Nova Chemicals Novapol Pf 0118 C Butene Lldpe Film Resin

NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin

    • Product Name: NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 111130
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Form Pellets
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min
    Melt Flow Ratio 27
    Melting Point 122 °C
    Vicat Softening Point 96 °C
    Tensile Strength At Yield 11.0 MPa
    Tensile Strength At Break 27.6 MPa
    Elongation At Break 700%
    Tensile Modulus 0.276 GPa
    Dart Drop Impact 120 g
    Elmendorf Tear Md 200 g
    Elmendorf Tear Td 350 g
    Haze 12%
    Gloss 45 Degree 60
    Clarity 75%
    Coefficient Of Friction 0.2
    Blocking 50 g

    As an accredited NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; typically 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL: Novapol® PF-0118-C butene LLDPE film resin, 25 kg bags, palletized and stretch-wrapped; approx. 18–20 metric tons per container.
    Shipping Novapol® PF-0118-C Butene LLDPE Film Resin ships as non-hazardous polymer pellets. Standard packaging: 25 kg polyethylene bags on pallets, stretch-wrapped, or bulk in lined trucks/railcars. Keep dry, clean, and protected from heat, moisture, UV, and contamination. Follow SDS and local regulations.
    Storage Store NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags sealed, pallets stable and off the floor to prevent moisture pickup and contamination. Protect from UV, dust, and incompatible materials. Use first-in, first-out rotation, and refer to the SDS.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original packaging in a cool, dry, well-ventilated area.
    Application of NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin

    How Does High-Draw Cast Stretch Wrap Process This Butene LLDPE?

    On high-draw cast pallet wrap lines, Novapol® PF-0118-C is processed in monolayer or coextruded cast film configurations with die deckle widths from 1.5 m to 3.5 m and final film gauges from 8 µm to 35 µm. Melt temperature at the feedblock and die lip is held between 220 °C and 265 °C; the melt curtain is edge-pinned by an air knife or vacuum box and quenched on a polished chill roll at 15 °C to 25 °C. Inadequate pinning produces neck-in and edge-bead thickness variation that transfers to telescoping defects during winding on 76 mm and 152 mm core shafts. Melt flow rate is verified under ISO 1133-1:2022 at 190 °C and 2.16 kg, and lot-specific flow data determine the screw speed and die pressure settings on lines with extruder L/D ratios from 24:1 to 36:1. At line speeds from 300 m/min to 650 m/min, draw resonance and gauge banding are controlled by positioning the die-to-chill-roll gap between 25 mm and 60 mm and by maintaining a vacuum box pressure sufficient to pin the web across the full width. A polyisobutylene tackifier masterbatch is metered inline at 0.5 wt% to 2.5 wt% to create cling; cling force is quantified with ASTM D5458, and tensile strength and elongation are measured under ASTM D882-18. Puncture resistance of the finished wrap is characterized by ASTM D5748-19; acceptance limits are set by pallet weight class and load geometry, and published film-level values for this specific resin are limited.

    Gauge uniformity at the winding drum is maintained by a scanning beta or X-ray gauge with die bolt adjustment intervals between 15 s and 30 s; because PF-0118-C has a lower shear viscosity than LDPE at equivalent melt index, automatic die bolt movement produces a measurable thickness response within three scan passes. Edge trim and start-up film are recycled at 10 wt% to 20 wt% through a grinder and re-extrusion path; higher regrind fractions increase gel defects and reduce cling at a given tackifier dose, so an inline screen changer with 100 mesh to 120 mesh breaker plates is specified to protect the die lip. On a three-layer cast stretch line, the surface layer on the unwind side carries the cohesive cling, the air side is compounded with a slip/antiblock package to reduce unwind noise, and the core layer may contain a higher proportion of recycled film without directly contacting the load face. Polyisobutylene tackifier is concentrated in the cling layer via a side-arm extruder, and cling force is checked at both 0% and 200% pre-stretch because cohesive failure shifts with elongation. End products are machine-roll stretch wrap, hand-roll stretch wrap, and high-slip overwrap used for pallet stabilization in warehouse transshipment.

