| HS Code | 662293 |
| Product Name | NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin |
| Manufacturer | NOVA Chemicals |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.926 g/cm³ |
| Melt Index | 35 g/10 min (190°C/2.16 kg) |
| Melting Point | 124 °C |
| Vicat Softening Point | 94 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 14.5 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 276 MPa |
| Hardness Shore D | 48 |
| Tear Strength | 245 g/mil |
| Brittleness Temperature | < -70 °C |
| Additive | Antioxidant |
| Form | Pellets |
| Color | Natural |
As an accredited NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin is packaged in 25 kg polyethylene bags, typically on stretch-wrapped pallets. |
| Container Loading (20′ FCL) | 20′ FCL: 18 MT Novapol GI-3526-A LLDPE masterbatch resin in 25 kg bags, floor loaded and secured for ocean transport. |
| Shipping | NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin ships as non-hazardous polyethylene pellets. Standard packaging includes 25 kg polyethylene-lined bags, stretch-wrapped pallets, or bulk trucks/railcars. No DOT/IMDG/IATA hazard classification. Keep dry, away from heat, moisture, contamination, and static; handle per SDS and local regulations. |
| Storage | Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed and palletized off the floor. Protect from moisture, contamination, and physical damage. Avoid dust generation and static discharge. Observe good housekeeping, first-in/first-out stock rotation, and applicable local regulations. Consult the SDS for complete guidance. |
| Shelf Life | Typically 12 months from manufacture when stored in original unopened packaging under dry, ambient conditions, away from direct sunlight. |
In high-carbon-black masterbatch production for agricultural silage film and geosynthetic sheet, NOVA Chemicals Novapol® GI-3526-A is used as a carrier resin with nominal melt index 20 g/10 min at 190 °C/2.16 kg (ASTM D1238) and nominal density 0.924 g/cm³ (ASTM D792). A 40 wt% carbon black masterbatch is compounded on a co-rotating twin-screw extruder with L/D 44:1, polymer pellets entering barrel 1 and furnace black introduced through a side-stuffer at barrel 5. The formulation consists of 40 wt% high-structure furnace black, 8–10 wt% low-molecular-weight polyethylene wax, 0.2–0.4 wt% hindered phenol/phosphite process stabilizer, and the balance carrier resin. Barrel set points are 190–220 °C, with die melt temperature held at 210–230 °C; vacuum devolatilization at -0.08 MPa removes residual moisture and low-boiling wax fractions. Screw speed is set at 500–600 rpm on a 50 mm machine, producing specific energy input near 0.22 kWh/kg. Dispersion quality is monitored by pressure ahead of a 150/200/325 mesh screen pack. A progressive pressure rise from 8 MPa to 15 MPa over 4 h indicates screen plating from undispersed black agglomerates or condensed wax. The masterbatch is let down at 5–7 wt% into LLDPE/LDPE blown film to yield 2.0–2.8 wt% carbon black in the finished film. Film mechanical properties are tested according to ISO 527-3 and ASTM D882; carbon black dispersion in the compound is rated by ISO 18553. The finished film is used for silage protection covers and temporary geomembrane sheeting where carbon black loading balances UV absorption and tensile retention.
To maintain screen-pack pressure below 12 MPa and opacity above 85% in white extrusion-coating masterbatches, TiO₂ concentrate producers compound rutile titanium dioxide at 65–70 wt% with GI-3526-A at 20–30 wt%, oxidized polyethylene wax at 4–8 wt%, and zinc stearate at 0.2–0.5 wt%. The TiO₂ is side-fed into the melt stream after the polymer is fully molten, typically in barrel 4 of a co-rotating twin-screw extruder with L/D 48:1. Barrel temperatures are maintained from 180 °C in the feed section to 230 °C at the die; specific energy input of 0.18–0.24 kWh/kg is required to break down TiO₂ agglomerates without degrading the wax phase. A vacuum vent at -0.09 MPa removes volatiles that otherwise create pinholes in the coated web. The masterbatch is tumble-blended with LDPE extrusion-coating resin at 8–12 wt%, producing 5.2–6.4 wt% TiO₂ in the applied layer. At line speeds above 150 m/min, let-down above 12 wt% can reduce draw-down stability and edge tear resistance because the high-flow carrier shifts melt elasticity of the LDPE host. White paperboard cups and liquid-packaging board coated with this compound are tested for opacity by ISO 2471 and for adhesion by peel pull of 2.0 N/15 mm using ASTM D1876. Food-contact compliance for the polyethylene food-contact layer follows 21 CFR 176.170(c) and Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² under OM2 test conditions.
