    Specifications
    HS Code 847151
    Manufacturer Mitsubishi Engineering Plastics
    Product Name Lumiloy® PBT Alloy AP-2110
    Material Type PBT alloy
    Density 1.22 g/cm³
    Molding Shrinkage 0.5–0.7 %
    Water Absorption 0.08 %
    Tensile Strength 55 MPa
    Tensile Elongation At Break 50 %
    Flexural Modulus 2200 MPa
    Flexural Strength 85 MPa
    Charpy Notched Impact Strength 10 kJ/m²
    Hdt At 1 82 Mpa 90 °C
    Vicat Softening Temperature 120 °C
    Volume Resistivity >1E16 ohm·cm
    Dielectric Strength 20 kV/mm
    Flammability UL94 HB

    As an accredited Mitsubishi Engineering Plastics Lumiloy® PBT Alloy AP-2110 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant bags, palletized for shipment; bulk 500 kg bags may be available.
    Container Loading (20′ FCL) 20′ FCL container loaded with securely palletized, shrink-wrapped Mitsubishi Engineering Plastics Lumiloy® PBT Alloy AP-2110, safely stowed for ocean transport.
    Shipping Lumiloy® PBT Alloy AP-2110 is typically shipped as nonhazardous plastic resin pellets in moisture-barrier bags or bulk containers. Store in a cool, dry area away from direct sunlight and heat. Use standard freight; follow SDS and local regulations for handling and transport.
    Storage Store Lumiloy® PBT Alloy AP-2110 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, open flames, and moisture. Keep containers closed and undamaged; prevent exposure to humid air and strong oxidizers. Protect from physical damage and incompatible chemicals. Use first-in, first-out inventory practices, avoid excessive stacking, and follow the supplier’s SDS and local regulations.
    Shelf Life Typically 24 months in dry, cool storage in sealed original packaging; verify against manufacturer’s lot date and handling guidance.
    Free Quote

    Competitive Mitsubishi Engineering Plastics Lumiloy® PBT Alloy AP-2110 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The Mitsubishi Engineering Plastics Lumiloy® AP-2110 product designation identifies a PBT-based alloy supplied as ready-to-mold pellets for injection moulding applications where unfilled PBT homopolymer is limited by notch sensitivity, low-temperature brittleness, or post-moulding shrinkage anisotropy. The AP-2110 grade identifier places the formulation within the Lumiloy alloy series and does not carry a glass-fibre or mineral-filler code, indicating that the grade is not specified as a reinforced compound. Lot-specific certificates of analysis remain the authoritative source for numerical property limits; the following content describes the processing, comparative positioning, and verification logic for this PBT alloy class.

    How Does the Processing Window of Lumiloy AP-2110 Constrain Tooling and Drying Conditions?

    Before first melt processing, the feedstock is dried in a desiccant-bed dryer capable of holding the inlet air dew point below -30 °C. Production-scale experience with PBT alloy grades analogous to Lumiloy AP-2110 shows that moisture entering the barrel hydrolyses polyester linkages and produces splay, gate smear, and weak weld lines. The practical drying condition is 120 °C for 4 h to 6 h, with residual moisture controlled below 0.02 %. These values are class-representative; if the AP-2110 lot card carries a tighter specification, the lot card governs.

    Barrel temperature profiles are selected to keep the melt temperature between 240 °C and 260 °C. Screw recovery and cushion settings should limit total melt residence time to 5 min to 8 min. At melt temperatures above 280 °C, PBT-rich polyester sequences can undergo thermal and hydrolytic chain scission, observed as a drift in melt viscosity and reduced notched impact toughness. On hot-runner systems with dead spots or unnecessarily long manifolds, residence time should be verified with a purge study rather than assumed from screw capacity.

    Mould surface temperature is maintained between 60 °C and 90 °C for unfilled PBT alloy grades. Surface temperatures below 60 °C may quench the melt into low-crystallinity skin layers, increasing post-moulding dimensional variation and reducing chemical resistance. Temperature uniformity across the cavity, measured with a surface probe rather than the controller display, is more important than the setpoint itself when wall thickness varies by more than 1 mm.

    Across multicavity tools, gate dimensions and melt temperature interact with the pseudoplastic viscosity of the alloy. A worn non-return valve increases shot-to-shot variation more noticeably in unfilled alloys than in glass-fibre-reinforced grades because the melt is more compressible and less abrasive. Production injection moulding machines with electric screw drives and active cushion control should maintain a cushion between 2 mm and 5 mm; drift beyond that range is a diagnostic signal for viscosity instability, moisture re-absorption, or check-ring leakage.

    Injection Moulding Trials Quantify the Cost of Hydrolytic Degradation

    PBT ester bonds are cleaved by water at processing temperatures. The resulting molecular weight reduction is measurable as an increase in melt volume-flow rate under ISO 1133-1:2022 and a decline in notched Charpy impact under ISO 179-1/1eA. In production data from PBT alloy feedstock, undried resin can lose a substantial fraction of dry-as-molded impact toughness before tensile strength falls below specification. The relationship is not linear: a residual moisture change from 0.02 % to 0.08 % may produce only a modest tensile change while disproportionately reducing ductility. Published data for AP-2110 specifically is limited; the trend is well documented for PBT and PBT blend systems.

    Drying hoppers with insufficient airflow or poorly maintained desiccant beds are a common root cause of intermittent splay on otherwise stable tools. The dryer should be specified for the polymer throughput, and return-air monitoring should confirm that the bed regenerates to a dew point below -30 °C. If the surrounding plant floor exceeds 60 % relative humidity, hopper throat purging with dry air or nitrogen reduces re-absorption before the feed zone.

