Mitsubishi Engineering Plastics Lumiloy Pbt Md30 Mr2000

Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000

    • Product Name: Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 688988
    Filler Content 30% mineral
    Density 1.65 g/cm³
    Mold Shrinkage Flow 0.3-0.6%
    Mold Shrinkage Cross Flow 0.5-0.9%
    Water Absorption 0.06%
    Tensile Strength 60 MPa
    Tensile Elongation 2.5%
    Flexural Modulus 6000 MPa
    Charpy Notched Impact Strength 3 kJ/m²
    Hdt At 1 8 Mpa 110°C
    Hdt At 0 45 Mpa 190°C
    Melting Point 224°C
    Volume Resistivity 1×10^15 Ω·cm
    Dielectric Strength 20 kV/mm
    Flammability HB

    As an accredited Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Mitsubishi Lumiloy® PBT+MD30% MR2000 is supplied in 25 kg moisture-barrier bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000, securely palletized, stowed, and sealed for ocean transport.
    Shipping Shipping description: Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000 is supplied as thermoplastic pellets, typically in moisture-barrier bags or octabins on pallets. Normally non-hazardous for transport; keep dry, cool, and protected from sunlight. Follow the SDS and local regulations for packaging, labeling, and handling.
    Storage Store Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, moisture, and incompatible substances. Keep containers tightly closed, protect from contamination or physical damage, and avoid dust generation and static discharge. Use first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Store dry, sealed, cool, and protected from moisture; recommended shelf life is about two years in original packaging.
    Free Quote

    Competitive Mitsubishi Engineering Plastics Lumiloy® PBT+MD30% MR2000 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Lumiloy® PBT+MD30% MR2000 identifies a mineral-reinforced polybutylene terephthalate injection-molding compound supplied by Mitsubishi Engineering Plastics. The suffix MD30 denotes a nominal mineral filler content of 30% by weight; MR2000 is the formulation and viscosity-series identifier. This grade occupies a position between unfilled PBT and glass-fiber-reinforced PBT: it is specified where reduced anisotropic shrinkage, improved flatness, and moderate mechanical stiffness are more important than tensile strength and impact resistance.

    Certificates of analysis for Lumiloy® PBT+MD30% MR2000 report the product designation, batch number, melt volume-flow rate under ISO 1133-1:2022, ash content under ISO 3451-1, tensile properties under ISO 527-1/-2, flexural properties under ISO 178, notched Izod impact under ISO 180/1A, and mold shrinkage under ISO 294-4. The material is characterized through standard test methods rather than vendor-typical values alone. Tensile properties are reported under ISO 527-1/-2; flexural properties under ISO 178; notched Izod impact under ISO 180/1A; heat deflection temperature under ISO 75-1/-2 with 1.80 MPa loading. Melt viscosity comparisons use melt volume-flow rate at 250 °C and 2.16 kg according to ISO 1133-1:2022. Mold shrinkage is evaluated on ISO 294-4 plaques. For mineral-filled PBT compounds, mold shrinkage in the flow direction commonly falls between 0.7% and 1.1%, while transverse shrinkage falls between 0.9% and 1.3%; the exact values for MR2000 must be taken from the current supplier datasheet.

    Representative comparative property ranges for unfilled PBT, mineral-filled PBT compounds, and glass-fiber-reinforced PBT compounds. Ranges are industrial reference values, not product-specific guarantees.
    Property / test condition Unfilled PBT PBT+MD30 compound PBT+GF30 compound
    Tensile strength, MPa, ISO 527-1/-2 50–60 40–55 90–120
    Tensile modulus, MPa, ISO 527-1/-2 2,500–2,800 4,000–5,500 7,000–9,000
    Flexural strength, MPa, ISO 178 80–90 80–100 150–190
    Flexural modulus, MPa, ISO 178 2,300–2,600 3,800–5,000 6,800–8,500
    Notched Izod impact, kJ/m², ISO 180/1A 3–5 3–4 8–11
    Heat deflection temperature, 1.80 MPa, ISO 75-1/-2 55–60 °C 80–100 °C 190–205 °C
    Mold shrinkage, flow / transverse, % 1.5–2.0 / 1.5–2.0 0.7–1.1 / 0.9–1.3 0.3–0.5 / 0.8–1.2

