/min
    Hazardous substancesRoHS 2011/65/EUXRF screening and confirmatory wet chemistry
    REACH registrationEC 1907/2006Safety data sheet, Annex II

    Calcium carbonate filler masterbatches destined for cast film and extrusion coating require a carrier resin that maintains melt homogeneity at high filler loadings. For breathable and non-breathable cast film, the masterbatch is formulated with ground or surface-treated calcium carbonate at 50–75 wt%, PI-2024-A carrier resin at 20–40 wt%, and a fatty acid or metallocene-based dispersant at 1–3 wt%; the masterbatch is let down into natural LLDPE or LDPE at 5–30 wt% depending on target elongation and film thickness. The filler masterbatch is produced on a vented co-rotating twin-screw line with side forced feeding of filler, screw speed 350–600 rpm, melt temperature 190–230 °C, and a screen pack of 120–200 mesh to protect the die. The cast film line is configured with a slot die, automatic die-bolt thickness control, an air gap of 10–15 cm, a chill roll maintained at 15–25 °C, and line speeds of 150–300 m/min. In breathable film production, the calcium carbonate loading in the final film is high enough that machine-direction stretching creates micropores; the carrier resin must produce a dispersion that resists microvoid coalescence during the breathable orientation step. Terminal products include breathable hygiene backsheet, medical gown films, protective apparel, agricultural stretch film, and industrial liners. Compliance for hygiene and food-contact cast film includes FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011, with residual moisture controlled to below 0.1 wt% by the masterbatch manufacturer; pre-drying at 80–100 °C for 2–4 h is applied when storage relative humidity exceeds 60%.

    When Rotomoulding Cycles Exceed 35 Minutes in LLDPE Carrier-Based Additive Masterbatches

    Rotomoulding additive masterbatches based on PI-2024-A carrier resin are used to deliver ultraviolet stabiliser, antioxidant, and processing aid packages into natural LLDPE powders. A typical formulation contains 55–75 wt% carrier resin, 8–15 wt% hindered amine light stabiliser, 2–5 wt% UV absorber, and 0.5–2 wt% phenolic/phosphite antioxidant; the masterbatch is ground to a powder and dry blended into natural rotomoulding resin at 3–8 wt%. When oven cycle time exceeds 35 minutes, the stabiliser package can be partially consumed during prolonged exposure to 280–320 °C, particularly in thick-wall parts where the inner air temperature remains elevated after the outer wall has densified. This threshold requires evaluation of residual stabiliser concentration by oxidative induction time testing under ISO 11357-6:2018. The rotomoulding process uses a high-intensity mixer to blend powder for 60–120 s, followed by charging into a steel or aluminium mould rotated biaxially in an oven at 280–320 °C for 35–60 min, with controlled cooling rates of 5–15 °C/min. Terminal products include outdoor chemical storage tanks, agricultural sprayer tanks, marine buoys, and playground equipment. Weathering performance is assessed by accelerated weathering under ISO 4892-2 and tensile retention under ASTM D638-14; chemical storage tanks may further require compliance with EN 13575 or national tank standards. Published data for this specific resin in rotomoulding additive masterbatch configurations is limited, so oven trials with residual OIT measurement are required before specifying a commercial let-down ratio.

    When food-contact film producers replace a fractional melt index carrier with a higher-flow LLDPE masterbatch resin, the slip and antiblock additive package must be rebalanced to avoid plate-out on the die lip. For PI-2024-A-based antiblock and slip masterbatch, a starting formulation contains 70–85 wt% carrier resin, 5–10 wt% erucamide or oleamide slip agent, 10–20 wt% synthetic silica or zeolite antiblock, and 0.5–1 wt% processing aid; the masterbatch is let down into blown film resin at 1–3 wt%. Production of the antiblock/slip masterbatch uses a co-rotating twin-screw extruder configured with L/D of 36:1–44:1, melt temperature limited to 180–210 °C, and liquid amide injection after the melting zone to reduce volatilisation. Higher processing temperatures above 250 °C increase amide volatilisation and die-lip plate-out, which is a known operational boundary for this class. Film blowing uses a spiral mandrel die with die gap 1.5–2.0 mm, barrel temperatures of 170–205 °C, die temperature 195–215 °C, and blow-up ratio 2.5:1. Terminal products include bread bags, vegetable bags, frozen food film, and overwrap for packaged goods. Food-contact compliance requires olefin polymer and additive conformance with FDA 21 CFR 177.1520 and EU Regulation 10/2011, with specific migration limits for erucamide and oleamide verified under the test conditions of EN 1186-1:2002 and relevant 10/2011 migration methods.

