| HS Code | 250563 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melt Flow Ratio I21 I2 | 30 |
| Tensile Strength At Yield | 9.7 MPa |
| Tensile Strength At Break | 27.6 MPa |
| Elongation At Break | 700% |
| 1 Secant Modulus | 207 MPa |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12% |
| Gloss 45 | 55 |
| Vicat Softening Point | 100°C |
| Melting Point | 120°C |
As an accredited NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Novapol PF-Y821-BP Butene LLDPE Film Resin is packaged in 25 kg PE bags, 55 bags per pallet (1,375 kg). |
| Container Loading (20′ FCL) | 20′ FCL loading: NOVA Novapol PF-Y821-BP butene LLDPE film resin in 25 kg bags, palletized, shrink-wrapped, secured for ocean transit. |
| Shipping | NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin is shipped as non-hazardous, free-flowing resin pellets. Standard packaging: 25 kg polyethylene bags, palletized and stretch-wrapped, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from heat, moisture, and ignition sources. No special transport placards required. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, strong oxidizers, and incompatible materials. Keep original bags or containers closed, palletized, and off the floor. Protect from moisture, dust, and physical damage. Avoid excessive stacking and contamination. Maintain good housekeeping. Follow the manufacturer’s SDS and local regulations for safe handling and storage. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored in a cool, dry, well-ventilated area away from direct sunlight. |
On high-throughput pallet unitization lines where powered pre-stretch carriages sustain elongations of 200–250% at wrapping speeds above 40 revolutions/min, PF-Y821-BP is processed as the core constituent of a three-layer cast stretch film. A 90 mm barrier screw extruder with a 30:1 L/D ratio, a 2,400 mm coathanger die, and a 1,000 mm chrome-plated chill roll held at 20–24 °C are used, with the resin blended at 75–85 wt% in the core and a lower-melt-index LDPE skin layer at 10–20 wt% to reduce edge neck-in. Melt temperature is maintained at 240–260 °C; die gap is set to 0.5–0.7 mm; line speeds of 350–550 m/min are typical before draw resonance instability begins. Polyisobutylene cling additive at 0.5–1.5 wt% is metered into one or both skin layers, while 5–15 wt% edge trim regrind is returned to the core without measurable loss of dart drop impact under ASTM D1709 when the regrind fraction is kept below 15 wt% and 80/120 mesh screen packs are used. Finished film of 12–23 µm thickness is evaluated under ASTM D882 for tensile elongation at break, which typically falls in the 350–500% range for butene LLDPE films of this density class, and under ASTM D5748 for protrusion puncture resistance. The resin’s olefin polymer status supports compliance with FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011 when the stretch film is used in indirect food-contact transport applications, while REACH SVHC restrictions are managed through the supplier’s product stewardship declarations. Terminal roll goods include 250 mm and 500 mm wide machine-film rolls for rotary ring wrappers and hand-film rolls for low-volume warehouses.
Blown film lines running 40 µm monolayer or three-layer structures for frozen vegetable and seafood packaging encounter puncture propagation failures when the butene LLDPE layer is diluted beyond 20 wt% LDPE or when the frost line is set too high, producing a quenched skin with lower post-crystallization ductility. With PF-Y821-BP as the core layer at 70–80 wt% and a branched LDPE carrier at 20–30 wt%, the bubble is processed at a blow-up ratio of 2.5:1 to 3.0:1, with frost line height controlled between 6 and 8 die diameters to preserve machine-direction tear resistance. Melt temperature at the die is held at 195–215 °C; die gap is set at 1.2–1.8 mm for a 250 mm die. Under ASTM D1709 Method A, 40 µm film structures generally exhibit dart impact values above 150 g, while Elmendorf tear propagates at 20–35 g in the machine direction and 35–60 g in the transverse direction under ASTM D1922, with lot-to-lot variation of ±10% observed on production lines. Low-temperature ductility at -20 °C is assessed through tensile impact per ISO 8256, and film failure under cold-chain distribution is most frequently observed as brittle splitting at heat-seal corners when seal bar temperature exceeds 150 °C and dwell time falls below 0.5 s. The compliance table below identifies the principal food-contact and mechanical test standards required for frozen-food converters.
