Nova Chemicals Novapol Pf 0218 J Butene Lldpe Film Resin

NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 534237
    Resin Type Butene LLDPE
    Density 0.918 g/cm³
    Melt Index 2.0 g/10 min at 190 °C/2.16 kg
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Tensile Strength At Break Md 34.5 MPa
    Tensile Strength At Break Td 27.6 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Dart Drop Impact 110 g
    Haze 14%
    Gloss 45 55%
    Coefficient Of Friction 0.20
    Blocking 50 g

    As an accredited NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; 55 bags per pallet, totaling 1,375 kg.
    Container Loading (20′ FCL) 20′ FCL: 20 pallets, 25 kg bags, 1,000 kg/pallet; total 20 MT NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin.
    Shipping NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin is a non-hazardous, solid polyethylene resin. It is typically shipped in 25 kg bags, bulk bags, or bulk trucks/railcars. Not regulated for transport by DOT, IMDG, or IATA. Store closed, away from heat and moisture.
    Storage Store Novapol® PF-0218-J Butene LLDPE Film Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and incompatible materials. Keep original bags or containers closed to prevent moisture, dust, and contamination. Palletize securely; avoid excessive stacking. Use first-in, first-out stock rotation. Protect from UV, weather, and physical damage. Follow the supplier SDS and local regulations.
    Shelf Life Shelf life is not applicable; stable under normal storage conditions when kept cool, dry, and away from heat and sunlight.
    Application of NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin

    Horizontal and vertical form-fill-seal lines converting frozen vegetables, IQF poultry portions, and dry sauce mixes at web speeds between 28 m/min and 45 m/min impose a specific set of sealing and abuse-resistance requirements on the sealant web. The resin, a butene-1 linear low-density polyethylene with a nominal density of 0.918 g/cm³ and a melt index of 1.0 g/10 min under ISO 1133-1:2022 condition 190 °C/2.16 kg, is typically coextruded as the skin layer over an MDPE or HDPE core in a three-layer blown film structure. On a 65 mm grooved-feed single-screw extruder having an L/D of 30:1 and a 250 mm diameter die with a die gap of 1.8 mm, a layer ratio of 35/30/35 is used when the total gauge is 50 µm. The skin layer itself is commonly modified with 15 wt% to 25 wt% of a fractional-melt LDPE to improve melt strength and reduce bubble instability during high-output runs. The melt-temperature profile is set between 175 °C and 210 °C, with the feed zone kept below 140 °C to avoid polymer melting on the grooved bushing and the resulting screw-slip oscillation of ±3 rpm observed on production logs when the feed throat overheats.

    The seal-initiation requirement for this structure is set by the package converter at 110 °C to 125 °C for the skin layer, with hot-tack measured on a commercial hot-tack tester under ASTM F1921. Under these conditions, a seal strength of 6 N/25 mm to 12 N/25 mm is achieved at jaw dwell settings of 35 ms to 60 ms; lower dwell times reduce the seal window of butene-1 LLDPE relative to EVA and force the operation toward the upper temperature limit. When film is stored on a slitter at winding tension above 0.35 N/mm², blocking of the slip-containing skin can increase the static coefficient of friction from 0.15 to above 0.45 after 48 h at 35 °C, as measured by ISO 8295. This is a recognized production failure mode in VFFS because the film no longer tracks over the forming collar without creasing. The grade therefore requires release of winding tension before shipment to tropical climates and verification of slip level by solvent extraction before first-use approval.

    Food-contact use is supported by compliance with FDA 21 CFR 177.1520(c) for olefin polymers, subject to the conditions of use specified in 21 CFR 176.170(c). For European Union sale, the finished film falls under Commission Regulation (EU) No 10/2011, with overall migration testing conducted under EN 1186-1:2002 in food simulants selected according to the food type. The additive package, if containing erucamide slip and synthetic amorphous silica antiblock, must be verified against the positive list in EU Regulation 10/2011 Annex I and the specific migration limits applicable to each additive. When the film is used for packaging aqueous foods, the converter typically measures global migration below 10 mg/dm² in simulant A for 10 days at 40 °C; for fatty foods, simulant D2 at 20 °C for 10 days is used.

