| HS Code | 593260 |
| Manufacturer | NOVA Chemicals |
| Product Name | Novapol PF-Y821-B |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene |
As an accredited NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL: 10 pallets, 25 kg bags, 13.75 MT; shrink-wrapped, strapped, and loaded in a clean, dry container. |
| Shipping | NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin is a non-hazardous polymer resin, typically shipped in 25 kg bags, bulk bags, or bulk trucks/railcars. Keep packages dry, clean, and away from heat or UV. It is not regulated for transport under DOT, IMDG, or IATA. |
| Storage | Store at ambient temperature, protected from weather. Keep Novapol® PF-Y821-B resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags or containers closed, clean, dry, and palletized; avoid punctures and moisture uptake. Use first-in, first-out inventory and observe shelf-life guidance. Maintain good housekeeping to prevent pellet spills and slipping. |
| Shelf Life | No specific shelf life; stable under normal storage conditions in a cool, dry, well-ventilated area away from heat and sunlight. |
In blown-film conversion of heavy-duty shipping sacks with a target finished thickness of 100–140 µm, PF-Y821-B is let down at 20–30 wt% into a high-pressure LDPE carrier resin to offset the reduced extensional viscosity of butene-copolymer LLDPE. The formulation for filling-head impact resistance typically contains 2.5–5.0 wt% of a carbon black or white pigmented masterbatch and 0.5–1.5 wt% of a fluoroelastomer processing aid to suppress melt fracture on high-output grooved-feed extruders. The linear backbone raises slow puncture resistance under ASTM D5748 and dart impact under ASTM D1709, but it narrows the blow-up ratio window because the low melt strength of butene LLDPE produces bubble flutter when frost line height exceeds 8 die diameters.
On a 65 mm grooved-feed extruder with a 30:1 L/D barrier screw and temperature profile 190–230 °C, die gap 1.2–2.0 mm, blow-up ratio 2.0:1–2.8:1, and die exit melt temperature below 240 °C, the blend maintains acceptable gauge uniformity. Above 30 wt% PF-Y821-B, machine-direction Elmendorf tear measured under ISO 6383-2 increases, but bubble oscillation frequency rises on oscillating haul-off equipment and edge creasing becomes visible in collapsed film. Published data for this specific blend on large-scale sack lines is limited; the maximum practical letdown depends on tower height, collapsing frame geometry, and air-ring control algorithm.
Finished sacks converted from this structure are used for compression-stacked polymer pellets, fertilizer, and lightweight mineral fillers, where bottom-seal creep under 25–35 kg fill mass is evaluated by stacking tests under ASTM D642 and, when UN certification applies, by drop and stacking performance under ADR/RID or 49 CFR 178 packaging instructions. For non-food industrial sacks, the structure is assessed against REACH 1907/2006; if the film functions as a direct food-contact liner, the olefin polymer composition falls under FDA 21 CFR 177.1520 and migration testing under EU Regulation 10/2011 must confirm overall migration below 10 mg/dm².
Cast hand-wrap film at 23 µm total thickness imposes edge-necking limits on PF-Y821-B because butene branches produce less pronounced shear thinning than octene-copolymer LLDPE used in high-performance stretch wrap. On a 75 mm cast-film extruder with a 30:1 L/D screw, coat-hanger die, air gap 45–75 mm, melt temperature 245–260 °C, and chill roll temperature 18–28 °C, PF-Y821-B at 10–20 wt% in the core layer can be run with electrostatic edge pinning. Above 30 wt%, observed edge-necking and web break frequency become line-speed dependent; published data for this specific configuration is limited, and a pilot trial is required to establish the upper letdown.
The formulation segregates PF-Y821-B to the core layer, while the cling layer contains 2–5 wt% polyisobutylene or an EVA-based cling concentrate to maintain unwind forces. Finished films are tested for probe puncture under ASTM D5748, machine-direction elongation under ASTM D882, and cling release under ASTM D5458. Direct food-contact outer layers must comply with FDA 21 CFR 177.1520 and EU Regulation 10/2011; a functional barrier justification may be used for the core layer where migration of core-layer additives is not analytically detectable.