| Requirement | Standard/Designation | Test Parameter |
|---|---|---|
| FDA olefin polymer | 21 CFR 177.1520(c) | Extraction limits |
| EU food contact | Regulation (EU) No 10/2011 | OML and specific migration |
| Dart impact | ASTM D1709 Method A | Failure mass |
| Elmendorf tear | ASTM D1922 | MD/TD tear force |
| Tensile properties | ASTM D882 | Elongation at break |
| Tensile impact | ISO 8256 | Cold-chain ductility |
Agricultural silage cover and greenhouse film production relies on monolayer or three-layer blown film lines where PF-Y821-BP is combined with UV-stabilized masterbatch and EVA to achieve weathering resistance and puncture toughness. In a 60 mm grooved-feed extruder with a 28:1 L/D ratio, a 200 mm die, and a dual-lip air ring, the formulation generally includes 80–90 wt% PF-Y821-BP, 5–10 wt% EVA with 18% vinyl acetate, and 3–6 wt% HALS-based UV masterbatch; dispersed silica antiblock is added at 3,000–6,000 ppm to prevent film blocking on rewind. The bubble is run at a blow-up ratio of 2.0:1 to 2.8:1, with frost line height fixed at 5–7 die diameters and die temperature of 200–220 °C. Film thickness of 25–50 µm is verified by capacitance gauge and controlled within ±5% to prevent thin spots that fail under wind-induced flutter. Retention of tensile elongation after 12 months of outdoor exposure is evaluated under EN 13206 for silage films, while UV degradation is monitored by carbonyl index increase through FTIR per ASTM D5576. The main production failure mode is bubble instability in high ambient humidity above 70% RH, which is corrected by raising air ring temperature and reducing internal bubble cooling airflow by 15–20%. Terminal products include 25–50 µm greenhouse side films and 45–75 µm silage covers.
Flexible packaging converters producing extrusion-laminated sealant layers from PF-Y821-BP evaluate seal strength performance after duplex or triplex lamination to PET, BOPP, or aluminium foil. The resin is extruded through a 90 mm flat-die cast line at 250–280 °C with a die gap of 0.5–0.7 mm into a 15–30 µm coating on the primary web, then nipped against a chilled roll at 15–20 °C and corona-treated to 38–42 dyn/cm before adhesive lamination. Draw resonance and edge weave appear when melt temperature exceeds 280 °C or when the line accelerates above 200 m/min, producing gauge defects that lower heat-seal strength. On a laboratory heat sealer with a 2 mm sealing bar, 25 µm sealant films achieve seal initiation at 95–110 °C and plateau seal strengths of 12–18 N/25 mm under ASTM F88, depending on seal dwell time of 0.5–1.0 s and pressure of 0.3 MPa. The resin’s compliance with FDA 21 CFR 177.1520 and EU Regulation No 10/2011 permits use as a food-contact sealant layer in snack food pouches and dry-mix packaging, provided migration testing under the finished laminate is completed according to EN 1186. Terminal products include 100–500 g stand-up pouches, lidding films for dairy cups, and medical device pouch sealants where tear propagation under ASTM F2029 is monitored.
