| HS Code | 449645 |
| Grade | Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 |
| Polymer Type | PBT, unfilled |
| Filler Content | 0% |
| Density | 1.21 g/cm³ |
| Mold Shrinkage | 0.6–0.8% |
| Tensile Strength | 50 MPa |
| Elongation At Break | 50% |
| Flexural Modulus | 2100 MPa |
| Charpy Notched Impact Strength At 23 C | 10 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | 80°C |
| Vicat Softening Temperature | 120°C |
| Flammability Rating | UL94 HB |
| Water Absorption 24 H | 0.1–0.2% |
As an accredited Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant bags, palletized and stretch-wrapped: Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 resin. |
| Container Loading (20′ FCL) | Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 is palletized and securely loaded into a clean, dry 20′ FCL container. |
| Shipping | Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 is shipped as thermoplastic resin pellets in sealed moisture-barrier bags, cartons, and palletized units. Keep dry and ventilated at ambient temperature, away from direct sunlight, heat, and moisture. Handle as non-hazardous industrial material and follow applicable transport regulations. |
| Storage | Store Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and incompatible materials. Keep containers tightly sealed to prevent moisture pickup and contamination. Avoid prolonged exposure to humid air; pre-dry before processing as recommended. Follow the SDS and local storage regulations. |
| Shelf Life | Shelf life is typically indefinite when stored sealed in a cool, dry, dark place, protected from moisture, heat, and sunlight. |
Competitive Mitsubishi Engineering Plastics Lumiloy® PBT Unfilled GN1100 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The Lumiloy® PBT Unfilled GN1100 grade supplied by Mitsubishi Engineering Plastics Corporation is an unreinforced polybutylene terephthalate grade intended for injection moulding and extrusion. The base polymer is a semi-crystalline thermoplastic polyester produced from terephthalic acid and 1,4-butanediol. The GN1100 designation identifies a product that does not carry glass fibre, mineral filler, conductive carbon, or halogenated flame-retardant packages. It is supplied as pellets and is positioned for applications where moderate strength, predictable shrinkage, low moisture absorption, high surface gloss, and good electrical insulation are more important than load-bearing performance. The unfilled grade is frequently evaluated for low-voltage connector housings, relay bobbins, terminal blocks, sensor brackets, and small gear carriers where dimensional stability and low wear on tooling are required. PBT is differentiated from nylon 6 and nylon 66 by lower water absorption—typically 0.2% by ISO 62 after 24 h—which reduces hygroscopic swelling and preserves electrical properties in humid service. The material also offers good resistance to many automotive fluids, greases, and aliphatic hydrocarbons; strong alkalis and hot concentrated acids are not recommended, and continuous service above 80 °C in hot water should be validated because the ester backbone is prone to hydrolysis. The melt processability of GN1100 is typical of medium-flow unfilled PBT, with stable spiral-flow behaviour in thin-wall sections and a lower screw/barrel wear factor than glass-filled alternatives. Regulatory status, including REACH and RoHS compliance, is lot- and formulation-specific and should be confirmed with the manufacturer before use. The values and comparisons in this technical note are based on standard unfilled PBT datasets and should be verified against the current manufacturer’s technical data sheet and certificate of analysis for a specific batch.
In converting semi-crystalline PBT, moisture control is the first boundary condition. PBT is hydrolytically sensitive; the ester linkages in the polymer backbone undergo chain scission when melt moisture exceeds approximately 0.02%. Pre-drying in a dehumidifying dryer at 120 °C for 3–4 hours is required after exposure to relative humidity above 60%. The dryer dew point should be below −30 °C, and conditioned pellets should be conveyed with dry-air purging or used from closed hoppers. If dry pellets remain in open containers for more than 2 hours, re-drying is advisable. Melt temperature should be kept within 240–270 °C. At the lower end below 245 °C, thin-wall sections below 1 mm may show short-shot sensitivity if the filling speed is not adjusted; above 270 °C, yellowing, gas generation, and molecular weight loss from acid-catalysed decomposition become more pronounced. Mould temperature should be maintained between 40 °C and 80 °C. Mould surfaces near 80 °C increase crystallinity and provide better dimension control and surface gloss, while lower mould temperatures allow shorter cycles but can reduce long-term thermal ageing resistance. Production-scale exercises on 80–150 t clamp-force injection moulding machines indicate that unfilled PBT grades with similar flow lengths require specific injection pressures of 70–120 MPa, hold pressures of 40–70 MPa, and screw cushions of 8–12 mm to avoid gas entrapment. Screw recovery should use a low-compression screw with L/D ratio of 18–22 and back pressure below 10 bar to limit shear heating. Residence time at melt temperature should not exceed 10 minutes; frequent production interruptions require purging to avoid black specks. Regrind addition beyond 25 wt% should be validated because each thermal pass through a compounding or moulding unit can shift melt-flow rate and impact strength. In twin-screw extrusion operations using L/D ratios of 32–44 with vacuum venting, melt temperature, screw speed, and throughput should be matched to prevent excessive residence time and hydrolysis. Additive packages containing primary or secondary amines should be avoided in PBT compounding because aminolysis accelerates molecular weight reduction; if colour concentrates are used, the carrier resin should be PBT-compatible.