    Static-Dissipative Corrugated Pipe Extrusion Demands Conductive Masterbatch Discipline

    Static-dissipative corrugated pipe made from HDPE requires a conductive carbon black masterbatch that can be processed through a pipe extrusion line without excessive torque. A PI-2024-A carrier-based conductive masterbatch is formulated with conductive carbon black at 35–50 wt%, carrier resin at 45–60 wt%, processing aid at 2–5 wt%, and antioxidant at 0.2–0.5 wt%; the masterbatch is let down into pipe resin at 4–10 wt% to achieve surface resistivity in the range of 10^3–10^6 Ω/sq under ASTM D257. Conductive masterbatch production requires a high-torque co-rotating twin-screw line with melt temperature 240–270 °C, screw speed 400–650 rpm, and a water ring pelletizer to prevent conductive strand breakage. Pipe extrusion of the let-down compound uses a grooved feed section to control pressure, barrel temperatures 190–230 °C, die temperature 200–220 °C, and vacuum calibration for corrugated wall geometry. Terminal products include static-dissipative corrugated drainage pipe, mine ventilation duct, and dust extraction pipe, where electrostatic discharge control is required under IEC 60079-0 or NFPA 77 because the pipe surface must dissipate charge in explosive dust atmospheres. Loading conductive carbon black above 50 wt% in the masterbatch is generally avoided because the resulting melt viscosity increases extruder torque beyond typical drive limits and reduces output stability. Extruder ampacity and surface resistivity after pipe ageing should be verified on production-scale equipment before commercial qualification.

    Free Quote

    Competitive NOVA Chemicals Novapol® PI-2024-A LLDPE Masterbatch Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Novapol® PI-2024-A is supplied as a linear low density polyethylene masterbatch carrier resin for colour, filler, and functional additive concentrates. The product’s primary specification anchors are a nominal melt index of 20 g/10 min measured under 190 °C/2.16 kg according to ASTM D1238 and a nominal density of 0.924 g/cm³ measured according to ASTM D792. These values do not describe a film resin; they describe a high-flow polyolefin carrier selected to reduce melt pressure and torque in high-loading masterbatch extrusion. The 0.924 g/cm³ density places the grade close to standard LLDPE diluents, which limits density stratification at the let-down step in blown film and extrusion coating. Because the backbone is linear rather than branched, the resin exhibits a narrower molecular weight distribution than a branched LDPE of similar melt index, producing lower melt elasticity and a more pronounced shear-thinning viscosity profile. This linear structure also has implications for strand stability, dispersion shear, and the dimensional consistency of the compounded pellet.

    Apparent specification and processing anchor points for NOVA Chemicals Novapol® PI-2024-A
    ParameterReference condition / equipmentValue / range
    Nominal melt indexASTM D1238, 190 °C, 2.16 kg20 g/10 min
    DensityASTM D7920.924 g/cm³
    Typical barrel set-point rangeCo-rotating twin-screw extruder, 40:1 L/D180–220 °C
    Maximum continuous melt temperatureMelt thermocouple, pre-die≤250 °C

    How Does PI-2024-A Perform Under High-Shear Dispersion of Inorganic and Organic Pigments?

    In masterbatch manufacture, dispersion quality is governed by the applied shear stress relative to pigment aggregate strength. A 20 g/10 min LLDPE carrier has a lower apparent viscosity than a 1.0–2.0 g/10 min LLDPE film resin at the same shear rate. This reduces screw torque and die pressure, but it also reduces the maximum shear stress available at constant screw speed. On a production-scale co-rotating twin-screw extruder with 40:1 L/D and kneading blocks in barrel zones 5 through 8, typical barrel set points of 180–220 °C are used. The actual melt temperature is not equal to the barrel set point; viscous dissipation in the kneading section can raise melt temperature by 15–25 °C when screw speed exceeds 600 rpm at a throughput of 400 kg/h. Because the oxidation threshold is 250 °C, the operator must measure melt temperature with a pre-die thermocouple rather than infer it from barrel-zone set points. At screw speeds above 600 rpm, the residence time shortens, but local melt-temperature spikes in the kneading blocks can still degrade heat-sensitive pigments.

