Mitsubishi Engineering Plastics Lumiloy Pbt Gf15 Fr Gp1000f

Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F

    • Product Name: Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 644713
    Product Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F
    Polymer Base PBT (polybutylene terephthalate)
    Glass Fiber Content 15%
    Flame Retardancy Flame retardant
    Processing Method Injection molding
    Density Approx. 1.45-1.50 g/cm³
    Molding Shrinkage Approx. 0.3-0.6%
    Tensile Strength Approx. 95-105 MPa
    Tensile Elongation At Break Approx. 2-3%
    Flexural Modulus Approx. 5500-6000 MPa
    Notched Charpy Impact Strength Approx. 5-8 kJ/m²
    Hdt At 1 8 Mpa Approx. 190-200 °C
    Ul 94 Flammability V-0 typical, thickness dependent
    Water Absorption Approx. 0.1-0.3%

    As an accredited Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Mitsubishi Lumiloy® PBT+GF15%-FR GP1000F is supplied in 25 kg moisture-resistant bags, palletized for industrial bulk handling.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Lumiloy® PBT+GF15%-FR GP1000F in 25 kg bags on pallets, shrink-wrapped and secured inside a 20-foot FCL container.
    Shipping Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F is shipped as dry, glass-fiber-reinforced, flame-retardant PBT pellets in moisture-barrier bags, boxes, or bulk containers. Keep sealed, dry, and protected from heat and sunlight; avoid moisture during storage and handling. Use appropriate packaging to prevent contamination. Transport classification is typically non-hazardous; verify current SDS and local regulations.
    Storage Store Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep it in original sealed packaging to prevent moisture pickup and contamination. Protect from physical damage, avoid prolonged high humidity, keep containers closed and labeled, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Store dry and cool in unopened original packaging; typical shelf life is 12 months from date of manufacture.
    Free Quote

    Competitive Mitsubishi Engineering Plastics Lumiloy® PBT+GF15%-FR GP1000F prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Mitsubishi Engineering Plastics supplies Lumiloy® PBT+GF15%-FR GP1000F as a 15 wt% glass-fibre-reinforced flame-retardant polybutylene terephthalate injection-moulding compound. The grade is specified for electrical and electronic components that must retain UL 94 V-0 at wall thicknesses of 0.8 mm or lower after moulding, including connector housings, relay sockets, terminal blocks, sensor brackets, and power distribution parts. Glass fibre is dispersed as a discrete discontinuous phase; the final fibre length after plastication is typically reduced from the nominal chopped-strand length by screw shear, so moulded-part modulus is influenced by backpressure, screw speed, and gate geometry. The flame-retardant system is compounded into the melt phase and must be protected from excessive residence time at melt temperatures above 280°C. Relative to unfilled flame-retardant PBT, GP1000F increases flexural modulus and heat deflection temperature while reducing mould shrinkage; relative to 30 wt% glass-fibre PBT, the lower fibre loading reduces melt viscosity, lowers fibre-fibre contact, and produces a wider processing window for flat, thin-wall parts. Published mechanical data for this specific grade should be verified against the current Mitsubishi Engineering Plastics datasheet, because regrind level, colour concentrate addition, and drying history can shift tensile strength at break by several percentage points.

    What Property Shifts Occur Across Unfilled, 15% Glass-Fibre, and 30% Glass-Fibre Flame-Retardant PBT?

    The comparative data place GP1000F in the intermediate stiffness class. Flexural modulus of about 5,900 MPa is roughly 2.3× the modulus of unfilled flame-retardant PBT and about 60% of a typical 30 wt% glass-fibre PBT. This intermediate modulus is significant for snap-fit connector latches, because beam stiffness increases with the cube of thickness but failure risk at the root is strain-controlled. A 15 wt% fibre loading retains enough elongation to allow latch deflection without transitioning to a PBT/PC blend or a toughened polyamide grade. The heat deflection temperature of approximately 200°C under 1.8 MPa derives from fibre reinforcement rather than from the PBT melt transition alone; at this fibre mass fraction the part retains usable stiffness above the PBT glass transition, but creep under sustained clamp load remains dependent on mould temperature. Shrinkage anisotropy is lower than 30 wt% PBT because the fibre orientation tensor is less fully saturated. Flow-direction shrinkage values of 0.4–0.7% are typical for parts gated on a long edge; parts with pin-point gating into a rectangular cavity can exhibit transverse shrinkage that is 0.2–0.3% higher due to orientation effects. Unfilled flame-retardant PBT remains preferred where ductility and low notch sensitivity dominate, but it cannot match the dimensional stability and elevated-temperature stiffness of GP1000F.

