Nova Chemicals Novapol Pf 0218 D Butene Lldpe Film Resin

NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 450670
    Productname NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin
    Manufacturer NOVA Chemicals
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Meltindex 2.0 g/10 min (190°C/2.16 kg)
    Meltflowratio 28
    Meltingpoint 121 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 24.1 MPa
    Elongationatbreak 700%
    Onepercentsecantmodulus 207 MPa
    Dartdropimpact 120 g
    Elmendorftearmd 250 g
    Elmendorfteartd 350 g
    Haze 12%
    Gloss45 55%
    Coefficientoffriction 0.15
    Blocking 50 g

    As an accredited NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin is supplied in 25 kg polyethylene bags, palletized for transport.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin, shrink-wrapped and secured.
    Shipping Novapol PF-0218-D Butene LLDPE Film Resin ships as non-hazardous solid pellets in sealed 25 kg bags or bulk trucks/railcars. Palletized loads are stretch-wrapped and secured. Transport in clean, dry equipment away from heat, moisture, and contaminants. Avoid punctures and direct sunlight. No special transport placards required.
    Storage Store in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed to prevent moisture, dust, and contamination. Place on pallets, avoid excessive stacking, and protect from weather. Use first-in, first-out inventory and consult the SDS for complete guidance. Do not store near food or drinking water.
    Shelf Life Stable under normal storage conditions; no specific shelf life. Store cool, dry, away from heat, sunlight, and contaminants.
    Application of NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin

    Film converted for use as a sealant web on a high-speed flexographic lamination line is routinely produced from Novapol PF-0218-D at 25–40 µm thickness. The resin’s nominal melt index of 2.0 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022) and density of 0.918 g/cm³ (ASTM D1505) place it in a viscosity range that permits drawdown without excessive neck-in on blown-film towers. Seal initiation is measured according to ASTM F88/F88M-21 at a jaw pressure of 0.4 MPa, dwell 1.0 s, and an upper-jaw temperature ramp of 10 °C/min; butene short-chain branching generally lowers initiation by 6–10 °C relative to a metallocene octene grade of similar density, although published data for this specific configuration is limited. On a solventless lamination line running at 250–350 m/min, the sealant web must maintain a hot-tack strength above 1.0 N/15 mm at 115 °C (ASTM F1921-12(2018)) to resist pouch-mouth opening during product drop. The treatment level on the sealant surface is normally held between 34 dyn/cm and 38 dyn/cm; treatment above 45 dyn/cm has been associated with oxidative species that interfere with seal initiation and contribute to off-odour in sensitive dry-food packaging. Migration compliance must be verified on the final laminate structure, not on the bare resin pellet, because lamination adhesives and printing inks alter the overall migration profile.

    Compliance referenceTest parameterLimiting condition
    U.S. FDA 21 CFR 177.1520(c) item 3.2aOlefin polymer food-contact layerEnd-use temperature and food-type restrictions apply
    EU Regulation 10/2011 Annex I, Annex IIOverall migration10 mg/dm²; specific migration limits apply to additives
    EU Regulation 10/2011 Annex VMigration testing simulantsAqueous, acidic, and fatty simulants selected by food category
    U.S. FDA 21 CFR 176.170(c)Polymer-coated paper/boardExtractives measured against coating weight and temperature

    What controls melt fracture onset in monolayer blown film lines above 120 kg/h throughput?

    Production-scale data from 90 mm barrier-screw extruders with 30:1 L/D indicate that melt temperature at the adapter should be held between 210 °C and 225 °C when Novapol PF-0218-D is run neat. Barrel setpoints from feed to metering zone are typically 170 °C, 190 °C, 205 °C, and 215 °C, with a screen pack of 20/40/60/80 mesh; die setpoints are held at 215–225 °C. Exceeding 235 °C for more than 4 min residence time initiates oxidative gel formation in the butene backbone, visible as fisheyes in 25 µm film and a subsequent dart impact loss. Running below 195 °C elevates melt pressure above 320 bar on a 250 mm die and forces the polymer into high-shear regimes at the die lip that exceed 1500 s⁻¹, producing sharkskin. Die gap is set at 1.8–2.3 mm; reducing below 1.5 mm without raising die temperature has caused melt fracture onset on monolayer lines. Frost line height is held at 8–10 die diameters for balanced MD/TD orientation; a frost line below 6 diameters quenches rapidly and lowers dart impact by 10–15%, whereas above 12 diameters produces a wandering bubble and gauge scatter exceeding ±8% on automatic scanning frames. For bubble internal cooling, chilled air at 5–15 °C and bubble diameter control within ±2% reduce tramline gauge variation and prevent the cyclic collapse observed when the frost line oscillates more than 3 cm.

