| HS Code | 236352 |
| Manufacturer | NOVA Chemicals |
| Product Name | Novapol® GM-1224-A Butene LLDPE Masterbatch Resin |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.924 g/cm³ |
| Melt Index 190 C 2 16 Kg | 12 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 11 MPa |
| Ultimate Tensile Strength | 24 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 260 MPa |
| Hardness Shore D | 50 |
| Thermal Stabilization | Yes |
| Physical Form | Pellets |
| Color | Natural |
As an accredited NOVA Chemicals Novapol® GM-1224-A Butene LLDPE Masterbatch Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Novapol® GM-1224-A Butene LLDPE Masterbatch Resin is packaged in 25 kg bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | Loaded in 20′ FCL container: NOVA Chemicals Novapol® GM-1224-A Butene LLDPE Masterbatch Resin, packaged in 25 kg bags, palletized, shrink-wrapped. |
| Shipping | NOVA Chemicals Novapol® GM-1224-A Butene LLDPE Masterbatch Resin ships as non-hazardous plastic resin pellets. It is not regulated by DOT, IMDG, IATA, or TDG; no UN number, hazard class, or packing group applies. Use original sealed bags, boxes, or bulk containers. Store cool, dry, away from heat and ignition. |
| Storage | Store Novapol GM-1224-A in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep material in original, closed packaging, palletized and off the floor to prevent moisture pickup and contamination. Avoid excessive stacking; rotate stock FIFO. Ensure containers are tightly sealed when not in use. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Manufacturer-recommended shelf life is 24 months from manufacture when stored in original packaging under cool, dry conditions, away from direct sunlight. |
Novapol® GM-1224-A is a butene linear low-density polyethylene (LLDPE) masterbatch carrier resin with a nominal density of 0.918 g/cm³ (ASTM D792) and a melt index of 2.0 g/10 min (ASTM D1238, 190 °C/2.16 kg). The grade is designed for high-loading masterbatch production where lot-to-lot melt flow consistency and low gel counts determine filter pressure rise and pigment dispersion uniformity. Published data for this specific grade configuration is limited to standard physical property datasheets; the following scenarios use industrial compounding ranges anchored to standard test methods, production-scale equipment specifications, and regulatory clauses. The scenarios are limited to downstream masterbatch routes for which published industrial data or standard test methodology can be cited.
| Scenario | Standard designation | Relevant clause / test method | Typical condition or threshold |
|---|---|---|---|
| Color masterbatch | EN 71-3 | Migration of certain elements | element-specific limits as specified in EN 71-3:2019 |
| Color masterbatch | FDA 21 CFR 177.1520(c) | Olefin polymers | food types per Table 1 of 21 CFR 177.1520 |
| Carbon black masterbatch | ASTM D5596 | Carbon black dispersion in polyethylene | dispersion index < 3 |
| White masterbatch | FDA 21 CFR 176.170(c) | Paper and paperboard components | extraction limits per 21 CFR 176.170(d) |
| Slip/antiblock masterbatch | ASTM D1894 | Static and kinetic coefficients of friction | COF < 0.2 |
| Filler masterbatch | ISO 11607-1 | Packaging for terminally sterilized medical devices | seal strength and microbial barrier validation |
| Processing aid masterbatch | FDA 21 CFR 178.3900 | Adjuvants, production aids, and sanitizers | as listed in component inventory |
Production-scale color masterbatch compounding using GM-1224-A as carrier resin operates at carrier loadings of 30–55 wt% depending on pigment type and final letdown ratio. For iron oxide yellow (CI Pigment Yellow 42) loadings of 40–70 wt%, the carrier resin fraction must remain sufficient to wet pigment surfaces and maintain melt phase continuity. Compounding is performed on co-rotating twin-screw extruders with L/D ratios of 40:1–52:1 and screw speeds of 400–800 rpm. Specific energy input ranges between 0.12 kWh/kg and 0.18 kWh/kg, with melt temperatures held at 190–220 °C. Screen pack assemblies using 150/200 mesh gauge bands generate pressure-rise data; a pressure increase exceeding 80 bar over a 60-minute run indicates inadequate pigment dispersion or filter blinding. Industry compliance for packaging-grade color masterbatch includes EN 71-3 migration limits for heavy metals, CONEG total lead/cadmium/mercury/chromium(VI) below 100 mg/kg, and EU 10/2011/EC Annex I for food-contact plastics when the final film or injection-molded article is intended for food use. Under FDA 21 CFR 177.1520(c), olefin polymers may be used in contact with food types listed in Table 1 of the regulation, provided the final article passes extraction tests specified in 21 CFR 177.1520(d). Terminal finished product types include black masterbatch pellets for HDPE injection-molded crates, yellow iron oxide masterbatch for polypropylene caps, and green chromium oxide masterbatch for LLDPE blown film agricultural covers. Process limitations observed on production lines include torque spikes above 85% of motor nameplate when screw speed exceeds 600 rpm with pigment loadings above 60 wt%, requiring either reduced feed rates or increased carrier resin fraction.