On heavy-duty sack lines producing 60–120 µm blown film for resin pellet bags and construction product packaging, PF-Y821-BP is processed with 10–20 wt% HDPE or high-molecular-weight LDPE to increase modulus without sacrificing dart impact. A 75 mm barrier-screw extruder with a 30:1 L/D ratio feeds a 300 mm die with 1.2–2.0 mm die gap; blow-up ratio is held at 2.0:1 to 2.5:1 to balance machine-direction tensile strength and transverse tear resistance. At 80 µm thickness, dart impact measured by ASTM D1709 Method B generally remains above 300 g, while Elmendorf tear values in the transverse direction are 50–80 g under ASTM D1922. The film is converted into side-gusseted or bottom-gusseted sacks on form-fill-seal equipment running 20–40 bags/min, where heat-seal jaw temperatures of 140–160 °C with 1.0–1.5 s dwell are typical. Field failure modes include seam splitting at the top closure when extrusion melt temperature falls below 195 °C and incomplete homogenization creates melt fracture, and pinholes near the gusset crease when the film is drawn below 60 µm. Sack drop resistance is evaluated per ASTM D5276 at a drop height of 1.2 m with a 25 kg load. Terminal products include 25 kg resin pellet sacks, 10–40 kg construction adhesive bags, and woven laminate outer plies for export packaging.
Where inflatable dunnage bags are sealed from monolayer blown film, the inner ply must retain air at 0.2–0.4 bar without pinhole leakage or creep deformation during road, rail, or ocean transit. PF-Y821-BP is extruded through a 55 mm single-screw blown film line with a 150 mm die at 190–210 °C, with a blow-up ratio of 2.0:1 to 2.5:1 and film thickness controlled at 50–80 µm. Published datasheet values for this specific gel count configuration are limited; converters therefore establish internal limits using film quality analyzers. The film generally requires a gel count below 10 particles per 1,000 cm², because gel particles above that threshold nucleate pinholes under cyclic inflation loads. Sealing jaws are run at 1.5–2.0 s dwell and 0.4 MPa pressure to produce through-width seals that hold 0.3 bar for 24 h during leak-down testing. The terminal dunnage bags are filled to 20–40% of void volume with compressed air and are used as 90–120 cm wide load restraint cushions between pallets in containerized shipments.
Competitive NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVAPOL® PF-Y821-BP from NOVA Chemicals is a butene-comonomer linear low density polyethylene supplied for blown-film extrusion. The resin’s nominal melt flow rate is 0.8 g/10 min at 190°C/2.16 kg when determined by ISO 1133-1:2022 or ASTM D1238; its nominal density is 0.921 g/cm³ when determined by ISO 1183-1:2019 or ASTM D1505. This places the material above the common 0.918 g/cm³ butene-film baseline and below typical MDPE densities of 0.926–0.940 g/cm³. The butene comonomer differentiates PF-Y821-BP from hexene- and octene-based LLDPE grades: short-chain branch distribution is broader, and the concentration of effective tie molecules at equivalent density is lower. The grade is therefore specified where film stiffness, yield strength, and dimensional stability are weighted more heavily than high-speed puncture.
| Parameter | Published nominal value | Test method |
|---|---|---|
| Melt flow rate (190°C/2.16 kg) | 0.8 g/10 min | ISO 1133-1:2022 / ASTM D1238 |
| Nominal density | 0.921 g/cm³ | ISO 1183-1:2019 / ASTM D1505 |
| Comonomer | Butene | Supplier-controlled; FTIR or NMR verification |
| Product form | Pellet | Hopper handling and conveying |
| Primary conversion route | Blown-film extrusion | Not applicable |
High-stalk blown-film extrusion imposes anisotropic melt stretching that the bubble must sustain without oscillation. PF-Y821-BP has a melt flow rate of 0.8 g/10 min, which is lower than the 1.0 g/10 min common in general-purpose film grades. On smooth-bore extruders, this increases head pressure and shear heating. If the screw speed and temperature profile are retained from a 1.0 g/10 min resin, discharge melt temperature can rise by 5–15°C. When melt temperature exceeds 227°C, surface oxidation and gel formation may become measurable as film specks. A grooved-feed extruder with L/D ratio of 25:1–30:1 is preferred for this grade because the grooved section controls solids conveying and permits lower barrel temperature settings.