    Regulatory InstrumentDesignation / ClauseTest ConditionOperational Limit
    U.S. FDAFDA 21 CFR 177.1520(c)Olefin polymers; use conditions per 21 CFR 176.170(c)No visible extractables in finished film; density and molecular weight specifications apply to base resin
    European UnionEU 10/2011 Annex IEN 1186-1:2002 migration testingOML < 10 mg/dm²; specific migration limits for additives per Annex I
    Global MFRISO 1133-1:2022190 °C/2.16 kgNominal 1.0 g/10 min; lot-to-lot acceptance ±0.15 g/10 min
    Seal integrityASTM F88/F88M-21Jaw dwell 40 ms; sealing bar 130 °CMinimum seal strength 8 N/25 mm for frozen-food application

    On the packaging line, the converter validates the distribution cycle by subjecting filled bags to drop testing under ASTM D5276 and puncture resistance under ASTM D5748. The butene-1 comonomer provides a broader sealing window than LDPE alone but a reduced hot-tack ceiling compared with octene-1 LLDPE; this distinction defines the practical upper web speed on multi-head weighers. For operations running faster than 50 m/min, a tie layer or an EVA-based skin is preferred because the butene skin cannot recover quickly enough from the elongation of the fin seal. A converter that attempts to solve this by raising sealing-bar temperature beyond 145 °C typically induces smoke generation from oxidized polymer at the seal edge, leading to loss of package appearance without meaningful increase in hot-tack strength.

    Why Does Agricultural Silage Overwrap Demand Tighter Melt-Fracture Control Than Standard Packaging Film?

    Agricultural silage overwrap and bale wrap produced from PF-0218-J require a different additive and extrusion strategy than VFFS because the film must survive six to nine months of outdoor exposure on farm storage pads. The base resin is extruded at a gauge of 100 µm to 150 µm as a monolayer or coextruded with a photostabilized skin containing 2 wt% to 4 wt% of a hindered amine light stabilizer masterbatch and 1 wt% to 2 wt% of a medium-die-strength carbon black masterbatch when black silage film is specified. The melt temperature is limited to 190 °C to 210 °C because the presence of carbon black and hindered amine stabilizer increases viscosity at the die lip and lowers the critical shear rate for melt fracture. A die gap of 2.0 mm is used in combination with a BUR of 2.0:1 to 2.4:1; tighter BUR reduces tear strength in the transverse direction and leads to split initiation along the bale edge. The film is tested for tensile properties under ISO 527-3 and for tear resistance under ASTM D1922. For a 100 µm monolayer containing 20% fractional-melt LDPE, published data for this specific additive package is limited, so acceptance is based on batch testing rather than fixed reference values.

    On farm, film failure is most commonly observed as transverse splitting initiated by punctures from stalk ends or by wind-induced flutter at the bale edge. The recommended puncture resistance test is ASTM D5748 for stretch-wrap and agricultural films; a minimum retained puncture resistance after 2,000 h of accelerated weathering under ISO 4892-2 is often specified by large dairy cooperatives. The butene-1 resin itself does not provide UV resistance, so any reduction in masterbatch concentration below 2 wt% shifts the failure mode from ductile tear to embrittlement cracking within the first season. Processors that reuse post-industrial scrap from silage film at levels above 15 wt% face an additional risk of film grain and gel specks because the reprocessed film contains soil fines and partially consumed light stabilizer; the reclaim stream should be hot-melt filtered through 80 mesh or better before being reintroduced into the skin layer.

    Chemical Sack Liner Extrusion at High Silica Loadings

    Gusseted liners for granular fertilizers, precipitated silica, and cementitious dry blends are run on large blown-film towers with die diameters from 250 mm to 400 mm and total gauge between 80 µm and 150 µm. The film is produced as a tube with a lay-flat width of 400 mm to 700 mm and is subsequently gusseted and sealed on a bottom-seal bag machine. Because the filled product often has sharp particle edges and high bulk density, the film structure includes a core of PF-0218-J at 60 wt% to 80 wt% blended with fractional-melt LDPE, and an outer layer containing 2 wt% to 5 wt% of an antiblock masterbatch to prevent blocking during warehousing at 50 °C stack temperatures. The melt pressure at the die entrance is monitored continuously; when the silica-filled masterbatch level exceeds 5 wt%, the pressure typically rises from 280 bar to 360 bar on a 75 mm extruder, reducing output by 8% to 12% unless screw speed is increased.