At production-scale twin-screw compounding lines running carbon black masterbatches for agricultural mulch and geosynthetic liners, GM-1224-A is added at 40–60 wt% as the carrier phase, while carbon black (N220 or N550 grade) is side-fed at 40–50 wt%. Antioxidant addition of 0.2–0.5 wt% and a metal stearate processing aid at 0.1–0.3 wt% maintain melt stability during extended runs. The masterbatch is let down at 5–10 wt% into LLDPE or LDPE blown film to achieve carbon black concentrations of 2.0–3.0 wt% in the finished film, the range required for UV stabilization in greenhouse films under ISO 4892-2 weathering protocols. Compounding uses either internal Banbury-type mixers with drop temperatures of 160–180 °C followed by sheeted pelletizing, or co-rotating twin-screw extruders with L/D of 44:1–48:1 and melt temperatures of 200–240 °C. Water-ring pelletizing followed by drying at 80 °C for 2 h is required to reduce residual moisture below 0.05 wt%. Dispersion quality is assessed per ASTM D5596 for carbon black dispersion in polyethylene; a dispersion index below 3 is generally accepted for agricultural film applications. Compliance for food-contact use of black masterbatch in films that may contact dry food is evaluated under EU 10/2011 and FDA 21 CFR 177.1520, with additional REACH Annex XVII restrictions for PAH content in carbon black used in consumer articles. Terminal finished products include black silage wrap film, greenhouse mulch film, landfill geomembrane sheet, and HDPE carrier pipe.
High-opacity white masterbatch for extrusion coating paperboard uses rutile titanium dioxide (TiO₂) at 45–65 wt% with GM-1224-A carrier resin at 35–55 wt% and a calcium stearate lubricant at 0.5–1.5 wt%. The carrier resin’s melt index of 2.0 g/10 min (ASTM D1238) and density of 0.918 g/cm³ (ASTM D792) permit pigment wetting at lower melt temperatures, reducing TiO₂ photocatalytic degradation. Compounding proceeds on a co-rotating twin-screw extruder with L/D 48:1, side-stuffing TiO₂ at barrel 5–6, and maintaining melt temperature at 200–230 °C. Melt filtration through screen packs of 100–200 µm aperture removes agglomerates larger than 150 µm. Strand pelletizing is followed by centrifugal drying. Compliance for finished coated paperboard intended for aqueous, acidic, or fatty food contact is governed by FDA 21 CFR 176.170(c) for paper and paperboard components and EU 10/2011 with specific migration limits for titanium dioxide and processing aids. Opacity of the extruded coating is measured per ISO 2471; coatings containing 10–15 wt% TiO₂ in the final polymer layer achieve opacity values of 85–95% at a coat weight of 15–20 g/m². Terminal finished products include food-service paper cups, folding carton stock for frozen foods, and liquid packaging board with white outer ply. A process constraint encountered on industrial lines is TiO₂ dusting at side-feed ports, requiring enclosed feeder systems and forced venting to maintain melt pressure stability.
