| HS Code | 608056 |
| Glass Fiber Content | 15% |
| Flame Retardancy | Yes |
| Density | 1.55 g/cm3 |
| Water Absorption | 0.04% |
| Linear Mold Shrinkage Flow | 0.2-0.4% |
| Linear Mold Shrinkage Transverse | 0.4-0.6% |
| Tensile Strength At Break | 100 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 5.5 GPa |
| Flexural Strength | 150 MPa |
| Izod Notched Impact Strength | 5 kJ/m2 |
| Deflection Temperature At 1 8 Mpa | 200 deg C |
| Melting Point | 225 deg C |
| Ul94 Flammability Rating | V-0 at 0.8 mm |
| Volume Resistivity | 1E15 ohm-cm |
| Dielectric Strength | 20 kV/mm |
As an accredited Nan Ya PBT-FR 1403G3 GNC6 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Nan Ya PBT-FR 1403G3 GNC6 is supplied in 25 kg moisture-proof bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | Nan Ya PBT-FR 1403G3 GNC6 is palletized, securely loaded into a 20′ FCL container, and stowed for safe ocean transport. |
| Shipping | Nan Ya PBT-FR 1403G3 GNC6 is a flame-retardant, glass-fiber-reinforced PBT resin supplied as pellets. Ship in sealed moisture-proof bags or cartons on pallets, labeled with product, batch, and SDS details. Keep dry, cool, and away from sunlight; generally handled as non-hazardous industrial resin unless SDS states otherwise. |
| Storage | Store `Nan Ya PBT-FR 1403G3 GNC6` in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and oxidizing agents. Keep in original sealed packaging on pallets to prevent moisture ingress and contamination. Avoid prolonged high humidity or temperature exposure; follow SDS and local regulations. |
| Shelf Life | Typically 24 months when stored in original unopened packaging under dry, cool conditions, away from direct sunlight. |
Competitive Nan Ya PBT-FR 1403G3 GNC6 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Nan Ya PBT-FR 1403G3 GNC6 is a halogenated flame-retardant polybutylene terephthalate compound reinforced with a glass-fiber loading identified by the G3 suffix in the producer’s nomenclature. In the Nan Ya PBT system, G3 is conventionally associated with a 15% glass-fiber fraction by weight, whereas G6 corresponds to a 30% glass-fiber reinforcement level. The GNC6 tail code denotes the color and packaging configuration; the NC element is consistent with a natural resin pellet, but the full code should be verified against the certificate of analysis before production. The matrix is semicrystalline PBT with a melting peak in the region of 220–230 °C. The flame-retardant system is a halogenated package, generally composed of a brominated aromatic species with an antimony trioxide synergist. This chemistry permits the compound to achieve a V-0 classification under UL 94 in thin wall sections, but it also increases melt degradation sensitivity and makes mold ventilation mandatory.
The grade is positioned for injection-molded electrical and electronic components such as connector housings, relay bases, terminal strips, bobbins, motor end caps, and switch bodies. The 15% glass loading provides a balance between stiffness and dimensional stability. It has a lower flow-to-transverse shrinkage differential than 30% glass-reinforced PBT grades, and higher heat resistance than unreinforced flame-retardant PBT. The product is not a structural material; sharp corners, weld lines, and metal-insert stresses must be managed because the halogenated flame-retardant package reduces elongation at break relative to non-flame-retardant PBT. Published data for this specific configuration is limited in open literature; the grade-specific technical datasheet and UL yellow card remain the controlling documents for design values.
Hydrolytic degradation is the primary processing risk. PBT is a polyester and undergoes chain scission when pellets contain more than 0.02% moisture by weight. Production-scale desiccant dryers with a dew point below -40 °C are required. The supplier’s processing recommendations for 15% glass-filled flame-retardant PBT typically specify drying at 120 °C for 3–4 h. If bags have been opened in ambient relative humidity above 60%, the drying time should be extended to 6 h and the moisture content verified with a Karl Fischer titrator.
The melt processing window is narrow relative to unfilled PBT. Barrel temperatures are normally set between 245 °C and 260 °C, with the nozzle at 250–260 °C and the mold at 60–90 °C. Melt temperatures above 270 °C accelerate decomposition of the brominated flame-retardant package, generating free bromine species that cause silver streaks, yellowing, and tool corrosion. The maximum recommended melt residence time is 5 min, and the screw should be sized so that shot weight represents 40–70% of barrel capacity. Screw speed should be held between 50 rpm and 150 rpm; back pressure of 0.3–0.7 MPa prevents glass-fiber agglomeration without creating excessive shear heating. For thin-wall connector bodies, fill times of 0.5–1.5 s are typical, with hold pressure at 40–60% of peak injection pressure.