    Heavy-duty sack films blown from PF-0118-C on high-output lines typically target finished thicknesses from 90 µm to 180 µm for form-fill-seal packaging of granular resins, fertilizers, pet food, and lightweight construction aggregates. Low-stalk bubble geometry is used because the resin's low melt tension under elongation, measured on a Rheotens device at 190 °C, makes high-stalk pockets prone to instability at die diameters above 250 mm; production equipment generally uses a 200 mm to 400 mm annular die with a die gap of 1.5 mm to 2.5 mm and a blow-up ratio from 1.8:1 to 2.5:1. Melt temperature at the die is controlled between 185 °C and 230 °C, and frost line height is set at 200 mm to 500 mm above the die lip to balance impact toughness against transverse direction tear retention. Extruders with 30:1 to 36:1 L/D and barrier screws with Maddock mixing sections are used; backpressure and barrel temperature profiles are adjusted so that melt temperature at the die does not overshoot the setpoint by more than 5 °C during high-output operation. Dart impact is measured by ASTM D1709/ASTM D1709M, Elmendorf tear by ASTM D1922-15, and seal strength by ASTM F88/F88M; seal initiation temperature is characterized by ASTM F1921, and production jaws are run 10 °C to 20 °C above the measured seal initiation value to maintain open-time robustness.

    Dart impact and Elmendorf tear are anisotropic in these films; machine direction tear often drops below the transverse direction value as frost line height and blow-up ratio are increased. For sacks filled with sharp-edged granules, the specification is normally written around low-temperature dart impact after conditioning at -10 °C or -18 °C, rather than room-temperature values, because polymer toughness falls as temperature approaches the beta relaxation region. Seal integrity is tested with flat jaw or crimp jaw configurations at pressures from 2 bar to 4 bar and dwells from 0.5 s to 1.5 s; the common line defect is not low average seal strength but intermittent seal channels caused by gauge bands in the gusset fold area. Therefore, the film is produced with a 180° reverse oscillating haul-off to randomize gauge variation, and the gusset board geometry is inspected after every reel change. Finished sack failures on filling lines are commonly traced to insufficient dart impact against sharp-edged granules or to seal creep at warehouse temperatures above 40 °C; both failure modes are controlled by maintaining film gauge within ±5% and by conditioning reels for 24 h before conversion. End-use forms include FIBC liners, pinch-bottom heavy-duty sacks, and gusseted industrial bags.

    When Butene LLDPE Is Coextruded into Frozen Food Packaging Laminates

    When a three-layer blown film line is configured for frozen food pouches, the PF-0118-C sealant skin usually occupies 20% to 40% of the total thickness at a finished structure gauge from 50 µm to 80 µm. The critical variable shifts from melt temperature to low-temperature impact toughness, because the finished pouch must survive distribution at -30 °C to -18 °C without brittle punctures. The coextruded film is produced with a die gap of 1.2 mm to 2.0 mm, a blow-up ratio from 2.0:1 to 3.0:1, and melt temperatures between 195 °C and 235 °C; frost line height is lowered relative to heavy-duty sack production to increase quench rate and reduce internal haze in the sealant layer. Cold-impact properties are evaluated by ASTM D1709/ASTM D1709M after 24 h conditioning at -18 °C, and tear propagation in the machine direction is tested by ASTM D1922 because the pack peel path often runs parallel to the film's primary orientation. Heat seal strength is measured under ASTM F88/F88M at a seal dwell of 0.5 s to 1.0 s and jaw temperature settings derived from the seal initiation curve measured by ASTM F1921.

    In frozen food lamination, the PF-0118-C sealant layer is often treated with a low-slip or medium-slip additive package so that pouch opening behavior on high-speed vertical form-fill-seal machines does not cause feed hesitation. The extruder profile is configured with a grooved feed section and a barrier screw that maintains melt temperature at the die below 240 °C, because prolonged exposure above this threshold can increase odour and taint compounds in the film; sensory testing is often part of the qualification. Layer distribution is checked by microscopy or differential scanning calorimetry on die-cut sections, because seal layer thickness below 15% of total gauge creates a risk of heat-seal failure under drop loading at -25 °C. Food contact compliance requires that the finished structure meet US FDA 21 CFR 177.1520 for olefin polymers and the overall migration limit of 10 mg/dm² under EU Regulation 10/2011; final declarations are generated from each converted article because migration depends on the surface area-to-volume ratio and the adhesives and inks in the laminate. Typical end products are IQF vegetable bags, frozen meat and poultry pouches, and overpack bags for chilled seafood export cartons.