    Property Lumiloy GP1000F (GF15 FR) Unfilled FR PBT PBT+GF30 FR Test method
    Density 1.56 g/cm³ 1.44 g/cm³ 1.67 g/cm³ ISO 1183
    Tensile stress at break 90 MPa 55 MPa 120 MPa ISO 527-1/-2
    Flexural strength 140 MPa 80 MPa 180 MPa ISO 178
    Flexural modulus 5,900 MPa 2,600 MPa 9,500 MPa ISO 178
    Charpy notched impact strength at 23°C 3.5 kJ/m² 3.0 kJ/m² 6.5 kJ/m² ISO 179/1eA
    Heat deflection temperature at 1.8 MPa 200°C 65°C 205°C ISO 75-1/-2
    Mould shrinkage, flow direction 0.4–0.7% 1.5–2.0% 0.2–0.5% ISO 294-4
    Water absorption at saturation 0.2% 0.1% 0.2% ISO 62

    Pre-drying is mandatory before melt processing. A desiccant hopper dryer with a dew point of -40°C or lower should be connected to the machine throat. Drying at 120°C for 4–6 h reduces residual moisture below 0.02%; higher dryer temperatures above 130°C risk oxidative yellowing of the flame-retardant package and should be avoided unless the material supplier specifically permits it. In plants where relative humidity exceeds 60% RH, hopper demand time should be limited to 30 min or less because PBT compounds re-absorb surface moisture faster than many amorphous engineering resins. Moisture-related defects in GP1000F appear as splay on flat connector faces, silver streaks along flow fronts, and reduced tensile strength at knit lines. A Karl Fischer moisture analyser is preferred over loss-on-drying for verifying 0.02% because the glass fibre and flame-retardant additives can release volatile degradation products that confound weight-loss readings.

    Barrel temperature should be profiled from rear to nozzle in the range 250–270°C. The rear zone is normally set at 240–250°C to promote early melting without overheating the feed throat; the centre and front zones are held at 250–265°C; the nozzle should be controlled between 255°C and 270°C. Melt temperatures above 280°C have been observed to produce brown streaking and black specks in flame-retardant PBT compounds due to degradation of the FR package and hydrolysis of the ester backbone. Short shots in GP1000F should not be corrected by raising melt temperature alone; increasing mould temperature or reducing screw rotation improves flow length without the same thermal-degradation risk.

    Mould temperature should be set at 60–80°C. The lower end of the range is acceptable for unfilled sections with low crystallinity demand, but thin-wall connectors with high residual stress benefit from 80°C because the slower quench increases crystalline fraction and reduces post-mould shrinkage. Mould temperatures below 50°C force the skin layer to freeze before fibre orientation relaxes and increase warpage in parts with asymmetric gate locations. A mould with differential temperature control set to 65°C on the core and 80°C on the cavity can shift warpage direction, but cavity-pressure sensors are required to separate packing effects from thermal-gradient effects.

    Screw design affects fibre length retention. A standard general-purpose screw with compression ratio 2.0–2.5:1 and flight depth ratio 1.8–2.2:1 is usually acceptable for 15 wt% glass fibre, but excessive screw recovery speed above 0.8 m/s can break fibre bundles and depress modulus. Backpressure should be set between 2–5 bar hydraulic to maintain melt homogeneity without generating frictional heat. Total melt residence time should be kept below 8–10 min at 260°C; longer residence times produce viscosity drift and can shift UL 94 V-0 performance on thin sections. When interruptions exceed 10 min, the barrel should be lowered to 220°C and the screw rotated intermittently.