Bubble stability is governed by die gap, blow-up ratio, frost line height, and the resin’s elongational viscosity. On typical monolayer lines with die diameter 200–300 mm and die gap 1.5–2.2 mm, the resin is usually run at a blow-up ratio of 2.0–3.0. Frost line height is commonly maintained at 3–5 die diameters for high-stalk operation. Below that range, the stalk may freeze too quickly and produce uneven gauge bands; above that range, the bubble can oscillate because the melt has not locked tensile orientation. These ranges are starting points rather than product-specific guarantees. They require adjustment for die design, air-ring performance, and temperature control.
When PF-Y821-BP is processed as a core layer in three-layer structures, bubble stability typically improves because the skin layers contribute melt strength and seal behavior. Published data for PF-Y821-BP in high-stalk three-layer structures remains limited. A processor should record gauge variation by scanning film at 10–15 cm intervals around the circumference and compare it with the incumbent grade. Acceptable gauge variation is commonly maintained below ±5% for converting operations.
During coextrusion with lower-density skin layers, the combination of a PF-Y821-BP core and 0.918 g/cm³ skins raises overall modulus while retaining seal initiation below 110°C if the skin is formulated for low seal initiation. The actual seal initiation must be verified by ASTM F1921 or ASTM F2029; the core layer does not seal but influences thermal conduction during heat sealing and gauge distribution after film blowing.
The density increase from 0.918 g/cm³ to 0.921 g/cm³ is small numerically but meaningful in semi-crystalline polyethylene because crystalline fraction rises and the amorphous tie-molecule population shifts. In comparative film samples at 50 μm thickness, PF-Y821-BP is expected to show higher secant modulus at 1% strain than a 0.918 g/cm³ butene grade, while dart impact measured by ASTM D1709A may be lower by a double-digit percentage. Elmendorf tear values measured by ASTM D1922 also depend on orientation; because PF-Y821-BP has lower melt flow, machine-direction orientation can be higher at the same frost line height. That may depress MD tear unless frost line or blow-up ratio is adjusted.
Compared with an octene LLDPE of equivalent density, PF-Y821-BP typically exhibits lower dart impact and lower Elmendorf tear at equal gauge. The mechanistic distinction is that octene comonomer produces longer short-chain branches that form a higher concentration of tie molecules between lamellae; butene branches are shorter and less effective. The butene grade, however, often has higher melt strength and easier bubble stability on long-stalk equipment because of the broad molecular weight distribution of Ziegler-Natta LLDPE. The tradeoff is processability and stiffness against impact and tear.
Water-vapor transmission rate of the higher-density grade should be measured directly by ASTM F1249 at 38°C and 90% RH rather than inferred from density alone. In opaque packaging, the appearance shift is not critical; in clear retail packaging, a lower-density hexene or metallocene grade may be preferable because greater crystalline fraction can raise haze measured by ASTM D1003 and reduce gloss measured by ASTM D2457.
| Attribute | PF-Y821-BP | 0.918 butene LLDPE | 0.918 octene LLDPE |
|---|---|---|---|
| Nominal density | 0.921 g/cm³ | 0.918 g/cm³ | 0.918 g/cm³ |
| Nominal melt flow rate | 0.8 g/10 min | 1.0 g/10 min typical | 1.0 g/10 min typical |
| Film stiffness at equal gauge | Higher | Baseline | Equivalent to slightly lower |
| Dart impact at equal gauge | Lower | Baseline | Higher |
| Elmendorf tear at equal gauge | Lower | Baseline | Higher |
| Melt strength and bubble stability | Higher | Baseline | Lower to equivalent |
| Low-temperature toughness | Lower than octene | Baseline | Higher |
The rankings in Table 2 assume identical film thickness, blow-up ratio, die gap, and quench conditions. They are comparative relationships rather than engineering design data.
Heavy-duty sack and liner applications commonly use a 0.918 g/cm³ butene LLDPE blended with LDPE to improve tear and dart. Replacement with PF-Y821-BP raises blend density and decreases melt flow. On a three-layer line, the resin is usually placed in the core or a sub-skin layer to control stiffness without sacrificing seal integrity. Before replacement, the converter should calculate blend density and melt flow from the component values and compare them with the target. A shift in blend melt flow from 1.0 g/10 min to 0.9 g/10 min may be sufficient to change backpressure and pressure drop in the filtering system.