    Application sectorReference standard or regulationTest condition / equipmentTypical control parameter
    Cast pallet stretch wrapASTM D5748-19, ASTM D882-18, ASTM D5458Chill-roll cast line, die-to-chill gap 25 mm–60 mm, line speed 300 m/min–650 m/minCling force and puncture force limits set by pallet class; gauge control ±3%
    Heavy-duty sack filmASTM D1709, ASTM F88/F88M, ASTM F1921Blown film line, die 200 mm–400 mm, BUR 1.8:1–2.5:1Dart impact and seal initiation; film gauge 90 µm–180 µm
    Frozen food laminate sealantASTM D1709, ASTM F88/F88M, EU 10/2011, FDA 21 CFR 177.1520Three-layer blown film, 195 °C–235 °C, conditioning -18 °CMigration 10 mg/dm², seal strength after 0.5 s–1.0 s
    Agricultural silage coverEN 13206, ISO 527-3, ISO 6383-2, ISO 7765-1Blown film, BUR 2.0:1–2.8:1, film 100 µm–200 µmHALS concentration 0.2 wt%–0.8 wt%, tear and puncture minimums
    Lamination sealant webASTM D2578, ASTM D1876, ASTM F88/F88MCorona treater, solventless laminator, nip 60 °C–80 °CWetting tension 38 mN/m–42 mN/m, T-peel bond after 24 h
    Collation shrink filmASTM D2732, ASTM D1922Blown film, BUR 2.0:1–2.5:1, shrink tunnel 120 °C–160 °CFree shrink in MD/TD, LLDPE blend ratio 30 wt%–60 wt%

    Typically, agricultural silage cover extrusion shifts the control burden from optical haze to puncture and tear resistance, because the film must survive repeated mechanical loading, UV exposure, and contact with rough forage without splitting along contamination points. PF-0118-C is processed in thick-gauge blown film from 100 µm to 200 µm using a die gap of 1.8 mm to 2.4 mm and a blow-up ratio from 2.0:1 to 2.8:1; melt temperature is controlled in the 190 °C to 230 °C range to maintain output without inducing oxidative gel formation in the bubble. Because butene LLDPE provides lower low-temperature dart impact relative to octene LLDPE at equivalent density when measured under ISO 7765-1 or ASTM D1709, agricultural specifications often compensate through thicker gauge or blending with metallocene LLDPE at 10 wt% to 30 wt% to satisfy puncture and tear minimums. UV stability is supplied by a hindered amine light stabilizer concentrate at a total active loading of 0.2 wt% to 0.8 wt%, with the exact concentration determined by the expected exposure period and the finished film's surface-to-mass ratio; tensile properties are monitored by ISO 527-3, tear resistance by ISO 6383-2, dart impact by ISO 7765-1, and overall covering film requirements by EN 13206.

    Field service data from agricultural film conversion indicate that the dominant failure origin is mechanical damage at the anchor point and not UV embrittlement, provided the HALS package is uniformly dispersed. HALS dispersion is verified by pressing a film sample and checking agglomerates under transmitted light; agglomerate counts above 10/m² are rejected because they initiate tear propagation. Extrusion of thick agricultural films from butene LLDPE also requires control of bubble cooling because internal bubble pressure at high blow-up ratio can generate edge-strip orientation differences; a double-lip air ring and an adjustable stabilizer cage are common equipment. The film is post-gusseted rather than centre-folded on line when used for silage covering, because the centre fold creates a weak line that fails under repeated wind and frost loading. A common failure mode in field service is not puncture but tear propagation from a small perforation near the ground anchor; therefore production control includes measurement of transverse direction tear on reels conditioned at 23 °C and 50% RH for 48 h before release. End products include silage pit covers, round bale stretch films, mini-tunnel covers, and greenhouse side curtains.