Additive masterbatch for blown film slip and antiblock is compounded from GM-1224-A at 80–90 wt% as carrier resin with erucamide slip agent at 5–10 wt% and synthetic silica antiblock at 5–10 wt%, plus 0.1–0.3 wt% hindered phenolic antioxidant. The masterbatch is let down at 1–3 wt% into LLDPE or LDPE blown film resins to reduce coefficient of friction (COF) from above 0.6 to below 0.2 as measured by ASTM D1894. Single-screw extruders with distributive mixing elements and L/D of 30:1–40:1 operate at melt temperatures of 180–210 °C. Because erucamide migrates to the film surface, post-extrusion conditioning at 23 °C and 50% RH for 24–48 h is required before COF stabilizes. Compliance for food-contact film uses FDA 21 CFR 177.1520 and EU 10/2011, with erucamide included in the Union list of authorized substances. Terminal finished products include slip/antiblock masterbatch for bread bag films, frozen food packaging, form-fill-seal pouches, and heavy-duty shipping bags. Process limitations include screw slippage if silica absorbs excess moisture; pre-drying of silica at 80 °C for 4 h is required when ambient relative humidity exceeds 60%.
Highly filled calcium carbonate masterbatch for microporous breathable film requires carrier resin loadings of 20–30 wt% with uncoated or stearic acid-coated CaCO₃ at 70–80 wt%. The masterbatch is let down into LLDPE at 40–60 wt% to yield a film formulation containing 50–60 wt% CaCO₃ before machine-direction orientation. Compounding occurs on co-rotating twin-screw extruders with L/D 52:1 and side-feeding at barrel 6–8; melt temperatures are controlled to 200–230 °C and melt pump discharge pressure is maintained at 80–120 bar. Underwater pelletizing with die plate temperatures of 260–280 °C produces spherical pellets that meter consistently in downstream cast film feeding. After film casting at 220–240 °C, machine-direction stretching at ratios of 3:1–5:1 creates interconnected micropores; air permeability is measured by Gurley densometer per TAPPI T460 and ISO 5636-5 and falls below 3000 s/100 mL for diaper backsheet film. Compliance for hygiene films is evaluated against REACH and the European General Product Safety Directive 2001/95/EC, while medical packaging applications require ISO 11607-1 seal strength and microbial barrier validation. Terminal finished products include breathable backsheet film for infant diapers, feminine hygiene products, medical protective gowns, and breathable housewrap.
Because GM-1224-A exhibits a melt index of 2.0 g/10 min (ASTM D1238) and a density of 0.918 g/cm³ (ASTM D792), it functions as a carrier resin in fluoroelastomer processing aid masterbatch at loadings of 95–98 wt%, with the fluoropolymer additive at 2–5 wt%. The masterbatch is let down at 500–1000 ppm fluoropolymer in LLDPE blown film to eliminate sharkskin melt fracture at high shear rates above 500 s⁻¹. Compounding uses a twin-screw extruder with L/D 44:1 at melt temperatures of 170–200 °C, avoiding temperatures above 230 °C to prevent fluoropolymer degradation. Pelletizing is performed by strand water bath with pellet drying at 60 °C for 2 h. Compliance for food-contact film applications is assessed under FDA 21 CFR 177.1520 and EU 10/2011, with fluoropolymer processing aids typically cleared for use under FDA 21 CFR 177.1520 or 178.3900 depending on composition. Terminal finished products include processing aid masterbatch for LLDPE blown film, cast stretch film, and extrusion blow molded containers. A processing constraint on film lines is the need for initial purging at 1% masterbatch addition for 30–60 min to coat die surfaces before reducing fluoropolymer concentration to steady-state levels.
Competitive NOVA Chemicals Novapol® GM-1224-A Butene LLDPE Masterbatch Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® GM-1224-A is a butene linear low-density polyethylene masterbatch resin supplied in pellet form and intended primarily as a carrier for color, additive, and mineral filler concentrates. The grade is not marketed as a finished film resin; its performance is realized when diluted in LLDPE-rich film, extrusion coating, or injection moulding formulations at typical let-down ratios of 2% to 5% by weight. Because the resin is produced with a high melt index, it reduces melt viscosity during compounding and permits faster pigment wetting before extruder torque limits are reached. These characteristics define the operational role of the product, but final suitability must be established through pilot trials on the target diluting line.
The resin belongs to the butene-copolymer LLDPE class; butene is the short-chain comonomer distributed along a linear polyethylene backbone. The manufacturer’s technical data sheet identifies a melt index of 20 g/10 min at 190 °C/2.16 kg when tested to ASTM D1238 or ISO 1133-1:2022, and a density of 0.924 g/cm³ when tested to ASTM D792 or ISO 1183-1. The differential scanning calorimetry melting peak typically falls between 122 °C and 126 °C when evaluated by ASTM D3418 or ISO 11357-3. Pellet bulk density is commonly reported in the 0.50–0.54 g/cm³ range when measured by ASTM D1895 Method B. Because bulk density and pellet geometry influence gravimetric feeder accuracy, the certificate of analysis should be consulted for lot-specific values before automating masterbatch dosing.