Typical conversion setpoints for PF-Y821-B in blown and cast film applications are consolidated below. The ranges are industrial starting values, not supplier specifications.
| Conversion route | Parameter | Working window | Limiting observation |
|---|---|---|---|
| Blown film | Melt temperature | 190–240 °C | Exceeding 240 °C raises gel formation risk in butene LLDPE |
| Blown film | Die gap | 0.8–2.0 mm | Gaps below 0.8 mm require higher head pressure |
| Blown film | Blow-up ratio | 2.0:1–3.0:1 | Above 3.0:1, reduced melt strength may destabilize the bubble |
| Cast film | Chill roll temperature | 18–28 °C | Lower temperatures increase quench rate but can alter cling-layer migration |
| Cast film | Air gap | 40–90 mm | Above 90 mm, edge-necking increases |
When a 50 µm monolayer blown film is specified for rapid-freeze vegetable packaging, the low-temperature puncture behavior of PF-Y821-B is assessed after 24 h conditioning at −18 °C under ASTM D1709, while tensile elongation after conditioning is measured under ISO 527-3. The nominal density of 0.918 g/cm³ reduces crystalline fraction relative to HDPE and shifts the brittle failure threshold compared with LDPE-only films of equivalent melt index. In this application, PF-Y821-B is typically combined with 1–3 wt% of a silica-based antiblock masterbatch and 0.3–0.8 wt% of an erucamide slip concentrate to achieve a kinetic coefficient of friction below 0.25 under ASTM D1894.
Blown-film processing on a 50–75 mm extruder with 24:1–30:1 L/D, die gap 1.0–1.6 mm, blow-up ratio 2.2:1–2.8:1, and melt temperature 190–220 °C avoids excessive gel formation. Finished products include frozen vegetable bags, frozen potato product overwrap, and ice-pack pouches, where heat seals are produced at 130–150 °C and seal strength is verified under ASTM F88/F88M. Food-law compliance for the film is provided by FDA 21 CFR 177.1520 and EU Regulation 10/2011, with migration testing under EC 1935/2004 supported by analytical screening for the specific slip and antiblock additives used.
Unpigmented PF-Y821-B blown film does not provide intrinsically low oxygen transmission; preservation of wrapped forage depends on total thickness, UV-opaque pigmentation, and mechanical integrity rather than on a high-barrier polymer matrix. Co-extruded silage wrap based on PF-Y821-B uses an outer white layer containing 3–6 wt% TiO₂ masterbatch and 0.2–0.5 wt% hindered amine light stabilizer, and an inner black layer containing 2–3 wt% carbon black masterbatch. Total thickness for round bale wrap is typically 25–50 µm, while silage pit covers are produced at 100–150 µm.
Processing on multi-layer blown-film towers with oscillating haul-off, die gap 1.6–2.5 mm, blow-up ratio 2.0:1–2.8:1, and melt temperature 200–230 °C provides sufficient gauge distribution for wrapper tensioning. Retained tensile properties after artificial weathering are assessed under ISO 4892-2 and EN 13206; elongation retention is more critical than tensile strength because bale wrap must accommodate respreading and punctures without splitting. This agricultural application is outside food-contact law and is assessed under REACH 1907/2006. Processors should verify cold impact at wrapper operating temperatures below 0 °C, because butene LLDPE exhibits lower elongation than EVA copolymers at freeze-zone temperatures.
In extrusion lamination of oriented polypropylene / cast polypropylene pouches, PF-Y821-B is deposited as an extrusion-coating sealant web at 20–40 µm thickness, die temperature 250–265 °C, and line speed 80–150 m/min. The sealant web may be blended with 5–10 wt% high-pressure LDPE to improve neck-in stability. Adhesion to the OPP substrate is promoted by ozone treatment of the melt curtain or by a 0.5–1.0 µm solventless polyurethane adhesive, while seal initiation temperature is evaluated against a registered control under ASTM F1921 and seal strength under ASTM F88/F88M. The sealant layer is regulated as a direct food-contact material under FDA 21 CFR 177.1520 and EU Regulation 10/2011; in multi-material laminated pouches, the specific migration limit for the complete structure must account for the barrier contribution of the outer polyester layer.
The 60:40 high-pressure LDPE/PF-Y821-B ratio balances dart impact and melt strength for thin-gauge produce bags from 12–25 µm. On a 45 mm smooth-bore extruder with 24:1 L/D, die gap 0.6–1.0 mm, blow-up ratio 2.8:1–3.2:1, and melt temperature 180–210 °C, the blend processes without sharkskin at screw speeds producing 40–60 kg/h. The low melting temperature reduces odor and oligomer buildup on the die lip, but output stability depends on a stable air-ring supply at 15–25 °C.