    Chemical compatibility is the primary operational boundary. The butene-1 LLDPE matrix resists aqueous fertilizer salts and dilute acids, but unsaturated oils, hydrocarbon solvents, and surface-active wetting agents can reduce environmental stress-crack resistance measured under ASTM D1693 condition B. When the liner is used for surfactant-containing products or oily formulations, the failure time in constant-stress testing can drop below 100 h at 50 °C, which is unacceptable for export shipments; in such cases a hexene- or octene-based LLDPE or a higher molecular-weight MDPE should replace PF-0218-J. The seal strength of the bottom gusset is evaluated under ASTM F88/F88M-21 after filling, and the drop test is performed in accordance with ASTM D5276. A liner that is too stiff will crack along the gusset fold; therefore, the film is typically annealed at 45 °C to 55 °C for 24 h after conversion to relax orientation before shipment.

    For general-purpose consumer carry-out bags, the grade is blended with 20 wt% fractional-melt LDPE and processed on a conventional 50 mm blown-film line at a BUR of 2.0:1 to 2.5:1 and a die gap of 1.2 mm, with film gauge controlled to ±1.5 µm under ISO 4593 because gauge variation between 18 µm and 22 µm at the punch-out station alters the bag tear orientation; no further formulation adjustment is required beyond routine slip and antiblock verification.

    When Butene LLDPE Replaces EVA in Laminated Sealant Webs for Dry-Product Pouches

    In adhesive-laminated structures of reverse-printed biaxially oriented polyester or BOPP over a sealant web, EVA is often replaced with PF-0218-J to lower cost and improve downgauging. The sealant web is either a monolayer blown film at 30 µm to 50 µm or a cast coextrusion with a total thickness of 25 µm to 40 µm. The butene-1 resin seals at temperatures of 120 °C to 145 °C, approximately 10 °C to 15 °C higher than a comparable EVA with 18% vinyl acetate, which reduces the maximum sealing speed on a horizontal pouch machine from 45 packs/min to 35 packs/min when dwell time remains at 50 ms. The adhesion between the polyester and the sealant is measured after lamination under ASTM D1876; values below 150 g/25 mm indicate inadequate solventless polyurethane cure or surface oxidation on the corona-treated LLDPE web.

    The process boundary arises from the lower hot-tack strength of butene-1 LLDPE relative to EVA, especially when the seal area is contaminated with powder fines. On machines that run fine powder fillers such as spices or instant coffee, a powder contamination level of 0.5 g/m² on the seal area can reduce hot-tack strength by 30% to 50%; therefore, vacuum extraction and sealing-jaw air knives are required. The finished laminate is tested for seal integrity under ASTM F88/F88M-21 and for bond strength under ASTM D1876. If the laminate is used for food contact, the complete structure must comply with FDA 21 CFR 177.1520(c) for the polyolefin layer and with the relevant sections of 21 CFR 177.1630 for the polyester layer, as well as EU 10/2011 for the finished laminate. Published data for PF-0218-J in this exact laminate configuration is limited, so incoming inspection should verify the seal initiation curve on each batch rather than relying only on nominal melt index.

    Does PF-0218-J Meet the Elongation Demands of Pallet-Hood Machinery?

    Stretch-hood machines used in pallet packaging draw a tubular polyethylene film over a loaded pallet at a stretch ratio that varies from 10% to 25% for low-draw hooders to 80% to 120% for high-draw systems. The butene-1 LLDPE grade is generally limited to low-draw systems and to core-layer usage in coextruded stretch-hood film because its strain-hardening response is lower than that of octene-1 LLDPE or very-low-density polyolefin plastomers. In a three-layer blown film structure consisting of two outer layers of 18 wt% butene-1 LLDPE and a core of 64 wt% octene-1 LLDPE, PF-0218-J improves bubble stability and reduces raw material cost while the octene-1 core supplies the required drawability. On a high-draw hooder stretching beyond 50%, monolayer film from PF-0218-J typically develops pinholes at the pallet corners; the failure is confirmed by a puncture resistance test under ASTM D5748 and by visual inspection after a simulated transport vibration test under ASTM D4728. For this reason, converters limit the use of the grade to hood films with a maximum elongation of 20% to 30% unless it is buried in a coextrusion where the outer layers constitute less than 30% of the total thickness. The coefficient of friction and blocking behavior follow the slip/antiblock package; for pallet hooding, a film-to-film coefficient of friction below 0.20 under ISO 8295 is needed to allow the hood to slide over the pallet without tearing at the gusset folds.