A process conflict at 190 °C governs silane-grafted carrier masterbatches used in low-smoke zero-halogen cable sheathing. In the initial compounding step, GI-3526-A is loaded at 65 wt% with 25 wt% N-β-(aminoethyl)-γ-aminopropyltrimethoxysilane, 5 wt% polyethylene wax, and 5 wt% antioxidant/processing package on a twin-screw extruder with L/D 36:1 and low-shear distributive mixing elements. Barrel temperatures are held at 140–160 °C; melt temperature at the die is limited to 170 °C. The carrier batch is then metered at 3–5 phr into an EVA/PE compound containing 160 phr aluminum trihydrate and 40 phr magnesium dihydrate. The silane package modifies filler surfaces during compounding to reduce moisture uptake and improve tensile elongation of the LSZH jacket. The processing window is narrow. ATH begins releasing chemically bound water near 190 °C; localized shear heating in high-shear kneading zones above 185 °C generates steam-induced porosity, visible as pinholes and surface roughness on the extruded cable jacket. On a 75 mm twin-screw line, increasing screw speed from 350 rpm to 420 rpm without additional barrel cooling raised melt temperature by 8 °C and produced surface defects. The finished LSZH sheathing is assessed by IEC 60754-1 for halogen acid gas generation, IEC 60754-2 for pH and conductivity of evolved gases, IEC 60332-1 for single cable flame propagation, EN 50267-2-2 for acidity of effluent, and IEC 61034-2 for smoke density. Applications include control cables and data cables installed in buildings.
Blown film lines running three-layer LLDPE/LDPE laminations require a silica/amide masterbatch whose coefficient-of-friction response is stable after 24 h aging at 23 °C. A typical formulation combines 10–15 wt% erucamide, 15–25 wt% synthetic amorphous silica, 60–75 wt% GI-3526-A, and 0.5–1.0 wt% ethylene-bis-stearamide dispersant. The masterbatch is compounded on a co-rotating twin-screw extruder at 170–200 °C; screw speed is set at 400–500 rpm to deagglomerate silica into the 4–6 µm range without causing carrier degradation. Silica moisture content is held below 0.5 wt% before compounding; if ambient relative humidity exceeds 60%, the silica is pre-dried at 90 °C for 2 h. The concentrate is metered at 2–4 wt% into the skin layers of a three-layer blown film die with gap 1.8 mm, blow-up ratio 2.2:1–2.8:1, and frost-line height 600–900 mm. Erucamide migrates to the film surface within 24–48 h; coefficient of friction measured by ASTM D1894 on film surfaces after 24 h aging is 0.15–0.25 for the treated surface. Haze measured by ASTM D1003 at 50 µm film thickness is 4–6%. Food-contact compliance relies on 21 CFR 177.1520 for the polyolefin matrix and 21 CFR 178.3860 for the fatty acid amide slip agent. Films are used for form-fill-seal laminations, heavy-duty sacks, and printable packaging.
| Masterbatch type | Carrier content | Active loading | Let-down ratio | Melt temperature | Key test method |
|---|---|---|---|---|---|
| Carbon black concentrate | 55–60 wt% | 40 wt% carbon black | 5–7 wt% | 210–230 °C | ISO 18553 |
| TiO₂ white concentrate | 20–30 wt% | 65–70 wt% TiO₂ | 8–12 wt% | 180–230 °C | ISO 2471 |
| Slip/antiblock concentrate | 60–75 wt% | 25–30 wt% silica/amide | 2–4 wt% | 170–200 °C | ASTM D1894 |
When the carrier resin is let down into HDPE closure compounds at 2–4 wt%, the viscosity differential between the 20 g/10 min carrier and a 4 g/10 min host resin shifts the plastication profile in injection molding. A color concentrate for tamper-evident beverage closures is compounded with 30–40 wt% organic pigment, 55–65 wt% GI-3526-A, 3–5 wt% polyethylene wax, and 0.2–0.5 wt% zinc stearate. Twin-screw compounding is carried out at 180–220 °C with L/D 32:1; the high-flow carrier lowers melt viscosity and improves pigment wetting but may reduce melt residence time in the injection screw. On accumulator-head machines with clamp force 250–400 t and hot-runner valve gates, back pressure is maintained at 0.5–0.8 MPa to prevent streaking in thick hoop sections. Lower back pressure produces visible pigment striations in closure walls. Food-contact closures are tested for overall migration under Regulation (EU) No 10/2011 with a limit of ≤10 mg/dm² and for organoleptic transfer using sensory panel procedures referenced in ASTM E2609. Cap torque retention after 24 h at 23 °C is evaluated by ASTM D3470. End products include pigmented screw caps and flip-top hinges for food and cosmetic bottles.
