Nan Ya Pbt Fr 140pg3

Nan Ya PBT-FR 140PG3

    • Product Name: Nan Ya PBT-FR 140PG3
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 634423
    Density 1.52 g/cm³
    Melt Flow Rate 15 g/10 min
    Tensile Strength 65 MPa
    Elongation At Break 3%
    Flexural Strength 100 MPa
    Flexural Modulus 5500 MPa
    Notched Izod Impact Strength 4 kJ/m²
    Heat Deflection Temperature 1 82 Mpa 200 °C
    Ul 94 Flammability Rating V-0 (1.5 mm)
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1E15 Ω·cm
    Water Absorption 0.05%
    Molding Shrinkage 0.4–0.8%
    Glass Fiber Content 15%

    As an accredited Nan Ya PBT-FR 140PG3 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Nan Ya PBT-FR 140PG3 is packaged in 25 kg moisture-resistant bags, palletized and clearly labeled with product and lot identification.
    Container Loading (20′ FCL) A 20′ FCL container carrying Nan Ya PBT-FR 140PG3 in sealed bags/pallets, properly secured and labeled for export shipment.
    Shipping Nan Ya PBT-FR 140PG3 typically ships as a non-regulated solid polymer in moisture-barrier bags or cartons, palletized and secured. Store in a cool, dry, ventilated area away from sunlight, heat, and ignition sources. Follow the SDS and local regulations; avoid package damage and environmental release.
    Storage Store Nan Ya PBT-FR 140PG3 in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep original containers tightly closed to prevent moisture pickup and contamination. Avoid dust generation and static buildup. Segregate from strong oxidizers and acids. Follow the SDS and local regulations; use first-in, first-out stock rotation.
    Shelf Life Store in a dry, cool place in original sealed packaging; typical shelf life is about 12 months.
    Free Quote

    Competitive Nan Ya PBT-FR 140PG3 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The Nan Ya PBT-FR 140PG3 grade is a 30 wt% glass-fibre-reinforced, flame-retardant polybutylene terephthalate injection-moulding compound supplied in pellet form. The PG3 suffix identifies the 30% glass-fibre reinforcement level within the Nan Ya PBT range, while the FR designation indicates the flame-retardant formulation. The material is intended for electrical and electronic components requiring a UL 94 V-0 classification at 1.6 mm nominal wall thickness when tested to IEC 60695-11-10. Manufacturer-published typical values for dry-as-moulded specimens include a density of 1.55 g/cm³ to ISO 1183-1:2019, tensile strength at break of 110 MPa to ISO 527-2:2012, tensile elongation at break of 2.0%, flexural modulus of 8.0 GPa to ISO 178:2019, flexural strength of 180 MPa, notched Izod impact at 23°C of 7.5 kJ/m² to ISO 180:2023, and heat deflection temperature of 205°C at 1.82 MPa to ISO 75-2:2013. Melt volume-flow rate is reported in the range of 10 cm³/10 min to 15 cm³/10 min at 250°C and 2.16 kg to ISO 1133-1:2022. These single-point specimen values are not specification minima; part geometry, weld lines, and moulding conditions can reduce them in service.

    Relative to unfilled flame-retardant PBT grades, 140PG3 shifts mechanical behaviour from moderate stiffness and higher ductility to high flexural rigidity and reduced creep under load. The glass-fibre network raises flexural modulus from approximately 2.6 GPa in a standard unfilled FR PBT to 8.0 GPa in the reinforced product, while tensile elongation at break drops from above 10% to approximately 2.0%. The reduction in elongation changes the design envelope for snap-fit beams, latch arms, and thin-walled edges: these features should be deflection-limited rather than stress-limited, because permanent set and brittle fracture at knit lines become the dominant failure modes in glass-reinforced material. Moulded parts also exhibit a coefficient of linear thermal expansion of approximately 30 µm/m·°C in the flow direction and 60 µm/m·°C transverse to flow to ISO 11359-2:2021. This anisotropy is lower than that of unfilled PBT in the flow direction but higher than unfilled PBT in the transverse direction, and it must be compensated in tool design.