Finished roll bags for retail produce are commonly perforated and fortified with 1–2 wt% silica antiblock and 0.2–0.5 wt% erucamide to maintain a coefficient of friction of 0.20–0.30 under ASTM D1894. The film is rated for direct food contact under FDA 21 CFR 177.1520 and EU Regulation 10/2011; it is not intended for high-fat fresh meat contact without additional barrier verification because butene LLDPE has limited fat resistance. Heat-seal settings for impulse sealers on automated bagging lines are typically 130–150 °C with 0.2–0.4 MPa jaw pressure.
Compliance verification matrix for the above PF-Y821-B structures is consolidated below.
| Application | Framework or test standard | Evidence or requirement |
|---|---|---|
| Food contact films | FDA 21 CFR 177.1520 | Olefin polymer compositional compliance |
| Food contact films sold in the EU | EU Regulation 10/2011 | Overall migration below 10 mg/dm²; additive-specific migration testing |
| Industrial stretch wrap | REACH 1907/2006 | SDS disclosure, SVHC screening, Annex XVII restrictions |
| Agricultural silage film | EN 13206 | Mechanical property retention after artificial weathering |
| Stretch wrap puncture resistance | ASTM D5748 | Probe puncture force and energy absorption |
| Heat-seal strength | ASTM F88/F88M | Seal strength at defined temperature, dwell, and pressure |
Cast or blown film of 100–200 µm thickness containing PF-Y821-B as the primary resin is converted into construction waste liners, pallet covers, and automotive protective shrouds. The film formulation uses 1–3 wt% UV stabilizer masterbatch only when outdoor exposure exceeds 30 days; unstabilized material is acceptable for short-term internal transport protection. Chemical exposure must be validated under ASTM D543 before contact with aromatic hydrocarbons, chlorinated solvents, or oxidizing acids, because butene LLDPE swells and loses tensile strength in these environments. Heat sealing for industrial liners is performed at 130–150 °C and 0.2–0.4 MPa pressure; seal strength is checked by ASTM F88/F88M on the target film gauge. Regulatory assessment for this non-food segment is limited to REACH 1907/2006 and general packaging waste regulations; no food-contact declaration applies unless the film is subsequently used as a food-contact inner liner and tested accordingly.
Competitive NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® PF-Y821-B is a butene linear low-density polyethylene film resin identified in manufacturer technical literature for blown-film applications. The nominal melt index is 0.80 g/10 min when determined at 190 °C under 2.16 kg load using ISO 1133-1:2022 or ASTM D1238-20 Procedure A. The nominal solid density is 0.918 g/cm³ when determined using ISO 1183-1:2019 or ASTM D1505-18. The butene comonomer produces a linear backbone with short-chain branches that lower melting point and crystallinity relative to high-density polyethylene while retaining higher stiffness than a typical high-pressure LDPE of similar melt index.
The grade suffix B is commonly associated with a formulated additive package in NOVA Chemicals film grades. Slip agent, antiblock, and processing stabilizer loadings are lot-specific and should be confirmed from the supplier’s certificate of analysis before startup. Published product data identify the resin for heavy-duty film structures, including shipping sacks, industrial liners, construction films, and agricultural overwrap, where optical clarity is not a primary design requirement.
Molecularly, the butene branch content of PF-Y821-B is not sufficient to produce the high tie-molecule concentration required by high-dart-impact film. The short-chain branching distribution is comparatively broad due to conventional Ziegler-Natta catalysis, producing a wider molecular weight distribution than metallocene grades. This distribution contributes to reduced melt fracture sensitivity and lower extrusion pressure at shear rates between 100 s⁻¹ and 1000 s⁻¹.
Process stability in blown-film extrusion is governed by the balance between melt rheology, bubble cooling, and film gauge control. For PF-Y821-B, a melt temperature below 175 °C may increase melt viscosity enough to generate high die pressure and sharkskin melt fracture, while melt temperature above 230 °C can induce oxidative degradation and gel formation. The recommended die melt temperature range is 190–220 °C when running monolayer film at 25–100 µm. Die gap is typically set between 1.5 mm and 2.5 mm; a gap below 1.0 mm raises shear rate and lowers the melt fracture threshold, while a gap above 2.5 mm can reduce drawdown and destabilize the bubble. Blow-up ratio should be maintained between 2.0:1 and 2.8:1 to balance machine-direction and transverse-direction properties. On production lines, frost-line height is controlled at 6–10 die diameters; if frost-line height varies by more than 15% from target, bubble wander and gauge bands appear. Cooling air temperature in the air ring is commonly held at 8–15 °C. On a 65 mm single-screw extruder with 30:1 L/D barrier screw, maximum throughput is typically limited by air-ring heat removal rather than screw torque. Internal bubble cooling can increase output but requires tight frost-line control to avoid blocking and tear anisotropy.