    In heavy-duty liner fabrication from 50–75 µm film, the property emphasis shifts to dart impact and tear propagation. On a 70 mm extruder fitted with a 2.0 mm spiral die and run at 2.2:1 BUR, MD Elmendorf tear measured per ASTM D1922 declines when the frost line is lowered below 8 die diameters because the faster quench freezes orientation before relaxation. Dart impact under ASTM D1709 Method B rises as gauge increases from 50 µm to 75 µm, but the improvement is nonlinear; above 80 µm, the melt index of 2.0 g/10 min begins to limit drawdown on single-lip air rings, producing lower bubble stability and increased edge wrinkles at the collapsing frame. Winding tension is typically reduced to 8–12 N/100 mm web width to prevent blocking on the roll. PF-0218-D is supplied without release additives; slip and antiblock masterbatches must be compounded into the resin before or during extrusion. Final coefficient of friction measured per ISO 8295:1995 should remain below 0.30 for converter-fed bag machines. Published data for this specific configuration is limited, and the operational limits described are ordinary range values for butene LLDPE of this density class.

    When 8–12 wt% LDPE is added to lower seal initiation for frozen vegetable pouches

    Blending Novapol PF-0218-D with a fractional-melt, high-clarity LDPE at 8–12 wt% lowers the seal initiation temperature by 5–9 °C on a vertical form-fill-seal line running 80 pouches/min. The shift is measured as the temperature at which seal strength reaches 1.0 N/15 mm under 0.4 MPa jaw pressure and 100 ms dwell according to ASTM F88/F88M-21; above 12 wt% LDPE, hot-tack force at 110 °C declines and the pouch loses mouth-opening resistance when frozen peas drop from a fill height of 40 cm. At 10 wt% LDPE the blend remains processable on the same 65 mm blown film line with melt temperature reduced by 5–8 °C, but dart impact under ASTM D1709 Method A typically drops by 10–15% relative to the neat resin. Gas chromatography migration screening under EU Regulation 10/2011 must be repeated on the final blend because the addition of a second polyolefin changes the overall migration surface-to-volume ratio in contact with aqueous and fatty simulants. Storage of the pellets at ambient conditions below 50% relative humidity requires no pre-drying; when pellets are transferred from a cold silo at 5 °C into a warehouse above 70% relative humidity, surface condensation must be avoided before blending.

    Garment bag film converted from PF-0218-D on a cast line with 1200 mm slot die and 0.8 mm die lip opening is typically drawn at 150–250 m/min. The butene comonomer distribution produces higher neck-in than octene-copolymer grades, and edge bead formation is controlled by reducing the die-to-nip distance to 15–20 mm. Quench-roll surface temperature is maintained at 18–24 °C; at settings above 28 °C, roll blocking and transfer of low-molecular-weight species to the chrome surface reduce clarity and produce surface defects on rewind. Haze measured per ASTM D1003 on 30 µm cast web is sensitive to melt draw ratio and to the finish of the polished roll; use of a matte roll above 0.1 µm Ra surface roughness can raise haze by 2–4% absolute relative to mirror chrome. The resin’s melt index of 2.0 g/10 min reduces motor load at 200 m/min, but melt curtain sag becomes visible when the melt temperature is raised above 240 °C; therefore die temperatures are kept between 220 °C and 230 °C. Nip roll pressure is held below 6 N/mm to avoid gauge variation below ±3% as measured on a beta gauge scanner.

    Agricultural mulch film field exposure must be stabilised beyond the standard antioxidant package

    When PF-0218-D is drawn to 25 µm on a monolayer line for short-season mulch applications, the base resin contributes processability but no inherent UV resistance. A UV masterbatch with HALS chemistry is added at 5–10 wt% to deliver a final HALS level of 0.3–0.6 wt% in the film; for black mulch, carbon black concentrate is added at 3–6 wt% to achieve 1.5–2.5 wt% carbon black dispersion. Retained elongation under ASTM G154 cycle 1 at 500 h remains above 50% only when the UV package is dispersed through a twin-screw masterbatch dilution at 190–200 °C; excessive melt temperatures above 230 °C during letdown cause HALS volatilization and reduce field life. Blown film die gap of 1.8–2.0 mm and BUR of 2.5:1 are used to balance transverse tear against machine-direction splitting during mechanical laying. After film installation, wind-driven flapping exposes the butene copolymer to stress crack at fold creases; this failure mode is not mitigated by the base resin and must be addressed through gauge design above 20 µm.