    Pigment loading windows depend on the specific surface area and oil absorption of the pigment. For a phthalocyanine blue pigment with BET surface area above 50 m²/g, carrier demand commonly falls in the 60–70 wt% range to prevent excessive screen-pack pressure and press outlet temperature. For a titanium dioxide grade with an alumina-organic surface treatment, carrier content may be reduced to 30–50 wt% because the pigment aggregates are less cohesive and have lower oil absorption. The carrier density of 0.924 g/cm³ is not the primary variable controlling pigment wetting; dispersant chemistry and the sequence of pigment addition along the extruder barrel dominate. PI-2024-A is introduced at the main feed throat, while heat-sensitive organic pigments may be side-fed at zone 7 after the first melt seal to reduce total thermal history. Published data for specific side-feeding configurations with PI-2024-A is limited; equipment trials should define the exact split-feed position.

    Specific energy input during masterbatch compounding is typically recorded in kWh/kg. For a 20 g/10 min LLDPE carrier, specific energy input can be 0.15–0.25 kWh/kg for low-viscosity formulations and 0.30–0.45 kWh/kg for high-loading black masterbatches. Because the carrier reaches full melting early in the screw, downstream dispersion zones operate in a lower-viscosity melt; this reduces power consumption but also means that dispersive mixing must be achieved through kneading-block geometry rather than prolonged high-viscosity shear. The resin is compatible with melt filtration using 100–200 mesh screens, but high filler loadings may require a continuous screen changer with two parallel cavities to avoid pressure drops above 8 MPa. Pressure drop across the melt filter should be logged every 15 min during production to detect screen blinding at an early stage.

    From a comparative standpoint, replacing a 20 g/10 min branched LDPE carrier with PI-2024-A changes strand pelletization behaviour more than dispersion energy. Branched LDPE shows elongational strain hardening, which stabilizes the molten strand between die and water bath. PI-2024-A, by contrast, has lower melt elasticity, so strand breakage becomes more likely if water-bath temperature is above 40 °C or if pelletizer feed speed is not matched to extruder output. On lines equipped with a strand die and a stainless-steel water slide, operators typically reduce water temperature to 30–40 °C and increase the air-knife air flow to remove surface moisture before the strand enters the pelletizer. In diluted compounds, the LLDPE carrier contributes higher tensile strength and environmental stress-crack resistance than a branched LDPE carrier of equivalent melt index. This is important in packaging applications where the masterbatch is let down at 3–5 wt% into LLDPE or LDPE blown film. The melt-flow shift of the final compound follows a roughly logarithmic mixing relationship; the exact shift must be measured by ISO 1133-1:2022 because the diluent melt index and molecular weight distribution interact with the carrier.

    Compared with a standard 1.0 g/10 min LLDPE film grade, PI-2024-A exhibits approximately 20 times greater melt flow under the same ASTM D1238 condition. This is the central difference in carrier selection: the higher melt flow permits finer dispersion aids, higher filler loadings, and lower head pressure, but it reduces melt strength and may require tighter pelletizer control. Against metallocene-catalyzed LLDPE carriers of similar density and melt index, PI-2024-A may have a broader comonomer distribution. The broader distribution can affect seal initiation temperature in final films if the masterbatch is used at high let-down ratios. However, because carrier addition is typically 2–5 wt%, the effect is minor relative to the base resin. Published data for seal initiation shifts in PI-2024-A-containing films is limited; film converters should confirm seal performance by ASTM F88/F88M on the final structure.

    Comparison of typical carrier categories
    Carrier typeMelt indexDensityMelt strengthDispersion energy requirement
    Novapol PI-2024-A LLDPE20 g/10 min0.924 g/cm³Low to moderateModerate
    Branched LDPE carrier20 g/10 min0.923 g/cm³HighModerate
    Standard LLDPE film resin1.0–2.0 g/10 min0.918–0.920 g/cm³ModerateHigh
    HDPE masterbatch carrier8–20 g/10 min0.953–0.958 g/cm³LowHigh for polar liquids