Tooling should use hardened, corrosion-resistant steel because the flame-retardant decomposition products can corrode unprotected steel. Vent gaps of 0.02–0.03 mm along the last-fill regions reduce gas burns and deposit formation. Hot-runner systems should avoid dead spots and retain temperature control within ±5 °C. When molding around metal inserts, preheat inserts to 80–120 °C to reduce thermal shock and avoid premature solidification around the insert. The screw should be a general-purpose polyolefin screw with a compression ratio of 2.0–2.5:1 and a check ring clearance sufficient for glass fiber. Bimetallic barrels, hardened screw tips, and nitrided barrel liners are recommended because glass fiber is abrasive. For machines with L/D ratios below 18:1, melt homogeneity may be insufficient, leading to visible glass bundles at the surface. For L/D ratios above 24:1, melt residence time may increase and flame-retardant degradation risk rises. The measured melt pressure during injection should remain below 150 MPa; if peak pressure exceeds this value, gate and runner sizing should be re-evaluated.
Continuous-use temperature for this product family is generally bounded by thermal-oxidative embrittlement rather than softening. Published data for this specific configuration is limited; representative data for 15% glass-reinforced brominated flame-retardant PBT compounds indicate tensile strength retention of 80% after 1,000 h at 160 °C, while at 180 °C the same retention may occur after 300–500 h. The material should not be applied at continuous air temperatures above 140 °C when high elongation retention is required. Because PBT absorbs less moisture than PA66, the grade maintains more stable dielectric properties in humid environments. Equilibrium moisture absorption at 23 °C and 50% relative humidity is below 0.1%.
Hot-water exposure above 80 °C is a more severe limit than hot air. Hydrolysis reduces molecular weight and causes a measurable drop in tensile elongation and notched impact before tensile strength declines. In electrical connectors that experience condensing humidity, comparative tracking index and surface resistance should be measured on final color-matched parts. The comparative tracking index of brominated flame-retardant PBT grades is generally lower than that of non-flame-retardant PBT and many non-halogenated flame-retardant systems; end-product testing under IEC 60112 is required. The 15% glass reinforcement provides creep resistance under clamping and insertion loads, but sustained stress above 20 MPa at temperatures above 80 °C may produce stress relaxation that reduces contact force. The glass transition temperature of the PBT matrix is approximately 45–60 °C; below this the polymer is glassy and notch sensitive. At sub-zero temperatures, notched impact strength falls further, and the product should not be subjected to high-rate impact in snap-fit features unless validated with ISO 179-1/1eA or ISO 180:2023 at the lowest service temperature. The 15% glass reinforcement raises heat deflection temperature but does not eliminate low-temperature notch sensitivity.
| Property | Test method | PBT-FR 1403G3 GNC6 class | 30% glass-fiber PBT flame-retardant reference |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.54–1.58 g/cm³ | 1.65–1.69 g/cm³ |
| Tensile stress at break | ISO 527-2:2012 | 95–105 MPa | 115–130 MPa |
| Flexural modulus | ISO 178:2019 | 5,500–6,500 MPa | 8,500–10,000 MPa |
| Notched Izod impact | ISO 180:2023 | 5–7 kJ/m² | 7–9 kJ/m² |
| Heat deflection temperature at 1.8 MPa | ISO 75-2:2020 | 200–210 °C | 205–215 °C |
| Flow-direction mold shrinkage | ISO 294-4:2018 | 0.5–0.8% | 0.3–0.5% |
| Transverse mold shrinkage | ISO 294-4:2018 | 0.8–1.2% | 0.7–1.0% |
In multi-pin connector bodies and relay bases with wall sections below 1.0 mm, the 30% glass-reinforced grade often shows greater differential shrinkage and higher warpage than the 15% glass product. The G3 grade reduces flow-to-transverse shrinkage difference and produces a smoother surface in thin ribs. This is advantageous when coplanarity of solder tails must be held within 0.1 mm across a 50 mm connector length. However, the lower glass fraction also lowers flexural modulus and heat deflection temperature relative to the G6 grade; the design must not rely on 30% glass-fiber stiffness. Pin retention in a 0.5 mm interference hole is higher than unfilled flame-retardant PBT, but lower than 30% glass-filled PBT. The exact retention force depends on hole geometry, pin surface finish, and wall thickness, not on the material grade alone.