Pressure pipe formulations based on PE100 and carbon black rely on masterbatch dispersion at ISO 18553 rating ≤3 because undispersed carbon black agglomerates act as crack-initiation sites under slow crack growth. A pipe-grade black masterbatch is produced with 40 wt% high-structure furnace black, 55–58 wt% GI-3526-A, 1.0–2.0 wt% polyethylene wax, and 0.2–0.4 wt% calcium stearate. Compounding takes place on a 44:1 L/D twin-screw extruder with melt temperature 190–220 °C and vacuum venting at -0.08 MPa. Let-down into PE100 pipe resin at 6.0–7.5 wt% yields 2.2–2.5 wt% carbon black in the finished compound. Because carrier melt flow index is 20 g/10 min, the blend at 6 wt% addition lowers PE100 melt strength slightly; pipe extrusion lines compensate with barrel temperatures 180–220 °C and reduced draw-down tension. Finished HDPE water pipe is tested for long-term hydrostatic strength by ISO 9080, with design stress specified in ISO 4427-1. Carbon black dispersion in the extruded pipe is evaluated by ISO 18553; additional weathering assessment conforms to ISO 4892-2 for UV exposure. Published data for GI-3526-A in PE100 pipe applications is limited; formulators rely on extrusion trials to qualify the carrier for specific pipe grades.
Competitive NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin is a linear low density polyethylene carrier resin manufactured for masterbatch and compounding operations. The product is pelletized and is characterized by a nominal density of 0.935 g/cm³ under ASTM D792-20 and a melt index of 2.6 g/10 min at 190°C and 2.16 kg load under ASTM D1238-20. These values place the grade in the medium-density segment of LLDPE, above conventional film carriers near 0.918–0.922 g/cm³ and below rotomolding or compounding grades near 0.940 g/cm³. In masterbatch service the carrier is usually introduced into end products at 2–8 wt%, meaning the carrier’s rheology, crystallinity, and antioxidant package influence final part performance. The grade is designed for letdown in polyolefin processing lines, not as a stand-alone performance resin for mechanically critical parts. Because polymer datasheets are product-version and site-specific, the values stated here are representative and must be checked against the current certificate of analysis.
The product may be classified as a masterbatch resin rather than a general-purpose extrusion grade because its additive package is adjusted for repeated heat histories. In masterbatch compounding, the resin is first melted to wet pigment surfaces, then pelletized, then melted again during letdown in injection molding, blow molding, film extrusion, or profile extrusion. Each heat cycle adds oxidative stress. A carrier resin with insufficient stabilisation can develop yellowness index drift under ASTM E313-20; therefore, the grade is specified with an antioxidant package that is verified by lot release. The density of 0.935 g/cm³ also gives higher crystallinity than LLDPE film carriers, producing harder pellets that resist blocking during railcar unloading and silo storage. In high-temperature silos, pellet blocking remains possible above 50°C, and pellet cooling before packaging is standard.