    Ash content determined by ISO 3451-1 verifies the nominal 30% filler loading, not including pigments or processing aids. The coefficient of linear thermal expansion is measured by ISO 11359-2; mineral-filled PBT displays lower transverse-to-flow anisotropy than glass-fiber-reinforced PBT, which reduces the tendency to bow after thermal cycling. Published data for Lumiloy® MR2000-specific reflectance, flammability, and long-term oxidative aging are limited and must be confirmed for the actual color, wall thickness, and additive package.

    The melt rheology of a 30% mineral-filled PBT is shear-thinning but less strongly shear-thinning than glass-fiber compounds because the particles have lower aspect ratio. Capillary rheometry at 250 °C shows that apparent melt viscosity decreases with shear rate, and the flow activation energy remains close to that of the PBT matrix. In practice, hot-runner pressure drop may be higher than unfilled PBT because of increased melt rigidity at low shear rate. Mold-filling simulations therefore need the actual filler-specific viscosity parameters and not generic PBT data. Spiral-flow tests are sometimes used on the production floor; a spiral length measured under fixed injection pressure and mold temperature provides a relative lot-to-lot flow index but is not an ISO standardized property.

    What Limits Mold Shrinkage Uniformity in MD30-Filled PBT?

    Filler aspect ratio and flow-induced orientation control shrinkage. Because mineral particles have an aspect ratio closer to unity than milled or chopped glass fibers, they do not align in the flow direction to the same extent. In a flat edge-gated plaque of 100 mm × 100 mm × 2.0 mm, unfilled PBT can develop post-mold distortion after 48 h at 23 °C due to continuing crystallization and moisture equilibration; an MD30 compound typically shows less total deviation from the cavity dimension. The improvement is conditional on gate placement, packing time, and mold wall temperature. Mold temperatures below 50 °C freeze the surface before sufficient crystallization occurs, producing late shrinkage and curl. Production tooling is therefore run at 70 °C to 100 °C for dimensionally stable flat parts.

    For parts with wall thickness below 1.0 mm, the higher melt viscosity of the mineral-filled compound reduces flow length. Mold-filling simulation should use filler-specific Cross-WLF viscosity coefficients, not unfilled PBT data. A thickness reduction from 2.0 mm to 1.0 mm can raise injection pressure demand by roughly 30% to 50%, depending on flow length and gate geometry. Hot-runner drops and sprue bushings are specified larger than in unfilled PBT to limit shear heating and pressure drop. Weld-line areas retain a lower fraction of base tensile strength because filler particles interfere with polymer interdiffusion; double-gated tensile tests under ISO 527-1/-2 commonly show weld-line strength retention of 40% to 60%. Weld lines should be placed away from load paths and, where unavoidable, moved by gate relocation or overflow wells.

    Drying, Hydrolysis, and Residence-Time Control in Production

    PBT hydrolyzes at melt temperatures if moisture is present. Pellet moisture above 0.02 wt% causes measurable loss of tensile elongation and notched impact even when visual appearance remains acceptable. Desiccant dryers with -40 °C dew point air are set to 120 °C to 130 °C for 3 h to 5 h. At relative humidity above 60%, dried pellets reabsorb surface moisture within minutes; transfer to the hopper should minimize open air exposure, and closed hopper systems with dry air purge are recommended. Over-drying above 140 °C can yellow light-colored grades and promote pellet sticking in the hopper or feed throat.

    In hot-runner molds, stagnant melt volumes expose material to high temperature. Residence times beyond 10 min at 260 °C can generate black specks, acidic odor, and surface streaks. Purging with a neutral polyolefin after shutdown reduces carbonized deposits. On the injection unit, mineral filler accelerates wear of the screw tip, check ring, and barrel; bimetallic barrels and hardened screw flights are specified for long production campaigns. A worn check ring causes shot-weight variation, weak packing, sink marks, and dimensional drift. Production lots should be logged with dryer set point, dew point, residence time, and shot weight to separate material variation from machine wear.