    Lamination Sealant Web Geometry and Interlayer Adhesion in Barrier Structures

    A recurring limitation in lamination sealant webs is the loss of surface wetting after corona treatment ages, which directly reduces interlayer adhesion on metallized polyester and aluminium foil substrates. PF-0118-C is extruded as a cast or blown web at 15 µm to 30 µm thickness, then corona treated inline to a wetting tension of 38 mN/m to 42 mN/m measured by ASTM D2578. Over-treatment above 50 mN/m generates a brittle surface layer that can fail cohesively during T-peel testing under ASTM D1876, so the treater output is trimmed to the substrate pairing rather than set at maximum power. Lamination to aluminum foil, metallized PET, or oriented polyamide is performed with a solventless adhesive applied at 1.5 g/m² to 2.5 g/m²; the nip temperature is held at 60 °C to 80 °C, and laminated reels are aged for 24 h to 48 h before seal testing. Seal strength is measured by ASTM F88/F88M on 25 mm wide strips after jaw sealing at temperatures derived from ASTM F1921, with typical validation windows of 0.4 s to 0.8 s dwell.

    After lamination, the sealant web is converted on pouch lines with a seal bar profile that may include a PTFE-coated constant-heat jaw or an impulse jaw; the PF-0118-C layer requires a lower seal initiation temperature than high-density polyethylene and therefore permits reduced cycle time on multi-lane machines. However, the reduction in seal initiation temperature narrows the hot-tack window; hot-tack strength is measured according to ASTM F1921, and the seal jaw temperature is controlled within ±3 °C to avoid erratic opening force. Since butene LLDPE contains low molecular weight fractions that may migrate into the adhesive layer, bond decay is evaluated by comparing 24 h T-peel values with values after 7 days at 40 °C; a drop exceeding 20% indicates a need to reduce corona treat level or reformulate the adhesive. This resin is specified for dry, chilled, and frozen laminate applications rather than retort pouches because butene LLDPE has a lower upper service temperature than propylene copolymers. Finished pack forms include stand-up pouches for snacks and pet food, dry chemical sachet laminates, pillow packs for powdered beverages, and bag-in-box liners.

    Across Collation Shrink and Protective Packaging Lines

    With tunnel temperatures between 120 °C and 160 °C, collation shrink films based on PF-0118-C and high-pressure LDPE blends encounter a specific balance between free shrink and seal window. The PF-0118-C fraction is usually set at 30 wt% to 60 wt% of the blend; higher levels improve dart impact and tear resistance but reduce transverse direction free shrink measured by ASTM D2732, which can leave insufficient corner tightness on bottle bundles. The blend is processed on a blown film line with a die gap from 1.2 mm to 2.0 mm, a blow-up ratio from 2.0:1 to 2.5:1, and melt temperature between 190 °C and 225 °C. Frost line height is set lower than in heavy-duty sack production to produce higher molecular orientation in the bubble, and the collapsing frame angle is adjusted to avoid MD/TD shrink imbalance. Seal initiation is characterized by ASTM F1921, and seal strength by ASTM F88/F88M.

    At LLDPE blend ratios above 60 wt%, tunnel shrinkage can become insufficient at the package corners, and the film may distort rather than tighten around the bundle. The shrink tunnel is operated with a residence time of 3 s to 8 s and air velocity from 3 m/s to 8 m/s; insufficient residence time at the lower tunnel temperature causes incomplete shrinkage, while excessive tunnel temperature causes puckering and burn-through on narrow heat-shrink areas. The film's seal window on collation bundlers is narrower with high LLDPE content because the seal initiation temperature is lower but the plateau seal strength is more sensitive to seal jaw temperature fluctuations; therefore, line operators monitor seal jaw temperature within ±3 °C and validate seal strength every reel change by ASTM F88/F88M. Free shrink is measured on 100 mm × 100 mm specimens immersed in a silicone oil bath per ASTM D2732-14. Edge-bead is controlled by gauge variation within ±5%, because thick edges produce uneven shrink force and trigger package distortion on the tunnel conveyor. End products include multi-pack bottles, glass container bundles, canned goods collations, and overwrap films for protective packaging of low-density rigid items.

