| HS Code | 138837 |
| Material | Polybutylene terephthalate (PBT), flame retardant, glass fiber reinforced |
| Glass Fiber Content | 30% |
| Flame Retardancy | Halogen-free flame retardant |
| Ul 94 Flammability Rating | V-0 |
| Density | 1.58 g/cm³ |
| Tensile Strength | 110 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 9500 MPa |
| Notched Izod Impact Strength | 7 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | 205 °C |
| Melting Temperature | 225 °C |
| Mold Shrinkage | 0.2–0.5% |
| Water Absorption | 0.06% |
| Volume Resistivity | 1E16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
As an accredited Nan Ya PBT-FR 140PG6 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-barrier bags, palletized, and labeled with product identification, lot number, and safety handling information. |
| Container Loading (20′ FCL) | 20′ FCL loading of Nan Ya PBT-FR 140PG6 flame-retardant PBT resin in 25 kg bags, palletized, shrink-wrapped, and securely stowed. |
| Shipping | Nan Ya PBT-FR 140PG6 ships as flame-retardant polybutylene terephthalate resin pellets, typically in sealed moisture-barrier 25 kg bags or bulk containers. Store dry, away from heat and sunlight. Unless the supplier’s SDS states otherwise, it is not regulated as dangerous goods for transport. Use standard freight handling. |
| Storage | Store Nan Ya PBT-FR 140PG6 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and ignition sources. Keep containers tightly closed in original packaging; protect from moisture, dust, and physical damage. Separate from strong oxidizers and incompatible chemicals. Store only in approved, labeled containers. Follow the manufacturer’s SDS, local regulations, and first-in, first-out stock rotation. |
| Shelf Life | Nan Ya PBT-FR 140PG6 typically has a 24-month shelf life when stored dry, below 30 °C, in its original sealed packaging. |
Competitive Nan Ya PBT-FR 140PG6 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Nan Ya PBT-FR 140PG6 is a flame-retardant polybutylene terephthalate compound reinforced with a nominal 30 mass% of short glass fibre. The grade is supplied for injection-moulded electrical and electronic components where dimensional stability, mechanical stiffness, and a thickness-dependent UL 94 V-0 flammability classification are design inputs. In the supplier’s nomenclature, the G6 marker identifies the glass-fibre loading, and the FR marker separates this product from the non-flame-retardant PBT 140PG6. The base polymer is an aromatic polyester derived from 1,4-butanediol and terephthalic acid; the glass reinforcement raises tensile modulus and heat deflection temperature but introduces anisotropic mould shrinkage and lowers notched impact compared with the unreinforced matrix. The compound is normally supplied as pellets and is processed on conventional injection-moulding equipment used for glass-filled polyesters, provided the flame-retardant package is not exposed to excessive moisture, shear, or residence time. The grade is not a general-purpose PBT; it is specified when the end product must satisfy flammability requirements without sacrificing the creep resistance and reduced thermal expansion contributed by the glass fibre.
Because the ester linkages in PBT undergo hydrolysis at melt-processing temperatures, residual moisture is the primary process variable. The pellets are dried in a desiccant dryer at 120–130°C for 4 h until the moisture content falls below 0.02 wt%; the dryer dew point should be −40°C or lower and the airflow should be 0.5–1.0 m³/h per kg/h of material throughput. At ambient relative humidity above 60% RH, open hopper residence is limited to 30–60 min unless closed-loop dry-air conveying is used. If the residual moisture specification is not met, moulded parts show splay, silver streaks, gate-area delamination, and a measurable loss in molecular weight. Production-scale moulding trials on electrical housings have shown that wet pellets can reduce notched Izod impact by more than 15% because hydrolysis cleaves the polymer backbone before the fibre-matrix interface can transfer load. Unopened bags stored at 10–30°C in a dry area retain processability for at least 12 months; opened bags should be re-dried if exposed to ambient air for more than 4 h. The crystalline melting point of the PBT matrix is 223–225°C by ISO 11357-3; processing temperatures are therefore set above this value but below the decomposition threshold of the flame-retardant system.
