Nova Chemicals Novapol Pf 0118 D Butene Lldpe Film Resin

NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 688315
    Product Name NOVA Chemicals Novapol PF-0118-D Butene LLDPE Film Resin
    Resin Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min (190 °C/2.16 kg)
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Brittleness Temperature < -70 °C
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1400 psi
    Tensile Strength At Break Md 5000 psi
    Tensile Strength At Break Td 4500 psi
    Elongation At Break Md 700%
    Elongation At Break Td 800%
    Elmendorf Tear Strength Md 250 g/mil
    Elmendorf Tear Strength Td 400 g/mil
    Dart Drop Impact 120 g
    Haze 12%
    Gloss 60%
    Coefficient Of Friction 0.2
    1 Secant Modulus Md 25000 psi
    1 Secant Modulus Td 30000 psi
    Heat Seal Initiation Temperature 110 °C
    Blocking Force 50 g

    As an accredited NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin is supplied in 25 kg polyethylene bags, 40 per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL loads approx. 18–20 MT NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin in 25 kg bags on pallets.
    Shipping NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin is non-hazardous and not regulated for transport. It is shipped in moisture-barrier bags, lined cartons, or bulk containers. Store in a cool, dry, ventilated area away from ignition sources. Handle pellets carefully to minimize dust and slipping.
    Storage Store in original unopened packaging in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, sparks, flames, and strong oxidizers. Maintain dry conditions; protect from moisture, dust, and contamination. Stack pallets safely off the floor to prevent bag damage. Use first-in, first-out rotation, observe shelf life, and follow the SDS and local regulations.
    Shelf Life Typically 24 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin
    In monolayer blown-film extrusion of consumer refuse sacks, drawstring liners, and construction debris bags, PF-0118-D is run on air-cooled lines with screw diameters from 55 mm to 90 mm and a 30:1 L/D barrier screw. The nominal melt index of 1.0 g/10 min at 190 °C/2.16 kg (ASTM D1238) and density of 0.918 g/cm³ (ASTM D1505) keep melt pressure within a controlled range on 1.8 mm to 2.5 mm die gaps, but the butene branch distribution does not generate the melt tension required for very high blow-up ratios. Bubble stability is maintained when the blow-up ratio is kept between 2.0:1 and 3.0:1 and the frost line is positioned 450 mm to 850 mm from the die face. On lines without internal bubble cooling, output rates are limited by bubble fluttering rather than screw recovery; thickness variation measured by capacitance gauge can exceed ±8% when the frost line is raised above 900 mm in 28 °C ambient air. Dart impact resistance measured under ASTM D1709-22 Method A on a 50 µm film commonly falls between 90 g and 140 g for general-purpose butene LLDPE, although published data for this specific formulation is limited and converter trials remain the primary dataset. Elmendorf tear values tested to ASTM D1922 generally show lower machine-direction tear than transverse-direction tear, a directional imbalance that affects sack-opening force and tear resistance in waste liners. The practical upper thickness limit for stable monolayer bubble production is approximately 200 µm; above this value, molten web sagging and gauge variation become difficult to manage without blending with HDPE or LDPE.

    What Processing Boundaries Emerge Below 25 µm in Stretch Hood and Collation Shrink Film?

    Down-gauging to 18–24 µm changes the failure mode from tensile yield to puncture and tear propagation. On cast-film lines fitted with a 0.6 mm die gap and 50 mm air gap, neck-in increases as film thickness decreases; edge-trim losses of 8–15 wt% are recorded on single-layer cast lines when butene LLDPE is processed at a density of 0.918 g/cm³. Dart impact values determined by ASTM D1709-22 decline non-linearly with thickness reduction. A monolayer film tested at 35 µm can show a dart impact value 1.8–2.5 times higher than the same formulation at 20 µm, so down-gauging decisions must be validated against pallet containment requirements rather than tensile yield data alone. For stretch hood applications, the film is pre-stretched to 50–70% elongation on rotary applicators with variable prestretch arms; residual tension in the film after relaxation must remain above 12–20 N/50 mm to prevent billowing under wind load. Coefficient of friction measured under ASTM D1894 is an operational boundary: dynamic COF below 0.10 on the exterior can cause roll telescoping, while dynamic COF above 0.20 can block on unwind during pre-stretch. The specific slip package in a given PF-0118-D lot must be confirmed from the certificate of analysis because additive migration kinetics in the polymer matrix change with storage temperature and time. No predrying is normally required at relative humidity below 60%; however, resin transferred from unheated silos into a warm casting room can carry surface condensation that introduces melt pressure fluctuations and streak defects.