Table 1. Typical property window and test designations for GM-1224-A.
| Property | Typical lot value or range | Test designation |
|---|---|---|
| Melt index at 190 °C/2.16 kg | 20 g/10 min | ASTM D1238; ISO 1133-1:2022 |
| Density | 0.924 g/cm³ | ASTM D792; ISO 1183-1 |
| Melting peak | 122–126 °C | ASTM D3418; ISO 11357-3 |
| Bulk density | 0.50–0.54 g/cm³ | ASTM D1895 Method B |
Incoming quality-control protocols for GM-1224-A should include melt index by ASTM D1238, density by ASTM D792, and pellet size distribution on a sieve stack according to ASTM D1921. Melt-index variation greater than ±2 g/10 min between lots can shift gravimetric feeder calibration and downstream let-down accuracy. Density variation greater than 0.002 g/cm³ may signal comonomer drift and should trigger a review of masterbatch rheology. For critical automotive or high-speed packaging applications, an additional oxidative induction time test by ASTM D3895 at 200 °C is used to detect antioxidant variability before the resin enters production.
The distinction from a film-grade butene LLDPE is primarily rheological. Film grades often have melt indices below 2.0 g/10 min, producing high extruder drive load and poor pigment penetration when used as masterbatch carriers. GM-1224-A at 20 g/10 min reduces melt viscosity sufficiently to wet pigment surfaces under shear, but the high-flow architecture also lowers melt strength, which makes it unsuitable as a neat blown-film resin. Compared with high-pressure LDPE carriers of similar melt index, GM-1224-A has a linear backbone with short-chain butene branches rather than long-chain branching. The linear architecture reduces melt elasticity and may improve compatibility with LLDPE-rich host formulations, while LDPE carriers can offer higher bubble stability in LDPE-dominant blown film lines. Against metallocene-catalyzed LLDPE carriers, GM-1224-A typically has a broader molecular weight distribution; this can reduce specific energy input but may produce slightly lower optical clarity in thin-gauge film. The choice among these carriers should be made through capillary rheometry and pilot let-down trials, not solely on melt index.
Capillary rheometry according to ASTM D3835 at 190 °C is the most direct method for comparing GM-1224-A with an incumbent carrier. A high-melt-index LLDPE carrier typically exhibits shear-thinning behavior with apparent viscosity values lower than film-grade LLDPE across the 100 s&supminus;¹ to 1000 s&supminus;¹ range. This property reduces pressure drop across screen packs and melt pumps but also lowers viscous heating; extruder set points may need to be 10 °C to 15 °C higher than those used for a comparable LDPE carrier to achieve the same melt temperature. The melt pump inlet pressure should be maintained above 5 bar absolute to ensure stable delivery to the die plate. Users should not compare resins solely by melt index; density and molecular weight distribution affect low-shear viscosity and pigment wetting independently.
Table 2. Architectural and processing comparison for carrier resin classes.
| Carrier class | Melt index range at 190 °C/2.16 kg | Branching architecture | Typical compounding consequence |
|---|---|---|---|
| High-MI butene LLDPE carrier such as GM-1224-A | 20 g/10 min | Linear backbone with short-chain butene branches | Lower motor load; high pigment loading before torque or backpressure limits |
| High-pressure LDPE carrier | 20–22 g/10 min | Long-chain branched | Higher melt elasticity; improved bubble stability but lower tensile modulus after let-down |
| Metallocene LLDPE carrier | 15–30 g/10 min | Uniform short-chain branching | Narrower melting and molecular weight distribution; potentially higher optical performance and higher specific energy input |
On a co-rotating twin-screw extruder with 40:1 L/D and segmented screw elements, GM-1224-A is typically processed with barrel set points of 180 °C to 210 °C and a die head set point of 200 °C to 220 °C. Pellet feed throat cooling is recommended because the high melt index and relatively low melt temperature can soften pellets at the feed zone walls and cause bridging. Specific energy input in the range 0.12–0.18 kWh/kg is common for high-load pigment concentrates, but the exact value must be established on the target line because screw configuration, feeder accuracy, and vent vacuum alter energy balance. Atmospheric or vacuum venting reduces volatile carryover from wax dispersants and wet pigments; a vacuum level of −0.2 bar to −0.6 bar gauge is common.