The preferred equipment configuration is a grooved-feed extruder with a barrier screw and L/D of 30:1. In this configuration, melt temperature can be held at 210–230°C at the die while maintaining output. Die pressure should be monitored; for a 250 mm die with 2.0 mm die gap, pressure increases above those of a 1.0 g/10 min grade are commonly observed. Screen changer pressure drop should be kept below the manufacturer’s rated intermittent and continuous limits. Pellet fines generated during transfer can raise pressure drop by 0.5–2.0 MPa depending on filter area and flow rate.
Film mechanical tests for heavy-duty sacks should include ASTM D882 tensile, ASTM D1922 Elmendorf tear, ASTM D1709A dart, and ASTM D5748 puncture. Gauge reduction can proceed only after confirming that tear and puncture remain above the customer specification. Stiffness improvement alone does not guarantee fitness when sacks are dropped, dragged, or folded at stress concentration points.
PF-Y821-BP is not hygroscopic in the manner of polyamide or polyester, but condensation formed during silo or railcar transfer can become entrained in the melt and appear as bubble defects. If pellets are delivered cold and the receiving environment has a dew point higher than the pellet surface temperature, allow 4–6 h in a dry indoor silo before conveying. Avoid blending with acidic purge compounds or high-peroxide masterbatches without verifying compatibility with the supplier’s antioxidant package.
Capillary rheometry of PF-Y821-BP by ASTM D3835 at 190°C typically shows a shear-thinning response characteristic of broad molecular weight distribution Ziegler-Natta LLDPE. The flow curve is steeper than that of a metallocene hexene grade at equivalent melt flow rate; therefore, shear viscosity at high channel rates is lower than would be predicted from the low melt index alone. This shear thinning assists film blowing but does not eliminate the high-pressure contribution of the 0.8 g/10 min melt flow rate. In additive letdown, the higher low-shear viscosity can increase power consumption of a single-screw side-arm extruder on the film line. The side-arm temperature may need to be raised by 5–10°C to avoid granule bridging.
Extensional thickening in the bubble is less pronounced than in LDPE long-chain branched grades. This means PF-Y821-BP will not provide the same strain-hardening bubble stability as an LDPE-rich blend. Processors who replace LDPE with PF-Y821-BP in bubble-stability-critical structures should monitor stalk diameter variation and replace only a portion of the LDPE, not the entire long-chain branched component.
Polyethylene base resin with density 0.921 g/cm³ falls within the description of FDA 21 CFR 177.1520(c) for olefin polymers under conditions of use specified in that section. However, grade-specific approval must include antioxidants and process aids; the base resin citation alone is insufficient for direct food-contact decisions. The supplier’s food-contact status letter should be requested for the specific product lot and matched to the packaging end use. For EU applications, overall migration and specific migration must meet Commission Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² for food contact materials. Compliance with REACH and RoHS must be confirmed from the safety data sheet and regulatory declarations; these do not automatically follow from the base resin.
Incoming resin inspection should verify melt flow rate and density against the supplier’s certificate of analysis. A density shift of 0.0005 g/cm³ can change water-vapor transmission and modulus, and a melt flow shift outside the specified range can alter backpressure and gauge uniformity. These two properties should be recorded for every lot. If film tear or dart shifts are observed, the next step is to check lot-to-lot molecular weight distribution or additive package by gel permeation chromatography or rheological analysis.
Application of PF-Y821-BP in frozen-food packaging requires low-temperature toughness data. The film should be conditioned at -20°C and tested for dart impact or puncture using the same methods as the incumbent structure. Because published data for PF-Y821-BP under frozen-food converting conditions remains limited, pilot-scale trials on the intended line are necessary before replacing a hexene or octene grade. Surface properties such as slip and antiblock must be adjusted by the processor unless the supplier’s technical data sheet confirms the resin already contains the required additive package.