    When the Resin Is Utilized as a Carbon Black Masterbatch Carrier

    Carbon black masterbatches represent a demanding test environment because the filler increases melt viscosity and produces severe abrasive wear. In a 50 mm co-rotating twin-screw extruder operating at 300 kg/h, a typical screw configuration for 40 wt% carbon black in PI-2024-A includes two high-shear kneading sections followed by a vacuum vent at zone 9. Barrel temperatures are held at 180–220 °C, and the vacuum vent is maintained at -0.08 MPa to remove adsorbed moisture and low-molecular-weight volatiles. The high melt flow of the carrier reduces the pressure drop across the downstream 200-mesh screen pack, but it does not eliminate screen-pack fouling if carbon black agglomerates are poorly dispersed. When pelletizing high-loading black masterbatch, melt strength limitations become evident: strand cooling must be rapid and uniform; water-bath temperature above 40 °C leads to strand sagging and pelletizer jam. The use of a strand die with multiple holes smaller than 3 mm diameter increases die pressure and should be avoided unless the extruder has adequate specific torque. Published data for this exact PI-2024-A carbon black configuration is limited; robust scale-up should include melt-filter pressure monitoring, melt thermocouple mapping, and pellet bulk-density verification before full production.

    In injection molding masterbatches, the high melt flow of PI-2024-A improves distribution in polypropylene and polyethylene matrices at low let-down ratios. When the masterbatch is added at 2–4 wt% to a 10 g/10 min polypropylene homopolymer, the carrier’s 20 g/10 min flow reduces the possibility of unmelted concentrate pockets in the metering zone. On a 1200 kN clamp-force injection molding machine running a 24-cavity thin-wall mould, screw recovery time and melt temperature are typically more sensitive to the base resin than to the masterbatch at 2 wt% addition. However, if the masterbatch is poorly dispersed, black specks and colour streaks appear before mechanical properties change; therefore, filter testing with a 100 mm single-screw extruder equipped with a 25 mm melt filter is used as a quality gate. Tensile yield strength of injection-molded specimens should be determined by ASTM D638-14 on neat carrier and on diluted formulations to separate dilution effects from pigment effects. Published data for PI-2024-A in thin-wall injection molding is limited; the carrier should be evaluated with the specific pigment loading and part wall thickness.

    Moisture uptake in the carrier is largely a surface phenomenon. At ambient relative humidity above 60%, surface condensation on pellets can introduce 0.05–0.1 wt% moisture at the feed throat; this is sufficient to create strand porosity in an open-vent extruder. Pre-drying in a desiccant or hot-air hopper at 70–80 °C for 1–2 h reduces surface moisture below 0.05 wt%. Storage below 40 °C and exclusion of direct sunlight are standard for polyolefin carriers; ultraviolet exposure causes chain scission and an upward drift in melt index over months of outdoor storage. From a regulatory standpoint, a masterbatch carrier cannot confer blanket food-contact approval to the final compound. The formulated masterbatch must be evaluated under the relevant end-use regulation, such as FDA 21 CFR 177.1520(c) for olefin polymers in food-contact articles or EU Regulation 10/2011. REACH and RoHS declarations for PI-2024-A should be obtained from the supplier as lot-specific compliance documents. Published data for this specific grade in fatty-food simulants is limited; extraction testing should be performed on the diluted final compound rather than inferred from the carrier alone.

    Rheological Boundaries and Additive Interaction Limits

    Rheological boundaries are defined by the low zero-shear viscosity and the shear-thinning character of the linear polymer. At 190 °C, a 20 g/10 min LLDPE of this class exhibits an apparent viscosity approximately one order of magnitude lower than a 2.0 g/10 min LLDPE at equivalent high shear rate. This allows high filler loadings to pass through 200-mesh screen packs, but it limits the shear stress available for dispersing tightly bound organic pigment agglomerates. The processing window narrows when the formulation includes additives that alter thermal stability. Amine-based flame retardants or free-amine-containing stabilizers can accelerate oxidative degradation at melt temperatures above 230 °C; pre-screening by oxidative induction time according to ASTM D3895 is required before production scale-up. Fluoroelastomer processing aids are effective at 300–500 ppm for controlling die-lip fouling in high-flow LLDPE, but their benefit diminishes at melt index values above 20 g/10 min because the carrier already develops a thin surface layer at the die. Chlorinated additives should be avoided in high-temperature compounding above 220 °C due to potential release of hydrogen chloride, which corrodes nitrided barrel surfaces. If the masterbatch is intended for subsequent multilayer film structures, the carrier’s viscosity mismatch with tie-layer resins should be evaluated by parallel-plate rheometry at 190 °C across shear rates from 0.01 s⁻¹ to 100 s⁻¹. Published data for PI-2024-A in multilayer tie-layer coextrusion is limited; rheological compatibility must be confirmed with the specific coextruded structure.

    Top