Melt temperature is the principal process variable controlling degradation of GM-1224-A. The resin should be maintained below 240 °C during compounding; prolonged exposure above this threshold accelerates chain scission, broadens molecular weight distribution, and increases melt index drift. Residence time at temperature should not exceed 10 min to 15 min; production stops longer than this require purging with a low-melt-index LDPE or a commercial purge compound to prevent oxidized holdup. Extruder barrel set points of 180 °C to 210 °C and a die head set point of 200 °C to 220 °C are typical starting conditions for a 40:1 L/D co-rotating twin-screw extruder. The feed throat should be water-cooled because high-MI pellets soften near the feed zone and can bridge; feed throat temperature above 50 °C is a common cause of irregular solids conveying.
Pre-drying is not required for sealed, undamaged packaging. If resin has been stored at relative humidity above 60%, drying at 60 °C for 4 h reduces surface moisture before processing. Vacuum venting with −0.2 bar to −0.6 bar gauge is used to remove moisture and low-molecular-weight waxes from the melt; vent plugging is an operational indicator that moisture or volatile load exceeds the system’s stripping capacity. Certain metal stearate lubricants and amine-based antistatic agents can interact with antioxidants or exhibit thermal decomposition above 220 °C; compatibility should be confirmed by oxidative induction time testing according to ASTM D3895 or ISO 11357-6 and by screw-pull inspection after a trial run.
High-intensity tumble mixers and heated plow mixers are used to pre-coat pigment with carrier resin before extrusion. In these operations, GM-1224-A can be used as the wetting resin at addition levels of 2% to 5% by weight of the mix. Defects such as unmixed pigment agglomerates in the final pellets, amperage cycling on the extruder drive, and vent plugging are typically traced to mixer discharge temperature below the resin’s melting range or insufficient mixing time. The mix should reach a discharge temperature above 100 °C for dry pigment coating; for wax-containing systems, the temperature must remain below the wax melting range to prevent paste-like buildup. Pelletization defects including tailing, doublets, and fines generation are traced to die-face temperature above 230 °C, dull cutter blades, or water bath temperature above 45 °C. These failure modes are not unique to GM-1224-A; they are common to high-melt-index LLDPE carriers with similar density.
In color masterbatch production, GM-1224-A is typically introduced at the first barrel section of a twin-screw compounder with a side-fed pigment or filler downstream to minimize thermal history. For carbon black concentrates, loadings of 40% to 50% are common, depending on carbon black grade and dispersant package; titanium dioxide concentrates may reach 60% to 70% loading on specialized lines. A strand pelletizing system with water bath temperature 30 °C to 45 °C and pellet cutter gap set to manufacturer tolerance is recommended; pellet smearing or tailing indicates excessive die-face temperature. In extrusion coating, let-down ratios of 3% to 6% are typical; the carrier should be matched to the host resin’s melt index to avoid surface haze and die-lip buildup. For blown film lines processing LLDPE-rich feeds, the addition of GM-1224-A at 5% can shift bubble stability if the host resin has low melt strength; a wider die gap of 2.0–2.5 mm or a reduced frost-line height may be required. Published data for this specific grade in high-speed cast film conversion is limited; pilot trials are recommended where die lip build-up is a known failure mode.
The base olefin resin is generally recognized for food-contact use under FDA 21 CFR 177.1520 when the finished article meets end-use limitations, but the masterbatch itself must be evaluated for the pigments and dispersants selected. The applicable subparagraphs of 21 CFR 177.1520 depend on density, melting range, and use conditions. In the European Union, plastics intended for food contact must comply with Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² for plastic materials, unless a specific migration limit applies to a component. Compliance with REACH (EC 1907/2006) and RoHS (Directive 2011/65/EU) is formulation-dependent and must be verified at the masterbatch level before shipment. No declaration of food-contact compliance should be made for the product as supplied without reviewing the complete additive formulation.