    Specifications
    HS Code 251538
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Tensile Strength 120 MPa
    Elongation At Break 3%
    Flexural Modulus 8500 MPa
    Flexural Strength 180 MPa
    Notched Izod Impact Strength 8 kJ/m²
    Heat Deflection Temperature At 1 8 Mpa 200 °C
    Melting Point 225 °C
    Mold Shrinkage 0.3–0.8%
    Water Absorption 0.03%
    Flammability Rating UL94 HB

    As an accredited Nan Ya PBT+GF 1210G6 ANC1 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Nan Ya PBT+GF 1210G6 ANC1 is supplied in 25 kg moisture-proof paper sacks, palletized for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized bags of Nan Ya PBT+GF 1210G6 ANC1, evenly distributed, strapped, and secured for export.
    Shipping Nan Ya PBT+GF 1210G6 ANC1 is shipped as non-hazardous thermoplastic resin pellets, typically in moisture-proof 25 kg bags or octabins, palletized and stretch-wrapped. Keep dry, cool, and protected from sunlight; avoid moisture pickup and physical damage during transport.
    Storage Store Nan Ya PBT+GF 1210G6 ANC1 in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and ignition sources. Keep in original sealed, labeled packaging to prevent contamination and moisture pickup. Maintain stable temperature and low humidity; follow FIFO. Use appropriate spill containment and keep containers closed when not in use.
    Shelf Life For Nan Ya PBT+GF 1210G6 ANC1, shelf life is about 12 months in original sealed packaging, stored dry, cool, and protected from sunlight.
    Free Quote

    Competitive Nan Ya PBT+GF 1210G6 ANC1 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Nan Ya Plastics Corporation supplies PBT+GF 1210G6 ANC1 as a glass-fiber reinforced polybutylene terephthalate injection-molding compound. The designation places the product within the 1210 PBT series; the G6 suffix indicates a nominal glass-fiber loading of 30 wt%, and the ANC1 suffix is a manufacturer-controlled lot, colour, or stabilization identifier that must be read from the batch certificate rather than treated as a general property descriptor. The material is supplied in pellet form for drying and injection molding and is specified where unfilled PBT lacks short-term stiffness, creep resistance, and dimensional stability under load.

    Representative data in this document are class ranges for a 30% glass-reinforced PBT; the lot-specific certificate of analysis for PBT+GF 1210G6 ANC1 controls the exact values. Published third-party data for the ANC1 identifier is limited, and critical applications should be validated with first-article testing under the relevant standards.

    PropertyStandard methodRepresentative range for 30% glass-reinforced PBT class
    DensityISO 1183-1 / ASTM D7921.53–1.60 g/cm³
    Tensile strength at breakISO 527-1/-2120–140 MPa
    Tensile modulusISO 527-1/-28,500–11,000 MPa
    Flexural strengthISO 178190–220 MPa
    Flexural modulusISO 1788,000–10,000 MPa
    Notched Izod, 23 °CISO 180/A8–12 kJ/m²
    Heat deflection temperature, 1.82 MPaISO 75-1/-2200–220 °C
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-1:202210–25 cm³/10 min
    Mold shrinkage, flow directionISO 294-40.2–0.5 %

    What separates a G6 ANC1 variant from unfilled and lower-glass PBT compounds?

    Compared with unfilled PBT, the 30 wt% glass reinforcement in 1210G6 ANC1 raises flexural modulus from 2,300–2,800 MPa to 8,000–10,000 MPa when measured to ISO 178. Heat deflection temperature under ISO 75-1/-2 at 1.82 MPa rises from approximately 50–60 °C to 200–220 °C, while mold shrinkage in the flow direction under ISO 294-4 drops from 1.5–2.0% to 0.2–0.5%. This is accompanied by a loss in tensile elongation at break from 10–30% to 2–3%, making the material far less ductile than unfilled PBT in snap-fit and living-hinge features.

    Against a 15% glass PBT grade, the G6 variant typically adds 60–80% flexural modulus and improves creep resistance, but the higher glass content increases melt viscosity and reduces weld-line strength in complex parts. In unfavourable gate locations, tensile strength at a knit line can fall by 20–40% relative to the bulk flow-direction value. Against a 45% glass PBT, the G6 has lower stiffness and heat deflection temperature, but its melt viscosity is lower, thin-wall filling at nominal walls of 0.8–1.2 mm is more consistent, and screw, barrel, and check-ring abrasion are reduced.

    Glass-fiber orientation also introduces anisotropy. Flow-direction tensile modulus may exceed transverse-direction modulus by 30–50% depending on gate type and packing. Unfilled PBT does not show this orientation-dependent modulus split to the same magnitude, which is a critical difference for parts designed with finite-element assumptions based on isotropic material properties.

    Drying and injection-molding parameter bands: specific control limits

    PBT is a polyester, and hydrolytic degradation at processing temperatures is the primary processing risk for 1210G6 ANC1. The compound is dried in a desiccant-bed dryer to a residual moisture level of ≤0.02 wt%. Drying temperature is held at 120–130 °C for 4–6 h from sealed packaging. The dryer deliver-air dew point is maintained at ≤ −40 °C, and the return-air temperature is kept below 80 °C to avoid thermal cycling of the desiccant bed. Hot-air tray drying alone is not reliable for this grade because shallow-bed depth is required; material beds in tray dryers should not exceed 3–5 cm to limit moisture variability between top and bottom pellets.