    Melt degradation is not limited to moisture. Long residence time at 260 °C or above can promote ester-exchange reactions and colour shift. The recommended response is to reduce the barrel capacity utilisation, lower the back pressure, or increase shot frequency so that material does not remain stagnant in front of the screw. These measures are more effective than raising barrel temperature to lower viscosity, which accelerates degradation.

    Test methodology matrix applicable to lot verification of Lumiloy AP-2110
    Property or characteristicStandard designation and specimen condition note
    Melt volume-flow rateISO 1133-1:2022; nominal condition printed on lot certificate
    Tensile modulus and strengthISO 527-1/-2; Type 1A specimen, 23 °C
    Flexural modulusISO 178; 23 °C
    Notched Charpy impactISO 179-1/1eA; edgewise notch, 23 °C
    Heat deflection temperatureISO 75-2/B; 0.45 MPa, flatwise
    DensityISO 1183-1
    Mould shrinkage parallel and normalISO 294-4; plaque 60 mm × 60 mm × 2 mm

    Within this matrix, the certificate of analysis supplies the numerical values. Because AP-2110 is an alloy, the verification programme may be supplemented by notched Izod impact under ISO 180/1A and Vicat softening temperature under ISO 306/B50 when design requirements demand short-term impact or thermal data. Published data for this specific configuration is limited in the present document, so prototype evaluation on the production tool is mandatory for safety-relevant dimensions.

    When a PBT Alloy Replaces Glass-Filled PBT in Thin-Wall Enclosures

    In thin-wall electronic housings and connector bodies, glass-fibre-reinforced PBT provides high stiffness but introduces anisotropic shrinkage, fibre prominence on matte surfaces, and weld-line weakness. Lumiloy AP-2110 may be selected because the grade identifier does not indicate fibrous reinforcement. The absence of glass reduces directional fibre orientation, but the part design must accept lower flexural modulus and higher thermal expansion than a filled grade. A design change from 30 wt% glass-filled PBT to an unfilled PBT alloy requires revised gate placement and rib-to-wall ratio because the alloy will shrink more and provide less creep resistance.

    Thin-wall sections below 1.5 mm require fast filling and adequate venting. In an unfilled PBT alloy, viscosity at the recommended melt temperature is often high enough to produce gas accumulation at the end-of-fill if vent depth is insufficient. Production tools designed for filled PBT may need additional parting-line vents and wider gates. No AP-2110 modulus value is asserted here; ISO 527-1/-2 tensile modulus and ISO 178 flexural modulus values on the MEP data sheet should be used in simulation databases.

    Snap-fit arms, bosses, and screw bosses should be redesigned to account for the lower weld-line strength of unfilled alloy flow fronts. In a multicavity tool with a cold runner, weld lines are moved away from snap-fit roots by sequential valve-gating or by changing gate location. If moving the weld line is not possible, weld-line specimens prepared from the production tool are tested under ISO 179-1/1eA or ISO 527-1/-2 to establish a design allowable.

    Comparative Performance Boundaries Against Homopolymer PBT and Other Lumiloy Grades

    Compared with unfilled PBT homopolymer, the alloying modification in Lumiloy AP-2110 is typically used to reduce notch sensitivity and improve low-temperature ductility. The secondary polymer phase disrupts large spherulite formation, which can lower shrinkage anisotropy and reduce warpage in flat parts. The trade-off is usually a reduction in solvent resistance and heat deflection compared with pure PBT. For applications requiring maximum crystallinity, flow, or chemical resistance, a homopolymer PBT grade may be more appropriate; for applications balancing impact and dimensional stability, the alloy class is evaluated.

    Compared with other Lumiloy grades, AP-2110 represents one position in the alloy family. The letter and number suffix does not signal a filled system, but it may distinguish flow, impact, or stabilisation packages among available alloys. Selection between AP grades is made from the MEP data sheet curve set, not from the grade code alone. Where electrical tracking resistance or low-smoke behaviour is required, the specific grade must be verified under IEC 60112 or IEC 60695-11-10 because published data for AP-2110 is limited in this document.

    Chemical exposure limits are governed by the ester linkage. Applications involving prolonged contact with hot water above 60 °C, strong acids, strong bases, or amine-containing agents are generally avoided. Intermittent contact with automotive fuels, engine oils, and many neutral solvents is acceptable for PBT alloy class materials, but the alloy phase may modify solvent resistance relative to homopolymer PBT. Candidate fluids should be evaluated by immersion testing according to ISO 175 before specification. Compounding with amine-based additives should be avoided unless pre-tested, because aminolysis of ester bonds can occur under melt-processing conditions.

    Because PBT alloy components are frequently selected for snap-fit features in automotive interior trim and electrical enclosures, the local weld-line region is often the limiting design location. In a multicavity production tool, the first injection trial should deliberately produce short shots from each gate and then sacrifice parts cut along the suspected weld line. This approach identifies whether the main strength loss occurs at the weld line or at a stress concentration such as a boss root. For AP-2110, published data for this specific configuration is limited, so the production tool trial is the only reliable basis for setting clamp force, boost time, and switch-over position.

    Compliance with regulatory requirements is established through lot-level certification rather than grade-family assumptions. The applicable framework includes 2011/65/EU as amended by (EU) 2015/863 for RoHS-restricted substances, and EC 1907/2006 for REACH SVHC communication. A UL Yellow Card may exist only for selected grades; no AP-2110 flammability classification is asserted here. When a customer-specific substance list applies, the supplier control document should be referenced before production release.

    Top