Mold-fill simulation for the 15% glass product should use a melt density near 1.35 g/cm³ and a specific heat capacity of 1.5–1.8 J/g·K. The crystallization peak from differential scanning calorimetry at 20 K/min cooling is expected between 190 °C and 200 °C. Weld-line strength in glass-reinforced PBT is highly dependent on melt temperature and venting; a weld line can retain only 40–60% of the base tensile strength, so gate locations should be arranged so that high-stress regions do not contain weld lines. For flat parts with rib-to-wall ratios above 0.6, the 15% glass grade may still produce sink marks. Rib thickness should be limited to 50–60% of nominal wall. Bosses for self-tapping screws should have an outside diameter 2–2.5 times the screw diameter to prevent boss cracking. The use of 30% glass PBT would increase modulus and reduce sink depth slightly, but the higher viscosity could increase gas traps in thin bosses. Gate location should place the weld line away from the boss. If cosmetics are critical, a quick-change mold with poppet valve gates may be necessary for this grade because the brominated flame-retardant system can leave gate blush in hot-runner drops.
Field data from high-cavitation connector tools show that lot-to-lot variation in pellet moisture and glass distribution can shift peak injection pressure by 5–10 MPa at the same fill profile. The injection unit should maintain a stable cushion of 2–5 mm; a cushion below 2 mm may increase glass-fiber breakage and reduce mechanical properties. Regrind can be used at 15–30% in non-safety electrical parts, but parts that must meet UL 94 V-0 in production should be validated with the exact regrind fraction. Regrind from containers exposed to humidity should be re-dried at 120 °C for 2–4 h, and residence time in the melt stream should be reduced because regrind has a lower melt viscosity and a higher degradation rate than virgin pellets.
The halogenated flame-retardant package, especially when exposed to moisture and electric potential, can generate trace ionic species that migrate to metal contacts. This does not automatically disqualify the product, but it requires qualification. For switching devices that operate above 24 V or 0.5 A, contact-resistance testing under condensing humidity, for example IEC 60068-2-60, is recommended. The mold should be protected with corrosion-resistant steel or hard-chrome plating. In thermal decomposition above 250 °C, brominated flame-retardant systems release acidic gases that can corrode unprotected tooling and damage ventilation ducting. The product should not be processed with PVC or acetal residues in the same barrel; cross-contamination can generate decomposition products and surface defects.
Regulatory status must be obtained from the supplier’s certificate. If the compound contains a brominated flame retardant and antimony trioxide, it may still conform to RoHS Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006, but it is not halogen-free. Applications requiring halogen-free materials under IEC 61249-2-21 should select a non-halogenated PBT flame-retardant grade. Non-halogenated flame-retardant PBT grades generally require higher flame-retardant loadings, which reduce melt flow and notched impact, increase density, and may make thin-wall molding more difficult. The halogenated 1403G3 GNC6 retains better flow and thinner-wall V-0 performance at the expense of environmental and contact-corrosion trade-offs. The grade is not recommended for direct contact with strongly alkaline solutions, high-temperature amine-based stabilizers, or steam above 100 °C, because these conditions accelerate hydrolysis and surface deterioration. The antimony trioxide synergist raises density and opacity; natural-colored parts may have a slight ivory-yellow tint, not a water-white appearance. Color measurement should use a spectrophotometer with D65 illuminant and 10° observer, but color stability at melt temperatures above 260 °C is limited. If bright colors are required, the supplier’s GNC6 natural base should be color-matched under controlled moisture and regrind conditions.
In a fractional-horsepower motor end cap with a 2.0 mm nominal wall, a four-cavity hot-runner mold, and clamping force of 150–200 t, the 15% glass-filled flame-retardant PBT fills with a fill time near 0.8 s and exhibits acceptable warpage after a 30 s cycle. The end cap must pass the ball-pressure test at 125 °C under IEC 60695-10-2; the grade’s glass reinforcement and crystalline PBT matrix provide the necessary short-term heat resistance. Vent gaps of 0.02–0.03 mm along the last-fill radius prevent gas marks from the flame-retardant package. For terminal blocks operating at 600 V and 30 A, the material should be evaluated for comparative tracking index, glow-wire ignition, and creepage distance as a system; the resin supplier’s data alone is insufficient to qualify the part. Molders should record drying time, barrel residence time, regrind fraction, and peak injection pressure for each lot, because the interaction between these variables determines whether molded parts remain within the UL 94 V-0 classification and mechanical design window.