Nova Chemicals Novapol Gf 0218 F Butene Lldpe Masterbatch Resin

NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin

    • Product Name: NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 670906
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Melt Index 190 C 2 16 Kg 2.0 g/10 min
    Density 0.918 g/cm³
    Melting Point 120 °C
    Vicat Softening Point 98 °C
    Brittleness Temperature -70 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 27.6 MPa
    Elongation At Break 700%
    Flexural Modulus 207 MPa
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 10%
    Gloss 45 60%
    Coefficient Of Friction 0.2
    Form Pellets
    Color Natural

    As an accredited NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin is supplied in 25 kg polyethylene bags, typically 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) Container Loading (20′ FCL): NOVA Novapol GF-0218-F Butene LLDPE masterbatch resin, 25 kg bags, palletized, shrink-wrapped, secured, weight-compliant.
    Shipping NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin is shipped as solid pellets in 25 kg bags, octabins, or bulk trucks/railcars. Transport in dry, clean vehicles at ambient temperatures. Typically non-hazardous under normal conditions; keep away from heat, ignition, and moisture, and follow SDS and applicable regulations.
    Storage Store Novapol® GF-0218-F Butene LLDPE Masterbatch Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed, protect from moisture and contamination, and avoid strong oxidizers. Use first-in, first-out stock rotation; maintain good housekeeping and follow manufacturer/SDS guidance. Inspect containers regularly for damage or leaks. Store away from acids, bases, and incompatible materials.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in a cool, dry, well-ventilated area in original packaging.
    Application of NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin

    In color masterbatch production for thin-gauge blown polyethylene film, GF-0218-F operates as the carrier phase in pigment concentrates where butene-copolymer short-chain branching contributes to low-temperature melt elongation while the nominal melt flow rate of 2.0 g/10 min (190 °C / 2.16 kg, ASTM D1238-20) and density of 0.918 g/cm³ (ASTM D792-20) set the dilution viscosity range for downstream let-down. A representative titanium dioxide white masterbatch consists of 45–55 wt% rutile titanium dioxide, 6–12 wt% low-density polyethylene wax, 0.5–1.5 wt% calcium stearate, and the balance GF-0218-F. The addition ratio in final film is 2–6 wt% for high-opacity refuse sacks and 3–8 wt% for agricultural silage wrap; below 2 wt%, tinting-strength differences across reel lengths exceeding 2,000 m can exceed ΔE CMC 1.0, while above 8 wt% the viscosity mismatch between carrier and film skin layers can produce visible melt-flow lines on bubble surfaces. Compounding is carried out on co-rotating twin-screw extruders with L/D 36:1 to 44:1, screw diameters 50–92 mm, side-fed pigment at 170–200 °C, vent vacuum of −0.06 to −0.09 MPa, and melt filtration through 150–200 µm mesh packs. In blown film let-down, die gap 1.8–2.2 mm, blow-up ratio 2.2:1–2.8:1, melt temperature 195–225 °C, and cooling air at 8–15 °C are typical on three-layer lines. Compliance status for food-contact uses follows FDA 21 CFR §177.1520(c) for olefin polymers when the pigment system itself complies; EU Regulation (EU) No 10/2011 Annex I and REACH (EC) No 1907/2006 Annex XVII constrain heavy metals and primary aromatic amines; RoHS 2011/65/EU Annex II applies to packaging inserts for electrical and electronic equipment. Terminal finished articles include colored garbage bags, can liners, frozen-food bulk liners, industrial sacks, and silage wrap. Pre-drying of GF-0218-F is not required below 60% relative humidity; above this threshold, pigment and wax charges are pre-dried separately at 70–80 °C for 2 h to avoid hydrolytic vent-port fouling. Dispersion relies on wax and metal stearate wetting rather than polar interactions because the carrier has a non-polar hydrocarbon backbone, which is why melt temperature, shear rate, and residence-time distribution on the twin-screw line are the controlling parameters for pigment agglomerate breakdown.