    Cast film lamination webs for non-retortable pouch laminates use PF-0118-D as a sealant backing or core layer where hot tack is not the controlling requirement. On a cast film line with a die gap of 0.5 mm to 0.9 mm, an air gap of 25 mm to 75 mm, and a chill roll temperature between 15 °C and 30 °C, the resin is processed at melt temperatures from 200 °C to 240 °C. The melt index of 1.0 g/10 min keeps draw resonance on primary chill rolls manageable, while the butene branch distribution produces a broad molecular weight distribution that stabilizes the draw at line speeds up to 300 m/min. Haze values measured under ASTM D1003 are governed by chill roll replication and air gap distance; shorter air gaps increase optical contact but also raise neck-in. Seal initiation temperature measured by heat-seal testing according to ASTM F88/F88M typically falls between 95 °C and 110 °C for a 50 µm film, though laminate board stiffness and dwell time shift apparent seal initiation downward on production equipment. Laminating converters use PF-0118-D as a printed or adhesive-laminated backing film to oriented polyester or biaxially oriented polypropylene; the sealant layer remains compatible with solventless polyurethane adhesives after corona treatment. Because the final laminate is intended for dry food packaging, the film must be assessed under 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; overall migration must not exceed 10 mg/dm² when tested with food simulants assigned to the packaged food type. A compliance matrix for this downstream segment is given in Table 1 below.
    Standard / RegulationRequirement Relevant to FilmTest Method / Clause
    US FDA 21 CFR 177.1520(c)Olefin polymer for food contact; density and extractable limits must be met in the finished article21 CFR 177.1520(c)
    EU Regulation (EU) No 10/2011Overall migration limit 10 mg/dm²; specific migration limits for monomers and additivesEN 1186 series / EN 13130 series
    Packaging Directive 94/62/ECSum of lead, cadmium, mercury, chromium VI not to exceed 100 mg/kg in packagingAcid digestion with ICP-OES
    REACH Regulation (EC) No 1907/2006Article SVHC concentration below 0.1 wt%Candidate List screening

    Seal Initiation Temperature, Hot Tack, and Seal Strength in High-Speed Form-Fill-Seal Operations

    On vertical form-fill-seal lines running at 80–120 packages per minute, PF-0118-D is used for powder and granulate pouches where a low seal initiation temperature reduces dwell time and jaw temperature. Seal initiation values between 95 °C and 110 °C are typical for butene LLDPE of 0.918 g/cm³ density when tested according to ASTM F88/F88M at a dwell time of 0.5 s and a pressure of 0.275 MPa. Hot tack measured under ASTM F1921 remains positive at a sealing window from 105 °C to 140 °C; outside the upper limit, the seal becomes brittle and the film ruptures at the seal perimeter. The sealant layer is often coextruded with an outer layer of LDPE or HDPE to prevent blocking on the forming tube; PF-0118-D forms the inner sealing layer because its controlled melt range produces fewer flow disturbances at high seal pressure. On horizontal form-fill-seal machines with rotary seal jaws, dwell times of 0.15 s to 0.35 s require the seal bar temperature to be raised to 125 °C to 150 °C; hot tack failure and leaker rates increase when the seal bar temperature is below the point at which heat transfer through the film reaches seal initiation temperature. Because the film is used for dry powder packaging, the converter must verify that the slip additive does not migrate into the food contact surface at levels above the limits specified in 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011. Batch-to-batch variance in melt index of ±0.1 g/10 min can shift the seal initiation temperature by 3–5 °C on thin-gauge films, so incoming resin lots should be checked by melt flow rate and differential scanning calorimetry before high-speed qualification.

    When PF-0118-D is blended with HDPE at 15–30 wt% in flexible intermediate bulk container liners, extruder torque and die pressure rise by 5–12% relative to a neat butene LLDPE stream. The blend is processed on blown-film lines with a 2.2 mm die gap and a 2.5:1 blow-up ratio; the HDPE fraction increases stiffness and reduces racking under product load, but it also narrows the bubble cooling window. Frost line height must be lowered to 350–600 mm to prevent orientation release that creates transverse-direction tear weakness. The technical limitation is interlayer adhesion in coextruded structures; PF-0118-D does not develop strong interfacial bonding with polyamide or EVOH without a tie resin. In high-shear screw designs, the heat dissipation from HDPE blending can raise melt temperature beyond 240 °C, at which gel formation accelerates in butene LLDPE. The resulting gel density is measured by film scanner as hard gel counts per 1 m², and counts above 5 hard gels/m² are typically rejected for medical packaging. This application is not suitable for retort conditions above 121 °C; the film softens and loses seal integrity when exposed to superheated water beyond 100 °C for extended periods.