    Free Quote

    Competitive NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Novapol® PF-0118-C is a butene-copolymer linear low-density polyethylene film resin supplied by NOVA Chemicals Corporation for thin-gauge blown and cast film extrusion. The grade is defined by a nominal melt index of 1.0 g/10 min measured at 190 °C under a 2.16 kg piston load in accordance with ASTM D1238, and by a nominal density of 0.918 g/cm³ at 23 °C in accordance with ASTM D792. The butene comonomer introduces ethyl branches along the polyethylene backbone, reducing crystallinity and film stiffness relative to high-density polyethylene and establishing the processing and end-use performance of a C₄ LLDPE. Supplier technical literature identifies candidate applications including general-purpose liners, garment bags, produce bags, overwrap film, agricultural film, and shipping sacks; food-contact suitability must be verified against the current regulatory certificate because final film structure, additive loading, and converting conditions determine compliance. The “C” designation is associated with a formulated additive package; the exact slip and antiblock loadings are lot-specific and are disclosed through the certificate of analysis and safety data sheet rather than through a single fixed published value. Converters evaluating PF-0118-C against an unmodified base resin should compare coefficient of friction under ASTM D1894, blocking force under ASTM D3354, and corona wetting tension after treatment because these surface properties influence winding, printing, and pouch-forming behavior.

    PropertyPublished typical valueTest method
    Melt index at 190 °C/2.16 kg1.0 g/10 minASTM D1238
    Density at 23 °C0.918 g/cm³ASTM D792
    Comonomer typebutene (C₄)manufacturer designation
    Physical formpelletvisual inspection

    The density of 0.918 g/cm³ corresponds to a semicrystalline morphology with a crystalline fraction commonly observed in the range of 40% to 45% by differential scanning calorimetry. The principal melting peak for this density class appears near 121 °C to 124 °C; a broad secondary shoulder reflects lamellar thickness distribution. This crystallinity reduction lowers yield strength and increases elongation at break relative to high-density polyethylene, as measured by ASTM D882. Because polyethylene lacks polar functional groups, the uncoated film has high oxygen and carbon dioxide transmission rates compared with EVOH, polyamide, or PVdC; PF-0118-C is therefore used as a structural or sealing layer rather than as a high-barrier monofilm. Heat-seal initiation temperature for butene LLDPE of this density is generally lower than high-density polyethylene; converters should measure seal strength under ASTM F88 and hot-tack behavior under ASTM F1921 on the final film because slip additives migrate to the seal surface and can reduce seal strength. The molecular weight distribution of PF-0118-C is not published in the technical data sheet; lot-to-lot variability is controlled by melt index and density specifications. A high-load melt flow index can be measured under ASTM D1238 condition 190 °C/21.6 kg, but a grade-specific value must be obtained from the supplier.

    Which extrusion and conversion window applies to PF-0118-C?

    Melt processing of PF-0118-C follows the shear-thinning response characteristic of linear low-density polyethylene. The 1.0 g/10 min melt index places the grade in a medium-viscosity segment, requiring greater extruder torque than a 2.0 g/10 min LLDPE but less than a fractional-melt film resin. Single-screw extruders with barrier screws and 24:1 to 30:1 length-to-diameter ratios are typical on blown-film lines; grooved-feed sections can stabilize throughput when pellet bulk density varies. Blown-film temperature profiles from rear feed zone to die are generally set between 180 °C and 220 °C, with the adapter and die lips heated to minimize melt fracture. Die gaps range from 1.5 mm to 2.5 mm, and blow-up ratios from 2.0:1 to 2.5:1 provide a balance between machine-direction and transverse-direction tear. Frost-line height is commonly set at 1 to 3 die diameters; an elevated frost line may reduce haze but increases the probability of bubble instability and gauge bands. Cast-film lines operate at higher melt temperatures, commonly 220 °C to 240 °C, with chill-roll temperatures of 15 °C to 25 °C and a minimal air gap to limit neck-in. Surface oxidation and die-lip resin buildup can occur when the air gap is excessive or when extruder residence time exceeds the supplier-recommended limit.

    Polyethylene is non-hygroscopic and does not require predrying. Condensation on cold pellets stored below 10 °C can introduce enough surface moisture to generate pinholes in thin films when the pellets are moved into a warm extrusion area; if storage relative humidity exceeds 60%, a dry-air hopper or desiccant dryer set to 40 °C to 60 °C is used as a surface-moisture control measure rather than as a polymer drying requirement. Excessive hopper residence at elevated temperature should be avoided because it can accelerate additive migration and pellet blocking.