    Evaluating heat-seal strength scatter in vertical form-fill-seal pouch operations

    On vertical form-fill-seal machines producing 500 g detergent pouches at 90 packs/min, seal strength variability is measured across 30 sequential pouches per ASTM F88/F88M-21; a standard deviation above 0.4 N/15 mm triggers rejection. PF-0218-D sealed at 120 °C with 60 ms dwell and 0.5 MPa jaw pressure typically reaches 7–9 N/15 mm on 40 µm film, but contamination from product dust at the seal area reduces this to below 3 N/15 mm. Hot-tack force under ASTM F1921-12(2018) at 105 °C, 50 ms dwell, and 0.3 MPa pressure remains above 1.0 N/15 mm only when seal bar temperature uniformity is within ±3 °C across the 400 mm bar; temperature deviation above ±5 °C produces weak channels along the seal edge. The film is not treated above 38 dyn/cm and not below 34 dyn/cm for solvent-free lamination; high treatment dosage above 45 dyn/cm can create low-molecular-weight oxidation species that interfere with seal initiation.

    Free Quote

    Competitive NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVAPOL® PF-0218-D is a butene comonomer linear low density polyethylene film resin produced by NOVA Chemicals. The grade is specified at a nominal melt index of 2.0 g/10 min when measured at 190 °C under 2.16 kg load according to ASTM D1238 or ISO 1133-1, and a nominal density of 0.918 g/cm³ by ASTM D1505 or ISO 1183-1. The butene comonomer introduces short-chain branching that lowers crystallinity relative to high-density polyethylene and positions the resin in thin-gauge film conversion, particularly cast film, lamination layers, and light-gauge blown film structures.

    PF-0218-D is supplied as a formulated pellet; the grade-specific additive package is identified in the current manufacturer technical bulletin and safety data sheet. The product belongs to the LLDPE film segment in which density and melt index are balanced for controlled drawdown, gauge uniformity, and heat-seal response. Compared with higher α-olefin LLDPE resins based on hexene or octene, a butene-based film resin of equivalent nominal density generally exhibits a narrower melting range and lower dart impact and Elmendorf tear resistance at comparable gauge, but often provides a more accessible balance among stiffness, optical clarity, and line throughput. The resin should not be treated as a direct substitute for all butene LLDPE film grades, because molecular weight distribution, catalyst residuals, additive loading, and melt index differences modify gel count, drawdown behaviour, and seal initiation. Specific film properties for PF-0218-D, including dart impact, Elmendorf tear, haze, and gloss, should be obtained from the current NOVA Chemicals technical data sheet; third-party comparative data for this exact designation remain limited.

    Representative resin parameters and test designations for NOVAPOL® PF-0218-D
    Parameter Nominal value Test method
    Melt index 2.0 g/10 min ASTM D1238 / ISO 1133-1
    Density 0.918 g/cm³ ASTM D1505 / ISO 1183-1
    Comonomer type Butene Internal FTIR
    Pellet form Formulated film grade Internal QC specification

    How Does Butene Short-Chain Branching Affect Optical and Mechanical Uniformity?

    Butene incorporation shortens the average ethylene sequence length and widens the melting endotherm relative to HDPE. At a nominal density of 0.918 g/cm³, PF-0218-D exhibits lower stiffness than HDPE but higher puncture resistance than LDPE of comparable melt index. The short-chain branch architecture also alters strain hardening and orientation-induced crystallinity during high-speed film drawing. In cast film production, thickness uniformity across the die must be maintained because uneven orientation creates tear anisotropy when tested by ASTM D1922 or ISO 6383-2.

    Optical haze is measured by ASTM D1003, and gloss is measured by ASTM D2457. These values are not intrinsic resin constants; they depend on melt temperature, die gap, cooling roll temperature, and film gauge. PF-0218-D is intended for applications where optical clarity and consistent surface quality are required, but optimum haze and gloss values are line-specific and must be established on the target extruder rather than inferred from a generic butene LLDPE datasheet. The lower tie-chain population characteristic of butene LLDPE, compared with hexene LLDPE, limits dart impact resistance under high-speed puncture events. Because dart impact values vary with gauge, frostline height, and orientation balance, converters should generate process-specific data using ASTM D1709 or ISO 7765-1.

    Extrusion Parameter Envelope and Screen-Pack Configuration

    On cast film lines using a single-screw extruder with a 30:1 to 40:1 L/D ratio and a barrier screw, PF-0218-D is typically processed in a melt temperature window of 220 °C to 280 °C. Elevated melt temperatures above 290 °C can increase oxidative degradation and gel formation, while melt temperatures below 200 °C may raise viscosity sufficiently to overload the drive and produce melt fracture. A graduated barrel profile can be set with feed temperatures between 40 °C and 80 °C, compression-zone temperatures between 180 °C and 230 °C, and metering and die temperatures between 240 °C and 270 °C. Actual settings are influenced by screw diameter, throughput, and die width.