Melt temperature is maintained at 245–265°C, with a default of 255°C; the upper limit is controlled less by the PBT matrix than by the thermal stability of the flame-retardant package. Barrel profiles from feed to nozzle are typically 240°C, 250°C, 255°C, and 255°C. Mould temperature is held at 80–100°C; below 80°C the part cools before reaching full crystallinity, producing post-mould shrinkage, gloss variation, and lower heat deflection temperature, while above 100°C cycle time increases without a proportional gain in crystallinity. A screw with compression ratio 2.0:1–2.5:1, a free-flow check ring, and bimetallic screw/barrel construction is recommended for glass-fibre abrasion. Back pressure is set between 50–150 bar to disperse fibre bundles without excessive shear heating. Screw peripheral speed is limited to 50–100 m/min and total residence time is kept below 300 s. On a 100 t clamp machine moulding relay housings with 0.8 mm walls, injection speed above 150 mm/s has been observed to produce jetting and surface streaks, while fill times below 0.5 s sheared glass fibre near the gate and reduced retained fibre length in the weld-line region. For multi-cavity connector moulds, valve-gated hot runners with manifold zones calibrated to ±5°C are used; an unbalanced manifold creates cavity-to-cavity variation in melt history and can shift flammability behaviour at the thinnest wall section.
The following ranges are consistent with published datasheets for a 30% glass-fibre flame-retardant PBT of this density class: tensile strength at yield 110–125 MPa by ISO 527-2; tensile elongation at break 1.5–2.5%; flexural modulus 9000–10000 MPa by ISO 178; notched Izod impact at 23°C 7–9 kJ/m² by ISO 180/1A; heat deflection temperature under 1.8 MPa 200–210°C by ISO 75-2/A; density 1.58–1.62 g/cm³ by ISO 1183-1. Mould shrinkage is anisotropic: 0.2–0.5% in the flow direction and 0.6–1.0% transverse by ISO 294-4. Melt volume-flow rate at 250°C/2.16 kg is typically 10–25 cm³/10 min by ISO 1133-1; lower values create filling-pressure limitations in thin-wall connectors, while higher values may indicate molecular weight loss from hydrolysis or overcompounding. Ash content by ISO 3451-1 is normally 28–32 mass%, corresponding to the nominal glass loading. A shift outside this range indicates dosing variation during compounding and will move tensile modulus and warpage. The comparative tracking index of glass-filled FR PBT commonly falls in the 250–300 V range by IEC 60112, but the exact value for this specific grade is lot- and formulation-dependent and must be confirmed on the current UL Yellow Card. The UL 94 V-0 classification is thickness-dependent; a rating at 0.8 mm does not automatically extend to a 0.4 mm wall, and the minimum approved thickness is the governing specification for end-product compliance. Test specimens are conditioned for 24 h at 23°C/50% RH unless otherwise stated on the datasheet. The controlling flammability document is the UL Yellow Card for the specific colour and thickness; the general datasheet value is not a substitute. Colour concentrates can shift the thin-wall classification, and black lots may achieve V-0 at a different minimum thickness than natural lots.
In board-to-board connectors and automotive harness connectors, PBT-FR 140PG6 substitutes for unreinforced FR PBT when pin-retention force and warpage control become limiting. A flexural modulus of 9000–10000 MPa permits thinner wall sections than a 15% glass-fibre FR grade without excessive flexural strain during mating. In relay bases, contactor housings, and terminal blocks, the compound is specified because the thickness-dependent UL 94 V-0 classification supports compliance with end-product standards such as IEC 60335-1 when the final part is tested at the minimum approved wall. Switchgear components and motor end caps use the grade where short-term resistance to lead-free soldering is required; the heat deflection temperature of 200–210°C provides short-term dimensional stability, but continuous exposure above 150°C will alter the flame-retardant package and should be evaluated by UL 746B relative temperature index data. Published data for this specific configuration in high-voltage electric-vehicle charging inlets is limited; qualification must include comparative tracking index, arc resistance, and glow-wire ignition temperature on the actual part geometry.