    What Limits Let-Down Uniformity in Three-Layer Greenhouse Film Additive Masterbatches?

    Additive masterbatches for three-layer agricultural greenhouse film typically incorporate 10–20 wt% hindered amine light stabilizer, 5–10 wt% secondary antioxidant, and 5–15 wt% anti-drip ethoxylated sorbitan ester in GF-0218-F. The final addition ratio in the middle layer is 5–12 wt%, yielding 0.5–2.0 wt% active HALS in the total structure; skin layers separately contain 2–5 wt% of a UV-absorber masterbatch to reduce surface chalking. The downstream process is a three-layer blown film line with barrier screws, die diameter 250–400 mm, die gap 2.0–2.4 mm, blow-up ratio 2.5:1–3.2:1, and haul-off speed 40–90 m/min. Middle-layer melt temperature is held at 185–215 °C; below 185 °C the carrier phase does not fully homogenize with LDPE/LLDPE skin layers, while above 215 °C low-molecular-weight anti-drip additives migrate to the die lip and form brittle deposits within 8–24 h of continuous operation. Outdoor weathering is assessed under ISO 4892-2:2013, tensile properties under ISO 527-3:2018, dart impact under ISO 7765-1:1988, and tear propagation under ISO 6383-2:1983. Terminal products include three-season greenhouse covers, low tunnel films, mulch films, and silage pit covers. Published data for long-term HALS migration from GF-0218-F-containing film under condensation cycling is limited; film processors therefore validate anti-drip persistence by 1,200 h of artificial weathering and field trials in high-humidity tunnels before full-scale supply. The failure mode most commonly observed on commercial lines is not haze generation but die-lip deposit accumulation, which forces line stoppages and reduces the effective operating window of the middle-layer extruder.

    When Calcium Carbonate Filler Masterbatch Is Melt-Blended with Post-Consumer Recyclate for Injection-Grade Compounds

    Filler masterbatches based on 70–80 wt% surface-coated calcium carbonate use GF-0218-F as the carrier and are let down at 10–25 wt% into washed post-consumer LLDPE/LDPE. Below 10 wt%, flexural modulus improvement under ISO 178:2019 is normally less than 8%; above 25 wt%, the compound melt flow rate can fall below 0.8 g/10 min (ISO 1133-1:2022), making thin-wall mould filling unreliable without raising melt temperature. Compounding uses a co-rotating twin-screw extruder with L/D 40:1, side feeding at 200–220 °C, screw speed 350–550 rpm, and a gear pump before a slide-plate screen changer fitted with 150–250 µm screens. The granulate is then injection moulded on machines with clamp force 800–1,500 tonnes, melt temperature 190–220 °C, and mould temperature 20–40 °C. Tensile yield stress is measured per ISO 527-2:2012, flexural modulus per ISO 178:2019, Charpy notched impact per ISO 179-1:2010, and density per ISO 1183-1:2019. Applicable regulatory limits are defined in REACH (EC) No 1907/2006 Annex XVII and RoHS 2011/65/EU Annex II for electronic packaging items; the base olefin may be used under FDA 21 CFR §177.1520(c) when the recyclate stream meets food-contact quality requirements. Terminal products include distribution pallets, rigid bins, dunnage trays, automotive wheel arch liners, and household crates. The dominant process conflict on commercial compounding lines is screen-pack pressure rise caused by coarse filler particles above 20 µm top-cut; this is aggravated by side-feeder output surges and is monitored by differential pressure across the screen changer rather than by melt temperature alone.