The melt index of 2.6 g/10 min is a single-point capillary flow measurement under ASTM D1238-20; it does not provide a full viscosity curve. In a co-rotating twin-screw extruder with a 40:1 L/D barrel and screw diameter from 40 mm to 70 mm, shear heating and screw fill ratio determine actual melt temperature. Barrel temperatures are commonly set at 180–210°C in the feed zone and 220–240°C downstream for color masterbatches. The melting peak of a 0.935 g/cm³ LLDPE is normally near 124–127°C by differential scanning calorimetry under ASTM D3418-21, allowing a broad melt-temperature window. However, the practical upper temperature limit is constrained by pigment degradation and antioxidant depletion rather than the resin melting point. At die-head temperatures above 240°C, organic pigments can shade drift, and above 260°C oxidative gel formation may occur in stagnation zones. The grade is not hygroscopic, but storage in humid air above 60% RH can deposit surface moisture; a desiccant hopper set at 75–80°C for 2 h removes condensation and stabilizes gravimetric feed. Pellet bridging in loss-in-weight hoppers is a common production failure when bulk density shifts, and it is controlled by pellet geometry and surface moisture rather than resin density alone.
Carrier resin selection for masterbatch uses viscosity matching with the diluting resin. A melt-index difference above ±1.0 g/10 min between carrier and base resin can contribute to laminar flow segregation in thin-wall injection molded parts. When GI-3526-A is diluted at 5 wt% in a 0.918 g/cm³ film LLDPE, the density differential is approximately 0.017 g/cm³; this is below the typical level for melt phase separation but may still affect optical properties. Melt filtration on a single-screw extruder equipped with a 100-mesh screen pack detects gel defects above 100 µm; medium-flow carriers frequently show lower gel counts than fractional-melt carriers in this test because the higher flow assists dispersion, although high-melt-strength fractions can elongate into visible streaks under certain letdown conditions.
Rheological characterization for incoming lots is often limited to melt index and density; however, process development groups may use capillary rheometry under ASTM D3835-16 to obtain shear viscosity at shear rates of 100–1000 s⁻¹. A Carreau-Yasuda fit allows comparison with other carriers. Typical shear viscosity at 230°C and 100 s⁻¹ for a 0.935 g/cm³ LLDPE may range from 800 Pa·s to 1200 Pa·s depending on molecular weight distribution; however, published data for this specific grade is limited and inline rheometer verification is recommended.
The table below summarizes representative physical properties for material selection. The values are typical and should not be interpreted as formal specification limits. Lot-specific certificates of analysis remain the controlling document for density and melt index. Extended mechanical and rheological characterization is not always published for masterbatch carrier grades; therefore, formal application development must use current manufacturer data and internal testing.
| Property | Test method | Unit | Representative value |
|---|---|---|---|
| Resin class | — | — | Linear low density polyethylene |
| Melt index | ASTM D1238-20 / ISO 1133-1:2022 | g/10 min | 2.6 |
| Density | ASTM D792-20 / ISO 1183-1:2019 | g/cm³ | 0.935 |
| Melting peak | ASTM D3418-21 | °C | 124–127 |
| Stabilisation | Manufacturer antioxidant package | — | Multiple-heat-history control |
| Form | — | — | Pellets |
Mechanical properties such as tensile yield stress under ASTM D638-22 or flexural modulus under ASTM D790-17 are not tabulated here because they depend on specimen preparation, conditioning, and letdown composition. For masterbatch producers who require pellet-handling consistency, bulk density is measured under ASTM D1895-17; pellet geometry is controlled within manufacturer packaging and transport specifications. Batch-to-batch melt-index variation is typically controlled within narrow in-plant limits, but the certificate of analysis should be checked when converting from a pilot line to a production-scale twin-screw line.
In pigment masterbatch production on a 40:1 L/D co-rotating twin-screw extruder, the carrier is the continuous phase into which carbon black or inorganic pigments are dispersed. Carbon black at 40–50 wt% loading creates a high-viscosity compound, particularly when using high-structure pigments with oil absorption above 120 mL/100 g under ASTM D2414-19. The medium melt index of GI-3526-A provides a wider torque-limited throughput window than fractional-melt film carriers. On a 12-barrel extruder, side-feeding carbon black at barrel 5 after the first kneading block reduces heat history and permits higher filler intake. Vacuum venting at barrel 9 removes moisture and volatiles; if vent foaming occurs, the fill ratio may be too high or the melt index may be insufficient for the set throughput. A pressure rise above 80 bar at the screen changer during a 45 wt% carbon black run typically indicates agglomerate accumulation, and continued operation without screen replacement will transfer contamination to the pelletizer. Specific mechanical energy is typically observed between 0.16 kWh/kg and 0.24 kWh/kg in such operations, depending on screw design and pigment surface area.