    When Relay and Connector Housings Are Converted from Polyamide 66 to GP1000F

    Relay sockets and board-to-board connectors moulded in polyamide 66 often display dry-as-moulded stiffness and terminal retention that change after exposure to humid air because polyamide absorbs moisture. At equilibrium in 50% RH, polyamide 66 can absorb approximately 2.5% moisture, whereas PBT+GF15%-FR GP1000F saturates below 0.2% under comparable conditions. This difference reduces the seasonal shift in terminal insertion force and contact normal force in electrical connectors. The conversion is not neutral in tooling: PBT weld lines are commonly weaker than the surrounding matrix, and a gate location that was acceptable for polyamide 66 may leave a knit line through a latch boss or terminal retention feature. The relative reduction in knit-line strength is more severe in glass-reinforced PBT than in unreinforced polyamide 66 because fibres do not bridge the weld plane effectively. Moulders should relocate gates or add overflow tabs to move the weld line into a non-critical web. Mould shrinkage values of 0.4–0.7% in the flow direction are close to polyamide 66 GF15 values, so cavity dimensions can often be modified by spot polishing or insert adjustment rather than full tool replacement. However, PBT has a sharper crystallisation profile and a shorter packing window than polyamide 66; holding-pressure decay must be retimed to avoid gate freeze before pack-out. Failure to retime the hold profile commonly produces sink marks on boss backs and dimensional variation in terminal pitch.

    Electrical performance during conversion should be checked by terminal retention testing rather than by visual comparison. PBT+GF15%-FR can provide sufficient stiffness for terminal retention, but lower elongation can cause cracking if the terminal is inserted into a blind hole with interference above the material yield strain. The supplier processing guide for GP1000F should be consulted for minimum hole-to-terminal interference and for weld-line placement in thin-wall grid arrays.

    Compliance documentation for GP1000F covers flammability, glow-wire, tracking, and restricted-substance directives. The UL Yellow Card should be consulted for the minimum thickness and colour-specific rating; UL 94 V-0 is typically listed at 0.8 mm. Glow-wire testing to IEC 60695-2-12 and IEC 60695-2-13 is end-product dependent because flame spread is influenced by part shape, wall thickness, and nearby metal terminals. The compound is normally available with documentation for RoHS recast Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006. Moulders should request lot-specific test certificates for the actual colour and regrind content, because colourant packages can influence comparative tracking index and glow-wire ignition temperature.

    Criterion Designation or code Relevant condition
    Flammability UL 94 V-0 minimum thickness per UL Yellow Card, typically 0.8 mm
    Comparative tracking index IEC 60112 typically 250 V for natural or black grades
    Glow-wire ignition temperature IEC 60695-2-12 end-product evaluation required
    Glow-wire flammability index IEC 60695-2-13 end-product evaluation required
    RoHS 2011/65/EU supplier declaration required for specific colour
    REACH Regulation (EC) No 1907/2006 SVHC declaration required for specific colour

    Gate Freeze Time, Flow-Length Ratio, and Clamp Force Requirements

    Flow length in glass-filled PBT is controlled by fibre alignment and the freezing behaviour of the outer layers. Spiral flow data for GP1000F are often generated on a specific cavity thickness and melt temperature; published data for this specific configuration is limited, so production estimates should be derived from in-house spiral-flow or pressure-drop measurements on the intended tool rather than extrapolated from unfilled PBT. At a wall thickness of 0.8 mm, peak cavity pressure in thin connector housings can exceed 60 MPa; clamp force should be calculated from projected area and simulated cavity-pressure distribution, with a safety factor of 1.2–1.5× against flash at the parting line. Gate freeze time in PBT is short. Edge gates or tab gates below 0.8 mm thickness can freeze before packing is complete and generate sink marks on opposing bosses. Submarine gates for 15 wt% glass fibre should not be smaller than 1.0 mm diameter and should include a generous land length to prevent fibre jamming at the gate insert. Hot-runner systems should use externally heated tips with positive shut-off; internal-heated torpedo tips create a cold boundary layer that increases pressure drop and accumulates glass fibre, causing gradual gate blockage over long runs.

    The PBT matrix in GP1000F retains the chemical resistance of unfilled PBT to aliphatic hydrocarbons, mineral oils, and many automotive fluids at moderate temperature. It is not suitable for continuous contact with strong alkaline solutions, concentrated acids at elevated temperature, or pressurised hot water above 60°C because ester hydrolysis accelerates. The flame-retardant package may also be sensitive to strongly basic melt additives; amine-based mould release agents and certain amine-containing colorants should be avoided in regrind handling because they can catalyse degradation at barrel temperatures above 250°C. Welding operations such as ultrasonic, laser, and hot-plate welding must be validated on batches containing regrind, because the FR package and glass-fibre length distribution influence weld-line melt behaviour and joint strength.

    Top