    Frozen Food Packaging Demands Ductile Tear Below −25 °C and Low Temperature Seal Integrity

    Frozen vegetable and seafood films processed from PF-0118-D are tested for dynamic puncture and tear at freezer temperatures rather than at standard laboratory ambient. The film density of 0.918 g/cm³ places it below the brittle transition of high-density polyethylene, so ductile behavior is retained down to approximately −30 °C in thin-gauge films, although published data for this specific formulation is limited. Puncture resistance measured by ASTM D5748 at −25 °C is commonly 15–25% lower than the value at 23 °C; converting trials must account for this reduction when designing freezer-to-microwave pouches. The seal layer must be thick enough, typically 20–40 µm, to preserve seal integrity when impacted by frozen vegetables; seal failures occur not because of brittle cracking but because of localized stress concentration at the seal edge. Blown film produced with a BUR of 2.5:1 to 3.0:1 shows more balanced machine-direction and transverse-direction impact distribution than cast film, making blown film the preferred process for irregular frozen products. Compliance for freezer-to-microwave packaging requires the converter to verify that the finished pouch meets the food-contact migration limits of 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 under frozen and microwave reheating conditions; separate migration testing must be conducted with the actual food simulants because the time-temperature profile changes the diffusion coefficient of low-molecular-weight fractions. Polypropylene contamination must be kept below 5 wt%; unmelted PP inclusions create stress concentrators that reduce low-temperature puncture performance and produce visible gel nodules.

    Free Quote

    Competitive NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVAPOL® PF-0118-D is a butene copolymer linear low-density polyethylene film resin supplied by NOVA Chemicals in pellet form for blown-film conversion. The grade is specified with a nominal density of 0.918 g/cm³ determined under ASTM D1505 or ISO 1183 and a nominal melt index of 1.0 g/10 min determined under ASTM D1238 at 190 °C with a 2.16 kg load; the ISO equivalent is ISO 1133-1. The butene comonomer introduces short-chain branching that disrupts crystallinity and reduces density relative to high-pressure LDPE, while retaining sufficient melt strength for stable bubble formation. The product is positioned for general-purpose film applications including garment bags, carrier bags, industrial liners, overwrap, and thin-gauge produce packaging. In these applications, extrusion stability, sealability, and cost per kilogram generally outweigh maximum puncture toughness.

    What limitations follow from the butene comonomer architecture in PF-0118-D?

    Butene introduces ethyl short-chain branches rather than the longer hexene or octene branches used in higher-performance LLDPE grades. The resulting short-chain branch distribution is less effective in generating tie molecules between crystalline lamellae during film solidification. This molecular architecture limits ultimate Elmendorf tear strength and dart impact relative to hexene and octene copolymers of equivalent density and melt index. In blown-film converting, the practical consequence appears as a narrower down-gauging window before impact failure and as lower machine-direction tear resistance when bubble cooling is aggressive. At 25 µm gauge, a butene LLDPE grade typically exhibits lower puncture resistance than a comparable octene grade with equivalent density and melt index. Published data for this specific configuration is limited, but comparative studies on butene versus octene copolymers at 0.918 g/cm³ indicate that differences are measurable under ASTM D1709 and ASTM D1922.

    The structural difference also affects optical properties. Butene LLDPE generally produces higher haze than octene LLDPE because the shorter branches generate a broader distribution of crystallite sizes and surface micro-roughness in drawn film. Converters selecting PF-0118-D for clear film should therefore validate haze against ASTM D1003 before replacing an octene grade. The resin remains acceptable for many opaque or lightly printed films where the optical threshold is less stringent.

    Film extrusion lines with grooved-feed single-screw machines of 24:1–30:1 L/D are suitable for PF-0118-D. Barrel temperature profiles should be set to reach a melt temperature of 190–230 °C at the die entrance; residence time above 240 °C should be minimized to avoid oxidative degradation and gel formation. The die gap is typically held between 1.2 mm and 2.0 mm, with blow-up ratios of 2.0:1–3.0:1 for thin-gauge films. Frost-line height is adjusted to maintain bubble stability, particularly when the formulation includes recycled LLDPE at addition levels above 15 wt%.

    Blown-film extruder configuration, screw design, and barrel temperature profiles

    Shear viscosity at processing temperatures follows the power-law behaviour expected for a 1.0 dg/min LLDPE. The pelletized compound does not require high-shear dispersion of a separate masterbatch for stabilization because the base stabilizer package is distributed during pelletization. The melt is processed through barrier screws with Maddock mixing sections to reduce melt-temperature heterogeneity. Die inlet pressure is normally maintained below 35 MPa to prevent bubble chatter, although actual pressure depends on output rate, die gap, melt temperature, and screen pack condition. Excessive pressure usually indicates screen blockage or a melt temperature that is too low for the selected screw speed.