    For rotational molding lines producing hollow polyethylene tanks, GF-0218-F is dry-blended with 35-mesh polyethylene powder as a color concentrate at 1–4 wt%. The dry blend is tumbled for 20–30 min to reduce static segregation; electrostatic pinning can otherwise produce local pigment concentration differences visible as swirl marks on the inner surface. The rotational moulding oven is operated at 260–300 °C with cycle times of 18–30 min, and the biaxial rotation ratio is set at 4:1. Finished-part tensile strength is tested per ISO 527-2:2012, low-temperature impact per ISO 179-1:2010, and melt flow rate of the powder compound per ISO 1133-1:2022. Compliance for food and water contact follows FDA 21 CFR §177.1520 and EU Regulation (EU) No 10/2011 when the pigment package is compliant. Terminal products include chemical storage tanks, agricultural sprayer tanks, insulated containers, and playground components. Published data for GF-0218-F in rotomolding-specific dry blends is limited; particle-size distribution and bulk density matching are therefore verified on each lot to prevent the carrier-rich fines fraction from concentrating in corners during low-shear oven fusion.

    Cling and Slip Modification in Cast Stretch Film Requires Controlled Migration Kinetics

    In high-speed cast stretch film production, a cling masterbatch containing 20–40 wt% polyisobutylene or glycerol ester and 1–3 wt% erucamide slip agent in GF-0218-F is added at 1.5–4 wt% to the core layer of a five-layer cast stretch film. The downstream process extrudes through flat dies with die gap 0.4–0.8 mm, melt temperature 210–240 °C, chill roll temperature 20–30 °C, and line speed 300–600 m/min. Film properties are tested under ASTM D1894-14 for coefficient of friction, ASTM D5748-19 for puncture propagation resistance, ISO 527-3:2018 for tensile properties, and ISO 7765-1:1988 for dart impact. Addition above 4 wt% causes blocking after roll storage above 40 °C, while below 1.5 wt% cling force measured by ASTM D5458-95 falls below application-specific thresholds on high-slip polyethylene skin layers. Terminal products include pre-stretched pallet wrap, silage stretch film, and machine-film for automatic pallet wrappers. The critical operational boundary is migration time after winding; cling additives must reach the film surface within 24–72 h of storage without creating blocking between adjacent layers at the core radius, where roll compression is highest.

    Free Quote

    Competitive NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    NOVA Chemicals Novapol® GF-0218-F is a butene linear low-density polyethylene carrier resin supplied in pellet form. The grade is classified in the supplier’s product line as a masterbatch resin, meaning the base polymer is intended for compounding with pigments, slip agents, antiblock additives, process aids, or mineral fillers; it does not contain a pre-dispersed additive package. The melt mass-flow rate determined by ISO 1133-1:2022 at 190 °C with a 2.16 kg load is 2.0 g/10 min, and the density determined by ISO 1183-1:2019 at 23 °C is 0.918 g/cm³. These values place the product between 1.0 g/10 min blown-film grades and 5.0 g/10 min injection molding carriers. In masterbatch compounding, the intermediate melt mass-flow rate provides a defined viscosity window for pigment wetting and finite melt strength during film letdown.

    Supplier-published typical property set for Novapol GF-0218-F
    Property Test method Value
    Melt mass-flow rate, 190 °C / 2.16 kg ISO 1133-1:2022 / ASTM D1238-20 2.0 g/10 min
    Density at 23 °C ISO 1183-1:2019 / ASTM D792-20 0.918 g/cm³
    Comonomer type Supplier designation Butene
    Physical form Visual inspection Pellets

    Full mechanical, optical, and rheological data are not reproduced in this document because the supplier’s published technical data sheet is the controlling reference for lot-specific results. Current lot-specific values should be obtained from the certificate of analysis. Published data for this specific configuration are limited beyond the typical melt mass-flow rate and density values stated above.

    How Does Butene Comonomer Distribution Affect Masterbatch Let-Down Ratios?

    The butene comonomer introduces short-chain branches along the linear polyethylene backbone. These branches reduce density and crystallinity relative to high-density homopolymer carriers, producing a lower seal initiation temperature and lower modulus. In masterbatch compounding, the combined effect is a carrier melt that wets organic and inorganic particulates more readily than high-density polyethylene at the same melt mass-flow rate, while retaining greater toughness after solidification than a low-density homopolymer. Melt mass-flow rate remains the primary control for carrier viscosity; the 2.0 g/10 min value corresponds to lower viscosity than a 1.0 g/10 min film grade but higher viscosity than a 5.0 g/10 min linear carrier. This intermediate value permits higher pigment loadings on twin-screw equipment without the excessive melt temperature rise associated with low-MFR carriers.