    When High-Speed Filling Triggers Surface Splay in Thin-Wall Sections

    Thin-wall molding with mineral-filled PBT can produce flow marks and surface splay when the melt front is too cold or when gate shear exceeds the material limit. Tunnel or edge gates below 1.2 mm diameter impose high shear heating and can cause splay in the gate area. For wall thickness between 1.5 mm and 3.0 mm, start-up conditions often use barrel temperatures from 240 °C to 270 °C from rear to nozzle, mold temperature from 70 °C to 100 °C, injection speed from 30 mm/s to 80 mm/s, and holding pressure from 40% to 60% of the peak injection pressure. These conditions require mold-flow validation because filler orientation, gate freeze time, and part geometry shift the optimum.

    Splay is not always moisture-related; it can arise from gas trapped at the flow front. Fine vents of the depth recommended for PBT by the mold steel supplier reduce burn marks and gas marks. Vacuum-assisted venting is used for deep ribs and bosses. If the material is processed at melt temperatures above 270 °C, degradation products can produce brown streaks and odor; the upper melt-temperature boundary should be confirmed from the MR2000 product datasheet. Processors using closed-loop injection speed control can monitor fill time and transfer position; a shift in fill time at constant melt temperature indicates viscosity change from regrind, moisture, or filler lot variation.

    Compared with Glass-Fiber Reinforcement, the Advantage Is Not Strength but Shape Stability

    Glass-fiber-reinforced PBT, such as a typical GF30 grade, provides tensile strength in the 90 MPa to 120 MPa range and heat deflection temperatures approaching 200 °C under 1.80 MPa. An MD30 mineral-filled PBT does not reach those strength or thermal levels; its industrial tensile strength range is commonly 40 MPa to 55 MPa, and heat deflection temperature remains below 100 °C for most mineral-filled PBT compounds. The selection of MR2000 is therefore driven by shape stability, not load-bearing performance. Glass fibers orient during flow and create a large difference between flow and transverse shrinkage; mineral filler produces a more balanced shrinkage field, reducing warpage in flat parts such as housings, covers, and bezels. The surface appearance of mineral-filled PBT is also less fiber-prominent than glass-filled grades, which matters for visible surfaces.

    Unfilled PBT remains preferable where high elongation, impact toughness, and easy flow are required. Mineral-filled PBT exhibits lower notched Izod impact and lower weld-line strength than unfilled PBT. In snap-fit designs, the strain at break of the MD30 compound may be below 5%; design calculations should use tensile elongation measured on dry-as-molded specimens under ISO 527-1/-2, not standard unfilled PBT values. For parts requiring both low warpage and higher impact, a hybrid glass-mineral system may be considered, but the dimensional stability will shift toward the glass-filled side with increasing fiber content.

    Application sectors for Lumiloy® PBT+MD30% MR2000 include electrical housings, sensor brackets, lighting bezels, and flat covers where dimensional checks after 24 h to 48 h reject warped moldings. Temperature cycling tests from -40 °C to 85 °C are used to detect residual stress and cold-temperature cracking. Post-mold annealing at 120 °C to 130 °C for 30 min to 60 min can reduce molded-in stress but may alter dimensions and must be validated before production release. Chemical exposure to hot water, steam, strong alkalis, or hot amines should be avoided unless validated under ISO 175 or the OEM fluid compatibility protocol. Compliance with RoHS 2011/65/EU and REACH 1907/2006 must be based on the supplier statement for the actual grade, color, and lot, because downstream masterbatch and regrind alter the chemical inventory. Flame-retardant performance is not inherent: a mineral-filled PBT may remain UL 94 HB unless the specific MR2000 formulation is certified to a V-class rating at the tested thickness. If the part functions as a light reflector, reflectance and color-shift data under thermal aging are required; published data for this specific configuration is limited.

    Top