At the feed end, the extruder should use a barrier screw with 25:1–30:1 L/D and a Maddock mixing section. Screw speeds above 90 rpm on small lines may introduce shear heating that shifts melt temperature beyond the target window. Melt pressure at the die should be monitored; excursions above 35 MPa often indicate insufficient die gap, excessive screen-pack pressure drop, or feed zone bridging. Screen packs of 20/40/60/80 mesh are common, but pressure drop should be recalibrated after each screen change because aged screens and gels raise backpressure and reduce gauge uniformity. Residence time should not exceed 10 min above 220 °C to limit gel formation.
On production lines, the most common failure modes are bubble instability, gauge variation, and melt fracture. Bubble instability is usually traced to air-ring velocity, frost-line height, or irregular melt temperature; gauge variation above ±5% is addressed by die lip adjustment and air-ring distribution. Melt fracture appears as multiple surface scratches and is corrected by increasing melt temperature, widening die gap, reducing screw speed, or adding processing aid. Gels are often caused by oxidized resin, degraded additive masterbatch, or prolonged residence time above 230 °C; the screw and die should be purged at the first appearance of black specks. Sharkskin at the die exit is more common with narrow die gaps and high shear rates, and can be reduced by increasing die gap to 1.5 mm or above. Screw surging due to insufficient feed zone cooling or hopper bridging manifests as periodic gauge bands.
Film structures based on PF-Y821-B are processed on monolayer and coextruded blown-film lines at thicknesses usually between 40 µm and 100 µm in heavy-duty sack and liner applications. Drawdown ratios above 3:1 are avoided because conventional Ziegler-Natta butene LLDPE has relatively low melt strength compared with high-pressure LDPE, and high-stalk processing can produce unstable bubble geometry. Tensile strength and puncture resistance are sufficient for granular fertilizers, polymer pellets, and textile rolls; however, for sharp-edged contents or high stacking loads, blending with 10–20% hexene LLDPE or HDPE is common. The resin can be used in cast film only if melt strength and edge bead control are addressed by blending with LDPE or using a vacuum box; otherwise, neck-in and draw resonance may limit line speed.
For blown film at 25 µm, machine-direction tensile yield strength typically falls between 10 MPa and 12 MPa under ISO 527-3:2018 or ASTM D882-18, and elongation at break exceeds 700% in both directions. Dart drop impact, measured using ASTM D1709-16a Method A, is commonly in the 90–130 g range for a 0.918 g/cm³ butene LLDPE, but lot-specific values shift with die gap, frost-line height, and blow-up ratio. Elmendorf tear strength under ASTM D1922-15 is usually lower in the machine direction than in the transverse direction, with MD values around 250–400 g and TD values around 450–650 g at 25 µm. Published data for this specific configuration is limited; laboratory-scale film evaluation is required to establish final specification limits because additive package and processing history influence impact and tear. Haze at 25 µm under ASTM D1003-21 is generally above 10%, excluding the product from high-clarity display packaging. The DSC melting peak under ISO 11357-3:2018 is typically observed between 121 °C and 125 °C, and the Vicat softening temperature under ISO 306:2022 or ASTM D1525-17e1 is usually 100–108 °C.
Compared with hexene LLDPE of equivalent density and melt index, the butene grade has lower dart impact and transverse tear after orientation. The difference arises because the shorter C4 branch does not bridge adjacent crystalline lamellae as effectively as a C6 branch. In comparison with metallocene LLDPE, the broader molecular weight distribution of PF-Y821-B enables lower extrusion pressure and better bubble stability, but optical and seal properties are inferior. Against high-pressure LDPE, PF-Y821-B provides higher tensile yield and puncture resistance but lower melt strength.