    What critical drying and melt-temperature boundaries govern the 140PG3 moulding window?

    Hydrolysis is the primary processing risk. The resin is dried to a residual moisture content below 0.02% before plastication. Dehumidifying hopper dryers are set at 120°C for 4 h, with a dew point of -40°C or lower. If the drying hopper remains stopped, pellet residence above 6 h at temperature can yellow the grade. Barrel profiles are typically rear 240°C, centre 250°C to 260°C, and nozzle 255°C; measured melt temperature should not exceed 265°C. At melt temperatures above 265°C, the halogenated flame-retardant system can liberate acidic decomposition products that corrode screw, barrel, and hot-runner surfaces. Screw geometry with L/D 20:1 to 22:1 and compression ratio 2.5:1 to 3.0:1 is recommended; vented barrels are generally avoided because the glass-fibre compound has reduced melt strength at the vent. Mould temperature is controlled between 60°C and 100°C, with the upper range used where flatness and post-mould crystallinity are critical. Injection pressures in production tools are commonly 80 MPa to 120 MPa hydraulic for flow-length to wall-thickness ratios up to 150:1; beyond this ratio, short shots occur because the melt front solidifies before end-fill. In hot-runner systems, shear rate at the gate should remain below 50,000 s⁻¹ because higher shear heating leads to gate blush, additive degradation at the gate tip, and brownish streaks. Weld-line tensile strength in 30% glass-fibre FR PBT is usually 40% to 60% of the unreinforced base strength, so gate location should place knit lines away from snap-fit and electrical contact retention features.

    Packing pressure and hold time affect dimensional stability more than peak injection pressure. Production-scale settings are typically 50% to 70% of peak injection pressure for 5 s to 10 s, and final cushion is maintained at 3 mm to 5 mm to avoid fibre segregation at the screw tip. In multicavity tools, fill balance is checked with short-shot series; cavity-to-cavity weight variation above 0.5% may indicate gate wear or hot-runner imbalance that produces differential crystallinity and warpage. Capillary rheometry for this reinforcement class typically shows shear thinning from approximately 200 Pa·s at 100 s⁻¹ to 60 Pa·s at 1,000 s⁻¹ at 250°C; however, grade-specific curves should be obtained from the supplier before hot-runner sizing.

    Across thin-wall relay bases and sensor connectors, mould shrinkage is direction-dependent. In the flow direction, linear mould shrinkage is generally 0.2% to 0.5%; transverse to flow, 0.5% to 1.0% depending on part thickness and packing pressure. Toolmakers compensate by using unequal cavity dimensions or by adding ribbing to hold flatness in parts below 1.0 mm wall. Because post-mould crystallisation can continue for up to 24 h, parts removed from the tool may exhibit additional room-temperature shrinkage of 0.05% to 0.10% if hold time and packing pressure are too low. For insert-moulded parts, hole diameter allowances of 0.02 mm to 0.05 mm are used to absorb differential expansion between brass or steel inserts and the PBT matrix. The thermal expansion data to ISO 11359-2:2021 are used for finite-element warpage prediction; however, actual warpage can deviate because glass-fibre orientation varies with gate location and part thickness.

    Comparative electro-mechanical data for material-replacement decisions

    The table below compares 140PG3 with two adjacent material classes: unfilled flame-retardant PBT and 30% glass-fibre-reinforced non-flame-retardant PBT. Values are typical dry-as-moulded data and do not replace part-specific validation.