The selection of PBT-FR 140PG6 over non-FR PBT 140PG6 is driven by end-product flammability requirements. Non-FR 30% glass-fibre PBT exhibits similar stiffness and slightly higher notched impact because the flame-retardant package does not dilute the matrix. Compared with a 30% glass-fibre flame-retardant PA66, the PBT grade absorbs less moisture—generally below 0.4% at saturation by ISO 62, versus 2.0–2.5% for PA66—so electrical property retention and dimensional stability in humid service are superior. PA66-FR offers higher heat ageing resistance above 150°C and better resistance to hot oil, but it requires more aggressive drying and exhibits wider mould shrinkage. Compared with a 20% glass-fibre FR PBT, the 30% grade raises flexural modulus by roughly 1500–2500 MPa but increases orientation-induced warpage in flat covers; gate placement along the longest dimension and wall-thickness transitions no sharper than 1:3 are used to compensate. The following table summarises the comparative position of the product class.
| Property | PBT-FR 140PG6 class | Non-FR 30% GF PBT | 30% GF FR PA66 | Test method |
|---|---|---|---|---|
| Density | 1.58–1.62 g/cm³ | 1.53–1.57 g/cm³ | 1.35–1.45 g/cm³ | ISO 1183-1 |
| Tensile strength at yield | 110–125 MPa | 120–135 MPa | 130–160 MPa | ISO 527-2 |
| Flexural modulus | 9000–10000 MPa | 9000–10000 MPa | 8500–10000 MPa | ISO 178 |
| Notched Izod at 23°C | 7–9 kJ/m² | 9–11 kJ/m² | 8–10 kJ/m² | ISO 180/1A |
| HDT/A 1.8 MPa | 200–210 °C | 200–215 °C | 230–250 °C | ISO 75-2/A |
| Moisture uptake at saturation | 0.2–0.4% | 0.2–0.4% | 2.0–2.5% | ISO 62 |
| Flammability at 0.8 mm | UL 94 V-0 | UL 94 HB | UL 94 V-0 | UL 94 |
For injection-moulding simulation, the material database should include pressure-volume-temperature data, heat capacity, and shear-viscosity curves measured by capillary rheometry at 250°C, 260°C, and 270°C. The use of generic PBT data without glass-fibre orientation will overpredict shrinkage in the flow direction and underpredict warpage. Fibre orientation tensor values from mould-filling software must be validated on a shot-by-shot basis using flat plaques of 60 mm×60 mm×2 mm and measured shrinkage per ISO 294-4.
Long-term service temperature is bounded not only by the PBT matrix but also by the retention of the flame-retardant system. The material is not recommended for continuous exposure above 150°C in air without verification by UL 746B relative temperature index data. In hot and humid environments, especially above 60°C and 85% RH, PBT hydrolyses over time; design margins should account for a measurable drop in tensile strength after 1000 h of damp-heat ageing. The grade resists many automotive fluids, aliphatic hydrocarbons, and alcohols at room temperature, but strong bases, chlorinated solvents, and boiling water attack the polyester backbone. Outdoor UV exposure is not a primary design condition; unpigmented or natural mouldings will show surface chalking and embrittlement unless UV-stabilized or painted. Regrind from rejected parts and sprue/runner scrap is acceptable up to 20 wt% when the regrind is dry, free of oil and dust, and generated from the same material; higher levels reduce notched Izod and can move the thin-wall flammability result from V-0 to V-1 or V-2. The specific flame-retardant chemistry may not be fully disclosed in the supplier’s general literature; the material declaration required by REACH 1907/2006 and RoHS 2011/65/EU should be obtained for the production lot.