    In high-humidity production environments above 60% RH, pre-dried pellets are transferred from the dryer to the injection-molding machine hopper through closed conveying lines purged with dry air. Open containers left for more than 1 h can recover 0.01–0.02 wt% moisture and produce splay, silver streaking, and embrittled parts. Moisture-induced hydrolysis is particularly severe at nozzle melt temperatures above 270 °C, where tensile strength and Izod impact can drop substantially before visual surface defects appear.

    Melt temperature measured at the nozzle is maintained at 240–270 °C. Short excursions above 270 °C are tolerated only for residence times below 5 min; longer residence produces polymer degradation and black specks. Mold surface temperature is controlled at 60–100 °C using a pressurized-water thermolator or electric cartridge regulation. The lower portion of this mold-temperature band improves cycle time, while the upper portion promotes crystallinity, surface gloss, and dimensional stability after annealing. Mold temperatures above 100 °C can be used experimentally for high-heat applications but usually extend cycle time and increase ejection challenges.

    Injection speed is set in the medium-to-high range, typically 100–250 mm/s screw linear velocity, to avoid premature solidification in thin-walled sections. Peak cavity pressure measured with in-mold transducers is commonly controlled between 30–50 MPa. Hold pressure is transitioned from injection pressure at a screw-position-based velocity/pressure switchover, and hold time is set based on gate freeze rather than part cooling alone. Back pressure is kept at 0.2–0.5 MPa hydraulic; excessive back pressure raises melt temperature and breaks fiber length, reducing flexural modulus by 10–25% in overcooked material. The screw and barrel are wear-resistant bimetallic or nitrided types, with a screw L/D of 20:1–25:1 and a compression ratio of 2:1–2.5:1. The check ring is selected for glass-fiber abrasion and replaced on a preventive schedule because leakage across the check ring causes shot-weight drift and inconsistent packing.

    ParameterRecommended bandEquipment/control
    Drying temperature120–130 °CDesiccant-bed dryer
    Drying time4–6 hSealed hopper/loader
    Residual moisture≤0.02 wt%ISO 15512 Karl Fischer
    Melt temperature at nozzle240–270 °CMelt probe/IR
    Mold surface temperature60–100 °CPressurized-water thermolator
    Injection linear velocity100–250 mm/sScrew-velocity transducer
    Hydraulic back pressure0.2–0.5 MPaMachine setting
    Screw L/D20:1–25:1Bimetallic or nitrided barrel

    Field experience on production molding lines shows that hot-runner systems with poorly balanced manifolds can create glass-fiber accumulation at the gate and surface streaks. Valve-gate systems with gate-land lengths of 0.8–1.2 mm generally produce less fiber skinning than open-edge gates in this material class. Cold-runner systems benefit from generous runner diameters to avoid frozen-layer effects because the filled melt is shear-sensitive and can solidify quickly in small-channel delivery systems.

    When elevated temperature and dimensional tolerance govern connector and housing design

    PBT+GF 1210G6 ANC1 is used in electrical connector bodies, relay bases, automotive sensor housings, cooling-fan impellers, and appliance structural components where dimensional tolerance, creep resistance, and short-term thermal stability are decisive. In board-level connectors exposed to solder reflow, the part surface may see 240–250 °C for 15–30 s; this exposure is near the heat deflection temperature measured at 1.82 MPa, so solder-process qualification is required. HDT alone does not guarantee reflow survival because the part is not uniformly loaded during reflow.

    In underhood sensor and housing applications, the material is typically evaluated for long-term thermal stability using UL 746B relative thermal index listings or OEM-specific aging programs. Creep resistance is assessed by ISO 899-1 under sustained tensile flexure or compressive load. The dimensional stability advantage of the glass-filled grade is useful in multi-pin connector pitch, but tool compensation must account for anisotropic shrinkage. Glass-filled PBT molded parts often show differential post-mold shrinkage between flow and transverse directions; parts should be measured after 24–48 h at 23 °C and after annealing where assembly temperatures exceed 100 °C.

    The material is not recommended for continuous exposure to steam or hot water above 80 °C, hot concentrated acids, alkaline aqueous solutions at elevated temperature, or long-term outdoor ultraviolet exposure without a UV-stabilized or painted version. Chemical compatibility for stressed parts exposed to automotive engine oils, brake fluids, or coolants is determined by ISO 22088-2 or OEM-specific immersion testing. Glass-reinforced PBT beneath high stress can fail by moisture-assisted degradation at sharp corners and weld lines, so stress-concentration features should be verified with actual chemical exposure rather than generic PBT compatibility tables.

    Electrical performance values such as volume resistivity, surface resistivity, dielectric strength, and comparative tracking index are colorant- and wall-thickness-dependent. Compliance statements and flammability classification are taken from the grade-specific supplier certificate and UL Yellow Card under UL 94. Regulatory evaluation includes RoHS 2011/65/EU and REACH 1907/2006, but the ANC1 suffix alone does not establish a flame-retardant rating or a specific electrical CTI value. Applications involving exposed electrical terminals under glow-wire conditions are tested to IEC 60695-2-12 on the final molded part thickness, not on the granulate alone.