Additive masterbatches present a different viscosity response. Erucamide slip agents at 5–10 wt% plasticize the melt and reduce strand integrity; carriers with melt index above 8 g/10 min frequently generate thin strands that break under a water-bath haul-off. The melt index of 2.6 g/10 min typically preserves strand integrity while still allowing the high-shear dispersion needed for fine pigment particle size. Underwater pelletizing with die-hole diameters of 2.5–3.5 mm and water temperatures of 25–40°C is compatible with this viscosity class, although die-hole pressure and pellet shape must be optimized for the specific masterbatch formulation.
The carrier's density contribution becomes measurable in the final part at letdown ratios of 8 wt%. For an injection molding compound based on a 0.918 g/cm³ polyethylene, a 0.935 g/cm³ carrier introduces higher crystallinity and reduces the softening effect of the masterbatch. Flexural modulus under ASTM D790-17 is therefore affected less than with a lower-density carrier. In blown film, the effect is reversed: the higher-density carrier may raise haze in 50 µm film tested under ASTM D1003-21 when the base film resin is a low-density LLDPE. For that reason, the grade is positioned for compounds, injection molding, and masterbatches where pellet hardness and stiffness retention matter more than film optics.
| Carrier type | Typical melt index (190°C/2.16 kg) | Typical density (g/cm³) | Operational difference |
|---|---|---|---|
| Novapol GI-3526-A LLDPE | 2.6 | 0.935 | Medium-viscosity carrier; balanced strand integrity, pellet hardness, and stiffness retention. |
| Butene-based film LLDPE | 1.0–2.0 | 0.918–0.922 | Lower stiffness contribution; may wet pigments at lower shear but has lower pellet hardness. |
| High-flow LDPE | 4.0–8.0 | 0.918–0.924 | Easier filler wetting at high loadings; lower melt strength and thermal stability. |
| EVA carrier | 6–60 | 0.940–0.960 | Greater polar adhesion to pigments; potential odor, hygroscopicity, and food-contact constraints. |
Because the grade is stabilised for multiple heat histories, it differs from general-purpose injection molding LLDPE in antioxidant loading as well as melt index and density. General-purpose resins may carry minimal stabilisation because they are expected to experience one heat history; masterbatch carriers must withstand compounding, storage, and final letdown. Oxidation induction time can be assessed under ASTM D3895-19 or ISO 11357-6:2018. In food-contact applications, the final compound—not the neat carrier—must comply with 21 CFR 177.1520 in the United States or Commission Regulation (EU) No 10/2011 in the European Union. Overall migration testing under EU 10/2011 must include the carrier contribution, because migration kinetics of low molecular weight fractions depend on molecular weight distribution, comonomer type, and use conditions.
Conductive masterbatches represent an operational boundary where the carrier itself is not conductive. Volume resistivity under ASTM D4496-21e1 and surface resistivity under ASTM D257-14 are controlled by the carbon black network. A 45 wt% carbon black masterbatch made with GI-3526-A requires letdown to a final carbon black concentration above the percolation threshold of the selected pigment and matrix. Published data for this specific conductive configuration is limited; pilot-line resistivity mapping is required before production release.
At production scale, the most common failure is feeder bridging caused by pellet geometry variations after long silo residence. Neat pellets may be stored under standard polyolefin warehouse conditions, but hot storage above 40°C can increase pellet blocking in bulk containers. Before shutdown, the extruder should be purged with polyethylene and the barrel should not be left at processing temperature above 200°C for more than 30 min, because stagnation zones can generate gel particles. Shared equipment that previously processed polycarbonate or polyamide must be thoroughly purged to avoid black-spec defects. The resin should not be stored or dry-blended with peroxide or pro-oxidant masterbatches, because free radicals can degrade the antioxidant package and drift the melt index. For compounding plants producing high-opacity injection molding masterbatches at 40–50 wt% carbon black, the selection of GI-3526-A is governed by torque-limited throughput, screen-pack pressure control, and final-part stiffness retention rather than film optics or high-flow wetting alone.