    A screen pack of 20/40/60 mesh is commonly applied to LLDPE cast film extrusion. Finer screens below 100 mesh may generate excessive pressure drop and reduce output without proportional gel reduction. The 2.0 g/10 min melt index facilitates drawdown to gauges between 10 µm and 25 µm in cast film; below 10 µm, edge bead instability and draw resonance can occur unless the line is equipped with precision die-bolt profiling, air-knife control, and roll-stack alignment. Die gaps of 0.5–0.8 mm are common for cast film, with thicker gaps selected where higher throughput is prioritised and thinner gaps used for gauge uniformity at low draw ratios.

    Because butene LLDPE is more shear-sensitive than LDPE at equivalent melt index, extruder pressure and motor drive load should be monitored during sustained high-output campaigns. If sharkskin or surface melt fracture appears, a polymer processing aid or adjusted die temperature may be required. Operators should avoid prolonged residence time at temperature, because crosslinked gels can accumulate at die lips and transfer to film surfaces. Purge procedures should include a transition material of similar density and melt index before shutdown.

    Surface-bound slip behaviour in PF-0218-D is evaluated by kinetic coefficient of friction using ASTM D1894. Target COF values depend on packaging machine requirements and should not be assumed stable at elevated storage temperatures above 40 °C, where migratory additives can bloom and alter surface friction. Blocking resistance is measured by film-to-film peel tests under load, but the most reliable indication is unwinding force on the actual slitting or converting line. The formulated antiblock package is intended to reduce blocking in roll form; excessive letdown or interaction with solvent-based inks can reduce seal strength and should be evaluated before committing to high-speed lamination or print applications.

    When PF-0218-D Replaces LDPE in Coextruded Lamination Layers

    Substitution of PF-0218-D for an autoclave LDPE at equal melt index generally increases extruder motor torque and die pressure because linear chains have higher shear viscosity than branched LDPE of the same melt index. Depending on the screw design and throughput, die pressure may increase by 15–30 %, and the drive load should be reviewed before the change is made permanent. In coextruded lamination structures, PF-0218-D can be used as a strength-bearing layer or seal layer, while LDPE or EVA provides heat-seal tack and low-temperature adhesion. The butene LLDPE layer increases toughness relative to LDPE, but the final structure should be tested for interlayer adhesion and seal strength rather than assuming direct equivalence.

    Compared with a hexene LLDPE film resin of comparable density and melt index, PF-0218-D typically produces lower Elmendorf tear and dart impact resistance but may offer advantages in optical clarity and raw-material cost control. Compared with a high-density polyethylene film layer, the 0.918 g/cm³ density provides lower stiffness and higher puncture resistance, making the grade suitable for lamination films where conformability and sealability are required. The actual balance depends on the coextruded structure, gauge distribution, and orientation.

    Published data for PF-0218-D in multi-layer cast film at specific gauges below 20 µm is limited; converter trials are necessary to establish the interlayer adhesion, COF, and seal-initiation temperature under the target machine conditions. Heat-seal strength is commonly measured according to ASTM F88, and seal initiation temperature is evaluated by ASTM F2029. Typical processing windows for butene LLDPE seal layers may range from 105 °C to 150 °C, but dwell time, pressure, and contamination affect the actual seal strength. The seal-initiation temperature of PF-0218-D should be determined on the specific packaging line rather than inferred from a single-point value.

    Interpreting Food-Contact Status Under 21 CFR 177.1520

    Food-contact acceptability for PF-0218-D must be confirmed against 21 CFR 177.1520(c), noting that the applicable subparagraph depends on density, olefin type, and extraction testing. Compliance is formulation-specific and should be documented by the resin manufacturer or the legal supplier for each end-use condition. For European Union food-contact applications, migration testing under EU 10/2011 must verify that overall migration does not exceed 10 mg/dm² for the intended food simulant and contact time. The converter is responsible for assessing the final article because printing inks, lamination adhesives, and recycled layers may alter overall migration behaviour.

    Compliance verification matrix for PF-0218-D
    Regulatory framework Relevant provision Verification obligation
    U.S. FDA 21 CFR 177.1520(c) Confirm subparagraph based on density and end use
    EU food contact EU 10/2011 Overall migration 10 mg/dm²
    REACH Title II registration Entity-specific registration review

    PF-0218-D is not hygroscopic, and pre-drying is not normally required unless condensation is present on pellet surfaces. If surface moisture is observed, a drying step at 60 °C to 80 °C for 2–4 h may be applied, but prolonged drying is unnecessary and may accelerate additive migration. The resin should be stored indoors, away from direct sunlight and strong oxidising agents, with warehouse temperatures maintained below 30 °C to preserve additive distribution. In compounding or melt blending, combination with acid-functional polyolefins or high levels of metal stearates should be evaluated for potential additive interaction. Operational boundaries for PF-0218-D therefore include controlled melt temperature, validated food-contact documentation, and process-specific mechanical testing rather than reliance on nominal resin parameters alone.

    Top