    When the grade is used in cast stretch film as a core layer, the film line speed can reach 600 m/min on three-layer cast lines, but the melt temperature must be held at 240 °C to 260 °C for cast processing; at these temperatures, degradation of slip additives can occur if residence time exceeds 20 min. The process is therefore limited to continuous operations with rapid purge cycles and no accumulation of melt in dead spots behind the die feedblock. Published data for PF-0218-J in cast stretch-hood geometries is limited; process validation must include measurement of tensile elongation under ISO 527-3 at 200 mm/min and a strip-retention test after 72 h on a loaded pallet.

    Free Quote

    Competitive NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Novapol® PF-0218-J is a butene comonomer linear low-density polyethylene film resin supplied by NOVA Chemicals. The grade is specified with a nominal density of 0.918 g/cm³ and a nominal melt index of 2.0 g/10 min when measured under ASTM D1238-20 at 190°C with a 2.16 kg piston load. The resin is designed for cast film and air-cooled blown film extrusion where the primary processing requirements include stable draw-down, moderate abuse resistance, predictable seal behavior, and cost-effective film conversion. It is not positioned as a direct metallocene clarity grade, nor as a high-pressure LDPE replacement for applications requiring high melt elasticity.

    Molecular architecture in PF-0218-J is based on ethylene copolymerized with butene, producing ethyl short-chain branches along the polyethylene backbone. The comonomer distribution is broader than that typically observed in metallocene-catalyzed ethylene-hexene or ethylene-octene copolymers. This broader short-chain branching distribution contributes to a wider molecular weight distribution, lower melt elasticity, and reduced tendency for draw resonance in cast film. At equal density and melt index, the butene-based resin generally exhibits lower dart impact resistance and lower tear propagation resistance than a hexene or octene LLDPE. The -J suffix in the grade designation identifies the additive package and should be verified against the current technical data sheet before production use, particularly when surface treatment, ink adhesion, or solvent-based lamination is specified.

    Rheological and Thermal Characterization Data

    The melt flow rate of 2.0 g/10 min places PF-0218-J in the medium-flow film extrusion range. Density is determined by ASTM D792-20 or ASTM D1505-18, with the nominal value of 0.918 g/cm³ corresponding to a crystalline fraction of approximately 45–50% for a butene LLDPE of this class. Peak melting temperature for this density range, measured by differential scanning calorimetry under ASTM D3418, generally falls between 120°C and 124°C. These values are class-typical; actual lot values should be obtained from the certificate of analysis. Published data for the additive package of this specific -J configuration is limited, so offline testing is required when surface properties are critical.

    PropertyNominal ValueTest Standard
    Melt index2.0 g/10 minASTM D1238-20
    Density0.918 g/cm³ASTM D792-20
    Comonomer typeButeneNOVA Chemicals grade designation
    Peak melting point, class typical120–124°CASTM D3418

    What Limits Butene Comonomer Performance in High-Draw Film?

    In monolayer cast film below 25 µm, the ethyl short branches introduced by butene are less efficient at generating tie-chain entanglement than the longer branches from hexene or octene. Consequently, PF-0218-J will generally produce lower values in ASTM D1709-16a dart drop impact and lower Elmendorf tear resistance under ASTM D1922-15 than a C6 or C8 LLDPE of equivalent density and melt index. The difference becomes more pronounced at high draw ratios above 2.5:1 and when the cast roll temperature is reduced below 20°C. Seal initiation temperature and hot tack should be benchmarked against the incumbent resin using ASTM F88/F88M-21 and ASTM F1921, respectively, because published data for this specific PF-0218-J configuration is limited. For applications requiring high puncture resistance or low-temperature abuse tolerance, a higher alpha-olefin LLDPE or a bimodal resin may be required.