    Letdown performance in downstream polyolefin film is not determined solely by carrier melt mass-flow rate. Final masterbatch particle size distribution, melt filter assembly, and draft ratio in the film line all interact. For formulations using 40 wt% to 70 wt% carbon black or titanium dioxide, the carrier resin should be evaluated for melt pressure stability, screen-pack pressure rise, and dispersion quality by optical microscopy according to ISO 18553:2002 or equivalent internal methods. Published data for GF-0218-F at a single universal letdown ratio are limited; therefore process capability should be established on the specific production line.

    On a co-rotating twin-screw extruder with an L/D ≥ 40:1, barrel set temperatures from 170 °C to 210 °C and die head temperatures from 190 °C to 220 °C are representative processing conditions for butene LLDPE carrier resins. The melt temperature should be verified by a downstream melt thermocouple; prolonged operation above 250 °C can accelerate oxidative chain scission and reduce the thermal stabilizer package. Pre-drying is not required when pellets are stored at ambient relative humidity below 60%; above that threshold, surface moisture can produce vent plugging, pellet porosity, and film defects. The resin should be purged from the extruder with a lower-viscosity polyolefin before shutdown to minimize long residence time in the die and adapters.

    When GF-0218-F Replaces LDPE Homopolymer in Masterbatch Carrier Formulations

    Low-density polyethylene homopolymer is produced in high-pressure autoclave or tubular reactors and contains long-chain branching, which provides strong shear thinning and high melt elasticity. GF-0218-F is a linear polyethylene with short-chain branches and no significant long-chain branching. The rheological consequence is that substitution of GF-0218-F for an LDPE carrier at equal melt mass-flow rate commonly raises melt pressure in the die and reduces melt strength in a blown film bubble. Blown film dies that previously ran LDPE carriers at a 1.0 mm die gap may require a 1.5 mm to 2.5 mm gap when the LLDPE carrier is used at high concentration to limit melt fracture.

    Tensile properties measured by ISO 527-3:2018 on 25 µm film will not be identical to LDPE. The linear butene backbone generally provides higher elongation at break and puncture resistance at equal density, while LDPE provides better clarity and easier drawdown in thin-gauge extrusion coating. The selection between carriers should be based on the end-use polymer matrix; GF-0218-F is more compatible with LLDPE-rich film formulations because the carrier and diluting resin share a similar backbone architecture. Ethylene-vinyl acetate carrier resins with vinyl acetate contents between 9 wt% and 28 wt% are polar and can wet many pigments more aggressively than nonpolar butene LLDPE. GF-0218-F contains no vinyl acetate comonomer, so it does not contribute acetic acid odor or corrosion potential during long-run compounding. This lower polarity is an operational advantage in polyolefin film letdown, but it limits wetting of unmodified polar pigments. For highly polar pigment systems, surface-treated pigments or a separate wetting agent should be considered.

    Compared with hexene LLDPE carriers at equal melt mass-flow rate and density, butene LLDPE typically shows lower dart impact strength measured under ASTM D1709-16a and lower Elmendorf tear strength measured under ASTM D1922-15 for 25 µm film. The difference is directional and not a universal specification; it arises because butene branches are shorter than hexene branches and are less effective at distributing stress in the amorphous phase. In optical-critical applications where haze below 5% at 25 µm is required under ASTM D1003-13, a metallocene-catalyzed hexene or octene LLDPE should be evaluated; GF-0218-F is a Ziegler-Natta butene product and is not represented as a high-clarity metallocene substitute. Published film data for this specific configuration are limited, and direct comparison on the intended film line is required.