    The recommended purge material is a low-melt-index LDPE or the same resin. Abrupt transitions from PF-0118-D to a lower-viscosity HDPE can lead to viscosity mismatch and flow instability at standard screw speeds; a transition purge of a fractional-melt LDPE is preferred before introducing HDPE. On extrusion lines equipped with internal bubble cooling, the cooling air volume should be increased gradually. Sudden increases in cooling air can over-stabilize the bubble and generate block marks or MD draw resonance.

    When PF-0118-D is coextruded with HDPE in high-stiffness sack applications

    In a three-layer coextruded film, PF-0118-D may occupy the core or seal layers while an HDPE skin contributes modulus and creep resistance. Interfacial compatibility of butene LLDPE and unimodal HDPE is generally sufficient for coextrusion without tie layers, but rheological differences require matched melt temperatures to prevent interfacial flow instabilities. The seal layer benefits from PF-0118-D’s broader hot-tack window relative to HDPE. Lower seal initiation allows faster jaw cycles on vertical form-fill-seal equipment. The relation between jaw pressure and seal strength should be validated under heat-seal conditions of 110–130 °C sealing temperature, 0.3–0.5 MPa jaw pressure, and 0.5–1.0 s dwell.

    When PF-0118-D is used as a core layer with HDPE skins, the film tends to exhibit higher stiffness than a monolayer butene LLDPE film of the same total gauge. However, the dart impact of the coextruded structure is still limited by the core layer. If the application requires heavy-duty abuse resistance, substituting an octene LLDPE core is preferred. The butene core may still be suitable for high-stiffness waste sacks where the primary mechanical requirement is tensile yield strength rather than impact or tear.

    Additionally, the resin is employed in thin-gauge produce bags and industrial liners where melt strength and bubble stability are required during continuous extrusion. On high-output lines exceeding 150 kg/h per die, the comparatively low melt index contributes to bubble stiffness, but output rate must be balanced against melt pressure and motor torque. When slip and antiblock behaviour is required, converters may combine PF-0118-D with a masterbatch containing erucamide and synthetic silica; the additive compatibility with butene LLDPE is established, but the addition level should not exceed 2 wt% to avoid plate-out on die lips and surface haze increase.

    Recognizing the difference between butene and octene short-chain branching

    Compared with a metallocene-catalysed octene LLDPE of the same 0.918 g/cm³ density and 1.0 dg/min melt index, PF-0118-D typically exhibits higher haze, lower dart impact, and lower Elmendorf tear in both machine and transverse directions. The measured differences are not processing artefacts but arise from comonomer length: octene branches are more efficient at creating tie chains, which increases fracture resistance and reduces haze through a more uniform crystallite distribution. In practice, PF-0118-D is selected when the performance requirement is dominated by tensile yield strength, seal integrity, or cost per kilogram. It is not selected for heavy-duty puncture-resistant packaging.

    A comparative data set generated under ASTM D1709, ASTM D1922, and ASTM D1003 should be obtained from the supplier before substituting octene grades. Differences in slip-agent migration kinetics should also be considered: erucamide migration in butene LLDPE can produce a time-dependent coefficient of friction that differs from octene LLDPE due to differences in amorphous-phase mobility. Surface coefficient of friction should be measured after storage at 23 °C and 50% RH for at least 24 h using ASTM D1894.

    Regulatory clearance under 21 CFR 177.1520 is not self-executing

    Food-contact use of PF-0118-D must be confirmed against the applicable regulatory framework for the intended food type, temperature, and contact duration. A resin listing in FDA 21 CFR 177.1520 does not alone establish compliance; the finished article must meet the end-use limitations and additive restrictions applicable to the specific olefin polymer. The following matrix summarizes the primary compliance references.

    JurisdictionStandard or referenceCompliance condition
    United StatesFDA 21 CFR 177.1520Olefin polymer clearance subject to density, additive, and intended food-contact conditions; finished article responsibility remains with converter.
    European UnionRegulation (EU) No 10/2011Overall migration limit of 10 mg/dm² for plastic food-contact materials, with specific migration limits for additives and monomers.
    CanadaHealth Canada Food Packaging MaterialsSupplier letter of assurance required for the specific food type and temperature; no generic resin clearance should be assumed.

    Operational boundaries include pre-drying only when surface moisture exceeds 0.05 wt%, although LLDPE is generally non-hygroscopic. Avoid blending with ionomer or acid-functional polymers because acid groups can catalyse oxidation of the polyethylene backbone. The resin should be stored below 50 °C and protected from ultraviolet exposure to preserve additive performance. At relative humidity above 60%, condensation on cold pellets can introduce water into the feed throat and reduce output stability or produce surface bubbles in the film.

    Top