    Sharkskin melt fracture appears first on the chill-roll side as matte transverse lines when the melt temperature at the die lip is too low; the usual recovery action is to increase the die-zone set point in 2 °C increments or open the die gap without raising the overall melt temperature. Oxidative gels present as translucent fisheyes and can accumulate on the screen pack; they are minimized by keeping flat temperature profiles below 240 °C and by purging with a polyolefin purge compound after shutdowns. Die-lip buildup is influenced by the additive package; periodic wiping and the use of a fluoropolymer-based processing aid are common on high-output cast-film lines. Gear-pump-assisted extrusion is used on some lines to stabilize output and reduce shear heating, but the pump must be sized to avoid excessive suction-side pressure at the 1.0 g/10 min melt index condition.

    Additive package differences among PF-series grades can shift coefficient of friction, blocking force, and optical haze. If switching from an unformulated or differently formulated PF-series grade to PF-0118-C, the film processor should requalify the film on the specific winding and bag-making lines because slip migration kinetics and antiblock particle density affect coefficient of friction in the first 24 h to 72 h after extrusion. The time-dependent bloom of slip additives follows lipid-like migration kinetics in semicrystalline polyethylene; coefficient of friction values measured immediately after extrusion are higher than values measured later. Corona treatment decay also depends on additive bloom; target wetting tension should be confirmed by dyne solution measurements under ASTM D2578 at the point of lamination or printing.

    Comparative position among C₄, C₆, and high-pressure film resins

    Comparative performance among polyethylene film grades is driven by comonomer type, molecular weight distribution, and additive formulation. PF-0118-C uses butene as the C₄ alpha-olefin; this generates ethyl branches, which are shorter than the butyl branches produced by hexene and the hexyl branches produced by octene. At equivalent density and melt index, butene LLDPE generally has lower dart impact strength when tested under ASTM D1709, lower puncture energy under ASTM D5748, and lower Elmendorf tear strength under ASTM D1922 than hexene LLDPE. The difference is attributed to fewer tie molecules bridging crystallites in the solid state; the longer branches of hexene and octene increase interlamellar entanglement. Machine-direction tear is particularly sensitive to blow-up ratio; values measured at low blow-up ratio can be misleading when comparing films. For downstream conversion, PF-0118-C often provides adequate toughness for thin-gauge liners and bags where hexene-copolymer performance is not required, and its density-controlled stiffness and lower seal initiation temperature are used in packaging lines.

    Against high-pressure LDPE, PF-0118-C has higher tensile strength at break and elongation at break under ASTM D882, which permits downgauging in applications such as carrier bags and liners. LDPE, however, retains higher melt strength and broader bubble stability; large-diameter blown-film lines running high stalk heights are easier with LDPE or LDPE/LLDPE blends. When compared with metallocene LLDPE grades, PF-0118-C may exhibit lower dart impact and less elastic melt behavior under certain processing conditions; however the conventional Ziegler-Natta architecture gives a familiar extrusion response and lower backpressure on older screw designs. The selection of PF-0118-C versus a metallocene C₄ or C₆ LLDPE should be made after comparing film dart impact at equal gauge, tear balance at the intended blow-up ratio, and seal strength under ASTM F88 or ASTM F2029.

    For converters using high levels of regrind or post-industrial film, the butene LLDPE response may be sensitive to contamination; calcium carbonate filler or off-spec LDPE blend fractions above 10 wt% can reduce dart impact and tear in a nonlinear manner. A processing trial with the actual regrind stream is necessary because published data for this specific configuration is limited.

    Regulatory control for a butene LLDPE film resin depends on the end-use market and the converted article.

    Standard/RegulationApplication scope
    FDA 21 CFR 177.1520(c)Olefin polymers permitted for food-contact use; condition-of-use and additive verification required
    EU Regulation (EU) No 10/2011Plastic food-contact materials; overall migration and specific migration limits must be measured on final film
    REACH (EC) No 1907/2006Registration and safety data sheet communication for monomers and additives
    ASTM D4976Polyethylene plastic molding and extrusion material specification; grade compliance by lot

    End-use limitations include continuous exposure to elevated temperatures above 60 °C where dimensional relaxation may occur, contact with strong oxidizing acids or aromatic solvents that can accelerate environmental stress cracking, and use as an uncoated barrier film for oxygen-sensitive products. The resin is not intended for medical implant or high-pressure gas containment service; converters must validate seal integrity, extractables, and migration for regulated packaging. Corona treatment to 38 mN/m to 42 mN/m is typically required for adhesive lamination and ink adhesion, while untreated film surfaces remain near 31 mN/m and are poorly wetting.