    On cast film lines, PF-0218-J is processed on extruders with L/D ratios of 24:1 or greater. Typical barrel zone settings for this resin class are 180–240°C, with melt temperatures of 240–260°C for general-purpose cast film. The polymer is extruded through a flat die with lip gaps commonly set between 0.5 mm and 1.0 mm, and the cast roll temperature is typically maintained at 15–30°C. These conditions are line-specific; no single profile applies to all cast film installations. Corona treatment to 38–42 dyn/cm surface energy is standard for printing and lamination, but treatment decay rate depends on the additive package and should be verified on the treated roll.

    When PF-0218-J Replaces a Hexene Copolymer in Blown Film

    When a blown film line replaces a hexene-based LLDPE with PF-0218-J, frost line height and air ring settings require re-optimization because the butene resin has lower melt elasticity. Bubble instability may occur at blow-up ratios above 3.0:1 and at film thicknesses below 20 µm. Operators commonly compensate by reducing air ring velocity or raising frost line height to 8–12 die diameters. Die gaps between 1.5 mm and 2.5 mm are typical, but the exact gap should be adjusted to maintain gauge control and melt pressure. A full-scale trial is required to map structure-property differences, because the published data for this specific grade configuration is limited.

    Blending with high-pressure LDPE is a standard method to recover bubble stability and increase machine-direction tear resistance on air-cooled blown film lines. LDPE addition levels of 10–20 wt% are used in butene LLDPE film structures. The long-chain branching in LDPE increases melt strength and reduces neck-in, but haze may increase if the blend is not homogeneously mixed. A barrier screw with a Maddock mixer section or a static mixer at the die adapter is recommended for blend consistency. The addition of LDPE also modifies the seal initiation temperature and should be evaluated under the intended packaging line conditions.

    PF-0218-J is used in coextruded structures for stretch wrap, overwrap, and surface-protection film where the core layer provides cling and the skin layers control slip and optics. In five-layer and seven-layer lines, the resin may be placed in the core or sub-skin layer. The lower density enables elongation on stretch-wrapping equipment without excessive unwind tension. However, for pre-stretch ratios above 250%, a metallocene or higher alpha-olefin LLDPE may be required to avoid film puncture and load loss during pallet wrapping.

    Regulatory Compliance Matrix and Food-Contact Status

    The food-contact status of PF-0218-J falls under 21 CFR 177.1520, which covers olefin polymers subject to extractives limitations and specific conditions of use. European Union food-contact compliance requires verification against the additive package and migration limits of Regulation (EU) No 10/2011. The following matrix provides the principal test standards applicable to film converted from this resin.

    Regulatory or Test DomainStandardTypical Applicability
    Food contact, United States21 CFR 177.1520Olefin polymers meeting extractives limits
    Melt mass-flow rateISO 1133-1190°C/2.16 kg procedure
    DensityISO 1183-1Immersion method
    Dart impactASTM D1709Method A or B depending on film thickness
    Elmendorf tearASTM D1922Machine and transverse direction
    Film hazeASTM D1003Illuminant C, 2° observer
    Kinetic and static frictionASTM D1894Film-to-film or film-to-metal surfaces

    Moisture uptake is negligible for polyethylene stored under normal indoor conditions. If pellets are exposed to high humidity or temperature cycling, surface condensation can generate film defects. Pre-drying at 60–70°C for 2–4 h is applied only when visible surface moisture is present. Sustained operation at melt temperatures above 280°C is not recommended because oxidative degradation can produce gel defects, off-odor, and color shifts. Contact with copper alloys in processing equipment should be avoided to reduce accelerated thermo-oxidative degradation at elevated temperatures.

    The operational boundary for PF-0218-J is moderate-abuse, thin-gauge packaging. The resin is not recommended for heavy-duty shipping sacks or industrial liners requiring high dart impact resistance and tear propagation resistance at sub-zero temperatures. In those applications, a 1-octene LLDPE or a bimodal HDPE/LLDPE blend with a density of 0.926–0.940 g/cm³ is preferred. The selection of PF-0218-J over a hexene or octene grade is therefore driven by cost per unit film and processability on older blown and cast film lines, rather than by maximum mechanical toughness or optical clarity.

    Top