    In cast film sealant layers, the lower density of 0.918 g/cm³ reduces seal initiation temperature relative to higher-density polyethylene grades. Seal initiation temperature measured by ASTM F2029-16 for film of 25 µm thickness is influenced by film cooling rate, additive bloom, and contamination on the seal bar. A butene LLDPE of this density class is often evaluated for form-fill-seal packaging where low seal initiation and adequate hot-tack strength are required. Hot-tack testing under ASTM F1921-12 on a machine-direction sealing apparatus is necessary to quantify the seal window; published data for GF-0218-F in this configuration are limited. The product should not be assumed to match the seal performance of a dedicated plastomer or ionomer sealant.

    In monolayer cast film on a 90 mm single-screw extruder with 30:1 L/D, melt temperatures of 220 °C to 240 °C and chill-roll temperatures of 15 °C to 30 °C are representative for butene LLDPE. The resin’s lower viscosity at 2.0 g/10 min permits moderate throughput but does not provide the melt strength of LDPE for thin-gauge drawdown below 15 µm. Coextrusion with an LDPE skin layer or blending with LDPE at 10 wt% to 30 wt% is often used to stabilize the melt curtain. These are standard processing observations for butene LLDPE; product-specific line data are not published in this document.

    What Limits the Upper Processing Temperature in Long-Residence-Time Compounding?

    Polyolefin thermal degradation is governed by both temperature and residence time. In air, polyethylene oxidation begins to generate carbonyl species near 200 °C, although melt processing is still feasible at 240 °C to 250 °C if residence time is short and the stabilizer package is intact. In long-residence-time compounding, the upper practical melt temperature for a butene LLDPE carrier is usually capped at 250 °C because oxidation products and crosslinked gels can form rapidly above this threshold. A melt temperature excursion to 260 °C with a hold time exceeding 5 min is a known processing risk for LLDPE carriers and may result in black specks, fisheyes, or screen-pack pressure rise. The extruder should be equipped with melt temperature and pressure sensors at the die and vent. If startup torque exceeds the drive limit, a lower-MFR purge grade should be used before introducing the product.

    For masterbatch operations with high loadings of temperature-sensitive organic pigments, the barrel profile should be set so that the pigment is exposed to temperatures above its decomposition threshold for less than 30 s. This requirement may conflict with the melt temperature needed for carrier viscosity; therefore feed sequencing and side-stuffing of pigments downstream of the melt seal should be used. The product’s published stabilizer composition is not disclosed in this document; the safety data sheet and technical data sheet remain the controlling references.

    Regulatory Documentation and Supply-Form Boundaries

    Compliance with food-contact, environmental, and electrical-equipment requirements depends on the final formulation and the masterbatch process. The following matrix identifies the applicable frameworks but does not constitute a supplier certification for this grade in a specific article.

    Applicable regulatory frameworks and verification boundaries
    Framework Reference Boundary
    United States food contact FDA 21 CFR 177.1520(c) Supplier certificate required for final article
    European Union food contact Regulation (EU) 10/2011 Migration testing required for final formulation
    REACH EC 1907/2006 SDS and SVHC status supplier-confirmed
    RoHS Directive 2011/65/EU Cadmium limit 100 ppm in homogeneous material; supplier certificate required

    The product is supplied as pellets; packaging configuration, lot numbering, and recommended storage conditions are defined in the supplier’s commercial documentation. Incoming resin should be sampled and tested for melt mass-flow rate according to ISO 1133-1:2022 or ASTM D1238-20 before large-scale masterbatch qualification, particularly if the material has been transferred through multiple warehouses or exposed to high ambient temperatures. Storage should avoid prolonged exposure to ultraviolet light and temperatures above 40 °C. Polyethylene pellets can accumulate electrostatic charge during conveying; grounding of silo and hopper equipment is required to avoid dust-cloud ignition. The pellets should not be exposed to open flame or hot surfaces above 300 °C. No forward-looking claim regarding end-use performance is made without lot-specific validation on the intended equipment.

    Top