    PropertyTest methodPBT-FR 140PG3Unfilled FR PBTGF30 non-FR PBT
    Glass fibre contentISO 3451-130%0%30%
    Flame class at 1.6 mmIEC 60695-11-10V-0V-0HB
    Tensile strength at breakISO 527-2:2012110 MPa55 MPa120 MPa
    Flexural modulusISO 178:20198.0 GPa2.6 GPa8.4 GPa
    Notched Izod at 23°CISO 180:20237.5 kJ/m²4.0 kJ/m²9.0 kJ/m²
    HDT at 1.82 MPaISO 75-2:2013205°C60°C210°C
    Comparative tracking indexIEC 60112225 V250 V600 V
    Moisture absorption at 23°C/50% RHISO 62:20080.07%0.07%0.07%

    The main trade-off is that the flame-retardant package in 140PG3 lowers tensile strength and impact toughness relative to a non-FR GF30 PBT but provides V-0 classification without changing the glass-fibre content. Compared with unfilled FR PBT, the 30% glass reinforcement raises flexural modulus and HDT substantially but reduces weld-line strength and increases anisotropy. The lower comparative tracking index relative to non-FR PBT requires a creepage and clearance review under IEC 60664-1 for high-voltage designs.

    Terminal-block and relay-housing applications use the grade because it combines V-0 compliance with high stiffness and predictable insert retention. In power-distribution connectors, the material is specified for terminal blocks, relay sockets, coil bobbins, switch components, and sensor connectors where the service temperature does not exceed the 130°C electrical relative thermal index. The dielectric strength on 2.0 mm plaques is commonly reported at 17 kV/mm to 20 kV/mm to IEC 60243-1, but glass-fibre ends reduce dielectric strength relative to unfilled FR PBT and can create local field enhancement. The comparative tracking index of approximately 225 V to IEC 60112 limits use in pollution degree 3 equipment above 250 V working voltage unless creepage distances are increased or the part is coated or potted.

    On production-scale injection-moulding machines with clamp force from 80 t to 150 t, the primary batch-to-batch variability observed in industrial practice is not resin molecular weight but fibre length distribution and flame-retardant dispersion. If fibre length distribution shifts to shorter fibres, tensile strength can fall by 5% to 10% while melt viscosity remains unchanged. If the flame-retardant package is poorly dispersed, ignition resistance can vary with part thickness and surface layer, and black streaks or white specks may appear at the gate. Quality checks should therefore include ash content to ISO 3451-1, melt volume-flow rate to ISO 1133-1:2022, and UL 94 flammability on end-part samples rather than on standard plaques only.

    When a 30% glass-fibre flame-retardant PBT replaces PA66 GF30 in electrical housings

    The polyester compound provides lower equilibrium moisture absorption of 0.07% at 23°C and 50% RH to ISO 62:2008, compared with 2.0% to 2.5% for PA66 GF30. This difference stabilises dielectric properties and dimensions in humid environments and reduces the need for pre-conditioning before electrical testing. The PBT grade also processes at lower melt temperature, typically 250°C to 260°C, than PA66 GF30 at 280°C to 300°C, allowing shorter start-up cycles and lower energy input. However, PBT has a sharper melting transition and lower melt strength on long flow paths; hot-runner and gate sizes may require an increase of 10% to 15% when converting from PA66. Continuous-use temperature under load is lower: published relative thermal index values for glass-reinforced FR PBT are generally 130°C electrical, 130°C mechanical with impact, and 130°C mechanical without impact, whereas PA66 GF30 can be listed at 140°C to 150°C. Substitution is therefore limited in environments where the part temperature exceeds 130°C continuously or 150°C intermittently.

    Operational boundaries for PBT-FR 140PG3 are most evident in chemical contact and reuse. The compound is not recommended for continuous exposure to hot water above 60°C, strong alkaline solutions, or amine-containing additives, because ester hydrolysis and flame-retardant interaction accelerate embrittlement. Blending with polycarbonate regrind is avoided; transesterification can reduce crystallinity and flame-retardant effectiveness. Regrind addition is generally limited to 20% by weight and must be dried to the same 0.02% moisture specification as virgin resin. For parts exposed to repeated thermal cycling, glass-fibre orientation creates stress concentrations at knit lines and insert boundaries. Published long-term data for this exact grade in aggressive automotive coolant or industrial solvent environments is limited; qualification for such applications requires immersion testing at the intended concentration and temperature rather than reliance on general PBT chemical resistance tables. Supplier documentation should be checked for RoHS 2011/65/EU and REACH SVHC reporting for the specific production batch, because flame-retardant raw-material sources can vary.

    Top