Because the butene comonomer is less efficient than hexene in tie-molecule generation, PF-Y821-B is not selected where high Elmendorf tear, dart impact, or low film thickness toughness is a hard specification. In coextruded structures, the product often appears in core or inner layers, while metallocene LLDPE or LDPE skins supply surface optics and low seal-initiation performance. For adhesive lamination films, the lower melt strength of the base resin may require blending with 15–25% LDPE to maintain bubble stability; for extrusion coating, this grade is not typical unless blended with a high-melt-strength component. In film resin selection, butene LLDPE occupies a position between LDPE and hexene or octene LLDPE: LDPE offers higher melt strength and lower haze but lower dart impact and tensile strength; hexene LLDPE provides higher dart impact and tear; octene LLDPE extends toughness further with higher flexibility and seal performance; metallocene LLDPE yields low seal initiation and low haze but may require wider die gaps and processing aids to avoid melt fracture. PF-Y821-B is selected when the film must balance stiffness, drawdown, and moderate impact at heavier gauge; it is not specified where the highest Elmendorf tear or optical clarity is required.
Heat-seal performance is a key difference between butene LLDPE and metallocene LLDPE. For PF-Y821-B film at 25 µm, seal initiation temperature is generally reported in the 95–105 °C range according to ASTM F1921-12 or ASTM F88/F88M-21; this is higher than the 80–90 °C range typical of metallocene LLDPE. In vertical form-fill-seal lines operating above 80 cycles/min, short dwell time may prevent adequate seal strength when sealing temperatures are set for metallocene films. Where seal-through-contamination or narrow seal bars are required, blending with 20–30% metallocene LLDPE or a plastomer lowers seal initiation temperature but increases extruder pressure and melt fracture risk. For heavy-duty sacks sealed at lower cycle speeds, seal strength reaches a stable plateau at 120–140 °C, which is usually sufficient for monolayer and laminate constructions.
Regulatory acceptability is determined by final article composition, not pellet compliance alone. The following standards are commonly referenced in product stewardship documentation.
| Standard or regulation | Designation | Relevant parameter |
|---|---|---|
| US FDA | 21 CFR 177.1520 | Olefin polymers for food contact; extraction limits and end-use conditions |
| European Union | Regulation (EU) No 10/2011 | Overall migration and specific migration limits for food contact plastics |
| European Union | Regulation (EC) No 1935/2004 | Framework for food contact materials |
| European Union | Regulation (EC) No 1907/2006 REACH | SVHC content and article notification obligations |
| European Union | Directive 2011/65/EU RoHS | Lead, mercury, cadmium, hexavalent chromium, PBB, PBDE |
Food contact compliance under 21 CFR 177.1520 and Regulation (EU) No 10/2011 depends on additive package, overall migration limits, and end-use temperature. Medical use is not covered by the general olefin polymer designation and requires additional validation under ISO 10993-1:2018. Published data for food-contact compliance at extreme sterilisation or retort conditions is limited; the final converter must perform end-article migration testing.
For mechanical recycling, PF-Y821-B is compatible with mixed polyolefin recompounding in non-food applications; however, slip and antiblock additives can migrate to the surface and alter coefficient of friction after reprocessing. Closed-loop recycling of edge trim and start-up scrap is standard on blown-film lines, but reclaimed content above 20–30% can increase gel count and reduce bubble stability if not homogenized. Coextruded structures containing barrier polymers, tie resins, or EVOH must be separated before mechanical recycling to avoid delamination and viscosity mismatches. Life-cycle assessment data for this specific grade is limited; process energy is dominated by extrusion and film take-off rather than polymerization.
Pellets should be stored below 50 °C and protected from ultraviolet radiation; long storage in direct sunlight can degrade surface additives and shift coefficient of friction. Polyethylene does not require drying under normal conditions, but if the resin is stored at relative humidity above 80% and transferred into a cold production area, surface condensation can introduce moisture-related defects. In that case, hopper drying at 60–70 °C for 2–4 h is sufficient. Dilute-phase conveying should be limited to 20 m/s to reduce fines and streamers; dense-phase conveying is preferred for long distances. Extruder feed throat temperature should remain below 50 °C to avoid pellet melting and bridging. The hopper loader should provide at least 20% capacity above maximum extruder consumption to prevent feed interruptions. Screw and barrel should be cleaned when changing from HDPE or PP to LLDPE to avoid unmelted particles and gels. In-line melt filtration is recommended when post-industrial recycled material is added, with continuous or automatic screen changers set to maintain pressure drop below 10 MPa.