For design analysis, the unfilled grade is best assessed through short-term mechanical values obtained under standardized specimen preparation. Table 1 compares the representative property envelope of unfilled GN1100 with a 30 wt% glass-fibre-reinforced PBT and a non-reinforced flame-retardant PBT.
| Property | Test method | Unit | Unfilled GN1100 typical | GF30 PBT typical | FR V-0 PBT typical |
|---|---|---|---|---|---|
| Density | ISO 1183 | g/cm³ | 1.31 | 1.53 | 1.44 |
| Tensile stress at yield | ISO 527-2 | MPa | 55 | 120 | 55 |
| Flexural modulus | ISO 178 | MPa | 2,400 | 8,500 | 2,300 |
| Charpy notched impact | ISO 179-1/1eA | kJ/m² | 3.0 | 8.0 | 3.0 |
| HDT at 1.8 MPa | ISO 75-2/Ae | °C | 60 | 200 | 80 |
| CTE flow direction | ISO 11359-2 | 10⁻⁶/K | 90 | 25 | 80 |
The unfilled GN1100 profile shows tensile stress at yield near 55 MPa by ISO 527-2, flexural modulus near 2,400 MPa by ISO 178, and Charpy notched impact of 3.0 kJ/m² by ISO 179-1/1eA at 23 °C. This places GN1100 in the low-to-moderate toughness class; designs with snap-fits or cold impact may require an impact-modified PBT. The heat deflection temperature at 1.8 MPa is approximately 60 °C by ISO 75-2/Ae, whereas the value at 0.45 MPa reaches roughly 150 °C. Continuous load-bearing service above 80 °C is not advised without verifying creep and hydrolysis ageing. The unfilled formulation exhibits lower thermal expansion than many unfilled polyolefins, with a flow-direction coefficient of linear thermal expansion near 90 × 10⁻⁶ /K by ISO 11359-2, but expansion in the transverse direction can be higher. Electrical insulation values include volume resistivity typically above 1 × 10¹⁴ Ω·m under IEC 62631-3-1 and dielectric strength near 17 kV/mm under IEC 60243-1. Comparative tracking index is generally reported in the 400–600 V range by IEC 60112, making the material suitable for low-voltage electromechanical parts. Moisture absorption of 0.2% by ISO 62 at 24 h is lower than that of PA66 and contributes to stable part dimensions in humid enclosures. The unfilled grade is normally classified as UL 94 HB at 0.75 mm; parts requiring V-0 should use a flame-retardant grade rather than relying on this material. The comparative values in Table 1 are representative typical data, not guaranteed specification minima, and lot-specific conformity should be taken from the manufacturer’s certificate of analysis.
When glass-fibre reinforcement is added to PBT, the tensile stress at yield can rise to approximately 120 MPa and flexural modulus to 8,500 MPa, but the part acquires anisotropic shrinkage and glass-rich surfaces. Unfilled GN1100 typically exhibits mould shrinkage in the range 1.5–2.0% along flow and 1.7–2.2% transverse, depending on wall thickness, gate type, and mould temperature. The anisotropy is much lower than in glass-filled grades, which may show flow-direction shrinkage of 0.3–0.8% and transverse values two to three times higher. This difference is important in flat connectors, sensor housings, and terminal blocks where edge curvature or pin-to-pin misalignment cannot be corrected by tool re-cutting. The absence of abrasive glass reduces screw, check-ring, and barrel wear in high-volume production; standard hardened tool steels may be used for mould construction, and polished surfaces remain free of fibre-induced streaking. GN1100 also avoids the melt pool line that commonly appears with glass-filled parts at weld lines. Compared to a non-reinforced flame-retardant PBT, GN1100 will not satisfy UL 94 V-0 at 0.75 mm unless externally coated or shielded. The FR grade may also exhibit reduced flow length, lower tensile strength after hot-oil ageing, and a higher risk of mould deposits caused by acidic degradation products from halogenated flame retardants. Compared to impact-modified PBT, GN1100 has lower notched impact at low temperatures and should not be used for snap-fit clips exposed to cold impact below −10 °C without validation. However, the unfilled grade often has better melt flow and lower creep under moderate load than soft impact-modified systems. For applications involving electrical loss at high frequency, unfilled PBT is typically assessed in the low-gigahertz range by the supplier; published data for GN1100 in specific connector designs is limited, so end-use validation is required. When good surface finish, low warp, and reliable insulation outweigh tensile strength, GN1100 can be selected over filled grades. When strength or fire resistance dominates, the design should migrate to glass-filled or flame-retardant Lumiloy grades.